Influence of EDTA{sup 2-} on the hydrothermal synthesis of CdTe nanocrystallites

Transformation from Te nanorods to CdTe nanoparticles was achieved with the assistance of EDTA as a ligand under hydrothermal conditions. Experimental results showed that at the beginning of reaction Te nucleated and grew into nanorods. With the proceeding of reaction, CdTe nucleus began to emerge on the surface, especially on the tips of Te nanorods. Finally, nearly monodispersed hexagonal CdTe nanoparticles with diameters of about 200 nm were obtained. The effects of EDTA on the morphology and formation of CdTe nanoparticles were discussed in consideration of the strong ligand-effect of EDTA, which greatly decreased the concentration of Cd{sup 2+}. Furthermore, the possible formation process of CdTe nanoparticles from Te nanorods was further proposed. The crystal structure and morphology of the products were investigated by X-ray diffraction (XRD) and scanning electron microscopy (SEM). - Graphical Abstract: Firstly, Te nucleated and grew into nanorods in the presence of EDTA{sup 2-}. Then CdTe nucleus began to emerge on Te nanorods and finally monodispersed CdTe nanoparticles were obtained. Highlights: Black-Right-Pointing-Pointer EDTA serves as a strong ligand with Cd{sup 2+}. Black-Right-Pointing-Pointer The existence of EDTA constrains the nucleation of CdTe and promotes the formation of Te nanorods. Black-Right-Pointing-Pointer With the proceeding of reaction, CdTe nucleus began to emerge on the surface, especially on the tips of Te nanorods. Black-Right-Pointing-Pointer Nearly monodispersed hexagonal CdTe nanoparticles with diameters of about 200 nm were finally obtained.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Post-treatment and characterization of novel luminescent hybrid bimodal mesoporous silicas

A novel luminescent hybrid bimodal mesoporous silicas (LHBMS) were synthesized via grafting 1,8-Naphthalic anhydride into the pore channels of bimodal mesoporous silicas (BMMs) for the first time. The resulting samples were characterized by powder X-ray diffraction (XRD), N{sub 2} adsorption/desorption measurement, Fourier transform infrared spectroscopy (FT-IR), Transmission electron microscopy (TEM), UV-vis absorption spectroscopy, and Photoluminescence spectroscopy (PL). The results show that 1,8-Naphthalic anhydride organic groups have been successfully introduced into the mesopores of the BMMs and the hybrid silicas are of bimodal mesoporous structure with the ordered small mesopores of around 3 nm and the large mesopores of uniform intra-nanoparticle. The excellent photoluminescent performance of LHBMS has a blue shift compared to that of 2-[3-(triethoxysilyl) propyl-1 H-Benz [de]isoquinoline-1, 3(2 H)-dione, suggesting the existence of the quantum confinement effectiveness. - Graphical abstract: A novel luminescent hybrid bimodal mesoporous silicas was synthesized via modification and then grafting with 1, 8-Naphthalic anhydride, which would be strong potential application in the photoluminescent fields.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Evolution Of Surface Topography On GaAs(100) And GaAs(111) At Normal And Oblique Incidence Of Ar{sup +}-Ions

Nanoscale surface structures emerging from medium energy (50-60 keV)Ar{sup +}-ion sputtering of p-type GaAs(100) and semi-insulating GaAs(111) substrates have been investigated. For normally incident 50 keV Ar{sup +}-ions of fluence 1x10{sup 17} ions/cm{sup 2} on GaAs(100) and GaAs(111) features in the form of nanoscale pits/holes without short range ordering are observed with densities 5.2x10{sup 9} /cm{sup 2} and 5.9x10{sup 9} /cm{sup 2}, respectively along with irregularly shaped patches of islands. For GaAs(111) on increasing the influence to 5x10{sup 17} /cm{sup 2} the pit density increases marginally to 6.2x10{sup 9} /cm{sup 2}. For 60 deg. off-normal incidence of 60 keV Ar.{sup +}-ions of fluence 2x10{sup 17} ions/cm{sup 2} on GaAs(100) microscale wavelike surface topography is observed. In all cases well-defined nanodots are absent on the surface.

36 MATERIALS SCIENCE↗

Effect of microstructure on Au/sapphire interfacial thermal resistance

We deposit Au films on single crystal sapphire substrates by sputtering and evaporation methods. The microstructure characteristics such as crystal textures, grain sizes, and fraction of contacted area of the films are examined by x-ray diffraction and transmission electron microscopy. The sputtered films have an average grain size of about 200 nm and perfectly attach to the substrates; the as-evaporated films partially attach to the substrate; the grain size varies from 10 to 30 nm, and after annealing, increases to 50 nm. Au{sub 2}Al phase is observed in the annealed samples. The interfacial thermal resistance is measured by a frequency domain thermoreflectance method. The thermal resistance of the sputtered Au/sapphire interfaces is 35.5x10{sup -9} m{sup 2} K W{sup -1}, and those of the evaporated samples are up to three times as large as this value. The change in interfacial thermal resistance is explained by the effect of detachment using a parallel arranged thermal resistance model, the effect of grain size, and the influence of chemical bonding at the interfaces.

36 MATERIALS SCIENCE↗

Synthesis and photocatalytic activity of co-doped mesoporous TiO{sub 2} on Brij98/CTAB composite surfactant template

Using composite surfactant templates, polyoxyethylene (20) oleyl ether (Brij98) and cetyl trimethyl ammonium bromide (CTAB), as structure-directing agents, N and La co-doped mesoporous TiO{sub 2} complex photocatalysts were synthesized successfully. The micromorphology of co-doped mesoporous TiO{sub 2} samples was characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), Fourier transformed infrared spectroscopy (FT-IR), energy-dispersive X-ray spectrometer (EDS) and N{sub 2} adsorption-desorption measurements. The results indicated that the complex photocatalyst prepared with a molar ratio of Brij98:CTAB=1:1 showed a uniform pore size of ca. 7 nm and a high specific surface area (S{sub BET}) of 279.0 m{sup 2} g{sup -1}, and exhibited the highest photocatalytic activity for degradation of papermaking wastewater under ultra-violet light irradiation. The chemical oxygen demand (CODc{sub r}) percent degradation was about 73% in 12 h and chroma percent degradation was 100% in 8 h. - Graphical abstract: CODc{sub r} percent degradation of papermaking wastewater is about 73% after 12 h over the co-doped mesoporous TiO{sub 2} prepared with a molar ratio of Brij98:CTAB=1:1.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Low-reactive circulating fluidized bed combustion (CFBC) fly ashes as source material for geopolymer synthesis

In this contribution, low-reactive circulating fluidized bed combustion (CFBC) fly ashes (CFAs) have firstly been utilized as a source material for geopolymer synthesis. An alkali fusion process was employed to promote the dissolution of Si and Al species from the CFAs, and thus to enhance the reactivity of the ashes. A high-reactive metakaolin (MK) was also used to consume the excess alkali needed for the fusion. Reactivities of the CFAs and MK were examined by a series of dissolution tests in sodium hydroxide solutions. Geopolymer samples were prepared by alkali activation of the source materials using a sodium silicate solution as the activator. The synthesized products were characterized by mechanical testing, scanning electron microscopy (SEM), X-ray diffractography (XRD), as well as Fourier transform infrared spectroscopy (FTIR). The results of this study indicate that, via enhancing the reactivity by alkali fusion and balancing the Na/Al ratio by additional aluminosilicate source, low-reactive CFAs could also be recycled as an alternative source material for geopolymer production.

36 MATERIALS SCIENCE↗

Effect of Pt addition on Ni silicide formation at low temperature: Growth, redistribution, and solubility

The formation of Ni silicide during the reaction between Ni(5% Pt) and a Si(100) substrate has been analyzed by differential scanning calorimetry (DSC), in situ x-ray diffraction (XRD), cross-sectional transmission electron microscopy (TEM), and {sup 4}He{sup +} Rutherford backscattering. The DSC measurements show evidence of the Ni{sub 2}Si nucleation followed by lateral growth formation. In situ XRD and TEM have been used to investigate the sequence of formation of the silicides. These experiments show that the formations of Ni{sub 2}Si and NiSi occur simultaneously in the presence of the Pt alloy. The redistribution of platinum at different stages of the Ni silicide growth has been determined. We have estimated the solubility limit of platinum (1 at. % at 573 K) in the Ni{sub 2}Si phase by extrapolation from a measured value at 1073 K. This redistribution is explained in terms of the solubility limits and the diffusion of Pt in the Ni{sub 2}Si and NiSi phases. Pt is more likely to reside at the silicide grain boundaries and the interfaces where it can slow down the silicide growth kinetics.

36 MATERIALS SCIENCE↗

Thermoelectric and microstructural properties of Pb{sub 0.9-x}Sn{sub 0.1}Ge{sub x}Te compounds prepared by spinodal decomposition

Three samples of Pb{sub 0.9-x}Sn{sub 0.1}Ge{sub x}Te with x=0.25, 0.35, 0.6 were prepared by heating the mixtures above the melting point of the constituent elements followed by quenching in water. The x=0.6 sample is close to the center of the immiscibility region, while the x=0.25 and 0.35 samples are in the Pb rich region inside the spinodal miscibility gap. Microstructural investigations using Powder X-ray Diffraction, Scanning Electron Microscopy and Energy Dispersive X-ray Spectroscopy revealed both GeTe-rich and PbTe-rich phases. The samples were uniaxially hot pressed and the thermoelectric properties were characterized in the temperature range 2-400 K using a commercial apparatus and from 300 to 650 K with a custom designed setup. The best sample (x=0.6) reached zT{approx}0.6 at 650 K, while the x=0.25 and 0.35 samples showed thermal instability at elevated temperatures. -- Graphical abstract: Spinodal decomposition in the GeTe-SnTe-PbTe system demonstrated by SEM and EXS images. Display Omitted Highlights: {yields} Investigation of Pb-rich part of the spinodal miscibility gap in PbTe-SnTe-GeTe. {yields} zT=0.6 at 650 K reproduced for Pb{sub 0.3}Sn{sub 0.1}Ge{sub 0.6}Te. {yields} Pb-rich phases shown to be thermally instable. {yields} Thermoelectric property characterization at low and high temperature. {yields} Microstructural investigations using PXRD, SEM, EDX and PSM.

36 MATERIALS SCIENCE↗

Encapsulation of caesium-loaded Ionsiv in cement

The microporous material Ionsiv is used for {sup 137}Cs removal from aqueous nuclear waste streams. In the UK, Cs-loaded Ionsiv is classed as an intermediate-level waste; no sentencing and disposal route is yet defined for this material and it is currently held in safe interim storage on several nuclear sites. In this study, the suitability of fly ash and blast furnace slag blended cements for encapsulation of Cs-Ionsiv in a monolithic wasteform was investigated. No evidence of reaction or dissolution of the Cs-Ionsiv in the cementitious environment was found by scanning electron microscopy and X-ray diffraction. However, a small fraction ({<=} 1.6 wt.%) of the Cs inventory was released from the encapsulated Ionsiv during leaching experiments carried out on hydrated samples. Furthermore, it was evident that K and Na present in the cementitious pore water exchanged with Cs and H in the Ionsiv. Therefore, cement systems lower in K and Na, such as slag based cements, showed lower Cs release than the fly ash based cements.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Synthesis and characterization of monodisperse spherical SiO{sub 2}-RE{sub 2}O{sub 3} (RE=rare earth elements) and SiO{sub 2}-Gd{sub 2}O{sub 3}:Ln{sup 3+} (Ln=Eu, Tb, Dy, Sm, Er, Ho) particles with core-shell structure

Spherical SiO{sub 2} particles have been coated with rare earth oxide layers by a Pechini sol-gel process, leading to the formation of core-shell structured SiO{sub 2}-RE{sub 2}O{sub 3} (RE=rare earth elements) and SiO{sub 2}-Gd{sub 2}O{sub 3}:Ln{sup 3+} (Ln=Eu, Tb, Dy, Sm, Er, Ho) particles. X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), transmission electron microscopy (TEM), photoluminescence (PL), and cathodoluminescence spectra as well as lifetimes were used to characterize the resulting SiO{sub 2}-RE{sub 2}O{sub 3} (RE=rare earth elements) and SiO{sub 2}-Gd{sub 2}O{sub 3}:Ln{sup 3+} (Eu{sup 3+}, Tb{sup 3+}, Dy{sup 3+}, Sm{sup 3+}, Er{sup 3+}, Ho{sup 3+}) samples. The obtained core-shell phosphors have perfect spherical shape with narrow size distribution (average size ca. 380 nm), smooth surface and non-agglomeration. The thickness of shells could be easily controlled by changing the number of deposition cycles (40 nm for two deposition cycles). Under the excitation of ultraviolet, the Ln{sup 3+} ion mainly shows its characteristic emissions in the core-shell particles from Gd{sub 2}O{sub 3}:Ln{sup 3+} (Eu{sup 3+}, Tb{sup 3+}, Sm{sup 3+}, Dy{sup 3+}, Er{sup 3+}, Ho{sup 3+}) shells. - Graphical abstract: The advantages of core-shell phosphors are the easy availability of homogeneous spherical morphology in different size, and its corresponding luminescence color can change from red, yellow to green.

36 MATERIALS SCIENCE↗

Sol-gel synthesis of mesoporous CaCu{sub 3}Ti{sub 4}O{sub 12} thin films and their gas sensing response

A new sol-gel synthesis procedure of stable calcium copper titanate (CaCu{sub 3}Ti{sub 4}O{sub 12}-CCTO) precursor sols for the fabrication of porous films was developed. The composition of the sol was selected in order to avoid the precipitation of undesired phases; ethanol was used as solvent, acetic acid as modifier and poly(ethyleneglycol) as a linker agent. Films deposited by spin-coating onto oxidized silicon substrates were annealed at 700 {sup o}C. The main phase present in the samples, as detected by X-ray diffraction and Raman spectroscopy, was CaCu{sub 3}Ti{sub 4}O{sub 12}. Scanning electron microscopy analysis showed that mesoporous structures, with thicknesses between 200 and 400 nm, were developed as a result of the processing conditions. The films were tested regarding their sensibility towards oxygen and nitrogen at atmospheric pressure using working temperatures from 200 to 290 {sup o}C. The samples exhibited n-type conductivity, high sensitivity and short response times. These characteristics indicate that CCTO mesoporous structures obtained by sol-gel are suitable for application in gas sensing. - Graphical abstract: A sol-gel synthesis procedure toward stable CaCu{sub 3}Ti{sub 4}O{sub 12}-precursor sols avoiding the precipitation of undesired compounds is proposed. Films deposited by spin-coating onto oxidized silicon substrates were annealed at 700 {sup o}C. The thickness varied between 200 and 400 nm depending on sol composition. The films, tested as gas sensors for O{sub 2}, showed n-type conductivity, good sensitivity and short response times.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Doping induced magnetism in Co-ZnS nanoparticles

Zn{sub 1-x}Co{sub x}S nanoparticles with x=0, 0.1, 0.2, and 0.3 were synthesized by the co-precipitation method using thiophenol as capping agent. The effect of Co doping on the structural, optical and magnetic properties are investigated. The X-ray diffraction patterns show single phase with cubic structure and the images of Transmission Electron Microscopy indicate an average particle size of 39 nm. Significant blue shift in the optical absorbing band edge was observed with increasing Co doping. In the Co doped samples, room-temperature (RT) magnetic hysteresis is observed and the magnetization reduces with increasing Co content. However, these samples show paramagnetic resonance instead of ferromagnetic resonance at both 300 and 80 K, suggesting that the origin of RT magnetization in these Zn{sub 1-x}Co{sub x}S nanoparticles involves with the frustration of antiferromagnetic interactions. - Graphical abstract: Figure shows the magnetization data of Zn{sub 1-x}Co{sub x}S (0.1<=x<=0.3) nanoparticles annealed at 573 K/2 h in vacuum and measured at 300 K. This interesting feature of systematic reduction in magnetization may be due to introduction of antiferromagnetic ordering with increasing 'Co' concentration which may be due to competition between the antiferromagnetic and ferromagnetic ordering within the sample. One could also observe the exchange bias effect which is an interface interaction observed in a ferromagnetic-antiferromagnetic mixture. The exchange bias field (loop shift) towards negative field was around 63 Oe for the Zn{sub 1-x}Co{sub x}S (0.1<=x<=0.3) nanoparticles.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Synthesis of carbon nanotube/anatase titania composites by a combination of sol-gel and self-assembly at low temperature

A simple method is described for the synthesis of carbon nanotube/anatase titania composites by a combination of a sol-gel method with a self-assembly technique at 65 {sup o}C. This method makes use of polyelectrolyte for wrapping multi-walled carbon nanotube (MWCNT) and providing them with adsorption sites for electrostatically driven TiO{sub 2} nanoparticle deposition. The composites were characterized using X-ray diffraction, transmission electron microscopy, Fourier transform infrared and X-ray photoelectron spectroscopy, and photoluminescence for analyzing their crystal phase, microstructure, particle size, and other physicochemical properties. The results showed that MWCNT were covered with an anatase TiO{sub 2} thin layer or surrounded by an anatase TiO{sub 2} thick coating, which is constructed of TiO{sub 2} particles about 6 nm in size. The composites were rich in surface hydroxyl groups. The excited e{sup -} in conduction band of TiO{sub 2} may migrate to MWCNT. Concerning the potential applicability, MWCNT/TiO{sub 2} composites showed excellent photocatalytic activity toward the photodegradation of methyl orange. -- Graphical abstract: MWCNT/anatase TiO{sub 2} composites have been prepared by a combination of a sol-gel method and a self-assembly technique in one step at low temperature without high temperature calcination. Display Omitted Highlights: {yields} MWCNT/anatase TiO{sub 2} composites could be prepared in one-pot at low temperature. {yields} MWCNT were covered with a TiO{sub 2} thin layer or surrounded by a TiO{sub 2} thick coating. {yields} Composites were rich in surface hydroxyl groups. {yields} Composites showed excellent photodegradation activity of methyl orange.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A nitrilo-tri-acetic-acid/acetic acid route for the deposition of epitaxial cerium oxide films as high temperature superconductor buffer layers

A water based cerium oxide precursor solution using nitrilo-tri-acetic-acid (NTA) and acetic acid as complexing agents is described in detail. This precursor solution is used for the deposition of epitaxial CeO{sub 2} layers on Ni-5at%W substrates by dip-coating. The influence of the complexation behavior on the formation of transparent, homogeneous solutions and gels has been studied. It is found that ethylenediamine plays an important role in the gelification. The growth conditions for cerium oxide films were Ar-5% gas processing atmosphere, a solution concentration level of 0.25 M, a dwell time of 60 min at 900 {sup o}C and 5-30 min at 1050 {sup o}C. X-ray diffraction (XRD), scanning electron microscope (SEM), atomic force microscopy (AFM), pole figures and spectroscopic ellipsometry were used to characterize the CeO{sub 2} films with different thicknesses. Attenuated total reflection-Fourier transform infrared (ATR-FTIR) was used to determine the carbon residue level in the surface of the cerium oxide film, which was found to be lower than 0.01%. Textured films with a thickness of 50 nm were obtained. - Graphical abstract: Study of the complexation and hydrolysis behavior of Ce{sup 4+} ions in the presence of nitrilo-tri-acetic acid and the subsequent development of an aqueous chemical solution deposition route suited for the processing of textured CeO{sub 2} buffer layers on Ni-W tapes.

36 MATERIALS SCIENCE↗

Immobilization of Thiadiazole Derivatives on Magnetite Mesoporous Silica Shell Nanoparticles in Application to Heavy Metal Removal from Biological Samples

In this report magnetite was synthesized by a coprecipitation method, then coated with a layer of silica. Another layer of mesoporous silica was added by a sol-gel method, then 5-amino-1,3,4-thiadiazole-thiol (ATT) was immobilized onto the synthesized nanoparticles with a simple procedure. This was followed by a series of characterizations, including transmission electron microscopy (TEM), FT-IR spectrum, elemental analysis and XRD. Heavy metal uptake of the modified nanoparticles was examined by atomic absorption spectroscopy. For further investigation we chose Cu{sup 2+} as the preferred heavy metal to evaluate the amount of adsorption, as well as the kinetics and mechanism of adsorption. Finally, the capacity of our nanoparticles for the heavy metal removal from blood was shown. We found that the kinetic rate of Cu{sup 2+} adsorption was 0.05 g/mg/min, and the best binding model was the Freundlich isotherm.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Surface Modification of Nickel Foams by a Slurry Aluminizing Process

A novel slurry-based process for aluminizing nickel foams while improving the mechanical properties and conserving the excellent ductility is reported. Cellular unalloyed nickel foams with 92% porosity and uniform pore size and distribution were used as a starting material. Several slurries of different compositions were examined to investigate the possibility of developing an aluminide-nickel intermetallic coating on a Ni foam without considerably degrading the original ductile properties of the foam. The process temperature was varying from 400 to 850 deg. C and the process holding time was ranging between 2h to 6h. Scanning electron microscopy with an energy dispersive X-ray spectrometry and X-Ray diffraction were applied to assess the effectiveness of the aluminizing process and determine both the optimum parameters of the procedure (slurry composition, holding temperature and time) and the concentration profiles across the coating cross-section. The mechanical behavior of the aluminized Ni-foams was evaluated by the conduction of micro-tension tests. The resulting Ni-foams after aluminization retain the pore structure of original Ni-foams and present a thick outer surface layer which consists of a range of aluminide phases. The mechanical properties of the Ni-foams aluminized in low process temperature were insignificantly affected.

36 MATERIALS SCIENCE↗

Microstructural features and domain formation in (Ba,Sr){sub 2}TiSi{sub 2}O{sub 8} fresnoites

The formation and co-existence of crystallographically modulated and non-modulated regions in (Ba,Sr){sub 2}TiSi{sub 2}O{sub 8} fresnoites is reviewed, particularly the dependence on local composition. It is shown that perturbations of the average fresnoite structure, determined from appreciable single crystals, are in some cases better described as nanometric domain intergrowths where departures from ideal stoichiometry are characteristics of incommensuration, while modulation is absent from volumes that are less perturbed chemically. Evidence for this differentiation is obtained from selected area electron diffraction (SAED) patterns and high-resolution transmission electron microscopy (HRTEM) images. The domains are readily distinguished by their unique contrast in bright field electron micrographs. Fourier reconstructions of HRTEM images collected from areas with darker contrast show that modulation can change within relatively small volumes. Nearby areas with lighter contrast were found by SAED to be free of structural disorder and incommensurate reflections. - Graphical abstract: Fresnoite layers contain SiO{sub 4} and TiO{sub 5} polyhedra that undergo run rotation and tilting to create 3D, 4D and 5D structural modulations that can be directly observed by electron diffraction and high resolution imaging. Highlights: {yields}(Ba,Sr){sub 2}TiSi{sub 2}O{sub 8} fresnoites contain commensurate and incommensurate domains. > Departures in stoichiometry promote the formation of nanostructured domains. > Domains formation may provide a means for reducing strain in single crystals.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Epitaxial germanidation of full-Heusler Co{sub 2}FeGe alloy thin films formed by rapid thermal annealing

The authors demonstrated that a full-Heusler Co{sub 2}FeGe (CFG) alloy thin film was epitaxially grown by rapid-thermal-annealing-induced germanidation of an Fe/Co/pseudo-Ge(001)-on-insulator (GOI) multilayer formed on a Si-on-insulator (SOI) substrate. X-ray diffraction (XRD) measurements with out-of-plane and in-plane configurations revealed that the CFG film was epitaxially grown along the [001] direction with the in-plane epitaxial relation of CFG[100] parallel GOI[100], although the film slightly contained a non-epitaxial component. The strong (111) and (200) superlattice diffraction intensities indicated that the CFG film had a high degree of order for the L2{sub 1} structure. Cross-sectional high-resolution transmission electron microscopy images of the film revealed that the film had dominant epitaxial and slight non-epitaxial components, which was consistent with the XRD measurements. The epitaxial component was grown directly on the buried oxide layer of the SOI substrate without formation of any interfacial layer.

36 MATERIALS SCIENCE↗