Search NASA⌕ Search

SEARCH · Search NASA

Results for “graphite anodes”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Self-healing SEI enables full-cell cycling of a silicon-majority anode with a coulombic efficiency exceeding 99.9%

Despite active developments, full-cell cycling of Li-battery anodes with >50 wt% Si (a Si-majority anode, SiMA) is rare. The main challenge lies in the solid electrolyte interphase (SEI), which when formed naturally (nSEI), is fragile and cannot tolerate the large volume changes of Si during lithiation/delithiation. An artificial SEI (aSEI) with a specific set of mechanical characteristics is henceforth designed; we enclose Si within a TiO 2 shell thinner than 15 nm, which may or may not be completely hermetic at the beginning. In situ TEM experiments show that the TiO 2 shell exhibits 5× greater strength than an amorphous carbon shell. Void-padded compartmentalization of Si can survive the huge volume changes and electrolyte ingression, with a self-healing aSEI + nSEI. The half-cell capacity exceeds 990 mA h g -1 after 1500 cycles. To improve the volumetric capacity, we further compress SiMA 3-fold from its tap density (0.4 g cm -3 ) to 1.4 g cm -3 , and then run the full-cell battery tests against a 3 mA h cm -2 LiCoO 2 cathode. Despite some TiO 2 enclosures being inevitably broken, 2× the volumetric capacity (1100 mA h cm -3 ) and 2× the gravimetric capacity (762 mA h g -1 ) of commercial graphite anode is achieved in stable full-cell battery cycling, with a stabilized areal capacity of 1.6 mA h cm -2 at the 100th cycle. The initial lithium loss, characterized by the coulombic inefficiency (CI), is carefully tallied on a logarithmic scale and compared with the actual full-cell capacity loss. In conclusion, it is shown that a strong, non-adherent aSEI, even if partially cracked, facilitates an adaptive self-repair mechanism that enables full-cell cycling of a SiMA, leading to a stabilized coulombic efficiency exceeding 99.9%.

25 ENERGY STORAGE↗

Investigation of Path Dependence in Commercial Li-ion Cells Chosen for PHEV Duty Cycle Protocols (paper)

Path dependence is emerging as a premier issue of how electrochemical cells age in conditions that are diverse and variable in the time domain. For example, lithium-ion cells in a vehicle configuration will experience a variable combination of usage and rest periods over a range of temperature and state of charge (SOC). This is complicated by the fact that some aging can actually become worse (or better) when a lithium-ion cell is idle for extended periods under calendar-life (calL) aging, as opposed to cycle-life (cycL) conditions where the cell is used within a predictable schedule. The purpose of this study is to bridge the gap between highly idealized and controlled laboratory test conditions and actual field conditions regarding PHEV applications, so that field-type aging mechanisms can be mimicked and quantified in a repeatable laboratory setting. The main parameters are the magnitude and frequency of the thermal cycling, looking at isothermal, mild, and severe scenarios. To date, little is known about Li-ion aging effects caused by thermal cycling superimposed onto electrochemical cycling, and related path dependence. This scenario is representative of what Li-ion batteries will experience in vehicle service, where upon the typical start of a HEV/PHEV, the batteries will be cool or cold, will gradually warm up to normal temperature and operate there for a time, then will cool down after the vehicle is turned off. Such thermal cycling will occur thousands of times during the projected life of a HEV/PHEV battery pack. We propose to quantify the effects of thermal cycling on Li-ion batteries using a representative chemistry that is commercially available. The secondary Li-ion cells used in this study are of the 18650 configuration, have a nominal capacity rating of 1.9 Ah, and consist of a {LiMn2O4 + LiMn(1/3)Ni(1/3)Co(1/3)O2} cathode and a graphite anode. Electrochemical cycling is based on PHEV-relevant cycle-life protocols that are a combination of charge depleting (CD) and charge sustaining (CS) modes discussed in the Battery Test Manual for Plug-in Hybrid Electric Vehicles (INL, March 2008, rev0). A realistic duty cycle will involve both CD and CS modes, the proportion of each defined by the severity of the power demands. We assume that the cells will start each cycling day at 90% SOC, and that they will not be allowed to go below 35% SOC, with operation around 70% SOC being a nominal condition. The 35, 70, and 90% SOC conditions are also being used to define critical aspects of the related reference performance test (RPT) for this investigation. There are three primary components to the RPT, all assessed at room temperature: (A) static and residual capacity (SRC) over a matrix of current, (B) kinetics and pulse performance testing (PPT) over current for SOCs of interest, and (C) EIS for SOCs of interest. The RPT is performed on all cells every 30 day test interval, as well as a pulse-per-day to provide a quick diagnostic snapshot. Where feasible, we utilize various elements of Diagnostic Testing (DT) to characterize performance of the cells and to gain mechanistic-level knowledge regarding both performance features and limitations. We will present the rationale behind the experimental design, early data, and discuss the fundamental tools used to elucidate performance degradation mechanisms.

25 ENERGY STORAGE↗

A Surface Se-Substituted LiCo[O 2-δ Se δ ] Cathode with Ultrastable High-Voltage Cycling in Pouch Full-Cells

Cycling LiCoO 2 to above 4.5 V for higher capacity is enticing; however, hybrid O anion- and Co cation-redox (HACR) at high voltages facilitates intrinsic O α - (α < 2) migration, causing oxygen loss, phase collapse, and electrolyte decomposition that severely degrade the battery cyclability. Hereby, commercial LiCoO 2 particles are operando treated with selenium, a well-known anti-aging element to capture oxygen-radicals in the human body, showing an “anti-aging” effect in high-voltage battery cycling and successfully stopping the escape of oxygen from LiCoO 2 even when the cathode is cycled to 4.62 V. Furthermore, ab initio calculation and soft X-ray absorption spectroscopy analysis suggest that during deep charging, the precoated Se will initially substitute some mobile O α - at the charged LiCoO 2 surface, transplanting the pumped charges from O α - and reducing it back to O 2- to stabilize the oxygen lattice in prolonged cycling. As a result, the material retains 80% and 77% of its capacity after 450 and 550 cycles under 100 mA g -1 in 4.57 V pouch full-cells matched with a graphite anode and an ultralean electrolyte (2 g Ah -1 ).

36 MATERIALS SCIENCE↗

Delineating the Impact of Transition‐Metal Crossover on Solid‐Electrolyte Interphase Formation with Ion Mass Spectrometry

Abstract Lithium‐metal batteries (LMB) employing cobalt‐free layered‐oxide cathodes are a sustainable path forward to achieving high energy densities, but these cathodes exhibit substantial transition‐metal dissolution during high‐voltage cycling. While transition‐metal crossover is recognized to disrupt solid‐electrolyte interphase (SEI) formation on graphite anodes, experimental evidence is necessary to demonstrate this for lithium‐metal anodes. In this work, advanced high‐resolution 3D chemical analysis is conducted with time‐of‐flight secondary‐ion mass spectrometry (TOF‐SIMS) to establish spatial correlations between the transition metals and electrolyte decomposition products found on cycled lithium‐metal anodes. Insights into the localization of various chemistries linked to crucial processes that define LMB performance, such as lithium deposition, SEI growth, and transition‐metal deposition are deduced from a precise elemental and spatial analysis of the SEI. Heterogenous transition‐metal deposition is found to perpetuate both heterogeneous SEI growth and lithium deposition on lithium‐metal anodes. These correlations are confirmed across various lithium‐metal anodes that are cycled with different cobalt‐free cathodes and electrolytes. An advanced electrolyte that is stable to higher voltages is shown to minimize transition‐metal crossover and its effects on lithium‐metal anodes. Overall, these results highlight the importance of maintaining uniform SEI coverage on lithium‐metal anodes, which is disrupted by transition‐metal crossover during operation at high voltages.

Chemistry↗

Mn versus Al in Layered Oxide Cathodes in Lithium-Ion Batteries: A Comprehensive Evaluation on Long-Term Cyclability

Nickel-rich layered oxide cathodes with the composition LiNi 1-x-y Co x Mn y O 2 (NCM, (1-x-y) ≥ 0.6) are under intense scrutiny recently to contend with commercial LiNi 0.8 Co 0.15 Al 0.05 O 2 (NCA) for high-energy-density batteries for electric vehicles. However, a comprehensive assessment of their electrochemical durability is currently lacking. Herein, two in-house cathodes, LiNi 0.8 Co 0.15 Al 0.05 O 2 and LiNi 0.7 Co 0.15 Mn 0.15 O 2 , are investigated in a high-voltage graphite full cell over 1500 charge-discharge cycles (≈5–10 year service life in vehicles). Despite a lower nickel content, NCM shows more performance deterioration than NCA. Critical underlying degradation processes, including chemical, structural, and mechanical aspects, are analyzed via an arsenal of characterization techniques. Overall, Mn substitution appears far less effective than Al in suppressing active mass dissolution and irreversible phase transitions of the layered oxide cathodes. The active mass dissolution (and crossover) accelerates capacity decline with sustained parasitic reactions on the graphite anode, while the phase transitions are primarily responsible for cell resistance increase and voltage fade. With Al doping, on the other hand, secondary particle pulverization is the more limiting factor for long-term cyclability compared to Mn. Finally, these results establish a fundamental guideline for designing high-performing Ni-rich NCM cathodes as a compelling alternative to NCA and other compositions for electric vehicle applications.

25 ENERGY STORAGE↗

Extending the Service Life of High–Ni Layered Oxides by Tuning the Electrode–Electrolyte Interphase

As a high-energy-density cathode for Li-ion batteries, high-Ni layered oxides, especially with ultrahigh Ni-content, suffer from short lifespans, due in part to their unstable electrode–electrolyte interphase (EEI). Herein, the cycle life of LiNi 0.94 Co 0.06 O 2 is greatly extended by manipulating the EEI with a lithium bis(oxalate) (LiBOB) additive even when operated at a moderately high voltage (4.4 V vs Li/Li + ). Impressively, the capacity retention can be increased from 61 to 80% after 500 cycles in a full cell paired with a graphite anode. Additionally, the presence of LiBOB enables a robust boron- and oxygen-enriched EEI that effectively inhibits continual electrolyte decomposition and offers a stable cathode surface. Moreover, the layered architecture of the cathode–electrolyte interphase (CEI) and the anode–electrolyte interphase (AEI) at the nanometer scale is revealed by time-of-flight secondary ion mass spectrometry. It is demonstrated that the cathode surface chemistry can significantly influence the AEI both chemically and physically, and AEI is modified from a thick “three-layer” to a thin “two-layer” architecture by tuning the cathode surface chemistry with LiBOB. Finally, this work presents a correlation between the EEI characteristics and battery performance and highlights the significance of manipulating surface chemistry in developing stable high-energy-density Li-ion batteries.

25 ENERGY STORAGE↗

A Comprehensive Analysis of the Interphasial and Structural Evolution over Long–Term Cycling of Ultrahigh–Nickel Cathodes in Lithium–Ion Batteries

Ultrahigh-Ni layered oxides hold great promise as high-energy-density cathodes at an affordable cost for lithium-ion batteries, yet their practical application is greatly hampered by the poor cyclability. Herein, by employing LiNi 0.94 Co 0.06 O 2 as a model cathode in a full-cell configuration, the interphasial and structural evolution processes of ultrahigh-Ni layered oxides are systematically investigated over the course of their service life (1500 cycles). By applying advanced analytic techniques (e.g., Li-isotope labeling, region-of-interest method), the dynamic chemical evolution on the cathode surface is revealed with spatial resolution, and the correlation between lattice distortion and cathode surface reactivity is established. Benefiting from in situ X-ray diffraction (XRD) analysis, the ultrahigh-Ni layered oxide is demonstrated to undergo dual-phase reaction mechanisms with huge lattice variation, which leads to a decrease in crystallinity and secondary particle pulverization. Furthermore, the critical impact of cathode surface reaction on the graphite anode–electrolyte interphase (AEI) is revealed at nanometer scale, and a universal chemical/physical evolution process of the AEI is illustrated, for the first time. Finally, the practical viability of ultrahigh-Ni layered oxides is demonstrated through Al-doping strategy. Finally, this work presents a comprehensive understanding of the structural and interphasial degradation of ultrahigh-Ni layered oxide cathodes for developing high-energy-density lithium-ion batteries.

25 ENERGY STORAGE↗

Stabilized Co-Free Li-Rich Oxide Cathode Particles with An Artificial Surface Prereconstruction

Li-rich metal oxide (LXMO) cathodes have attracted intense interest for rechargeable batteries because of their high capacity above 250 mAh g –1 . However, the side effects of hybrid anion and cation redox (HACR) reactions, such as oxygen release and phase collapse that result from global oxygen migration (GOM), have prohibited the commercialization of LXMO. GOM not only destabilizes the oxygen sublattice in cycling, aggravating the well-known voltage fading, but also intensifies electrolyte decomposition and Mn dissolution, causing severe full-cell performance degradation. In this study, an artificial surface prereconstruction (ASR) for Li 1.2 Mn 0.6 Ni 0.2 O 2 particles with a molten-molybdate leaching is conducted, which creates a crystal-dense anion-redox-free LiMn 1.5 Ni 0.5 O 4 shell that completely encloses the LXMO lattice (ASR-LXMO). Differential electrochemical mass spectroscopy and soft X-ray absorption spectroscopy analyses demonstrate that GOM is shut down in cycling, which not only stabilizes HACR in ASR-LXMO, but also mitigates the electrolyte decomposition and Mn dissolution. ASR-LXMO displays greatly stabilized cycling performance as it retains 237.4 mAh g –1 with an average discharge voltage of 3.30 V after 200 cycles. More crucially, while the pristine LXMO cycling cannot survive 90 cycles in a pouch full-cell matched with a commercial graphite anode and lean (2 g A –1 h –1 ) electrolyte, ASR-LXMO shows high capacity retention of 76% after 125 cycles in full-cell cycling.

25 ENERGY STORAGE↗

Ethylene Carbonate–Free Electrolytes for Stable, Safer High–Nickel Lithium–Ion Batteries

Ethylene carbonate (EC) is an important component in state-of-the-art electrolytes for lithium-ion batteries (LIBs). However, EC is highly susceptible to oxidation on the surface of high-nickel layered oxide cathodes, making it undesirable for next-generation high-energy-density LIBs. In this study, a simple, yet effective, EC-free electrolyte (20F1.5M-1TDI) is presented by adding 20 wt% fluoroethylene carbonate (FEC) and 1 wt% lithium 4,5-dicyano-2-(trifluoromethyl)imidazole (LiTDI) into 1.5 M LiPF 6 in an ethyl methyl carbonate (EMC) electrolyte. The 20F1.5M-1TDI electrolyte is found to efficiently passivate the graphite anode and stabilize high-nickel cathodes by a synergistic decomposition of FEC and LiTDI. The LiNi 0.9 Mn 0.05 Al 0.05 O 2 (NMA90)/graphite full cell with the 20F1.5M-1TDI electrolyte, therefore, exhibits an enhanced cycling stability and a suppressed voltage hysteresis growth compared to that with an EC-containing baseline electrolyte (1 M LiPF 6 in EC:EMC, 3:7 in weight, with 2 wt% vinyl carbonate). Advanced analytical tools, such as time-of-flight secondary ion mass spectrometry and X-ray photoelectron spectroscopy, are employed to understand the underlying working mechanism of the EC-free electrolyte. Furthermore, the present study clearly showcases the great potential of EC-free electrolytes as a straightforward, practical approach for LIBs with high-nickel cathodes.

electrode/electrolyte interface↗

Overcoming the Intrinsic Limitations of Fast Charging Lithium‐Ion Batteries Using Integrated Acoustic Streaming

A lithium‐ion battery's maximum charge rate and energy density are intrinsically limited by the ion diffusion rate in the electrolyte. Most research focuses on materials science solutions to this problem, with gradual improvement over the years. A mechanical solution is proposed to integrate an MHz‐order frequency surface acoustic wave (SAW) device into an existing 1.8 Ah multilayered Li‐ion pouch cell to enhance the ion diffusion rate and the overall battery performance. Both the charging rate and cycling lifetime are improved from SAW. At a 6C (10 min) charge and C/3 discharge rate, typical of electric vehicle applications, integrating SAW into the Li‐ion cell doubles the energy density and maintains at least 72% of the battery's initial capacity after 2000 cycles. Moreover, using SAW quantifiably reduces battery degradation in these conditions as determined by optical imaging, scanning electron microscopy, X‐ray diffraction, and neutron diffraction. The use of SAW appears to offer a method to avoid undesirable Li metal plating on the graphite anode during charging, and leads to a much longer battery lifetime and good charge capacity, all despite rapid charging.

Huang, An↗

Irreparable Interphase Chemistry Degradation Induced by Temperature Pulse in Lithium‐Ion Batteries

Abstract While it is widely recognized that the operating temperature significantly affects the energy density and cycle life of lithium‐ion batteries, the consequence of electrode‐electrolyte interphase chemistry to sudden environmental temperature changes remains inadequately understood. Here, we systematically investigate the effects of a temperature pulse (T pulse) on the electrochemical performance of LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) pouch full cells. By utilizing advanced characterization tools, such as time‐of‐flight secondary‐ion mass spectrometry, we reveal that the T pulse can lead to an irreversible degradation of cathode‐electrolyte interphase chemistry and architecture. Despite negligible immediate impacts on the solid‐electrolyte interphase (SEI) on graphite anode, aggregated cathode‐to‐anode chemical crossover gradually degrades the SEI by catalyzing electrolyte reduction decomposition and inducing metallic dead Li formation because of insufficient cathode passivation after the T pulse. Consequently, pouch cells subjected to the T pulse show an inferior cycle stability to those free of the T pulse. This work unveils the effects of sudden temperature changes on the interphase chemistry and cell performance, emphasizing the importance of a proper temperature management in assessing performance.

Cui, Zehao↗

Irreparable Interphase Chemistry Degradation Induced by Temperature Pulse in Lithium–Ion Batteries

While it is widely recognized that the operating temperature significantly affects the energy density and cycle life of lithium-ion batteries, the consequence of electrode-electrolyte interphase chemistry to sudden environmental temperature changes remains inadequately understood. Here, we systematically investigate the effects of a temperature pulse (T pulse) on the electrochemical performance of LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) pouch full cells. By utilizing advanced characterization tools, such as time-of-flight secondary-ion mass spectrometry, we reveal that the T pulse can lead to an irreversible degradation of cathode-electrolyte interphase chemistry and architecture. Despite negligible immediate impacts on the solid-electrolyte interphase (SEI) on graphite anode, aggregated cathode-to-anode chemical crossover gradually degrades the SEI by catalyzing electrolyte reduction decomposition and inducing metallic dead Li formation because of insufficient cathode passivation after the T pulse. Consequently, pouch cells subjected to the T pulse show an inferior cycle stability to those free of the T pulse. Furthermore, this work unveils the effects of sudden temperature changes on the interphase chemistry and cell performance, emphasizing the importance of a proper temperature management in assessing performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Degradation Diagnostics from the Subsurface of Lithium-Ion Battery Electrodes

Despite the long-established rocking-chair theory of lithium-ion batteries (LIBs), developing novel characterization methodology with higher spatiotemporal resolution facilitates a better understanding of the solid electrolyte interphase studies to shape the reaction mechanisms. In this work, we develop a Xenon ion plasma focused ion beam (Xe + PFIB)-based characterization technique to probe the cross-sectional interface of both ternary cathode and graphite anode electrodes, with the focus on revealing the chemical composition and distribution underneath the electrode surface by in-depth analysis of secondary ions. Particularly, the lithium fluoride is detected in the pristine cathode prior to contact with the electrolyte, reflecting that the electrode degradation is in the form of the loss of lithium inventory during electrode preparation. This degradation is related to the hydrolysis of the cathode material and the decomposition of the PVDF binder. Here, through the quantitative analysis of the transition-metal degradation products, manganese is found to be the dominant element in the newly formed inactive fluoride deposition on the cathode, while no transition metal signal can be found inside the anode electrode. These insights at high resolution implemented via a PFIB-based characterization technique not only enrich the understanding of the degradation mechanism in the LIBs but also identify and enable a high-sensitivity methodology to obtain the chemical survey at the subsurface, which will help remove the capacity-fade observed in most LIBs.

25 ENERGY STORAGE↗

Solvent-Free Manufacturing of Lithium-Ion Battery Electrodes via Cold Plasma

Slurry casting has been used to fabricate lithium-ion battery electrodes for decades, which involves toxic and expensive organic solvents followed by high-cost vacuum drying and electrode calendering. This work presents a new manufacturing method using a nonthermal plasma to create inter-particle binding without using any polymeric binding materials, enabling solvent-free manufacturing electrodes with any electrochemistry of choice. The cold-plasma-coating technique enables fabricating electrodes with thickness (>200 μm), high mass loading (>30 mg cm -2 ), high peel strength, and the ability to print lithium-ion batteries in an arbitrary geometry. This crosscutting, chemistry agnostic, platform technology would increase energy density, eliminate the use of solvents, vacuum drying, and calendering processes during production, and reduce manufacturing cost for current and future cell designs. Here, lithium iron phosphate and lithium cobalt oxide were used as examples to demonstrate the efficacy of the cold-plasma-coating technique. It is found that the mechanical peel strength of cold-plasma-coating-manufactured lithium iron phosphate is over an order of magnitude higher than that of slurry-casted lithium iron phosphate electrodes. Full cells assembled with a graphite anode and the cold-plasma-coating-lithium iron phosphate cathode offer highly reversible cycling performance with a capacity retention of 81.6% over 500 cycles. For the highly conductive cathode material lithium cobalt oxide, an areal capacity of 4.2 mAh cm -2 at 0.2 C is attained. We anticipate that this new, highly scalable manufacturing technique will redefine global lithium-ion battery manufacturing providing significantly reduced plant footprints and material costs.

25 ENERGY STORAGE↗

Artificial cathode electrolyte interphase for improving high voltage cycling stability of thick electrode with Co-free 5 V spinel oxides

Spinel-type cathode LiNi 0.5 Mn 1.5 O 4 (LNMO) has intrigued the transportation industry due to its high operating voltage and total elimination of the expensive cobalt element. However, LNMO cathode with high mass loading (> 3 mAh/cm 2 in areal capacity) has suffered from excessive capacity degradation upon long cycling. Here, a robust Al 2 O 3 surface layer is introduced to the thick LNMO electrode via atomic layer deposition (ALD). The capacity retention in full cells with the graphite anode is improved from 46.3% to 75.3% after 300 cycles with cutoff voltage up to 4.85 V, while enabling average Coulombic efficiency of 99.9% during the cycling. The post-mortem analyses reveal that the Al 2 O 3 surface layer would convert to Al-O-F /Al-F species upon cycling, offering stable interphase to protect the cathode material. Furthermore, these results demonstrate the significance of surface modification enabling high voltage cathode for next-generation LIBs.

25 ENERGY STORAGE↗

Characterizing Hazardous Gases from NMC811 Materials and Coin Cells with TGA and Tube-Furnace FTIR-MS Evolved-Gas-Analysis

Abuse testing is useful for informing the risks of different battery chemistries but has been limited to larger formats. This paper conducted thermal abuse tests at the smaller coin cell level to determine its relevance in specifying vent gas flammability and toxicity. A nitrogen purge carried the evolved gases into a parallel Fourier-transform infrared spectrometer (FTIR) and a mass spectrometer (MS) downstream of the tube furnace. The experimental system was validated by comparing evolved gas data for single components between the tube furnace system and a thermogravimetric analysis (TGA) instrument. Multiple samples were tested during validation, including CaCO3, electrolyte, delithiated NMC 811 cathode, and lithiated graphite anode. Temperature-resolved gas evolution of HF, CO2, CO, H2, and hydrocarbons from isolated components helped to characterize the emission sources. A previously unreported H2 generation mechanism was found. It was shown that the reduced NMC cathode acts as a catalyst to crack polypropylene-decomposed hydrocarbons into H2 at around 450 degrees C. It was also shown, while studying LiPF6 thermal decomposition, that using the tube furnace with a coin cell casing as the sample holder has some advantages for evolved-gas analysis of environmentally sensitive samples relative to testing in TGA instruments. After validation with single components, a fully charged NMC 811 coin cell was failed in the tube furnace. The measured evolved gases were found to be a combination of the species measured from the single component tests. H2 formation related to the reduced cathode was found to have greater abundance than H2 formed from the anode. Hydrogen fluoride emission factors and diethyl carbonate conversion emission factors assist in understanding the gaseous hazards for larger format cells.

25 ENERGY STORAGE↗

A control oriented comprehensive degradation model for battery energy storage system life prediction

In order to ensure that stationary battery energy storage systems (BESSs) provide reliable energy buffering, both for power quality and economic purposes, the degradation must be considered. Cell degradation involves various side reactions and is highly dependent on its operating conditions. To accurately track cell degradation and predict its impact on battery behavior, a comprehensive physics-based degradation model based on an electrolyte phase-enhanced single particle (SP) model is developed. Key degradation physics, namely solid electrolyte interphase (SEI) layer formation and growth, Li plating on the graphite anode, and Mn dissolution on cathode of nickel-cobalt-manganese oxide (NMC622) are considered. The model is validated against experimental capacity data. The results reveal that the deposition rate of both SEI layer and Li metal increase as the charge voltage increases. At the cathode side, the solvent oxidation rate determines the Mn dissolution rate. As a result, the volume fraction of NMC622 in the cathode continually decreases at a gradually increasing rate.

25 ENERGY STORAGE↗