At least 235 records · Page 13

Optimizing feed modulation for coupled methane and NO x conversion over Pd-Pt/Mn 0.5 Fe 2.5 O 4 /Al 2 O 3 monolith catalyst

Here the impacts of feed modulation (frequency, amplitude) and catalyst design (composition and architecture) parameters are reported for the conversion of methane and NO x over a dual-layer Pt+Pd/Al 2 O 3 + Mn 0.5 Fe 2.5 O 4 /Al 2 O 3 monolith. CH 4 and NO x conversion data show that the dual-layer catalyst outperforms single-layer samples having the same catalyst loadings, with and without spinel. Close proximity of the PGM and MFO functions in the mixed-layer catalyst lowers the CH 4 conversion at high temperature while separating the PGM and spinel layers with an intermediate Al 2 O 3 layer does not. Methane conversion enhancement is linked to its nonmonotonic dependence on O 2 . The performance gains are tied to a transient activity spike that occurs during the lean-to-rich feed transition when water is present in the feed. The transient spike is attributed to the removal of CO and H 2 products via reactions with stored O 2 in the spinel, eliminating inhibition of methane steam reforming.

03 NATURAL GAS↗

Influence of Pt-Metal Alloy Catalysts with Various Ionomers on Oxygen Reduction Reaction in Fuel Cell Application

Pt-M/C (M = Co, Ni, Mn, etc.) alloy catalysts exhibit superior oxygen reduction reaction (ORR) activity compared to pure Pt/C, leading to a high energy efficiency in hydrogen fuel cells. However, many Pt-M/C alloy catalysts were synthesized and evaluated at the lab scale in model test-bed systems like rotating disc electrodes, which don't always correlate to performance within a fuel cell system; there is a clear need to evaluate catalysts in electrodes that can be prepared at industrially relevant scales to evaluate how factors like ink formulation can greatly affect device-level of fuel cell performance. Herein, three commercial Pt-M/C alloy catalysts (two Pt-Co/C and one Pt-Ni/C) were comprehensively characterized by various techniques. The results show that the average particle sizes of the three catalysts are close to 5 nm; the atomic ratio of Pt/M is around 4; and the M was successfully embedded into Pt lattice, resulting in the positive shift of Pt 4f in XPS spectra and XRD patterns. These catalytic materials were incorporated into 9 different cathode catalyst layers (CCLs) with three kinds of ionomers (Nafion D2020, high oxygen permeability ionomer (HOPI), and Aquivion D79-25BS), and their performance in proton exchange membrane fuel cells (PEMFCs) were investigated. The results demonstrate that the Pt-Co/C catalysts possess a higher mass activity (MA) than Pt-Ni/C; the cathodes with Nafion ionomer provide the highest MA while electrodes with Aquivion ionomer showed the lowest activity, attributed to poor H+ conductivity resulting from suboptimal ionomer incorporation. Finally, these alloys were shown to exceed DOE targets for MA and H2/Air performance reported in the recent publications at beginning of life and after 90k cycle catalyst AST protocol. This study provides valuable performance benchmarks for these materials guiding future Pt-M/C catalyst design and material integration for heavy duty PEMFC applications.

08 HYDROGEN↗

Modeling gas-diffusion electrodes for CO 2 reduction

CO 2 reduction conducted in electrochemical cells with planar electrodes immersed in an aqueous electrolyte is severely limited by mass transport across the hydrodynamic boundary layer. This limitation can be minimized by use of vapor-fed, gas-diffusion electrodes (GDEs), enabling current densities that are almost two orders of magnitude greater at the same applied cathode overpotential than what is achievable with planar electrodes in an aqueous electrolyte. The addition of porous cathode layers, however, introduces a number of parameters that need to be tuned in order to optimize the performance of the GDE cell. In this study, we develop a multiphysics model for gas diffusion electrodes for CO 2 reduction and used it to investigate the interplay between species transport and electrochemical reaction kinetics. The model demonstrates how the local environment near the catalyst layer, which is a function of the operating conditions, affects cell performance. Finally, we also examine the effects of catalyst layer hydrophobicity, loading, porosity, and electrolyte flowrate to help guide experimental design of vapor-fed CO 2 reduction cells.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

3D Analysis of Fuel Cell Electrocatalyst Degradation on Alternate Carbon Supports

Understanding the mechanisms associated with Pt/C electrocatalyst degradation in proton exchange membrane fuel cell (PEMFC) cathodes is critical for the future development of higher-performing materials; however, there is a lack of information regarding Pt coarsening under PEMFC operating conditions within the cathode catalyst layer. We report a direct and quantitative 3D study of Pt dispersions on carbon supports (high surface area carbon (HSAC), Vulcan XC-72, and graphitized carbon) with varied surface areas, graphitic character, and Pt loadings ranging from 5 to 40 wt %. This is accomplished both before and after catalyst-cycling accelerated stress tests (ASTs) through observations of the cathode catalyst layer of membrane electrode assemblies. Electron tomography results show Pt nanoparticle agglomeration occurs predominantly at junctions and edges of aggregated graphitized carbon particles, leading to poor Pt dispersion in the as-prepared catalysts and increased coalescence during ASTs. Tomographic reconstructions of Pt/HSAC show much better initial Pt dispersions, less agglomeration, and less coarsening during ASTs in the cathode. However, a large loss of the electrochemically active surface area (ECSA) is still observed and is attributed to accelerated Pt dissolution and nanoparticle coalescence. Moreover, a strong correlation between Pt particle/agglomerate size and measured ECSA is established and is proposed as a more useful metric than average crystallite size in predicting degradation behavior across different catalyst systems.

36 MATERIALS SCIENCE↗

Degradation of Ionic Pathway in PEM Fuel Cell Cathode

The degradation of the ionic pathway throughout the catalyst layer in proton exchange membrane fuel cells was studied under an accelerated stress test of catalyst support (potential hold at 1.2 V). Electrochemical behaviors of the cathode based on graphitic mesoporous carbon supported Pt catalyst were examined using electrochemical impedance spectroscopy and cyclic voltammetry. Impedance data were plotted and expressed in the complex capacitance form to determine useful parameters in the transmission line model: the double-layer capacitance, peak frequency, and ionic resistance. Electrochemical surface area and hydrogen crossover current through the membrane were estimated from cyclic voltammogram, while cathode Faradaic resistance was compared with ionic resistance as a function of test time. It was observed that during an accelerated stress test of catalyst support, graphitic mesoporous carbon becomes hydrophilic which increases interfacial area between the ionomer and the catalyst up to 100 h. However, the ionic resistance in the catalyst layer drastically increases after 100 h with further carbon support oxidation. The underlying mechanism has been studied and it was found that significant degradation of ionic pathway throughout the catalyst layer due to catalyst support corrosion induces uneven hydration and mechanical stress in the ionomer.

08 HYDROGEN↗

Durability of Polymer Electrolyte Membrane Fuel Cells Operated at Subfreezing Temperatures

The structure, composition, and interfaces of membrane electrode assemblies (MEA) and gas-diffusion layers (GDLs) have a significant effect on the performance of single-proton-exchange-membrane (PEM) fuel cells operated isothermally at subfreezing temperatures. During isothermal constant-current operation at subfreezing temperatures, water forming at the cathode initially hydrates the membrane, then forms ice in the catalyst layer and/or GDL. This ice formation results in a gradual decay in voltage. High-frequency resistance initially decreases due to an increase in membrane water content and then increases over time as the contact resistance increases. The water/ice holding capacity of a fuel cell decreases with decreasing subfreezing temperature (-10°C vs. -20°C vs. -30°C) and increasing current density (0.02 A cm -2 vs. 0.04 A cm -2 ). Ice formation monitored using in-situ high-resolution neutron radiography indicated that the ice was concentrated near the cathode catalyst layer at low operating temperatures (≈-20°C) and high current densities (0.04 A cm -2 ). Significant ice formation was also observed in the GDLs at higher subfreezing temperatures (≈-10°C) and lower current densities (0.02 A cm -2 ). These results are in good agreement with the long-term durability observations that show more severe degradation at lower temperatures (-20°C and -30°C).

30 DIRECT ENERGY CONVERSION↗

Polarization loss correction derived from hydrogen local-resistance measurement in low Pt-loaded polymer-electrolyte fuel cells

The reduction of platinum-loading on the cathode side of polymer-electrolyte fuel cells leads to a poorly understood increase in mass-transport resistance (MTR) at high current densities. This local resistance was measured using a facile hydrogen-pump technique with dilute active gases for membrane-electrode assemblies with catalyst layers of varying platinum-loading (0.03-0.40 mgPt/cm²). Furthermore, polarization curves in H 2 /air were measured and corrected for the overpotential caused by the increased MTR for low loadings on the air side due to the reduced concentration of reactant gas at the catalyst surface. The difference in performance after correction for all resistances including the MTR is minor, suggesting its origin to be diffusive in nature, and proving the meaningfulness of the facile hydrogen-pump technique for the characterization of the cathode catalyst layer under defined operation conditions.

30 DIRECT ENERGY CONVERSION↗

Direct Simulations of Coupled Transport and Reaction on Nano-Scale X-Ray Computed Tomography Images of Platinum Group Metal-Free Catalyst Cathodes

The nano/micro-scale geometry of polymer electrolyte fuel cell (PEFC) catalyst layers critically affects cell performance. The small length scales and complex structure of these composite layers make it challenging to analyze cell performance and physics at the particle scale by experiment. We present a computational method to simulate transport and chemical reaction phenomena at the pore/particle-scale and apply it to a PEFC cathode with platinum group metal free (PGM-free) catalyst. Here, we numerically solve the governing equations for the physics with heterogeneous oxygen diffusion coefficient and proton conductivity evaluated using the actual electrode structure and ionomer distribution obtained using nano-scale resolution X-ray computed tomography (nano-CT). Using this approach, the oxygen concentration and electrolyte potential distributions imposed by the oxygen reduction reaction are solved and the impact of the catalyst layer structure on performance is evaluated.

36 MATERIALS SCIENCE↗

Water transport during startup and shutdown of polymer electrolyte fuel cell stacks.

A dynamic three-phase transport model is developed to analyze water uptake and transport in the membrane and catalyst layers of polymer electrolyte fuel cells during startup from subfreezing temperatures and subsequent shutdown. The initial membrane water content (?, the number of water molecules per sulfonic acid site) is found to be an important parameter that determines whether a successful unassisted self-start is possible. For a given initial subfreezing temperature at startup, there is a critical ? (?h), above which self-start is not possible because the product water completely engulfs the catalyst layers with ice before the stack can warm-up to 0 C. There is a second value of ? (?l), below which the stack can be self-started without forming ice. Between ?l and ?h, the stack can be self-started, but with intermediate formation of ice that melts as the stack warms up to 0 C. Both ?l and ?h are functions of the initial stack temperature, cell voltage at startup, membrane thickness, catalyst loading, and stack heat capacity. If the stack is purged during the previous shutdown by flowing air in the cathode passages, then depending on the initial amount of water in the membrane and gas diffusion layers and the initial stack temperature, it may not be possible to dry the membrane to the critical ? for a subsequent successful startup. There is an optimum ? for robust and rapid startup and shutdown. Startup and shutdown time and energy may be unacceptable if the ? is much less than the optimum. Conversely, a robust startup from subfreezing temperatures cannot be assured if the ? is much higher than this optimum.

30 DIRECT ENERGY CONVERSION↗

Regulating catalyst and ionomer interactions to promote oxygen transport in fuel cells

The cost of proton exchange membrane fuel cells (PEMFCs) has been a major impediment to their widespread commercialization. Reducing platinum (Pt) usage in PEMFC represents an essential step in lowering the cost. However, decreasing Pt loading in the cathode catalyst layer (CCL) often leads to a significant increase in the local oxygen transport resistance (R Local ), which not only slows the oxygen reduction reaction but also causes a higher polarization overpotential. The poisoning of Pt by perfluorosulfonic acid ionomers also becomes more predominant at low Pt loadings. Therefore, regulating catalyst and ionomer interactions by optimizing their interface in the CCL is crucial to improving PEMFC performance. Here, in this review, the strategies of improving oxygen transport by controlling Pt-ionomer interactions and interfaces through catalyst design, ionomer structure, and incorporation of additives are summarized. Finally, perspectives on future optimization of catalyst and ionomer interactions are proposed.

25 ENERGY STORAGE↗

Oxygen Reduction on Platinum-Nickel and Platinum-Cobalt Alloy Based Catalysts for High Temperature Proton Exchange Membrane Fuel Cells

Catalyst layers, with commercial PtNi/TKK (TECNiE52; platinum 46.5 wt%), PtCo/TKK (TEC36E52; platinum 45.8 wt%) catalysts, and an in-house catalyst PtNi-NC (platinum 38.4 wt%), synthesised using acoustic mixer and a tube furnace, are prepared using three different ionomers: 20 wt% Nafion®, 60 wt% polytetrafluoroethylene (PTFE), and an in-house 5 wt% ionomer (‘Ionomer X’). These inks are bar-coated onto carbon paper gas diffusion layers (GDLs), which are cut into 3 cm × 5 cm pieces. The coated layers are tested for oxygen reduction in a commercial gas diffusion electrode (GDE) test cell, FlexCell® (Gaskatel GmbH, Germany), using 85 wt% phosphoric acid at both room temperature and at 155°C. This study evaluates the polynorbornene (PNB)-based in-house ionomer performance as binder and in-house catalyst oxygen reduction reaction (ORR) activity in comparison to commercial products. The catalyst layers are characterised using X-ray diffraction (XRD) analysis, X-ray photoelectron spectroscopy (XPS), and high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM). Among the catalyst layers prepared with PTFE ionomer and tested at 155°C, the in-house catalyst demonstrates the highest ORR activity. Ionomer X proves to be a good candidate to be used as a per- and polyfluoroalkyl-free binder for high-temperature (HT) proton exchange membrane fuel cell (PEMFC) applications.

85 wt% phosphoric acid↗

Application of a temporal multiscale method for efficient simulation of degradation in PEM Water Electrolysis under dynamic operating conditions

Hydrogen is emerging as a vital energy carrier, driven by the need to reduce carbon emissions. Proton Electrolyte Membrane Water Electrolysis (PEMWE) enables hydrogen production under fluctuating renewable power conditions but requires improved understanding and stability of the anode catalyst layer under dynamic operating conditions, especially with low noble metal loadings. Long-term degradation experiments are both time-consuming and costly; therefore, a systematic, model-aided approach is essential. In the present work, a temporal multiscale method is applied to reduce the computational effort of simulating long-term degradation processes in PEMWE, with an exemplary focus on catalyst dissolution. A mechanistic model incorporating the oxygen evolution reaction, catalyst dissolution, and hydrogen permeation from the cathode to the anode was hypothesized and implemented. In this way, the local periodicity of transport and reaction processes in dynamic PEMWE operation, which influence the gradual degradation of the catalyst layer, is captured. The temporal multiscale method significantly reduces the computational effort of simulation, decreasing processing time from hours to mere minutes. This efficiency gain is attributed to the limited evolution of Slow-Scale variables during each period of time P of the Fast-Scale variables. Consequently, simulation is required only until local periodicity is achieved within each Slow-Scale time step. Hence, the fully resolved dynamic problem is decoupled into these two scales, employing a heterogeneous multiscale technique. The developed approach effectively accelerates parameter estimation and predictive simulations, supporting systematic modeling of PEMWE degradation under dynamic conditions.

08 HYDROGEN↗

Molybdenum Disulfide as a Protection Layer and Catalyst for Gallium Indium Phosphide Solar Water Splitting Photocathodes

Gallium indium phosphide (GaInP2) is a semiconductor with promising optical and electronic properties for solar water splitting, but its surface stability is problematic as it undergoes significant chemical and electrochemical corrosion in aqueous electrolytes. Molybdenum disulfide (MoS2) nanomaterials are promising to both protect GaInP2 and to improve catalysis since MoS2 is resistant to corrosion and also possesses high activity for the hydrogen evolution reaction (HER). In this work, we demonstrate that GaInP2 photocathodes coated with thin MoS2 surface protecting layers exhibit excellent activity and stability for solar hydrogen production, with no loss in performance (photocurrent onset potential, fill factor, and light limited current density) after 60 hours of operation. This represents a five-hundred fold increase in stability compared to bare p-GaInP2 samples tested in identical conditions.

14 SOLAR ENERGY↗

Ice formation in PEM fuel cells operated isothermally at sub-freezing temperatures

The effect of MEA and GDL structure and composition on the performance of single-PEM fuel cells operated isothermally at subfreezing temperatures is presented. The cell performance and durability are not only dependent on the MEA/GDL materials used but also on their interfaces. When a cell is operated isothermally at sub-freezing temperatures in constant current mode, the water formation due to the current density initially hydrates the membrane/ionomer and then forms ice in the catalyst layer/GDL. An increase in high frequency resistance was also observed in certain MEAs where there is a possibility of ice formation between the catalyst layer and GDL leading to a loss in contact area. The total water/ice holding capacity for any MEA was lower at lower temperatures and higher current densities. The durability of MEAs subjected to multiple isothermal starts was better for LANL prepared MEAs as compared to commercial MEAs, and cloth GDLs when compared to paper GDLs. The ice formation was monitored using high-resolution neutron radiography and was found to be concentrated near the cathode catalyst layer. However, there was significant ice formation in the GDLs especially at the higher temperature ({approx} -10 C) and lower current density (0.02 A/cm{sup 2}) operations. These results are consistent with the longer-term durability observations that show more severe degradation at the lower temperatures.

36 MATERIALS SCIENCE↗

High resolution neutron imaging of water in the polymer electrolyte membrane

To achieve a deeper understanding of water transport and performance issues associated with water management, we have conducted in situ water examinations to help understand the effects of components and operation. High Frequency Resistance (HFR), AC Impedance and neutron radiography were used to measure water content in operating fuel cells under various operating conditions. Variables examined include: sub-freezing conditions, inlet relative humidities, cell temperature, current density and response transients, different flow field orientations and different component materials (membranes, GDLs and MEAs). Quantification of the water within the membrane was made by neutron radiography after equilibration to different humidified gases, during fuel cell operation and in hydrogen pump mode. The water content was evaluated in bare Nafion{reg_sign} membranes as well as in MEAs operated in both fuel cell and H{sub 2} pump mode. These in situ imaging results allow measurement of the water content and gradients in the PEFC membrane and relate the membrane water transport characteristics to the fuel cell operation and performance under disparate materials and operational combinations. Flow geometry makes a large impact on MEA water content. Higher membrane water with counter flow was measured compared with co-flow for sub-saturated inlet RH's. This correlates to lower HFR and higher performance compared with co-flow. Higher anode stoichiometry helps remove water which accumulates in the anode channels and GDL material. Cell orientation was measured to affect both the water content and cell performance. While membrane water content was measured to be similar regardless of orientation, cells with the cathode on top show flooding and loss of performance compared with similarly operated cells with the anode on top. Transient fuel cell current measurements show a large degree of hysteresis in terms of membrane hydration as measured by HFR. Current step transients from 0.01 A cm{sup -2} to 0.68 A cm{sup -2} consistently show PEM wetting occurring within 5 to 20 sec. Whereas the PEM drying response to the reverse step transient of 0.68 A cm{sup -2} to 0.01 A cm{sup -2}, takes several minutes. The observed faster wetting response is due to reaction water being produced in the cathode and back diffusing into the membrane. The slower PEM drying is due to the water slowly being removed out of the wetted GDLs. This rate of removal of water and hence the PEM hydration level was found to be influenced strongly by the PTFE loadings in the GDL substrate and Microporous layer (MPL). The drying of the membrane is influenced by both the anode and cathode GDL PTFE loadings. Lower PTFE loading in the anode GDL leads to better membrane hydration probably due to the easier incorporation of water from the anode GDL into the membrane. Similarly a lower PTFE loading in the cathode GDL also results in better membrane hydration probably due to the better water retention properties (less hydrophobic) of this GDL. Fuel cells operated isothermal at sub-freezing temperatures show gradual cell performance decay over time and eventually drops to zero. AC impedance analysis indicates that losses are initially due to increasing charge transfer resistance. After time, the rate of decay accelerates rapidly due to mass transport limitations. High frequency resistance also increases over time and is a function of the initial membrane water content. These results indicate that catalyst layer ice formation is influenced strongly by the MEA and is responsible for the long-term degradation of fuel cells operated at sub-freezing temperatures. Water distribution measurements indicate that ice may be fonning mainly in the GDLs at -10 C but are concentrated in the catalyst layer at -20 C.

08 HYDROGEN↗

Intermediate Sr 2 Co 1.5 Fe 0.5 O 6-δ Tetragonal Structure between Perovskite and Brownmillerite as a Model Catalyst with Layered Oxygen Deficiency for Enhanced Electrochemical Water Oxidation

The generation of hydrogen in an environmentally benign way is highly essential to meet future energy demands. However, in the process of splitting water electrochemically, sluggish kinetics of the oxygen evolution reaction (OER) curtails its applicability, as it drags energy input. Herein, we synthesized SrCo-Fe-O oxides to optimize their OER activity by varying the Co/Fe ratio. Among them, Sr 2 Co 1.5 Fe 0.5 O 6-δ exhibited the best OER catalytic activity in the series, with an overpotential of 318 mV at 10 mA cm -2 and Tafel slope of 44.8 mV dec -1 . High-resolution neutron powder diffraction analysis identified an intermediate structure between the perovskite and brownmillerite, with alternating layers of disorderly orientated oxygen-deficient tetrahedra and fully stoichiometric octahedra. The unique stacking of tetrahedral and octahedral units facilitates desired interactions between the electrode surface and electrolyte. Theoretical calculations revealed that increased covalency of Co 3d and O 2p in Sr 2 Co 1.5 Fe 0.5 O 6-δ oxide is another primary contributor to its augmented water oxidation ability. As a model for developing catalysts with such an intermediate structure, the synergetic effect of oxygen vacancy and hybridization between Co 3d and O 2p assured the Sr 2 Co 1.5 Fe 0.5 O 6-δ oxide as a better catalyst for its enhanced OER activity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Revealing in-plane movement of platinum in polymer electrolyte fuel cells after heavy-duty vehicle lifetime

Fuel cell heavy-duty vehicles (HDVs) require increased durability of oxygen-reduction-reaction electrocatalysts, making knowledge of realistic degradation mechanisms critical. Here identical-location micro-X-ray fluorescence spectroscopy was performed on membrane electrode assemblies. The results exposed heavy in-plane movement of electrocatalyst after HDV lifetime, suggesting that electrochemical Ostwald ripening may not be a local effect. Development of local loading hotspots and preferential movement of electrocatalyst away from cathode catalyst layer cracks was observed. The heterogeneous degradation exhibited by a modified cathode gas diffusion layer membrane electrode assembly after HDV lifetime was successfully quantified by the identical-location approach. Further synchrotron micro-X-ray diffraction and micro-X-ray fluorescence experiments were performed to obtain the currently unknown correlation between electrocatalyst nanoparticle size increase and loading change. A direct correlation was discovered which developed only after HDV lifetime. Finally, the work provides a route to engineer immediate system-level mitigation strategies and to develop structured cathode catalyst layers with durable electrocatalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗