Search NASA⌕ Search

SEARCH · Search NASA

Results for “structural adhesives testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Impact Ice Adhesion at NASA Glenn: Current Experimental Methods and Supporting Measurements

When examining the literature on the adhesion strength of impact ice, there have been a wide range of methodologies tried to measure the required stresses to induce interfacial delamination. Utilizing the Icing Research Tunnel at the NASA Glenn Research Center to generate the impact ice required for this work, several different mechanical tests have been and are being developed to determine the stresses along the interface between ice and coupon. This set of tests includes the technical mature modified lap joint test which has been used to conduct ice adhesion studies through a wide sweep of icing conditions. To conduct in situ ice adhesion measurements inside of the Icing Research Tunnel, several new experiments are currently being developed to make ice adhesion measurements during and immediately after ice accretion. In addition to these experimental methods, several supporting measurement techniques have been developed to allow for a better understanding on the influence of icing cloud conditions on the mechanical behavior of impact ice. Digital image correlation has been successfully implemented to augment the data generated by the modified lap joint test with full field surface displacement and strain measurements which allow for insight into the deformation processes present during a test. Both optical microscopy of impact ice samples along with ice replication techniques have been used to study the grain structure of the impact ice. This has led to a deeper understanding of the results from the modified lap joint method and how the structure of impact ice changes as it is accreted during an icing spray. The freezing process of impact ice generated by supercooled liquid water is not a volume conserving process, which leads to the presence of residual strains along the interface between ice and substrate. These strains have been observed using both a simplified flat geometry and a representative airfoil. The data gathered by these experimental adhesion methods and supporting measurements allows for a comprehensive understanding on the behavior of impact ice which will be critical to the development of future ice shedding models.

Ice Adhesion↗

Impact Ice Adhesion at NASA Glenn: Current Experimental Methods and Supporting Measurements

When examining the literature on the adhesion strength of impact ice, there have been a wide range of methodologies tried to measure the required stresses to induce interfacial delamination. Utilizing the Icing Research Tunnel at the NASA Glenn Research Center to generate the impact ice required for this work, several different mechanical tests have been and are being developed to determine the stresses along the interface between ice and coupon. This set of tests includes the technical mature modified lap joint test which has been used to conduct ice adhesion studies through a wide sweep of icing conditions. To conduct in situ ice adhesion measurements inside of the Icing Research Tunnel, several new experiments are currently being developed to make ice adhesion measurements during and immediately after ice accretion. In addition to these experimental methods, several supporting measurement techniques have been developed to allow for a better understanding on the influence of icing cloud conditions on the mechanical behavior of impact ice. Digital image correlation has been successfully implemented to augment the data generated by the modified lap joint test with full field surface displacement and strain measurements which allow for insight into the deformation processes present during a test. Both optical microscopy of impact ice samples along with ice replication techniques have been used to study the grain structure of the impact ice. This has led to a deeper understanding of the results from the modified lap join method and how the structure of impact ice changes as it is accreted during an icing spray. The freezing process of impact ice generated by supercooled liquid water is not a volume conserving process, which leads to the presence of residual strains along the interface between ice and substrate. These strains have been observed using both a simplified flat geometry and a representative airfoil. The data gathered by these experimental adhesion methods and supporting measurements allows for a compressive understanding on the behavior of impact ice which will be critical to the development of future ice shedding models.

Ice Adhesion↗

Structure and Mutagenesis of Neural Cell Adhesion Molecule Domains Evidence for Flexibility in the Placement of Polysialic Acid Attachment Sites

The addition of {alpha}2,8-polysialic acid to the N-glycans of the neural cell adhesion molecule, NCAM, is critical for brain development and plays roles in synaptic plasticity, learning and memory, neuronal regeneration, and the growth and invasiveness of cancer cells. Our previous work indicates that the polysialylation of two N-glycans located on the fifth immunoglobulin domain (Ig5) of NCAM requires the presence of specific sequences in the adjacent fibronectin type III repeat (FN1). To understand the relationship of these two domains, we have solved the crystal structure of the NCAM Ig5-FN1 tandem. Unexpectedly, the structure reveals that the sites of Ig5 polysialylation are on the opposite face from the FN1 residues previously found to be critical for N-glycan polysialylation, suggesting that the Ig5-FN1 domain relationship may be flexible and/or that there is flexibility in the placement of Ig5 glycosylation sites for polysialylation. To test the latter possibility, new Ig5 glycosylation sites were engineered and their polysialylation tested. We observed some flexibility in glycosylation site location for polysialylation and demonstrate that the lack of polysialylation of a glycan attached to Asn-423 may be in part related to a lack of terminal processing. The data also suggest that, although the polysialyltransferases do not require the Ig5 domain for NCAM recognition, their ability to engage with this domain is necessary for polysialylation to occur on Ig5 N-glycans.

36 MATERIALS SCIENCE↗

PchE Regulation of Escherichia coli O157:H7 Flagella, Controlling the Transition to Host Cell Attachment

Shiga toxins and intimate adhesion controlled by the locus of enterocyte effacement are major enterohemorrhagic Escherichia coli (EHEC) virulence factors. Curli fimbriae also contribute to cell adhesion and are essential biofilm components. The transcriptional regulator PchE represses the expression of curli and their adhesion to HEp-2 cells. Past studies indicate that pchE also represses additional adhesins that contribute to HEp-2 cell attachment. In this study, we tested for pchE regulation of several tissue adhesins and their regulators. Three adhesin-encoding genes (eae, lpfA1, fliC) and four master regulators (csgD, stpA, ler, flhDC) were controlled by pchE. pchE over-expression strongly up-regulated fliC but the marked flagella induction reduced the attachment of O157:H7 clinical isolate PA20 to HEp-2 cells, indicating that flagella were blocking cell attachments rather than functioning as an adhesin. Chemotaxis, motor, structural, and regulatory genes in the flagellar operons were all increased by pchE expression, as was PA20 motility. This study identifies new members in the pchE regulon and shows that pchE stimulates flagellar motility while repressing cell adhesion, likely to support EHEC movement to the intestinal surface early in infection. However, induced or inappropriate pchE-dependent flagellar expression could block cell attachments later during disease progression.

59 BASIC BIOLOGICAL SCIENCES↗

3D PRINTED LAYER OF POLYANILINE-BASED CONDUCTIVE POLYMER FOR LIGHTNING STRIKE PROTECTION OF CFRPS

Manufacturing of Carbon Fiber Reinforced Plastics (CFRPs) using additive manufacturing (AM), or 3D printing, has gained popularity in recent years. It is believed that the AM industry has the potential to manufacture CFRP parts in a faster, easier and more economical way. Lightning strike damage to CFRP parts is not rare; therefore, additional lightning strike protection (LSP) technologies are applied on top of CFRP structures. However, there is no report of manufacturing lightning strike protection (LSP) technologies using the AM process. In the present work, the authors applied an electrically conductive layer via additive manufacturing. The material of the electrically conductive layer was a Polyaniline (PANI)-filled thermoset composite. This layer of PANI was deposited on top of the CFRP panels. The PANI-coated CFRP panels were tested against a simulated lightning strike made of a continuous waveform with component A (100 kA), component B (2 kA) and component C (470 A). The highly conductive PANI-layer worked as a capable Faraday cage to safely dissipate the lightning current. In PANI-based LSP, direct contact between PANI chains dominated the conduction behavior, which proved to be a highly efficient way to reduce resistive heating from the incident current. However, poor adhesion between the printed layer and the substrate structure needs to be improved in the future. The results from the thermal camera and the high-speed camera images showed an effective current dissipation through the printed layers. Non-destructive ultrasonic imaging was done to confirm the direct lightning damages to samples. The present work shows that a non-metallic conductive layer can be applied as an LSP of CFRP structures via an additive manufacturing technique.

Kumar, Vipin↗

The Ability of AMSTAR Dechlorination Solution to Remove and Degrade PCBs from Contaminated Surfaces

Polychlorinated biphenyls (PCBs) are a group of synthetic aromatic compounds with the general formula C12H(10-x)Cl(-x) that were historically used in industrial paints, caulking material and adhesives, as their properties enhanced structural integrity, reduced flammability and boosted antifungal properties. Although the United States Environmental Protection Agency (USEPA) has banned the manufacture of PCBs since 1979, they have been found in at least 500 of the 1,598 National Priorities List (Superfund) sites identified by the USEPA. Prior to the US EPA's ban on PCB production, PCBs were commonly used as additives in paints and asphalt-based adhesives that were subsequently applied to a variety of structures. Government facilities constructed as early as 1930 utilized PCB-containing binders or PCB-containing paints, which are now leaching into the environment and posing ecological and worker health concerns. In 2006, a commercially available product known as AMSTAR Dechlorination Solution was tested at NASA's Kennedy Space Center for its ability to remove and degrade PCBs from structural materials. This evaluation was requested by the Environmental Security Technology Certification Program (ESTCP) evaluating the ability of NASA's Bimetallic Treatment System (BTS) to remove and degrade PCBs from structural materials. The results of the laboratory testing are to be used to determine if a side-by-side field-scale test comparing BTS to AMSTAR was warranted. A recommended sampling and analysis testing program was submitted to ESTCP that included triplicate screening of AMSTAR's PCB dechlorination capabilities on a variety of surfaces including glass, bare metal, and painted metal coupons. The test procedures, analytical techniques and results obtained are presented in this interim report to ESTCP.

Quinn, Jacqueline E.↗

Characterization of Microbe Resistant Coatings for Use in the ISS Water System

The ISS is a highly controlled environment; however, there are still microbes on it that astronauts bring from their own microbiome. Once within the ISS water treatment system, these microbes not only pose a health risk for astronauts, but they can form biofilms, causing material degradation and system failure. Due to their protective structure, biofilms are notoriously resistant to disinfectants and antibiotics. One proposed solution is applying polymer coatings to the metal parts of the water system to prevent biofilms from forming. Two types of polyampholyte polymers with previously demonstrated nonfouling properties were sent to the ISS in 2021 to test their viability for preventing microbial adhesion in space. However, the only microbial assays performed were microscopy. To enhance this ongoing research project, I developed procedures for culturing, applying, and quantifying Ralstonia pickettii on these polymers. R. pickettii was chosen because it is one of the most prevalent microbes found in the ISS water treatment system. Optical density data was recorded to obtain a growth curve demonstrating a doubling time between 2.83 and 4.88 hours in 30°C, not shaken conditions. Optical density was also correlated to colony forming units in a plating experiment. Another result was design (and pilot testing) of a surface colonization experiment. These results provided vital knowledge about R. pickettii, which will be used for a 2023 payload of antimicrobial polymer coatings on stainless steel, and improved methods for biofilm analysis upon its return to evaluate the efficacy of the coatings.

microbiology↗

Test of superplastically formed corrugated aluminum compression specimens with beaded webs

Corrugated wall sections provide a highly efficient structure for carrying compressive loads in aircraft and spacecraft fuselages. The superplastic forming (SPF) process offers a means to produce complex shells and panels with corrugated wall shapes. A study was made to investigate the feasibility of superplastically forming 7475-T6 aluminum sheet into a corrugated wall configuration and to demonstrate the structural integrity of the construction by testing. The corrugated configuration selected has beaded web segments separating curved-cap segments. Eight test specimens were fabricated. Two specimens were simply a single sheet of aluminum superplastically formed to a beaded-web, curved-cap corrugation configuration. Six specimens were single-sheet corrugations modified by adhesive bonding additional sheet material to selectively reinforce the curved-cap portion of the corrugation. The specimens were tested to failure by crippling in end compression at room temperature.

Davis, Randall C.↗

CORROSION PERFORMANCE OF MIL-PRF-23377 PRIMER COATED ON LASER-INTERFERENCE STRUCTURED ALUMINUM ALLOY 2024

Laser-Interference Structuring (LIS) is a technique that was proposed to treat aluminum surfaces for improving primer adhesion. LIS may not require a series of chemical treatments, such as those used in chemical conversion coating (CCC) and sulfuric acid anodizing (SAA), which make the pre-treatment of Al panels simpler and quicker for primer painting. Previous test results indicated that LIS surface preparation enhances coating adhesion on Al 2024. To assess the effect of LIS on corrosion resistance of coatings, Al 2024 panels prepared by LIS, CCC and SAA were coated with MIL-PRF-23377 primers and exposed to salt spray environment according to ASTM B117. The exposure is currently in progress and the corrosion attack on the coated panels will be evaluated by the degree of blister formation and rust creepage according to ASTM standards.

Jun, Jiheon↗

VitriEdge: Repairable & Durable Vitrimer Coatings for Wind Turbine Blade Leading Edges

The primary goal of this Level 1b incubator project was to explore the use of vitrimer coatings for repair of leading-edge erosion on end-of-life wind turbine blade surfaces, beyond coating strength of adhesion which has previously been demonstrated in the Level 1a project. Uniform vitrimer coatings (thickness: 400 µm) were applied to two end-of-life wind turbine blades for flexural, fatigue, and laminate tensile testing where the addition of the coating did not produce any statistical variation in tensile properties with minor drops in flexural strength for some laminate formulations. However, a <2% variation in storage modulus was measured for laminate structures (i.e., blade samples with vitrimer coatings) across 100,000 flexural cycles and upon laminate tensile failure, the vitrimer coatings displayed no visible signs of delamination. In addition, three methods to heal vitrimer coating damage was displayed: oven heating, addition of hot water, and a forced convection heat gun. All three heating and healing mechanisms demonstrated significant healing with scratch depths decreasing between 79-91% at healing times ranging between 1-min and 10-minutes. Finally, a water jet machine was used to simulate rain erosion for both the blade surfaces and vitrimer-coated blade surfaces where the diameter and depth of the damage was recorded as a function of exposure time, water pressure, height of exposure, and angle of exposure. Of interest, while the vitrimer coating did not significantly lessen the damage experienced during rain erosion, the addition of vitrimer composite coatings(5 wt.% mica addition) did result in a crack-resistant, durable coating capable of self-healing behavior and in all cases the angle of rain exposure was the most critical parameter explored. It is crucial to continue exploring this space where vitrimer coatings are of interest for both their self-healing properties and potential use as reversible adhesives.

17 WIND ENERGY↗

On the cogent formulation of an elastomeric silicone ink material for direct ink write ( DIW ) 3D printing

Abstract Adhesives and sealants show fine rheology with good physical and mechanical properties as viscous pastes, a possible starting point for developing direct ink writing (DIW) 3D printing ink. However, many commercial adhesives and sealants take days or weeks to cure fully. DIW 3D‐printed parts made directly from these sealants are not designed for a scalable manufacturing process and high‐volume production. Moreover, most of these adhesives and sealants have volume shrinkage during cure. A systematic understanding of formulation methods and design principles for an elastomeric silicone DIW ink can overcome these issues. This study presents the cogent formulation development of a 3D printable thermoset elastomer silicone that gels and cures isotropically in minutes, reducing cycle time for rapid ink development with no shrinkage during cure. More specifically, we outline the principles of raw material selection of a formulation to achieve excellent rheology, printability, synchronized working, and gel time fitting requirements closer to scalable manufacturing. The reaction kinetics and their corresponding 3D‐printed structural properties are also described. Interest in future work is toward a rational DIW 3D printing ink material development protocol and use of machine learning (ML). Highlights Formulation method flexibility and design principle of DIW ink. Raw material selection principle to achieve optimal rheology for DIW printing. Ink gel kinetics for large‐scale DIW manufacturing. Hydrosilylation conversion over time at different ambient temperatures. Structural properties of DIW 3D printed parts.

36 MATERIALS SCIENCE↗

Fabrication of anti-adhesion surfaces on aluminium substrates of rubber plastic moulds using electrolysis plasma treatment

An anti-adhesion surface with a water contact angle of 167° was fabricated on aluminium samples of rubber plastic moulds by electrolysis plasma treatment using mixed electrolytes of C{sub 6}H{sub 5}O{sub 7}(NH{sub 4}){sub 3} and Na{sub 2}SO{sub 4}, followed by fluorination. To optimise the fabrication conditions, several important processing parameters such as the discharge voltage, discharge time, concentrations of supporting electrolyte and stearic acid ethanol solution were examined systematically. Using scanning electron microscopy (SEM) to analyse surfaces morphology, micrometer scale pits, and protrusions were found on the surface, with numerous nanometer mastoids contained in the protrusions. These binary micro/nano-scale structures, which are similar to the micro-structures of soil-burrowing animals, play a critical role in achieving low adhesion properties. Otherwise, the anti-adhesion behaviours of the resulting samples were analysed by the atomic force microscope (AFM), Fourier-transform infrared spectrophotometer (FTIR), electrons probe micro-analyzer (EPMA), optical contact angle meter, digital Vickers microhardness (Hv) tester, and electronic universal testing. The results show that the electrolysis plasma treatment does not require complex processing parameters, using a simple device, and is an environment-friendly and effective method. Under the optimised conditions, the contact angle (CA) for the modified anti-adhesion surface is up to 167°, the sliding angle (SA) is less than 2°, roughness of the sample surface is only 0.409μm. Moreover, the adhesion force and H{sub v} are 0. 9KN and 385, respectively.

36 MATERIALS SCIENCE↗

Resistance Spot Weld Failure Mode and Weld Performance for Aluminium Alloys

In this chapter, we present the strength and failure modes of reactive NanoFoil® bonded joints for similar and dissimilar lightweight materials. NanoFoil® is a multi-layer foil fabricated through the growth of thousands of nanoscale layers of aluminum and nickel by vapor deposition. Initiated by an energy impulse, the like-like bonds of the atoms of each layer in the foil are exchanged for more stable unlike bonds between atoms from neighboring layers. As the atoms of each layer mix, heat is generated, creating a self-sustaining reaction traveling along the length of the foil. The instantaneous release of heat energy by this reaction is controlled by the nanolayer thickness and lay-up, such that accurate control of a highly localized heat source can be realized, allowing bonding without compromising the properties/integrities of the base materials. First, solder and braze joints for similar and dissimilar material combinations of steel, aluminum and magnesium are fabricated. Static bond strength tests under tensile shear loading condition are then performed to quantify the bond strength for different material combinations. The through-thickness microstructure changes and modifications by the bonding process are quantified using SEM. Depending on the base material combinations, it is shown that the nanofoil bond strength is comparable to those of the conventional structural adhesive bonds.

36 MATERIALS SCIENCE↗

Anti-scalingproperties of SOCAL coating on aluminumsubstrate

n this work, we proposed an innovative coating on Aluminumwith exceptional anti-scalingperformance. The coating features a sandwich structure with electrophoresis deposited (EPD) SiO2as intermediate layer between aluminumsubstrate and SOCALomniphobic coating. This EPD SiO2coating shows unprecedented smoothnesswhich, combined with low surface energy SOCAL coating, translated toanti scaling property. To characterize scaling, we utilized CaSO4and CaCO3scale tests, showing up to 20X less scaling than uncoated aluminum. Descaling tests revealed that our SOCAL coatings dramatically decrease scale adhesion, resulting in rapid removal of scale buildup in highly supersaturated conditions.

Zhao, Hanyang↗

Encapsulation and backsheet adhesion metrology for photovoltaic modules

Photovoltaic modules are designed to operate for decades in terrestrial environments. However, mechanical stress, moisture, and ultraviolet radiation eventually degrade protective materials in modules, particularly their adhesion properties, eventually leading to reduced solar cell performance. Despite the significance of interfacial adhesion to module durability, currently there is no reliable technique for characterizing module adhesion properties. We present a simple and reproducible metrology for characterizing adhesion in photovoltaic modules that is grounded in fundamental concepts of beam and fracture mechanics. Using width-tapered cantilever beam fracture specimens, interfacial adhesion was evaluated on relevant interfaces of encapsulation and backsheet structures of new and 27-year-old historic modules. The adhesion energy, Gc [J/m 2 ], was calculated from the critical value of the strain energy release rate, G, using G = βP 2 , where β (a mechanical and geometric parameter of the fracture specimen) and P (the experimentally measured critical load) are constants. Under some circumstances where testing may result in cracking of brittle layers in the test specimen, measurement of the delamination length in addition to the critical load was necessary to determine G. Relative to new module materials, backsheet adhesion was 95% and 98% lower for historic modules that were exposed (operated in the field) and unexposed (stored on-site, but out of direct sunlight), respectively. Encapsulation adhesion was 87-94% lower in the exposed modules and 31% lower in the unexposed module. As a result, the metrology presented here can be used to improve module materials and assess long-term reliability.

14 SOLAR ENERGY↗

A Numerical Investigation of CFRP-Steel Interfacial Failure with Material Point Method

The success of retrofitting steel structures by using the Carbon Fibre Reinforced Polymers (CFRP) significantly depends on the performance and integrity of CFRP-steel joint and the effectiveness of the adhesive used. Many of the previous numerical studies focused on the design and structural performance of the CFRP-steel system and neglected the mechanical responses of adhesive layer, which results in the lack of understanding in how the adhesive layer between the CFRP and steel performs during the loading and failure stages. Based on the recent observation on the failure of CFRP-steel bond in the double lap shear tests, a numerical approach is proposed in this study to simulate the delamination process of CFRP sheet from steel plate using the Material Point Method (MPM). In the proposed approach, an elastoplasticity model with a linear hardening and softening law is used to model the epoxy layer. The MPM, which does not employ fixed mesh-connectivity, is employed as a robust spatial discretization method to accommodate the multi-scale discontinuities involved in the CFRP-steel bond failure process. To demonstrate the potential of the proposed approach, a parametric study is conducted to investigate the effects of bond length and loading rates on the capacity and failure modes of CFRP-steel system. The evolution of the CFRP-steel bond failure and the distribution of stress and strain along bond length direction will be presented. The simulation results not only well match the available experimental data but also provide a better understanding on the physics behind the CFRP sheet delamination process.

36 MATERIALS SCIENCE↗

Solid rocket motor nozzles

The steps in the nozzle design process are examined. The nozzle designer's role in defining design requirements and constraints is included along with discussions of each of the three basic phases of the nozzle design process itself: (1) aerodynamic design, in which the gas-contacting surfaces are configured to produce the required performance within the envelope limits; (2) thermal design, in which termal liners and thermal insulators are selected and configured to maintain the surfaces as closely as practical against effects of erosion and to limit the structure temperature to acceptable levels; and (3) structural design, in which materials are selected and configured to support the thermal components and to sustain the predicted loads. Analytical techniques that are used to establish thermal and structural design integrity and to predict nozzle performance are discussed along with methods for nozzle quality assurance. Emphasis is placed on nozzle design and materials for modern high-temperature aluminized propellants. Recurring nozzle design problems of graphite cracking and ejection, differential erosion at material interfaces, lack of sufficient proven nondestructive testing (NDT) techniques, the uncertainty of adhesive bonding, and inadequate definition of material properties, particularly at high temperatures are considered.

Ellis, R. A.↗

Field Evaluations Test Plan for Validation of Alternative Low-Emission Surface Preparation/Depainting Technologies for Structural Steel

Headquarters National Aeronautics and Space Administration (NASA) chartered the Acquisition Pollution Prevention (AP2) Office to coordinate agency activities affecting pollution prevention issues identified during system and component acquisition and sustainment processes. The primary objectives of the AP2 Office are to: (1) Reduce or eliminate the use of hazardous materials (HazMats) or hazardous processes at manufacturing, remanufacturing, and sustainment locations. (2) Avoid duplication of effort in actions required to reduce or eliminate HazMats through joint center cooperation and technology sharing. To achieve a substrate condition suitable for the application of a coating system, both new and old (in-situ) substrates must undergo some type of surface preparation and/or depainting operation to ensure adhesion of the new coating system. The level of cleanliness or anchor profile desired is typically a function of the type of coating to be applied and the specification being adhered to. In high performance environments, cleanliness and surface profile requirements for carbon steel (the dominant substrate for facilities, structures and equipment) dictates the use of abrasive media. Many of the abrasive media currently used across NASA and Air Force Space Command (AFSPC) installations generate large quantities of fugitive particulate emissions and waste. The high quantities of airborne dust and waste generated from these operations pose significant environmental concern. Efforts to contain emissions and the reduce quantity of waste generated have significant implications on project cost; this is often a deterrent to engaging in maintenance activities. In response to recent technological developments and NASA's and AFSPC's need to undertake environmentally conscious corrosion prevention projects, a review of the industry needs to be undertaken to evaluate surface preparation technologies (materials and processes) for embrace. This project will identify, evaluate and approve alternative surface preparation technologies for use at NASA and AFSPC installations. Materials and processes will be evaluated with the goal of selecting those processes that will improve corrosion protection at critical systems, facilitate easier maintenance activity, extend maintenance cycles, eliminate flight hardware contamination and reduce the amount of hazardous waste generated. This Field Evaluations Test Plan defines the field evaluation and testing requirements for validating alternative surface preparation/depainting technologies and supplements the JTP. The field evaluations will be performed at Stennis Space Center, Mississippi, under the oversight of the Project Engineer. Additional field evaluations may be performed at other NASA centers or AFSPC facilities.

Lewis, Pattie↗