Search NASA⌕ Search

SEARCH · Search NASA

Results for “scanning electron microscopy (SEM)”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Effect of temperature on abrasion erosion in particle based concentrating solar powerplants

The use of solid particles as a heat transfer medium is being explored for concentrated solar power plants (CSP) to increase their efficiency by achieving operating temperature >700 °C. During operation, these hot particles are expected to move along the various components within the collector system, resulting in material degradation from a combination of high-temperature oxidation and erosion. In the present study, the performance of candidate materials was evaluated through a series of abrasion erosion experiments at room temperature as well as at 800 °C. Wear in metallic and refractory type materials was investigated using CarboBead® HSP 40/70 particles inside a resistance heated kiln. Furthermore, cross-sectional scanning electron microscopy (SEM) and energy dispersive x-ray spectroscopy (EDS) analysis on the specimens tested at 800 °C determined that the specific wear rate in Inconel 740H and stainless steel 316 metallic specimens was influenced by the thermally grown oxide morphology. High chromium Inconel 740H specimens exhibited greater resistance to wear with a steady state specific wear rate of 1.92E-4 mm 3 N -1 m –1 compared to 5.7E-3 mm 3 N -1 m –1 for Stainless Steel 316.

14 SOLAR ENERGY↗

Field retrieved photovoltaic backsheet survey from diverse climate zones: Analysis of degradation patterns and phenomena

Understanding the impact of climate stressors on photovoltaic (PV) backsheet degradation in real-use conditions is critical to improve the accelerated testing exposures, extend the backsheet lifetime, and increase the confidence in PV reliability. Here, in this work, a total of 33 PV module backsheets were retrieved from six climatic zones worldwide with 2 - 28 years of exposure. These modules included five types of backsheet air-side materials (or outer layer): poly(vinylidene fluoride) (PVDF), poly(tetrafluoroethylene-co-hexafluoropropylene-co-vinylidene fluoride) (THV), poly(vinyl fluoride) (PVF), poly(ethylene terephthalate) (PET), and polyamide (PA). Attenuated total reflection Fourier-transform infrared spectroscopy (ATR-FTIR) was used to identify air-side materials. The degradation induced color change, gloss loss, and chemical material changes analyzed using optical microscopy, differential scanning calorimetry (DSC), scanning electron microscopy (SEM), colorimetry (yellowness index (YI)), and gloss measurements. PVDF, THV, and PVF air-side layer backsheets, in particular PVF, had minimal degradation in the air-side layer appearance and chemical structures after exposure in different climatic zones. The PET air-side backsheets exhibited obvious color increase (22.55 YI units after about 9 years exposure) and the PA/PA/PA backsheets showed large gloss loss (up to 76.4 %) relative to the unexposed backsheets. Severe cracks between cells that penetrated through the entire thickness of backsheets are observed on PA/PA/PA backsheets after 4-6 years of exposure in 6 climatic zones. The current indoor exposure standards were not sufficient to identify this degradation type. However, fluoropolymer based PV backsheets showed lower levels of degradation predictors and increased climatic resistance. Specific samples (PVF) showed little change from baseline after 28 years of outdoor exposure.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Characterization of front contact degradation in monocrystalline and multicrystalline silicon photovoltaic modules following damp heat exposure

Reliability and durability tests play a key role in the photovoltaic (PV) industry by minimizing potential failure risks for both existing and new cell and module technologies. In this work, a detailed study of contact degradation in monocrystalline and multicrystalline PV modules is performed. The modules are subjected to a sequence of damp heat (DH) exposures followed by electrical characterization after each step. Electroluminescence (EL) imaging shows different darkening patterns for monocrystalline modules compared to multicrystalline modules; the former shows darkening near the busbars and the latter shows it across virtually the entire cell surface. The primary loss mechanism is confirmed to be resistive after comparing the current-voltage (I–V) characteristics at each DH exposure step. Representative samples have been cored out from both the degraded modules and controls for materials characterization to gain further insights into the degradation mechanism. Top-down and cross-sectional scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and top-down high-resolution X-ray photoelectron spectroscopy (XPS) analysis performed on the cored samples confirm the degradation is due to metallization corrosion. Our study suggests that the difference in the darkening pattern can most likely be attributed to the different silver paste composition used for contacting each cell technology, particularly the composition of the glass frit.

36 MATERIALS SCIENCE↗

Impact of acetic acid exposure on metal contact degradation of different crystalline silicon solar cell technologies

Degradation due to acetic acid in photovoltaic (PV) modules has been a commonly observed phenomenon for both damp-heat exposure and outdoor operations. Acetic acid is a degradation byproduct of ethylene-vinyl acetate (EVA), a common module encapsulant. To address this issue, robust metallization pastes and cell technologies are being developed. However, it is important to assess how these technologies perform in an acetic acid environment and withstand degradation before they are implemented in the solar market. In this work, we investigate the impact of acetic acid exposure on four different cell groups: monofacial passivated emitter and rear contact (PERC) cells with advanced telluride-based front contact pastes, bifacial PERC cells with novel aluminum rear contact pastes, bifacial tunnel oxide passivated contacts (TOPCon) cells, and silicon heterojunction (SHJ) cells. These cells were exposed to acetic acid for different time increments. The recombination losses were characterized by Suns-VOC, and multi-variate regression analysis of intensity-dependent photoluminescence (PL) images with Griddler AI. Resistive losses were tracked with the transmission line method (TLM). Samples showing severe performance degradation were selected for further materials characterization to understand the root cause. Top-down and cross-sectional scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and X-ray photoelectron spectroscopy (XPS) were performed to investigate the change in materials properties. Our study shows that the front contacts of the bifacial TOPCon cells and monofacial PERC cells were significantly affected by acetic acid exposure. Here, the SHJ cells were found to be the most stable.

14 SOLAR ENERGY↗

Innovative recycling of high purity silver from silicon solar cells by acid leaching and ultrasonication

Precious and scarce silver (Ag) is used as a front electrical contact in silicon solar panels. With massive amounts of solar panel waste coming to end-of-life, it is imperative to recover all the Ag from these modules. In this paper, we propose a novel method to easily reclaim Ag from end-of-life silicon solar cells using low concentration sulfuric acid (H 2 SO 4 ) leaching followed by ultrasonication. Our process simplifies the Ag recycling procedure by directly recovering the Ag contacts from solar cells, eliminating the need for secondary precipitation/electrodeposition. First, scanning electron microscopy (SEM) with energy dispersive X-ray spectroscopy (EDX) and X-ray photoelectron spectroscopy (XPS) was used to study the leaching and ultrasonication process on rejected solar wafers. Next, a solar panel from landfill was heated in a furnace to burn off the polymer encapsulant. The silicon wafers were then collected from the burning process and leached in 2 M H 2 SO 4 at two different shaking speeds for 48 hours at room temperature. Finally, the end-of-life silicon wafer pieces were collected, sonicated in water, and then the sonication water was centrifuged to show a proof-of-concept to recover the Ag contacts. Inductively coupled plasma optical emission spectroscopy (ICPOES) is used to monitor dissolved elements in the leachate as a function of time and shaking speed. XPS is used to evaluate the composition of the silicon cell wafer surface before and after H 2 SO 4 leaching. SEM is used to image the recovered Ag contacts morphology and EDX confirms the recovered particles contain high amounts of Ag. Furthermore, a proposed schematic illustrates the authors’ hypothesis for the peeling mechanism.

14 SOLAR ENERGY↗

Effect of CMAS viscosity on the infiltration depth in thermal barrier coatings of different microstructures

Calcium magnesium aluminum silicate (CMAS) is one of the leading concerns for the gas turbine industry. The effects of CMAS viscosity and the coating microstructure on CMAS infiltration depth were explored by conducting a time dependent interaction study. Three CMAS compositions were used from literature, and their viscosities predicted through FactSage viscosity module were drastically different. The interaction was carried out on three different TBCs synthesized using the solution precursor plasma spray process (SPPS): two of the TBCs were made of yttrium aluminum garnet (YAG) having different microstructures that promote different modes of CMAS infiltration, and one TBC was made of gadolinium zirconate (GZO). All samples had stress relieving vertical cracks and different intensities of horizontally banded porosity, (inter pass boundaries IPBs). A concentration of 100 mg/cm 2 of CMAS was applied on the TBCs which were then subjected to a 5-minute interaction at 1300 °C. Samples were analyzed using scanning electron microscopy (SEM), electron dispersive X-ray spectroscopy (EDXS), and transmission electron microscopy (TEM). Low viscosity CMAS readily penetrated the TBCs while more viscous CMAS showed less penetration. The depth of CMAS infiltration depended on the coating microstructure. In the YAG with IPBs, the CMAS spread horizontally in the IPBs before infiltrating deeper, resulting in reduced infiltration depth compared to other samples in spite of having wider vertical cracks. TEM and EDXS analysis were performed to investigate the phases present in the CMAS-TBC interaction region in YAG. Two regions were chosen, the top TBC surface in direct contact with the sea of CMAS, and the region at the CMAS penetration ended within the coating. Finally, the results showed that no secondary phases like apatite were observed in YAG, thus it can be concluded that the arrest of CMAS happened solely because of CMAS viscosity and the short infiltration time.

36 MATERIALS SCIENCE↗

Corrosion protection of mild steel by superhydrophobic magnetite coating

Corrosion-resistant hydrophobic magnetite coatings on mild steel surfaces were developed by immersion method. The effect of steel surface roughness (R a ) on its hydrophobicity was systematically studied using contact angle measurement (CAM), scanning electron microscopy (SEM), and atomic force microscopy (AFM). The corrosion resistance of hydrophobic magnetite coatings was evaluated using a potentiodynamic polarization test. The durability of the coatings was assessed in air, tap water, and 3.5 wt% NaCl environments. Hydrophobic magnetite coating with a water contact angle of 146-152° showed excellent resistance to corrosion, longevity in atmospheric air, and significant self-cleaning properties. The primary focus of this study was to develop a quick and simple immersion technique to create hydrophobic surfaces on mild steel. Finally, results suggest that surface roughness plays a significant role in surface hydrophobicity, and enhancing the hydrophobicity of mild steel improves its corrosion resistance.

36 MATERIALS SCIENCE↗

Investigation of the temperature-dependent failure processes in PVD Cr-coated ZIRLO nuclear fuel cladding using in situ X-ray micro-tomography imaging

In this work, an accident tolerant fuel cladding system with Cr coating deposited using physical vapour deposition (PVD) method onto commercial Optimized ZIRLO™ was studied. The cladding tubes were machined into C-rings and loaded to failure under compression with real-time synchrotron micro-X-ray computed tomography (XCT) imaging at room temperature (RT), 345 °C, 650 °C and 950 °C in argon (Ar) atmosphere. The mechanical behaviour and failure processes were found strongly temperature-dependent where the Cr coating showed brittle fracture at RT and 345 °C, ductile fracture at 650 °C and a reversion to brittle fracture at 950 °C. Nanoindentation measurements and scanning electron microscopy (SEM) imaging were conducted on the materials after high temperature testing. It was found that recrystallisation of the Cr coating occurred at elevated temperatures, which significantly affected its local properties hence the failure behaviour at different temperatures. This work represents the first in situ 3D XCT observation of progressive failure processes in PVD Cr-coated ZIRLO claddings up to 950 °C providing critical insights into its brittle-to-ductile transition (BDTT) behaviour and subsequent ductile-to-brittle reversion with the increase in temperature. Moreover, results are compared with other PVD Cr-coated Zircaloy materials from open literature; the influences of the coating microstructure and local properties on the failure stress/strain and fracture processes are discussed.

Yuan, Guanjie↗

Silicon Dioxide Deposited Using Atmospheric Pressure Plasma Chemical Vapor Deposition for Improved Adhesion and Water Intrusion Resistance for Lightweight Manufacturing

This work aims to demonstrate the barrier coating, and adhesion promoting properties of silica-based coatings deposited using an atmospheric pressure plasma torch (APPT). This is achieved by applying an industrial grade adhesive to silica thin films deposited, on the surfaces to be joined, using atmospheric pressure plasma chemical vapor deposition (APP-CVD), to make single joint lap shear samples of different metal combinations commonly found in lightweight manufacturing such as aluminum and magnesium as well as steel. To deposit these thin films, two separate silicon based organic precursors, hexamethyldisiloxane (HMDSO), and tetraehylorthosilicate (TEOS), are used. Here, samples are bonded using DuPont Betamate 1486 adhesive, and the lap shear results for these films are compared to the lap shear results of a chemically cleaned control using the same adhesive. The APPT uses a microwave power supply and gas mixtures of N 2 and Ar. The adhesion of the films are tested using lap shear, and elevated temperature water soaks are conducted on the joints as well to simulate environmental exposure. Lap shear results from samples with silica thin films max shear stress are 25%-115% increase compared to control samples depending on material. After exposure to water soak the max shear strength of the joints decreased by less than 15%, which demonstrates the films capabilities as a water barrier. Film morphology is examined using Scanning Electron Microscopy (SEM), and the film’s composition and approximate thickness are obtained using Rutherford Backscattering Spectroscopy (RBS).

36 MATERIALS SCIENCE↗

Fractal analysis on Ag 2 O thin film using a data-driven approach

The synthesis of fractal Ag oxide (Ag 2 O) on the surface of Ag thin film has been achieved at room temperature by using Synchrotron X-ray irradiation. We have performed an automated quantitative analysis of a batch of 1879 fractal Ag 2 O patterns in a scanning electron microscopy (SEM) image within a radius of 2000 mm outward from the center of the X-ray beam. The morphology is similar to that of the diffusion-limited cluster aggregation (DLCA) model. The fractal dimension (D) of Ag 2 O is between 1.7 and 1.5 from the center to the edge. The area distribution density of fractal Ag 2 O follows a quadratic function with radius R. It is found that the branches’ number of fractal Ag 2 O is a key factor affecting the fractal dimension. The more branches the fractal has, the greater the D is. This is the first time that Ag fractal has been investigated by combining automated data analysis methods with batch experimental data. This data-driven approach provides a new research perspective for rationally regulating materials’ fractal morphology and performance.

36 MATERIALS SCIENCE↗

Cluster Analysis of Combined EDS and EBSD Data to Solve Ambiguous Phase Identifications

A common problem in analytical scanning electron microscopy (SEM) using electron backscatter diffraction (EBSD) is the differentiation of phases with distinct chemistry but the same or very similar crystal structure. X-ray energy dispersive spectroscopy (EDS) is useful to help differentiate these phases of similar crystal structures but different elemental makeups. However, open, automated, and unbiased methods of differentiating phases of similar EBSD responses based on their EDS response are lacking. This paper describes a simple data analytics-based method, using a combination of singular value decomposition and cluster analysis, to merge simultaneously acquired EDS + EBSD information and automatically determine phases from both their crystal and elemental data. I use hexagonal TiB 2 ceramic contaminated with multiple crystallographically ambiguous but chemically distinct cubic phases to illustrate the method. Code, in the form of a Python 3 Jupyter Notebook, and the necessary data to replicate the analysis are provided as Supplementary material.

47 OTHER INSTRUMENTATION↗

Heteroepitaxial Integration of ZnGeN 2 on GaN Buffers Using Molecular Beam Epitaxy

Recently theorized hybrid II-IV-N 2 /III-N heterostructures, based on current commercialized (In,Ga)N devices, are predicted to significantly advance the design space of highly efficient optoelectronics in the visible spectrum, yet there are few epitaxial studies of II-IV-N 2 materials. In this work, we present heteroepitaxial ZnGeN 2 grown on GaN buffers and AlN templates. We demonstrate that a GaN nucleating surface is crucial for increasing the ZnGeN 2 crystallization rate to combat Zn desorption, extending the stoichiometric growth window from 215 degrees C on AlN to 500 degrees C on GaN buffers. Structural characterization reveals well-crystallized films with threading dislocations extending from the GaN buffer. These films have a critical thickness for relaxation of 20-25 nm as determined by reflection high energy electron diffraction (RHEED) and cross-sectional scanning electron microscopy (SEM). The films exhibit a cation-disordered wurtzite structure, with lattice constants a = 3.216 +/- 0.004 A and c = 5.215 +/- 0.005 A determined by RHEED and X-ray diffraction (XRD). This work demonstrates a significant step toward the development of hybrid ZnGeN 2 -GaN integrated devices.

36 MATERIALS SCIENCE↗

Intercalation-Induced Topotactic Phase Transformation of Tungsten Disulfide Crystals

Recent research has demonstrated the potential for topological superconductivity, anisotropic Majorana bound states, optical nonlinearity, and enhanced electrochemical activity for transition metal dichalcogenides (TMDs) with a 2M structure. These unique TMD compounds exhibit metastability and, upon heating, undergo a transition to the thermodynamically stable 2H phase. The 2M phase is commonly made at high temperatures using traditional solid-state methods, and this metastability further complicates the growth of large 2M WS 2 crystals. Herein, a novel synthetic method was developed, focusing on a molten salt reaction to synthesize large 2H crystals and then inducing transformation to the 2M phase through intercalation and thermal treatment. The 2H crystals were intercalated via a room-temperature sodium naphthalenide solution, producing a previously unreported Na-intercalated 2H WS 2 phase. Thermal heating was required to facilitate the phase transition to the intercalated 2M crystal structure. This phase transition was studied by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), selected area electron diffraction (SAED), electron dispersive X-ray spectroscopy (EDS), and Raman spectroscopy, which confirmed the synthesis of the intercalated 2M phase. Upon deintercalation, crystal and powder samples showed superconductivity with a T c of 8.6–8.7 K, similar to previously reported values. The generality of this process was further demonstrated using alkali metal triethyl borohydride to intercalate 2H WS 2 and produced the desired 2M phase. This novel synthetic method has broad implications for discovering metastable phases in other TMD families and layered materials. Furthermore, separation of the intercalation and phase transition also has the potential to allow for large-scale synthesis of this technologically important phase with greater control over each step of the reaction.

36 MATERIALS SCIENCE↗

Role of Ammonium Hydroxide on Glucose Oxidase Immobilized in Metal–Azolate Framework-7 Enzyme Activity

Enzymes are nature’s catalysts, but their instability outside native environments limits practical applications. Metal–organic frameworks (MOFs) offer a promising platform for enzyme immobilization, enhancing stability, and reusability through their tunable porosity and crystallinity. While ZIF-based MOFs have been extensively studied, metal azolate framework-7 (MAF-7) remains largely unexplored for biomimetic mineralization. Its hydrophilic character makes it a promising alternative for enzyme encapsulation; however, the role of essential basic modulators such as ammonium hydroxide (NH 4 OH) on enzyme structure and function has not been investigated. Here, in this study, we examine the NH 4 OH mediated synthesis of glucose oxidase within MAF-7 using powder X-ray diffraction (PXRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), cryogenic transmission electron microscopy (cryo-TEM), and enzyme assays. Our results show that NH 4 OH modulates crystal morphology, enzyme activity, and nucleation behavior, with higher concentrations leading to partial enzyme denaturation and reduced catalytic performance. By integrating time-resolved cryo-TEM with activity assays, we uncover how modulator concentration impacts early stage crystallization and enzyme folding, a mechanistic insight not previously demonstrated in MOF systems. These findings highlight modulator chemistry as a critical, underexplored variable in MOF synthesis, advancing rational design strategies for enzyme@MOFs (E@MOF) beyond ZIFs and toward more tunable, biocompatible frameworks like MAF-7.

36 MATERIALS SCIENCE↗

Characterizing Pore-Scale Geochemical Alterations in Eagle Ford and Barnett Shale from Exposure to Hydraulic Fracturing Fluid and CO 2 /H 2 O

As demand increases for an affordable energy source that is tied to an environmental obligation to reduce greenhouse gas emissions and water usage, there is a growing consideration in shale production utilizing processes such as 1) enhancing hydrocarbon recovery via carbon dioxide (CO 2 ) flooding, 2) using CO 2 as a fracturing agent to minimize water use, and 3) storing CO 2 in depleted shale formations to mitigate emissions to the atmosphere. Understanding the geochemical reactions and alterations that occur as shale is exposed to fluids and CO 2 is necessary to develop and optimize each of these processes for field applications. While the majority of shale formations are stimulated using traditional fracturing fluid, some may be fractured using CO 2 or other non-traditional means. We examine the effect fracturing fluid has on shale and how it behaves with secondary exposure to dry CO 2 or CO 2 -saturated water using in situ Fourier Transform infrared spectroscopy (FTIR), feature relocation scanning electron microscopy (SEM), and surface area and pore size analysis using volumetric gas sorption. These techniques were performed on Eagle Ford and Barnett shale samples that were exposed to fracturing fluid and unexposed (as received). Shales that have been exposed to traditional fracturing fluid experienced two reaction fronts. The first reaction front was formed during exposure to the fracturing fluid (pH of ~1.4). A secondary reaction front was formed as a result of CO 2 -saturated fluid exposure in the form of carbonic acid (pH ~5.6). These two different reaction mechanisms drove multiple dissolution and precipitation cycles which altered petrophysical properties of the shale and could lead to a significant impact on flow pathways. FTIR showed that equilibration of carbonate dissolution and precipitation cycles could take as long as 35 days. Samples exposed to fracturing fluid showed significantly less carbonate reactivity compared to those exposed to water. Pore size analysis results indicate exposure to fracturing fluid blocked small nanopores (10-15 nm) reducing BET surface area and total pore volume. SEM results show barite precipitated heavily during exposure to fracturing fluid. It appeared that carbonic acid was able to extract sulfur from organic matter to form gypsum evaporites. The mineralogical (barite precipitation and calcite dissolution/precipitation) and pore-scale alterations observed in these samples may lead to enhancement of flow pathways for injected CO 2 or produced hydrocarbons.

04 OIL SHALES AND TAR SANDS↗

Effect of Adsorbed Carboxylates on the Dissolution of Boehmite Nanoplates in Highly Alkaline Solutions

Understanding the dissolution of boehmite in highly alkaline solutions is important to the processing of the complex nuclear wastes stored at the Hanford (WA) and Savannah River (SC) sites. Here, we report the adsorption of model carboxylate anions on boehmite nanoplates in alkaline solutions and their effects on subsequent boehmite dissolution in 3 M NaOH at 80 °C. Although expectedly lower than at circumneutral pH, adsorption of oxalate at pH 13 at room temperature was significant and remained so through a linear decrease to 3 M NaOH conditions with no evidence for the appearance of new phases. Modeling of the adsorption data and rate were consistent with the formation of outer-sphere surface complexes. By using these conditions to preload the boehmite nanoplates with oxalate, and separately acetate, we measured and compared their dissolution behavior at 80 °C and observed a clear suppression of the dissolution rate for the case of adsorbed oxalate by 23% and for adsorbed acetate by 10% compared to pure solids. Ex situ scanning electron microscopy (SEM) and transmission electron microscopy (TEM) characterization revealed no detectable difference in the morphologic evolution of the dissolving boehmite materials. In conclusion, we nonetheless conclude that pre-adsorbed carboxylate anions, even as nominally weakly bound outer-sphere complexes, can persist on the surface through highly alkaline conditions, decreasing the density of dissolution-active sites and thereby adding an extrinsic control on the dissolution rate.

Adsorption kinetics↗

Meniscus Guided Coating and Evaporative Crystallization of UiO-66 Metal Organic Framework Thin Films

Thin-film fabrication of metal organic frameworks (MOFs) has been explored for a range of applications, including separations, catalysis, sensing, and charge transport. However, many fabrication techniques have obstacles, including slow crystallization, control over film thickness, and control over crystallinity. Recently, a meniscus-guided coating technique, called solution shearing, has been shown to create MOF thin films within minutes and with control over the film thickness. However, there have been no previous reports of solution shearing based evaporative crystallization of zirconium-based MOFs, which have been widely studied for the aforementioned applications. In this work, for the first time, we show that (i) the zirconium 1,4-dicarboxybenzene MOF, UiO-66, can be formed using evaporative crystallization during solution shearing, and (ii) a wide range of parameters can be tuned to control the film thickness, coverage, and crystallinity. Finally, we bring the solution shearing technique closer to separation applications by growing a full film of UiO-66 crystals up to the resolution of scanning electron microscopy (SEM) on anodic alumina oxide (AAO). This is the first instance of UiO-66 crystals being formed using an evaporative crystallization-based flow coating method, and solution shearing shows the promise to be applicable to form large area zirconium-based MOF crystals in a rapid manner (within seconds to minutes).

42 ENGINEERING↗