Search NASA⌕ Search

SEARCH · Search NASA

Results for “interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

The Role of Oxygen in Lithiation and Solid Electrolyte Interphase Formation Processes in Silicon-Based Anodes

Silicon oxides (SiO x ) have been considered as promising alternatives to pure Si in high energy anodes in lithium-ion batteries (LIBs) due to their improved cycling stability. However, their fundamental lithiation mechanism has not yet been systematically investigated, and potential collateral downsides remain unclear. In this work, we report on the role of oxygen in lithiation/delithiation and solid electrolyte interphase (SEI) formation processes in SiO x thin film model electrodes with different oxygen contents. Here, we show that the SiO x anodes with higher oxygen content experience smaller volume change and form a thinner and more stable SEI, both of which are beneficial for cycling stability. However, these SiO x anodes also show an irreversible lithiation at around 0.7 V attributed to the reduction of Si oxides, leading to lower first cycle coulombic efficiency that is undesirable for practical applications. Overall, these results offer a balanced perspective on the advantages and disadvantages that oxygen brings to Si-based anodes in LIBs.

25 ENERGY STORAGE↗

Highly Quantitative Electrochemical Characterization of Non-Aqueous Electrolytes & Solid Electrolyte Interphases

The methods to measure solid electrolyte interphase (SEI) electrochemical properties and SEI formation capability of non-aqueous electrolyte solutions are not adequately addressed in the literature. And yet, there is a strong demand in new electrolyte generations that promote stabilized SEIs and have an influence to resolve safety, calendar life and other limitations of Li-ion batteries. To fill this gap, in situ electrochemical approach with new descriptive criteria for highly quantitative characterization of SEI and electrolytes is proposed. These criteria are: SEI formation capacity, SEI corrosion rate, SEI maintenance rate, and SEI kinetic stability. These criteria are associated with battery parameters like irreversible capacity, self-discharge, shelf-life, power, etc. Therefore, they are especially useful for electrolyte development and standard fast screening, allowing a skillful approach to narrow down the search for the best electrolyte. The characterization protocol also allows retrieving information on interfacial resistance for SEI layers and the electrochemical window of electrolytes, the other important metrics of characterization. The method validation was done on electrolyte blends containing phosphazenes, developed at Idaho National Laboratory, as 1.2M LiPF6 [80 % EC-MEC (2:8) (v/v) + 20% Phosphazene variety] (v/v), which were targeted for safer electrolyte variations.

25 ENERGY STORAGE↗

Intrinsic Properties of Individual Constituents of Silicon-Electrolyte Interphase

The stabilization of a solid electrolyte interphase (SEI) is one of the great challenges to utilize superior theoretical capacity (about 3,600 mAh g-1, almost 10 times higher than that of graphite) of a silicon (Si) as an anode in a next-generation advanced lithium-ion battery (LIB). A SEI remains a poorly understood and hardly studied topic relative to the research devoted to battery components due to its intrinsic properties of complexity, reactivity and continuous evolution. However, the SEI plays a key role in prevention of further electrolyte reduction and desolvation of Li+ ions, which is directly related to electrochemical performance, lifetime and safety of batteries. For example, the unstable SEI on a Si anode leads to initial irreversible capacity losses, poor cycling stability and a limited cycle life. 2-4 In this study each 'individual' component of SEI on a Si anode was prepared as a thin film, and the physical, electrochemical, mechanical and structural properties of prepared films were characterized using a variety of analytical equipment including electrochemical impedance spectroscopy, operando X-ray photoelectron spectroscopy, atomic force microscope, Fourier-transform infrared spectroscopy, scanning spreading resistance microscopy and time-of-flight secondary ion mass spectrometry. This study can provide a strong guidance to aid in the development of new electrolytes, additives and binders to stabilize SEI layer on a silicon anode by identifying beneficial components and providing mechanical explanation of a variety of reactions and phenomena in a SEI.

14 SOLAR ENERGY↗

Understanding Solid-Electrolyte Interphase Formation at the Lithium Metal Anode of Lithium-Sulfur Batteries

Lithium-sulfur (Li-S) batteries are one of the most promising chemistries for the next generation of energy storage devices. In a standard Li-S cell, the metallic lithium anode is an essential component of the battery due to its low density, extremely high theoretical specific capacity, and very low negative electrochemical potential. However, several challenges related to the use of Li metal have prevented this battery technology from becoming commercially available. For instance, Li-anodes are highly reactive, which results in the continuous decomposition of the electrolyte and the formation of the solid-electrolyte interphase (SEI) layer. This, combined with the non-uniform deposition of Liions during plating at the anode surface, can seriously affect the performance, cycling, and safety of the battery. In addition, it has been suggested that a controlled SEI formation at the metallic Li anode can yield enhanced battery performance. Hence, a comprehensive understanding of how the SEI layer is formed can help elucidate improvements in this battery technology. In this work, the formation of the SEI layer in Li-S batteries is investigated using density functional theory (DFT) and ab initio molecular dynamics (AIMD) simulations. The stability of liquid organic-based electrolyte components, salt concentration, electron-rich environments, and the use of inorganic solid-state electrolyte (SSE) materials are explored in order to provide molecular-level fundamental insights into how the nature and composition of the electrolyte can alter the initial stages of the SEI formation. The products of electrolyte decomposition and electro-/chemical reaction pathways of liquid electrolyte component such as solvent and salts are predicted from AIMD simulations of electrolyte-anode interfaces. Energetics of reactions from DFT ground-state optimizations are also presented to confirm the decomposition mechanisms. Some significant differences are then drawn regarding the use of low and high salt concentrations. Simulations under electron-rich environments show additional multielectron electrochemical reactions of solvent and salt decomposition taking place due to the excess of electrons and the presence of radical anions in the solution. Finally, the initial stages of formation, stability, and main constituents of interfaces between Li-metal and Sbased electrodes with sulfide-based SSEs are characterized in detail.

25 ENERGY STORAGE↗

In Situ Ion‐Exchange Metathesis Induced Conformal LiF Surface Films on Cathode (NMC811) as a Cathode Electrolyte Interphase

High-capacity cathodes (LiNi 0.8 Mn 0.1 Co 0.1 O 2 , NMC811) are promising for vehicle electrification because of their high gravimetric energy density. However, their electrochemical performance still relies upon the stability of the cathode electrolyte interphase (CEI). A highly reactive cathode interface leads to parasitic side reactions with electrolytes, resulting in accelerated capacity fading. Well-developed LiF and LiF-like inorganic compounds are believed to be good CEI components for stabilizing such reactive electrode interfaces. However, it is challenging to form an optimal surface sub-nanolayer of LiF on the cathode surfaces because of the complexity of the electrochemical reaction during battery cycling. Herein, the formation of a conformal LiF layer on the NMC811 electrode surface via an in situ ion-exchange metathesis process is reported, demonstrating a promising electrochemical performance because of a LiF-stabilized CEI. In situ generated LiF-coated NMC811 electrodes exhibit ≈97% capacity retention up to 100 cycles at a 0.3 C rate with average coulombic efficiency of ≈99.9% and ≈80% capacity retention up to 200 cycles at a 1 C rate with average coulombic efficiency of >99.6%. This finding may pave the way for reengineering the CEI to enhance the electrochemical performances and cycling stability of the high-capacity cathodes.

25 ENERGY STORAGE↗

3D Artificial Solid-Electrolyte Interphase for Lithium Metal Anodes Enabled by Insulator–Metal–Insulator Layered Heterostructures

Despite considerable efforts to prevent lithium (Li) dendrite growth, stable cycling of Li metal anodes with various structures remains extremely difficult due to the direct contact of the liquid electrolyte with Li. Rational design of solid-electrolyte interphase (SEI) for 3D electrodes is a promising but still challenging strategy for preventing Li dendrite growth and avoiding lithium–electrolyte side reactions in Li-metal batteries. Here, a 3D architecture is constructed with g-C 3 N 4 /graphene/g-C 3 N 4 insulator–metal–insulator sandwiched nanosheets to guide uniform Li plating/stripping in the van der Waals gap between the graphene and the g-C 3 N 4 , and the function of which can be regarded as a 3D artificial SEI. Li deposition on the surface of g-C 3 N 4 is suppressed due to its insulating nature. However, its uniform lithiophilic sites and nanopore channels enable homogeneous lithium plating between the graphene and the g-C 3 N 4 , prohibiting the direct contact of the electrolyte with the Li metal. The use of the g-C 3 N 4 -layer-modified 3D anode enables long-term Li deposition with a high Coulombic efficiency and stable cycling of full cells under high cathode loading, limited Li excess, and lean electrolyte conditions. The concept of a 3D artificial SEI will shed light on developing safe and stable Li-metal anodes.

25 ENERGY STORAGE↗

Delineating the Impact of Transition‐Metal Crossover on Solid‐Electrolyte Interphase Formation with Ion Mass Spectrometry

Abstract Lithium‐metal batteries (LMB) employing cobalt‐free layered‐oxide cathodes are a sustainable path forward to achieving high energy densities, but these cathodes exhibit substantial transition‐metal dissolution during high‐voltage cycling. While transition‐metal crossover is recognized to disrupt solid‐electrolyte interphase (SEI) formation on graphite anodes, experimental evidence is necessary to demonstrate this for lithium‐metal anodes. In this work, advanced high‐resolution 3D chemical analysis is conducted with time‐of‐flight secondary‐ion mass spectrometry (TOF‐SIMS) to establish spatial correlations between the transition metals and electrolyte decomposition products found on cycled lithium‐metal anodes. Insights into the localization of various chemistries linked to crucial processes that define LMB performance, such as lithium deposition, SEI growth, and transition‐metal deposition are deduced from a precise elemental and spatial analysis of the SEI. Heterogenous transition‐metal deposition is found to perpetuate both heterogeneous SEI growth and lithium deposition on lithium‐metal anodes. These correlations are confirmed across various lithium‐metal anodes that are cycled with different cobalt‐free cathodes and electrolytes. An advanced electrolyte that is stable to higher voltages is shown to minimize transition‐metal crossover and its effects on lithium‐metal anodes. Overall, these results highlight the importance of maintaining uniform SEI coverage on lithium‐metal anodes, which is disrupted by transition‐metal crossover during operation at high voltages.

Chemistry↗

Direct Visualization of the Solid Electrolyte Interphase and Its Effects on Silicon Electrochemical Performance

Fluoroethylene carbonate (FEC) as an electrolyte additive can considerably improve the cycling performance of silicon (Si) electrodes in Li‐ion batteries. However, the fundamental mechanism for how FEC contributes to solid electrolyte interphase (SEI) morphological changes and chemical composition is not well understood. Here, scanning transmission electron microscopy coupled with electron energy loss spectroscopy gives a comprehensive insight as to how FEC affects the SEI evolution in terms of composition and morphology throughout electrochemical cycling. In the first lithiation cycle, the electrode cycled in ethylene carbonate (EC): diethylene carbonate (DEC) forms a porous uneven SEI composed of mostly Li 2 CO 3 . However, the electrode cycled in EC/DEC/FEC is covered in a dense and uniform SEI containing mostly LiF. Interestingly, the intrinsic oxide layer (Li x SiO y ) is not observed at the interface of electrode cycled in EC/DEC/FEC after 1 cycle. This is consistent with fluoride anion formation from the reduction of FEC, which leads to the chemical attack of any silicon‐oxide surface passivation layer. Furthermore, surface sensitive helium ion microscopy and X‐ray photoelectron spectroscopy techniques give further insights to the SEI composition and morphology in both electrodes cycled with different electrolytes.

Sina, Mahsa↗

Preventing Electrolyte Decomposition on a Ca Metal Electrode Interface Using an Artificial Solid‐Electrolyte Interphase

Abstract Calcium ion batteries are gaining attention as alternatives to lithium‐ion technology because they offer comparable properties at reduced cost and improved safety. However, progress has been limited because of the inability to efficiently and reversibly plate and strip Ca metal anodes in organic electrolytes. Moreover, the inorganic components of the solid‐electrolyte interphase (SEI) that form via decomposition of the electrolyte often do not allow for the diffusion of Ca ions. In this work, an approach combining density functional theory and ab initio molecular dynamics (AIMD) simulations is utilized to show that the use of a preformed artificial SEI layer of amorphous can potentially prevent electrolyte decomposition. First, Ca is shown to be able to intercalate into an amorphous layer (up to Ca 1.5 Al 2 O 3 ) and diffuse through on a reasonable time scale. Through calculation of the density of states, the system is found to remain insulating up to the equilibrium stoichiometry. Finally, AIMD simulations with a realistic organic electrolyte environment are used to show that this calcinated layer completely prevents the decomposition of solvent molecules. This approach can provide a route to efficient rechargeable Ca ion batteries, paving the way for cheap large‐scale energy storage.

Young, Joshua↗

In Situ Measurement of Solid Electrolyte Interphase Evolution on Silicon Anodes Using Atomic Force Microscopy

In situ measurements of the growth of solid electrolyte interphase (SEI) layer on silicon and the lithiation-induced volume changes in silicon in lithium ion half-cells are reported. Thin film amorphous silicon electrodes are fabricated in a configuration that allows unambiguous separation of the total thickness change into contribution from SEI thickness and silicon volume change. Electrodes are assembled into a custom-designed electrochemical cell, which is integrated with an atomic force microscope. The electrodes are subjected to constant potential lithiation/delithiation at a sequence of potential values and the thickness measurements are made at each potential after equilibrium is reached. Experiments are carried out with two electrolytes—1.2 m lithium hexafluoro-phosphate (LiPF6) in ethylene carbonate (EC) and 1.2 m LiPF6 in propylene carbonate (PC)—to investigate the influence of electrolyte composition on SEI evolution. It is observed that SEI formation occurs predominantly during the first lithiation and the maximum SEI thickness is ≈17 and 10 nm respectively for EC and PC electrolytes. This study also presents the measured Si expansion ratio versus equilibrium potential and charge capacity versus equilibrium potential; both relationships display hysteresis, which is explained in terms of the stress–potential coupling in silicon.

36 MATERIALS SCIENCE↗

Electrolytes Polymerization‐Induced Cathode‐Electrolyte‐Interphase for High Voltage Lithium‐Ion Batteries

Abstract Lithium‐ion batteries (LIBs) based on LiNi x Co y Mn 1‐x‐y O 2 (NCM) cathode materials have been widely commercialized, because of their high energy density, favorable rate performance, and relatively low cost. However, with increased Ni content to further increase their energy density, their cycling stability deteriorates dramatically and thus fails to meet the commercial application requirements. The artificial cathode‐electrolyte‐interphase (CEI) is a promising approach to solve this problem. Here, a robust CEI is fabricated through in situ polymerization of ethylene carbonate induced by aluminum isopropoxide (AIP). By adding 1 wt.% AIP in a commercial electrolyte, the capacity retention of LiNi 0.8 Co 0.1 Mn 0.1 O 2 ||Li cell at 1 C rate has been significantly increased from 80.8% to 97.8% with a highly reversible capacity of 176 mA h g −1 after 200 cycles. AIP can be also used as an additive during the slurry‐making process, enabling a reversible capacity of 170 mA h g −1 for LiCoO 2 after 200 cycles even at a high charge cut‐off voltage of 4.6 V. It is confirmed that the in situ formed CEI layer can prevent the cathodes from cracking and reduce the irreversible phase transformation.

Yang, Jixiang↗

A Solution-Processable High-Modulus Crystalline Artificial Solid Electrolyte Interphase for Practical Lithium Metal Batteries

The solid electrolyte interphase (SEI) has been identified as a key challenge for Li metal anodes. The brittle and inhomogeneous native SEI generated by parasitic reactions between Li and liquid electrolytes can devastate battery performance; therefore, artificial SEIs (ASEIs) have been proposed as an effective strategy to replace native SEIs. Herein, as a collaboration between academia and industrial R&D teams, a multifunctional (crystalline, high modulus, and robust, Li + ion conductive, electrolyte-blocking, and solution processable) ASEI material, LiAl-FBD (where “FBD” refers to 2,2,3,3-tetra-fluoro-1,4-butanediol), for improving Li metal battery performance is designed and synthesized. The LiAl-FBD crystal structure consists of Al 3+ ions bridged by FBD 2– ligands to form anion clusters while Li + ions are loosely bound at the periphery, enabling an Li + ion conductivity of 9.4 × 10 –6 S cm –1 . Further, the fluorinated, short ligands endow LiAl-FBD with electrolyte phobicity and high modulus. The ASEI is found to prevent side reactions and extend the cycle life of Li metal electrodes. Specifically, pairing LiAl-FBD coated 50 μm thick Li with industrial 3.5 mAh cm –2 NMC811 cathode and 2.8 μL mAh –1 lean elec-trolyte, the Li metal full cells show superior cycle life compared to bare ones, achieving 250 cycles at 1 mA cm –2 .

25 ENERGY STORAGE↗

Solvent‐Phobic and Ionophilic Carboxylated Polythiophene Layer for Fluoride‐Rich Cathode Electrolyte Interphase

Abstract One focal area of contemporary organic mixed ionic‐electronic conductor (OMIEC) research relates to utilization of dual‐conductive properties to enhance the ion/electron transfer kinetics for energy storage applications. Insight regarding OMIEC response toward the electrolyte anion and solvent used in lithium‐ion batteries (LIBs), however, is limited. Here, for the first time, the solvent‐phobic and ionophilic (SP‐IP) properties of the OMIEC, poly[3‐(potassium‐4‐butanoate)thiophene‐2,5‐diyl] (P3KBT), are revealed through comprehensive evaluation and characterization. The solvent‐phobic characteristics arise from the cooperation of dispersive interaction, polar interaction, and hydrogen‐bonding between P3KBT and electrolyte solvent. The ionophilic nature is driven by electrostatic interactions between P3KBT side chain carboxylate groups and LiPF 6 , and the reversible electrochemical doping/de‐doping of the polythiophene backbone with PF 6 ⁻ . The SP‐IP properties induce formation of a LiF‐ rich , Li 2 CO 3 ‐ limited cathode electrolyte interphase (CEI) layer when a P3KBT coating layer is applied to the active material surface, significantly improving half‐cell life to over 1500 cycles at 2C.

Ren, Haoze [Department of Chemical and Bimolecular↗

Floatable Protective Layers: a Strategy to Minimize Solid Electrolyte Interphase Growth and Maximize the Lithium Utilization

Abstract Maximizing lithium (Li) utilization is crucial for enhancing the long‐term stability of Li‐based batteries. In anode‐free Li batteries (AFLBs), although the initial formation of solid electrolyte interphase (SEI) is beneficial on limiting further reaction between Li and electrolyte, large volume change of Li metal anode (LMA) during cycling often leads to continuous breakdown and re‐formation of SEI and formation of inactive Li, hindering its efficiency. In this study, a novel strategy is presented to protect Li metal by applying a floatable protection layer (FPL) on a copper substrate, enabling large Li particles to be primarily deposited below FPL, but SEI to be primarily formed above FPL. This approach effectively minimizes the direct contact between electrolyte and freshly deposited Li, therefore mitigating the continuous side reactions and early failure of AFLBs. As a result, Li consumption is minimized, and the overall stability of the battery is significantly enhanced. Further development of this approach can also be used to improve the performance of other Li‐based batteries for large‐scale applications.

Lim, Hyung‐Seok [Energy and Environment Directorat↗

An Inorganic‐Rich Solid Electrolyte Interphase for Advanced Lithium‐Metal Batteries in Carbonate Electrolytes

Abstract In carbonate electrolytes, the organic–inorganic solid electrolyte interphase (SEI) formed on the Li‐metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here, an inorganic‐rich SEI is designed on a Li‐metal surface to reduce its bonding energy with Li metal by dissolving 4 m concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene‐carbonate (FEC)‐based electrolyte. Due to the aggregate structure of NO 3 − ions and their participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 − ions. The weak bonding of the SEI (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping Coulombic efficiency of 99.55 % (1 mA cm −2 , 1.0 mAh cm −2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm −2 ) to retain 75 % of its initial capacity after 200 cycles with an outstanding CE of 99.83 %.

Liu, Sufu↗

Solid‐Adsorbed Polymer‐Electrolyte Interphases for Stabilizing Metal Anodes in Aqueous Zn and Non‐Aqueous Li Batteries

Abstract Polymers are known to adsorb spontaneously from liquid solutions in contact with high‐energy substrates to form configurationally complex, but robust phases that often exhibit higher durability than might be expected from the individual physical bonds formed with the substrate. Rational control of the physical, chemical, and transport properties of such interphases has emerged as a fundamental opportunity for scientific and technological advances in energy storage technology but requires in‐depth understanding of the conformation states and electrochemical effect of the adsorbed polymers. Here, we analyze the interfacial adsorption of oligomeric polyethylene glycol (PEG) chains of moderate sizes dissolved in protic and aprotic liquid electrolytes and find that there is an optimum polymer molecular weight of approximately 400 Da at which the highest columbic efficiency is achieved for both Zn and Li deposition. These findings point to a simple, versatile approach for extending the lifetime of batteries.

Jin, Shuo↗

Impacts of Dissolved Ni 2+ on the Solid Electrolyte Interphase on a Graphite Anode

Transition metal (e.g. Ni) ions dissolved from layered-structured Ni-rich cathodes can migrate to the anode side and accelerate the failure of lithium-ion batteries. The investigations of the impact and distribution of Ni species on the solid electrolyte interphase (SEI) on the anode are crucial to understand the failure mechanism. Herein, we used time-of-flight secondary ion mass spectroscopy (TOF-SIMS) coupled with multivariate curve resolution (MCR) analysis to intuitively characterize the distribution of Ni species in the SEI. We find that the SEI on the graphite electrode using an EC-based electrolyte exhibits a multi-stratum structure. During accelerated aging of the LiNi 0.88 Co 0.08 Mn 0.04 O 2 /graphite full cell, the dissolution of Ni aggravates significantly upon cycling. A strong correlation between the dissolved-Ni and organic species in the SEI on graphite is illustrated. Here, the ion-exchange reaction between Ni 2+ and Li + ions in the SEI is demonstrated to be the main reason for the increase of SEI resistivity.

25 ENERGY STORAGE↗

Solid–Adsorbed Polymer–Electrolyte Interphases for Stabilizing Metal Anodes in Aqueous Zn and Non–Aqueous Li Batteries

Polymers are known to adsorb spontaneously from liquid solutions in contact with high-energy substrates to form configurationally complex, but robust phases that often exhibit higher durability than might be expected from the individual physical bonds formed with the substrate. Rational control of the physical, chemical, and transport properties of such interphases has emerged as a fundamental opportunity for scientific and technological advances in energy storage technology but requires in-depth understanding of the conformation states and electrochemical effect of the adsorbed polymers. Here, we analyze the interfacial adsorption of oligomeric polyethylene glycol (PEG) chains of moderate sizes dissolved in protic and aprotic liquid electrolytes and find that there is an optimum polymer molecular weight of approximately 400 Da at which the highest columbic efficiency is achieved for both Zn and Li deposition. Furthermore, these findings point to a simple, versatile approach for extending the lifetime of batteries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗