Large area sheet task: Advanced Dendritic Web Growth Development

A melt level control system was implemented to provide stepless silicon feed rates from zero to rates exactly matching the silicon consumed during web growth. Bench tests of the unit were successfully completed and the system mounted in a web furnace for operational verification. Tests of long term temperature drift correction techniques were made; web width monitoring seems most appropriate for feedback purposes. A system to program the initiation of the web growth cycle was successfully tested. A low cost temperature controller was tested which functions as well as units four times as expensive.

Duncan, C. S.↗

Pellet Feed for Dendritic-Web Growth

Melt replenishment system sustains continuous growth of silicon dentritic web for several days. Substantially increases size of batch, limited mainly by level of impurities and life of crucible. Silicon pellets automatically added to crucible sustain crystal growth for days.

Duncan, C. S.↗

Large-area sheet task advanced dendritic web growth development

Thermal models were developed that accurately predict the thermally generated stresses in the web crystal which, if too high, cause the crystal to degenerate. The application of the modeling results to the design of low-stress experimental growth configurations will allow the growth of wider web crystals at higher growth velocities. A new experimental web growth machine was constructed. This facility includes all the features necessary for carrying out growth experiments under steady thermal conditions. Programmed growth initiation was developed to give reproducible crystal starts. Width control permits the growth of long ribbons at constant width. Melt level is controlled to 0.1 mm or better. Thus, the capability exists to grow long web crystals of constant width and thickness with little operator intervention, and web growth experiments can now be performed with growth variables controlled to a degree not previously possible.

Duncan, C. S.↗

Large-area sheet task advanced dendritic web growth development

The thermal stress model was used to generate the design of a low stress lid and shield configuration, which was fabricated and tested experimentally. In preliminary tests, the New Experimental Web Growth Facility performed as designed, producing web on the first run. These experiments suggested desirable design modifications in the melt level sensing system to improve further its performance, and these are being implemented.

Duncan, C. S.↗

Large-area sheet task advanced dendritic web growth development

The computer code for calculating web temperature distribution was expanded to provide a graphics output in addition to numerical and punch card output. The new code was used to examine various modifications of the J419 configuration and, on the basis of the results, a new growth geometry was designed. Additionally, several mathematically defined temperature profiles were evaluated for the effects of the free boundary (growth front) on the thermal stress generation. Experimental growth runs were made with modified J419 configurations to complement the modeling work. A modified J435 configuration was evaluated.

Duncan, C. S.↗

Large-area sheet task advanced dendritic web growth development

The "discrete shield' temperature model was completed and verified. Modifications to the J419 low stress configuration were tested experimentally to evaluate effects on growth speed. A composite lid and shield configuration combining the low stress features of the J419 with the width limiting characteristics of the J98M3 was fabricated and tested in the N-furnace. Several long crystals were grown with width limited to about 3.3 cm and with melt replenishment, although the configuration is not yet optimized for steady state growth.

Duncan, C. S.↗

Large-area sheet task: Advanced dendritic-web-growth development

Thermally generated stresses in the growing web crystal were reduced. These stresses, which if too high cause the ribbon to degenerate, were reduced by a factor of three, resulting in the demonstrated growth of high-quality web crystals to widths of 5.4 cm. This progress was brought about chiefly by the application of thermal models to the development of low-stress growth configurations. A new temperature model was developed which can analyze the thermal effects of much more complex lid and top shield configurations than was possible with the old lumped shield model. Growth experiments which supplied input data such as actual shield temperature and melt levels were used to verify the modeling results. Desirable modifications in the melt level-sensing circuitry were made in the new experimental web growth furnace, and this furnace has been used to carry out growth experiments under steady-state conditions. New growth configurations were tested in long growth runs at Westinghouse AESD which produced wider, lower stress and higher quality web crystals than designs previously used.

Duncan, C. S.↗

Large-area sheet task advanced dendritic web growth development

The thermal stress models were used to test the effect of melt level on stress generation and growth velocity. The results indicate that melt level has only small effects on stresses but significant effects on growth velocity. These results are consistent with experimental growth from measured melt levels. A new low-stress design concept is being evaluated with the models. A width-limiting version of the low-stress J460 configuration was tested experimentally with results consistent with the design goals.

Duncan, C. S.↗

Large-area sheet task advanced dendritic web growth development

Modeling in the development of low stress configurations for wide web growth is presented. Parametric sensitivity to identify design features which can be used for dynamic trimming of the furnace element was studied. Temperature measurements of experimental growth behavior led to modification in the growth system to improve lateral temperature distributions.

Duncan, C. S.↗

Production Line for Dendritic-Web Solar Cells

Direct inclusion of web-growth furnaces in production line expected to result in lower costs than current production processes using silicon wafers sliced from Czochralski boules. Silicon-web input capacity of line is 0.5 m2/min, which corresponds to total peak-power output of about 25 MW for 1 year of production. Line employs about 18 production people per shift and requires about 3,650 square feet of floorspace.

Page, D. J.↗

Dendritic growth and structure of undercooled nickel base alloys

The principal objectives of this overall investigation are to: study means for obtaining high undercooling in levitation melted droplets, and study structures produced upon the solidification of these undercooled specimens. Thermal measurements are made of the undercooling, and of the rapid recalescence, to develop an understanding of the solidification mechanism. Comparison of results is made with the modeling studies. Characterization and metallographic work is done to gain an understanding of the relationship between rapid solidification variables and the structures so produced. In ground based work to date, solidification of undercooled Ni-25 wt percent Sn alloy was observed by high-speed cinematography and the results compared with optical temperature measurements. Also in ground based work, high-speed optical temperature measurements were made of the solidification behavior of levitated metal samples within a transparent glass medium. Two undercooled Ni-Sn alloys were examined. Measurements were carried out on samples at undercoolings up to 330 K. Microstructures of samples produced in ground based work were determined by optical metallography and by SEM, and microsegregation by electron microprobe measurements. A series of flight tests were planned to conduct experiments similar to the ground based experiments. The Space Shuttle Columbia carried an alloy undercooled experiment in the STS 61-C mission in January 1986. A sample of Ni-32.5 wt percent Sn eutectic was melted and solidified under microgravity conditions.

Flemings, M. C.↗