Evaluation of high-contact-ratio spur gears with profile modification

Scoring tests, surface fatigue tests, and single-tooth bending fatigue tests were conducted with four sets of spur gears of standard design and three sets of spur gears of the new tooth form (NTF) design. Scoring tests were conducted in a gear test rig at a speed of 10,000 rpm using a synthetic polyester C5, C6, C7 substituted pentaerythritol oil. Surface fatigue tests were conducted in the same rig at a speed of 10,000 rpm and Hertz stresses of 173 x 10 to the 7th power and 143 x 10 to the 7th power Pa (250,000 and 214,000 psi). Single tooth bending fatigue tests were conducted on both the standard and NTF gears at an initial load that produced a 10.35 x 10 to the eight power Pa (150,000-psi) bending stress. The gears were load cycled to failure or for 3 x 10 to the 6th power cycles, whichever occurred first. The load was increased after test until failure occurred at 3 x 10 to the 6th power cycles or less. Both the standard and NTF gears scored at a gear bulk temperature of approximately 409 K (277 F). At this temperature the load on the NTF gears was 22 percent less than the load on the standard gears. The scoring failure was a function of gear bulk temperature, where for a given lubricant the temperature is a function of gear design, operating load, and speed.

Townsend, D. P.↗

Fabrication and Testing of Two Passively Actuated Creep-Fatigue Surveillance Test Articles

This report describes the fabrication, testing, and analysis of two families of passively-actuated creep-fatigue test articles. These test articles induce cyclic mechanical load in a test section actuated solely through a mismatch in the thermal expansion coefficient of two materials and driven by a change in the specimen temperature. Test articles of this type could provide material degradation data for a materials surveillance program in future operating molten salt reactors, where variations in the reactor temperature caused by normal or upset cycles would provide the temperature change in the sample. The purpose of the current experimental campaign is to demonstrate the feasibility of fabricating realistically-sized test articles, test the articles under repeated thermal cycling to assess their robustness, particularly the reliability of the bimetallic welds, and collect strain data from instrumented samples to validate the methods used to size the test articles to match key features of the mechanical response of operating reactor components. The thermal cycling tests are ongoing but the test data to date suggests the current test article design is viable, robust, and can be successfully designed to match a target mechanical response. Finally, the report describes preliminary work on welding refractory alloys to 316H stainless steel. Replacing the test article driver material, currently Alloy 617, with a refractory would increase the coefficient of thermal expansion mismatch and support further miniaturization of the test articles.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

ECAR-8446 Rev 0 MARVEL BPVC Section III Division 5 HBB Fatigue Acceptance Tests

The objective of this analysis is to evaluate the fatigue and creep behavior of 316 SS materials used in the Primary Coolant System (PCS) and Guard Vessel System (GVS) for the first two years of MARVEL reactor operation. The analysis follows the requirements set forth in ASME BPVC Section III, Division 5, HBB-2800, which mandates a fatigue test if operational conditions exceed allowable thresholds. By determining whether the materials meet the HBB-T-1324(a) and HBB-T-1324(b) criteria, this evaluation establishes whether a fatigue test is necessary, as well as the maximum allowable operational hours and temperatures before fatigue testing would be required. The deliverables of this analysis include calculations validating compliance with fatigue acceptance criteria, determination of maximum operational limits for the two-year period, and identification of conditions under which a fatigue test would be necessary. This ensures that the PCS and GVS can operate safely without premature material degradation and align with the design life requirements outlined in SPC-70731. Additionally, this evaluation provides conservative estimates for Service Level B occurrences and their impact on allowable Service Level A hours and temperatures, offering guidance for future operational assessments and potential life extensions beyond the initial two-year period.

21 - SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLAN↗

Effect of the overlapping factor on the microstructure and mechanical properties of pulsed Nd:YAG laser welded Ti6Al4V sheets

The effect of the overlapping factor on the microstructures and mechanical properties of pulsed Nd:YAG laser welded Ti6Al4V alloy sheets was investigated by microstructural observations, microhardness tests, tensile tests and fatigue tests. A microstructural examination shows that by increasing the overlapping factor, the grains in the fusion zone become coarser, and the width of the heat affected zone increases. As overlapping factor increases, the width of region composed completely of martensite α′ and the secondary α phase in the heat affected zone increases, consequently the gradient of microstructure along the direction from the fusion zone to base metal decreases, so does the gradient of microhardness. The results of tensile and fatigue tests reveal that the joints made using medium overlapping factor exhibit better mechanical properties than those welded with low and high overlapping factors. Based on the experimental results, it can be stated that a sound weld of Ti6Al4V alloy can be obtained if an appropriate overlapping factor is used. - Highlights: • The weld quality of Ti6Al4V alloy under various overlapping factors was assessed. • Tensile and fatigue tests were conducted with as-welded specimen. • Localized strain across the weld was measured using DIC photogrammetry system. • A sound weld of Ti6Al4V alloy is obtained by using right overlapping factor.

36 MATERIALS SCIENCE↗

Investigation of fatigue strength of multilayer advanced fiber composites

The analytical characterization of a multilayer fiber composite plate (without hole) was accomplished for both static and dynamic loading conditions using the finite difference technique. Thornel 300/5208 composites with and without holes were subjected to static and tensile fatigue testing. Five (5) fiber orientations were submitted to test. Tensile fatigue testing also included three (3) loading conditions and two (2) frequencies. The low-cycle test specimens demonstrated a shorter tensile fatigue life than the high-cycle test specimens. Failure surfaces demonstrated effect of testing conditions. Secondary failure mechanisms, such as: delamination, fiber breakage, and edge fiber delamination were present. Longitudinal delamination between plies also occurred in these specimens.

Thornton, H. R.↗

Evaluation of high-contact-ratio spur gears with profile modification

Scoring tests, surface fatigue tests, and single-tooth bending fatigue tests were conducted with four sets of spur gears of standard design and three sets of spur gears of new-tooth-form design. The new-tooth-form and standard gears scored at approximately the same gear bulk temperature of 409 K (277 F). The scoring load for the new-tooth-form gears was 22 percent less than that for the standard gears. The pitting fatigue lives of the standard and new-tooth-form gears were statistically equal for equal Hertz stress, while the surface fatigue life of the nw-tooth-form gears was approximately five times that of the standard gears at the same load. The standard gears failed at a 17 percent higher bending stress than the new-tooth-form gears when stress was calculated by the AGMA method. However, the difference is not statistically significant. The standard gears failed at a tooth load 1.9 times that for the new-tooth-form gears.

Towsend, D. P.↗

Fatigue Strength and Related Characteristics of Aircraft Joints I : Comparison of Spot-Weld and Rivet Patterns in 24s-t Alclad and 75s-t Alclad

Report contains detailed results of a number of fatigue tests on spot-welded joints in aluminum alloys. The tests described include: (1) fatigue tests on spot-welded lap joints in sheets of unequal thickness of alclad 24s-t. These tests indicate that the fatigue strength of a spot-welded joint in sheets of two different gages is slightly higher than that of a similar joint in two sheets of the thinner gage but definitely lower than that of a similar joint in two sheets of the thicker gage. (2) Fatigue tests on spot-welded alclad 75s-t spot-welded lap-joint specimens of alclad 75s-t were not any stronger in fatigue than similar specimens of alclad 24s-t. (3) Fatigue tests on lap-joint specimens spot -welded after various surface preparations--these included ac welding wire-brushed surfaces, dc welding wire-brushed surfaces, and dc welding chemically cleaned surfaces. While the ac welds were strongest statically, the dc welds on wire-brushed surfaces were strongest in fatigue. Specimens prepared in this way were very nearly as strong as the best riveted specimens tested for comparison. (4) Fatigue tests on specimens spot-welded with varying voltage so as to include a wide range of static spot-weld strengths. The fatigue strengths were in the same order as the static strengths but showed less range. (author)

Russell, H W↗

Fatigue strength of a single lap joint SPR-bonded

In the last years, hybrid joints, meaning with this the joints which consist in combining a traditional mechanical joint to a layer of adhesive, are gradually attracting the attention of various sectors of the construction of vehicles and transportation industries, for their better performance compared to just mechanical joints (self-piercing riveting SPR, riveting, and so on) or just to bonded joints.The paper investigates the fatigue behavior of a single lap joint self-piercing riveted (SPR) and bonded throughout fatigue tests. The considered geometric configuration allowed the use of two rivets placed longitudinally; an epoxy resin was used as adhesive. In the first part of the work static characterization of the joints was carried out through tensile tests. Then fatigue tests were made with the application of different levels of load. The fatigue curves were also obtained at the varying the distance between the two rivets in order to better assess the joint strength for a given length of overlap.

36 MATERIALS SCIENCE↗

Reliability aspects of a composite bolted scarf joint

The design, fabrication, static test, and fatigue test of both tension and compression graphite-epoxy candidates for a wing splice representative of a next-generation transport aircraft was the objective of the reported research program. A single-scarf bolted joint was selected as the design concept. Test specimens were designed and fabricated to represent an upper-surface and a lower-surface panel containing the splice. The load spectrum was a flight-by-flight random-load history including ground-air-ground loads. The results of the fatigue testing indicate that, for this type of joint, the inherent fatigue resistance of the laminate is reflected in the joint behavior and, consequently, the rate of damage accumulation is very slow under realistic fatigue loadings.

Reed, D. L.↗

Fatigue, Creep-Fatigue, and Thermomechanical Fatigue Life Testing of Alloys

The fatigue crack initiation resistance of an alloy is determined by conducting a series of tests over a range of values of stress amplitude or strain range. The observed number of cycles to failure is plotted against the stress amplitude or strain range to obtain a fatigue curve. The fatigue properties quoted for an alloy are typically the constants used in the equation(s) that describe the fatigue curve. Fatigue lives of interest may be as low as 10(exp 2) or higher than 10(exp 9) cycles. Because of the enormous scatter associated with fatigue, dozens of tests may be needed to confidently establish a fatigue curve, and the cost may run into several thousands of dollars. To further establish the effects on fatigue life of the test temperature, environment, alloy condition, mean stress effects, creep-fatigue effects, thermomechanical cycling, etc. requires an extraordinarily large and usually very costly test matrix. The total effort required to establish the fatigue resistance of an alloy should not be taken lightly. Fatigue crack initiation tests are conducted on relatively small and presumed to be initially crack-free, samples of an alloy that are intended to be representative of the alloy's metallurgical and physical condition. Generally, samples are smooth and have uniformly polished surfaces within the test section. Some may have intentionally machined notches of well-controlled geometry, but the surface at the root of the notch is usually not polished. The purpose of polishing is to attain a reproducible surface finish. This is to eliminate surface finish as an uncontrolled variable. Representative test specimen geometries will be discussed later. Test specimens are cyclically loaded until macroscopically observable cracks initiate and eventually grow to failure. Normally, the fatigue failure life of a specimen is defined as the number of cycles to separation of the specimen into two pieces. Alternative definitions are becoming more common, particularly for low-cycle fatigue testing, wherein some prescribed indication of impending failure due to cracking is adopted. Specific criteria will be described later. As a rule, cracks that develop during testing are not measured nor are the test parameters intentionally altered owing to the presence of cracking.

Halford, Gary R.↗

Cyclic torsion testing

Torsional fatigue testing and data analysis procedures are described. Since there are no standards governing cyclic torsion testing that are generally accepted on a widespread basis by the technical community, the different approaches that dominate current experimental activity, and the ramifications of each are discussed. Particular attention is given to the theoretical and experimental difficulties that have paced refinement and general acceptance of test procedures. Finally, specific quantities and nomenclature modelled after analagous axial fatigue properties are suggested as an effective way to communicate torsional fatigue results until accepted standards are established.

Leese, G. E.↗

Piezoelectric Bolt Breakers and Bolt Fatigue Testers

A proposed family of devices for inducing fatigue in bolts in order to break the bolts would incorporate piezoelectric actuators into resonant fixtures as in ultrasonic/ sonic drills/corers and similar devices described in numerous prior NASA Tech Briefs articles. These devices were originally intended primarily for use as safer, more-reliable, more-versatile alternatives to explosive bolts heretofore used to fasten spacecraft structures that must subsequently be separated from each other quickly on command during flight. On Earth, these devices could be used for accelerated fatigue testing of bolts. Fatigue theory suggests that a bolt subjected to both a constant-amplitude dynamic (that is, oscillatory) stress and a static tensile stress below the ultimate strength of the bolt material will fail faster than will a bolt subjected to only the dynamic stress. This suggestion would be applied in a device of the proposed type. The device would be designed so that the device and the bolt to be fatigue-tested or broken would be integral parts of an assembly (see figure). The static tension in the tightened bolt would apply not only the clamping force to hold the joined structures (if any) together but also the compression necessary for proper operation of the piezoelectric actuators as parts of a resonant structural assembly. The constant-amplitude dynamic stress would be applied to the bolt by driving the piezoelectric actuators with a sinusoidal voltage at the resonance frequency of longitudinal vibration of the assembly. The amplitude of the excitation would be made large enough so that the vibration would induce fatigue in the bolt within an acceptably short time. In the spacecraft applications or in similar terrestrial structural-separation applications, devices of the proposed type would offer several advantages over explosive bolts: Unlike explosive bolts, the proposed devices would be reusable, could be tested before final use, and would not be subject to catastrophic misfire. In fatigue-testing applications, devices of the proposed type would offer advantages of compactness and low cost, relative to conventional fatigue- testing apparatuses. In both structural- separation and fatigue-testing applications, bolts to be broken or tested could be instrumented with additional ultrasonic transducers for monitoring of pertinent physical properties and of fatigue failure processes.

Sherrit, Stewart↗

RDS-21 Face-Gear Surface Durability Tests

Experimental fatigue tests were performed to determine the surface durability life of a face gear in mesh with a tapered spur involute pinion. Twenty-four sets of gears were tested at three load levels: 7200, 8185, and 9075 lb-in face gear torque, and 2190 to 3280 rpm face gear speed. The gears were carburized and ground, shot-peened and vibro-honed, and made from VIM-VAR Pyrowear 53 steel per AMS 6308. The tests produced 17 gear tooth spalling failures and 7 suspensions. For all the failed sets, spalling occurred on at least one tooth of all the pinions. In some cases, the spalling initiated a crack in the pinion teeth which progressed to tooth fracture. Also, spalling occurred on some face gear teeth. The AGMA endurance allowable stress for a tapered spur involute pinion in mesh with a face gear was determined to be 275 ksi for the material tested. For the application of a tapered spur involute pinion in mesh with a face gear, proper face gear shim controlled the desired gear tooth contact pattern while proper pinion shim was an effective way of adjusting backlash without severely affecting the contact pattern.

Lewicki, David G.↗

Post-impact fatigue of cross-plied, through-the-thickness reinforced carbon/epoxy composites

An experimental investigation of the post-impact fatigue response of integrally woven carbon/epoxy composites was conducted. Five different through-the-thickness (TTT) reinforcing fibers were used in an experimental textile process that produced an integrally woven (0/90/0/90/0/90/0/90/0)(sub T) ply layup with 21K AS4 carbon tow fiber. The resin was Hercules 3501-6, and the five TTT reinforcing fibers were Kevlar, Toray carbon, AS4 carbon, glass, and IM6 carbon. The purpose of this investigation was to study the post-impact fatigue response of these material systems and to identify the optimum TTT fiber. Samples were impacted with one half inch diameter aluminum balls with an average velocity of 543 ft/sec. Post-impact static compression and constant amplitude tension-compression fatigue tests were conducted. Fatigue tests were conducted with a loading ratio of R=-5, and frequency of 4 Hz. Damage growth was monitored using x-radiographic and sectioning techniques and by examining the stress-strain response (across the impact site) throughout the fatigue tests. The static compressive stress versus far-field strain response was nearly linear for all material groups. All the samples had a transverse shear failure mode. The average compressive modulus (from far-field strain) was about 10 Msi. The average post-impact static compressive strength was about 35.5 Ksi. The IM6 carbon sample had a strength of over 40 Ksi, more than 16 percent stronger than average. There was considerable scatter in the S-N data. However, the IM6 carbon samples clearly had the best fatigue response. The response of the other materials, while worse than IM6 carbon, could not be ranked definitively. The initial damage zones caused by the impact loading and damage growth from fatigue loading were similar for all five TTT reinforcing materials. The initial damage zones were circular and consisted of delaminations, matrix cracks and ply cracks. Post-impact fatigue loading caused delamination growth, ply cracking and fiber bundle failures, typically 45 deg from impact load direction. During the initial 97 percent of fatigue life, delaminations, ply cracks and fiber bundle failures primarily grew at and near the impact site. During the final 3 percent of life, damage grew rapidly transverse to the loading direction as a through-the-thickness transverse shear failure. The stress-strain response was typically linear during the initial 50 percent of life, and stiffness dropped about 20 percent during this period. During the next 47 percent of life, stiffness dropped about 34 percent, and the stress-strain response was no longer linear. The stiffness decreased about 23 percent during the final 3 percent of life. These trends were typical of all the materials tested. Therefore, by monitoring stiffness loss, fatigue failure could be accurately anticipated.

Serdinak, Thomas E.↗

Effect of outdoor exposure at ambient and elevated temperatures on fatigue life of Ti-6Al-4V titanium alloy sheet in the annealed and the solution treated and aged condition

Specimens of Ti-6Al-4V titanium alloy sheet in the annealed and the solution-treated and aged heat-treatment condition were exposed outdoors at ambient and 560 K (550 F) temperatures to determine the effect of outdoor exposure on fatigue life. Effects of exposure were determined by comparing fatigue lives of exposed specimens to those of unexpected specimens. Two procedures for fatigue testing the exposed specimens were evaluated: (1) fatigue tests conducted outdoors by applying 1200 load cycles per week until failure occurred and (2) conventional fatigue tests (continuous cycling until failure occurred) conducted indoors after outdoor exposure under static load. The exposure period ranged from 9 to 28 months for the outdoor fatigue-test group and was 24 months for the static-load group. All fatigue tests were constant-amplitude bending of specimens containing a drilled hole (stress concentration factor of 1.6). The results of the tests indicate that the fatigue lives of solution-treated and aged specimens were significantly reduced by the outdoor exposure at 560 K but not by the exposure at ambient temperature. Fatigue lives of the annealed specimens were essentially unaffected by the outdoor exposure at either temperature. The two test procedures - outdoor fatigue test and indoor fatigue test after outdoor exposure - led to the same conclusions about exposure effects.

Phillips, E. P.↗

Advanced Failure Determination Measurement Techniques Used in Thermal Fatigue Life Testing of Electronic Packaging

Thermal fatigue life testing of various electronic packaging technologies is being performed by the Reliability Technology Group at the Jet Propulsion Laboratory. These testing efforts are in progress to improve uderstanding of the reliability issues associated with low volume packaging technologies for space applications and to develop qualification and acceptance approaches for these technologies. The work described here outlines the electrical failure detection techniques used during testing by documenting the circuits and components used to make these measurements, the sensitivity of the measurements, and the applicability of each specific measurement.

fatigue surface mount measurement testing thermal ↗

Multi Resolution In-Situ Testing and Multiscale Simulation for Creep Fatigue Damage Analysis of Alloy 617

This report outlines the research activities that were carried out for the integrated experimental and simulation investigation of creep-fatigue damage mechanism and life prediction of Nickel-based alloy, Inconel 617 at high temperatures (950° and 850°). First, a novel experimental design using a hybrid control technique is proposed. The newly developed experimental technique can generate different combinations of creep and fatigue damage by changing the experimental design parameters. Next, detailed imaging analysis and statistical data analysis are performed to quantify the failure mechanisms of the creep fatigue of alloy 617 at high temperatures. It is observed that the creep damage is directly associated with the internal voids at the grain boundaries and the fatigue damage is directly related to the surface cracking. It is also observed that the classical time fraction approach does not has a good correlation with the experimental observed damage features. An effective time fraction parameter is seen to have an excellent correlation with the material microstructural damage. Thus, a new empirical damage interaction diagram is proposed based on the experimental observations. Following this, a macro level viscoplastic model coupled with damage is developed to simulate the stress/strain response under creep fatigue loadings. A damage rate function based on the hysteresis energy and creep energy is proposed to capture the softening behavior of the material and a good correlation with life prediction and material hysteresis behavior is observed. The simulation work is extended to include the microstructural heterogeneity. A crystal plasticity finite element model considering isothermal and large deformation conditions at the microstructural scale has been developed for fatigue, creep-fatigue as well as creep deformation and rupture at high temperature. The model considers collective dislocation glide and climb of the grains and progressive damage accumulation of the grain boundaries. The glide model incorporates a slip resistance evolution model that characterizes the solute-drag creep effects and can capture well the stress-strain and stress time response of fatigue and creep-fatigue tests at various strain ranges and hold times. In order to accurately capture the creep strains that accumulate particularly at relatively low stress levels, a dislocation climb model has been incorporated into the crystal plasticity modeling framework. The dislocation climb model parameters are calibrated and verified through experimental creep tests performed at 950°. In addition, a cohesive zone model has been fully implemented in the context of the crystal plasticity finite element model to capture the intergranular creep damage. The parameters of the cohesive zone model have been calibrated using available experimental data. The numerical simulations illustrate the capability of the proposed model in capturing damage initiation and growth under creep loads as compared to the experimental observations. The microscale analysis sheds light on the crack initiation sites and propagation patterns within the microstructure. The model is also utilized to investigate the hybrid-controlled creep-fatigue tests and has been found to capture reasonably well the stress-strain response with different hold times and hold stress magnitudes.

36 MATERIALS SCIENCE↗

Continuation Report: Creep-fatigue Behavior and Damage Accumulation of a Candidate Structural Material for Concentrating Solar Thermal Receiver

At the start of this phase, six alloys were determined to be candidate materials for the concentrating solar power (CSP) thermal receiver: Alloys 617, 625, 740H, 230, 282 and Alloy X. From these, Alloys 740H and 282 were determined to be the most suitable, with both alloys exhibiting similar high temperature strength properties. Alloy 740H was selected due to its ease to work with (simpler heat treatments and welding procedures) and a larger database of existing data. Fatigue testing was started in this phase, with four fatigue tests having been completed, with additional fatigue testing planned, as well as tensile, creep and creep-fatigue tests starting in the next phase. Two fatigue tests performed at 850 °C and were completed in significantly fewer cycles than the two tests performed at 750 °C. Metallography was performed on the fatigued specimens to examine crack path and surrounding microstructure. These preliminary results suggest a significant drop in strength at elevated temperatures above 750 °C, however, more test results will be needed prior to setting design limits. Several potential model high temperature design methods were evaluated that could form the basis of our final recommended creep-fatigue design method for Alloy 740H. To do this we expanded on the receiver finite element model to develop a model representative of a potential Gen 3 design using KCl-MgCl2 salt coolant and operating with a salt inlet temperature of 550°C and salt outlet temperature of 720°C. Using the temperature fields from the model thermohydraulic analysis we determined the design life of the reference receiver assuming it was constructed from 740H seamless tubing and assuming high temperature design properties for 740H from literature data and, where required, naïve extrapolation. As experimental data is generated, these tentative design parameters will be updated to match the actual performance of 740H in elevated temperature service. The results of this design study are a rank ordering of potential design methods for two criteria: ease of use and design margin. The end goal of this project is to develop a creep-fatigue design method with adequate, but not over conservative, design margin that is straightforward to execute. Our receiver model is based on the preliminary design provided to DOE by Solar Reserve. Our analysis indicates a peak metal temperature of around 840° C for this design (comparable to Solar Reserve’s analysis, which shows a peak metal temperature of around 830° C). The Solar Reserve tube thickness is too thin to sustain creep-fatigue loading at this temperature. This means that the current trial design is not well-suited for evaluating different design methodologies, as we predict it will have a very short design life. We suggest that we modify our reference design with input from DOE in order to lower the maximum metal temperature to less than 800° C. We can then repeat these analyses and give a more meaningful comparison of different design methods before making a final selection.