Search NASA⌕ Search

SEARCH · Search NASA

Results for “voltage cycling”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 235 records · Page 13

Are Soft Short Tests Good Indicators of Internal Li-ion Cell Defects?

The self discharge test at full state of charge, may not be a good one to detect subtle defects since the li-ion chemistry has the highest self discharge at full state of charge. One should characterize self discharge versus storage time for each cell manufacturer/design to differentiate between normal self discharge and that due to a subtle manufacturing defect. The various soft short test methods indicate that if this test is carried out at full discharge (0% SOC) with all capacity removed (by lowering the current load in a stepwise manner to the same end of discharge voltage), then the cells need to be placed in storage for more than 72 hours to get a good analysis on the presence of subtle defects since it takes more than 72 hours to achieve voltage stabilization. If the cells are to be charged up even to a small percentage (ex. 1%), 72 hours are sufficient to determine issues. However, the pass/fail criteria should be based on a valid OCV decline. Less than 10 mV voltage decline is not a good method to detect subtle defects. As mentioned in the first bullet, self discharge is a competing reaction when a charge is introduced and hence a characterization of the self discharge versus storage time is required to fully correlate voltage decline to a failure due to a subtle defect. Soft short test method cannot be relied on for defect detection because cells with and without voltage decline seemed to have similar defects and characteristics. Screening methods such as internal resistance and capacity as well as a 3-sigma range for OCV, mass and dimensions should be used to screen out outliers. A very critical aspect in the understanding of subtle defects is to carry out destructive analysis of cells from every lot to confirm the quality of production and screen all cells and batteries in a stringent manner to have a high quality set of flight cells. Self Discharge Test: Fully charged cells shall be placed in Open circuit stand for 72 hours (OCV measurement twice a day); continue for total of 14 days with 1 reading per day 2. Soft Short Test 1: Fully charge; cells discharged to manufacturer's end of disch. Voltage (EODV) cutoff at C/5 rate; stand for 30 minutes; discharge with C/500 to the same EODV. stand for another 30 minutes; discharge the cells again using C/1000 current to the same EODV. OCV measurements twice a day for 72 hours and then for total of 14 days (data collection same as in 1.) 3. Soft Short Test 2: Fully charge; cells discharged to the manuf. EODV with a C/13 constant current; provide a 10 hour rest, discharge again to the same EODV with a current of C/250, provide a 10 hour rest, discharge again using a C/250 rate, provide a 24 hour rest, charge using C/250 to 3.15 V (for ~12 hours). OCV measurements twice a day for at 72 hours. (data collection same as in 1.) 4. Soft Short Test 3: Fully charge; cells shall be discharged using C/10 current to manuf. EODV. Allow the cell to remain at Open circuit for 10 seconds. Discharge the cell at C/20 rate to the same EODV, hold open circuit for 24 hours. Discharge the cells at C/200 rate to the same end of voltage cutoff and hold open circuit for 24 hours. Discharge the cells one more time at C/200 rate to the same EODV and hold open circuit for 36 hours. Charge at C/200 rate to 3.15 V and hold for 3 days. Record OCV during the open circuit stand periods every 12 hours and at the beginning and end of the 3 day hold (include the 12 hour OCV recording during this time also). Capacity Cycling: Cells with declining voltages - one cell from each manufacturer chosen for cycling Destructive Physical Analysis (DPA): Cells with and without decline chosen from each lot for DPA.

Jeevarajan, J.↗

Enabling Ether-Based Electrolytes for Long Cycle Life of Lithium-Ion Batteries at High Charge Voltage

Lithium-ion batteries (LIBs) with high-nickel (Ni) content LiNi x Mn y Co z O 2 ( x + y + z = 1) (NMC with Ni ≥ 0.6) cathodes operated at high charge voltages have been considered as one of the most promising candidates for addressing the challenge of increasing energy density demand. Conventional LiPF 6 –organocarbonate electrolytes exhibit incompatibility with such cell chemistries under certain testing conditions because of the instability of electrode/electrolyte interphases. In response to this challenge, ether-based electrolytes with finely tuned structure and composition of solvation sheaths were developed and evaluated in graphite (Gr)∥NMC811 cell chemistry in 2.5–4.4 V, despite ethers being conventionally considered to be unfavorable electrolyte solvents for LIBs because of their anodic instability above 4.0 V and cointercalation into Gr electrodes. Furthermore, the functional ether-based electrolytes in this work enable both excellent cycle life and high rate capability of Gr∥NMC811 cells. Mechanistic studies reveal that the unique structure and composition of the solvation sheath of the functional ether electrolytes are the main reasons behind their excellent anodic stability and effective protection of the Gr electrode and, consequently, the extraordinary cell performances when operated at high charge cutoff voltages. This work also provides a feasible approach in developing highly stable functional electrolytes for high-energy density LIBs.

25 ENERGY STORAGE↗

Sudden-Discharge Cycling Characteristics and Millisecond Dynamic Behaviors of a HTS Stainless-Steel Insulated Double-Pancake Coil With Thin Copper Plates

We have tested an intermediate-sized HTS stainless-steel (co-wound) insulated double pancake coil (~132 turns per coil) and discovered dynamic effects during sudden discharge on both millisecond and second scales. For soft break, the power supply is turned off suddenly but the shunt resistor (164 milliohm) is still connected; for hard break, a high voltage contactor is used to suddenly open the circuit so that the leads are completely open. Hard break is dangerous to traditionally insulated LTS magnets, but the SS-insulated HTS DPC retained integrity over ¡80 charge-discharge cycles. Voltage decay curves for soft and hard breaks are studied on short and long timescales. On long timescales, we observe the expected exponential decay and measure the time constant to calculate contact resistance. On short timescales, we observe highly dynamic effects: a hyper-exponential decay suggesting that the inductance or contact resistance is suddenly changing with time, likely an indication of the RL circuit forming. Moreover, peak voltage immediately (ms) after the sudden discharge were collected and compared. It is found that the peak voltage in soft-discharge is proportional to the applied current, while the those in hard-break has a unique pattern and tends to stay flat even though the applied current increases.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Impact of Mg Substitution on the Structure, Stability, and Properties of the Na 2 Fe 2 F 7 Weberite Cathode

Of the few weberite-type Na-ion cathodes explored to date, Na 2 Fe 2 F 7 exhibits the best performance, with capacities up to 184 mAh/g and energy densities up to 550 Wh/kg reported for this material. However, the development of robust structure–property relationships for this material is complicated by its tendency to form as a mixture of metastable polymorphs, and transform to a lower-energy Na y FeF 3 perovskite compound during electrochemical cycling. Our first-principles-guided exploration of Fe-based weberite solid solutions with redox-inactive Mg 2+ and Al 3+ predicts an enhanced thermodynamic stability of Na 2 Mg x Fe 2–x F 7 as the Mg content is increased, and the x = 0.125 composition is selected for further exploration. We demonstrate that the monoclinic polymorph (space group C2/c) of Na 2 Fe 2 F 7 (Mg0) and of a new Mg-substituted weberite composition, Na 2 Mg 0.125 Fe 1.875 F 7 (Mg0.125), can be isolated using an optimized synthesis protocol. The impact of Mg substitution on the stability of the weberite phase during electrochemical cycling, and on the extent and rate of Na (de)intercalation, is examined. Irrespective of the Mg content, we find that the weberite phase is retained when cycling over a narrow voltage window (2.8–4.0 V vs Na/Na+). Over a wider voltage range (1.9–4.0 V), Mg0 shows steady capacity fade due to its transformation to the NayFeF3 perovskite phase, while Mg0.125 displays more reversible cycling and a reduced phase transformation. Yet, Mg incorporation also leads to kinetically limited Na extraction and a reduced overall capacity. These findings highlight the need for the continued compositional optimization of weberite cathodes to improve their structural stability while maximizing their energy density.

25 ENERGY STORAGE↗

Factors affecting the open-circuit voltage and electrode kinetics of some iron/titanium redox flow cells

Performance of the iron-titanium redox flow cell was studied as a function of acid concentration. Anion permeable membranes separated the compartments. Electrodes were graphite cloth. Current densities ranged up to 25 mA/square centimeter. Open-circuit and load voltages decreased as the acidity was increased on the iron side as predicted. On the titanium side, open-circuit voltages decreased as the acidity was increased in agreement with theory, but load voltages increased due to decreased polarization with increasing acidity. High acidity on the titanium side coupled with low acidity on the iron side gives the best load voltage, but such cells show voltage losses as they are repeatedly cycled. Analyses show that the bulk of the voltage losses are due to diffusion of acid through the membrane.

Reid, M. A.↗

Cobalt-free composite-structured cathodes with lithium-stoichiometry control for sustainable lithium-ion batteries

Abstract Lithium-ion batteries play a crucial role in decarbonizing transportation and power grids, but their reliance on high-cost, earth-scarce cobalt in the commonly employed high-energy layered Li(NiMnCo)O 2 cathodes raises supply-chain and sustainability concerns. Despite numerous attempts to address this challenge, eliminating Co from Li(NiMnCo)O 2 remains elusive, as doing so detrimentally affects its layering and cycling stability. Here, we report on the rational stoichiometry control in synthesizing Li-deficient composite-structured LiNi 0.95 Mn 0.05 O 2 , comprising intergrown layered and rocksalt phases, which outperforms traditional layered counterparts. Through multiscale-correlated experimental characterization and computational modeling on the calcination process, we unveil the role of Li-deficiency in suppressing the rocksalt-to-layered phase transformation and crystal growth, leading to small-sized composites with the desired low anisotropic lattice expansion/contraction during charging and discharging. As a consequence, Li-deficient LiNi 0.95 Mn 0.05 O 2 delivers 90% first-cycle Coulombic efficiency, 90% capacity retention, and close-to-zero voltage fade for 100 deep cycles, showing its potential as a Co-free cathode for sustainable Li-ion batteries.

36 MATERIALS SCIENCE↗

Highly reversible Li 2 RuO 3 cathodes in sulfide-based all solid-state lithium batteries

The practical application of high-capacity lithium-rich cathode materials in lithium-ion batteries has been largely restricted by severe side reactions with electrolytes. Herein, we report a highly stable lithium-rich Li 2 RuO 3 cathode by forming a passivating solid electrolyte interphase at the interface with a sulfide solid electrolyte such as Li 6 PS 5 Cl in all-solid-state lithium batteries (ASSLBs), which efficiently suppresses serious parasitic interfacial reactions and fast-increasing interfacial impedance normally observed in liquid electrolytes. The exceptionally high interfacial stability of the Li 2 RuO 3 /sulfide electrolyte interface contributes to a high reversible capacity of 257 mA h g –1 of Li 2 RuO 3 at 0.05C rate, and unprecedented cycling stability with 90% capacity retention after 1000 cycles at 1C rate. Iin this work, comprehensive experimental characterizations and first-principles calculations disclose that electronically insulating interfacial reaction products forming at the interface between the Li 2 RuO 3 cathode and Li 6 PS 5 Cl facilitate the formation of a stable and passivating interphase and block the continuous side reactions. Importantly, reversible oxygen redox activity of Li 2 RuO 3 is well-maintained in this configuration of ASSLBs even after 600 cycles, thus the common voltage decay of the Li-rich material is also significantly reduced. These new discoveries demonstrate the critical role of interface design for achieving prolonged cycling stability of lithium-rich cathode materials.

25 ENERGY STORAGE↗

Serial Charging Test on High Capacity Li-Ion Cells for the Orbiter Advanced Hydraulic Power System

Although it looks like module level voltage drives the cutoff for charge, the actual cutoff is due to unbalanced cell voltages that drive the module voltage up. Individual cell voltage drives the cutoff for discharge Low resistance cells are the first to reach the low-voltage cutoff Cell-to-Cell voltage differences are generally small and show similar trends for each cycle Increase for a distinct window during charge and at the end of discharge Increase in max to min cell voltage difference with time/cycles Decrease in max to min cell voltage difference during high current pulses with time/cycles Individual cell voltage trends (with respect to other cells) are very repeatable from cycle to cycle, although voltage slowly degrades with time/cycles (resistance growth) Much more difference observed near end of discharge Little change in order of cell voltage (cell with highest voltage to cell with lowest voltage) Temp sensor on the side of cell (between 2 cells) shows much greater rise during discharge than for single cell tests (18 C vs 5 C) Conclusion: Serial Charging of this string of cells is feasible as it has only a minor impact on useful capacity

Jeevarajan, Judith A.↗

Pulse Electrodeposition for Carbonate-Rich Deposits from Seawater

Seawater electrodeposition is gaining renewed interest in the context of sustainable development, both to build climate-resilient coastal infrastructure and for ocean-based decarbonization applications. Most of the applications benefit from CaCO 3 -rich deposits, but constant-voltage electrodeposition results in a mixture of CaCO 3 and Mg(OH) 2 , especially at higher voltages where precipitation rates are more desirable. The use of pulse voltages can help control interfacial pH that dictates the precipitation reactions. Here, we explore the use of pulse electrodeposition as a function of pulse frequency and duty cycle to control deposit composition. The most CaCO 3 -rich deposits were obtained under 10 Hz frequency and 10% duty cycle conditions for the voltage window investigated (-0.8 V to -1.2 V vs. SCE). While pulsing the voltage increases the amount of CaCO 3 deposited, the energy required per gram of CaCO 3 is significantly higher (14.5×) when compared to the base case of applying a constant voltage of -0.8 V vs. SCE. Further optimization of pulse conditions, electrode materials, and system configuration could lead to finding parameters that result in exclusively carbonate deposits without compromising precipitation rates, which may prove to be more useful for corrosion protection, coastal infrastructure, and other applications in sustainable development.

54 ENVIRONMENTAL SCIENCES↗

Suppression of voltage-decay in Li 2 MnO 3 cathode via reconstruction of layered-spinel coexisting phases

Voltage decay, i.e., the voltage decrease during electrochemical cycling, has been a decade-long challenge for lithium-ion batteries. This issue not only leads to a substantial loss of energy density, but also raises challenges for the battery management system, hindering the commercial application of high capacity lithium-rich oxide. Here, we show that through a combination of electrochemical conditioning and thermal treatment, Li 2 MnO 3 , the parent compound of lithium-rich oxide, which typically displays severe voltage and capacity decay, could be converted into a new phase that essentially suppresses the voltage decay with improved capacity retention and rate performance. Furthermore, by combining atomic-sensitive nuclear magnetic resonance, differential electrochemical mass spectrometry and synchrotron-based resonant inelastic X-ray scattering, we disclose that treatment triggers the formation of three-coexisting phases, i.e., the lithium-rich layered, spinel and defect spinel phases, which enables improved reversibility of the oxygen redox activity and enhanced manganese redox reactions in the initial cycle. Our findings suggest the key role of the local structure in the voltage decay problem and provide insights for material optimizations towards lithium- and manganese-rich cathodes without the voltage decay.

25 ENERGY STORAGE↗

Effect of Inductance and Requirements for Surge Current Testing of Tantalum Capacitors

Surge current testing is considered one of the most important techniques to evaluate reliability and/or screen out potentially defective tantalum capacitors for low-impedance applications. Analysis of this test, as it is described in the MIL-PRF-55365 document, shows that it does not address several issues that are important to assure adequate and reproducible testing. This work investigates the effect of inductance of the test circuit on voltage and current transients and analyzes requirements for the elements of the circuit, in particular, resistance of the circuit, inductance of wires and resistors, type of switching devices, and characteristics of energy storage bank capacitors. Simple equations to estimate maximum inductance of the circuit to prevent voltage overshooting and minimum duration of charging/discharging cycles to avoid decreasing of the effective voltage and overheating of the parts during surge current testing are suggested.

Teverosky, Alexander↗

Ultra-Stretchable, Ionic Conducting, Pressure-Sensitive Adhesive with Dual Role for Stable Li-Metal Batteries

The practical application of lithium (Li) metal battery is impeded by the Li dendrite growth and unstable solid electrolyte interphase (SEI) layer. Herein, an ultra-stretchable and ionic conducting chemically crosslinked pressure-sensitive adhesive (cPSA) synthesized via the copolymerization of 2-ethylhexyl acrylate and acrylic acid with poly(ethyleneglycol)dimethacrylate as crosslinker (short for 70cPSA), is developed as both artificial SEI layer and solid polymer electrolyte (SPE) for stable Li-metal electrode, enabling all-solid-state Li metal batteries with excellent cycling performance. As an artificial SEI layer, the 70cPSA-modified electrodes exhibit excellent electrochemical performance in Li|70cPSA@Cu half cells and 70cPSA@Li|70cPSA@Li symmetric cells. In full cells with LiFePO 4 (LFP) as cathode, the 70cPSA@Li|LFP cell exhibits stable cycling performance over 250 cycles. Utilized as SPE, the all-solid-state Li|SPE|LFP cell delivers excellent cycling stability with a capacity retention of 86% over 500 cycles. With high-voltage LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) as cathode, the Li|SPE|NMC811 cell exhibits a discharge capacity of 124.3 mAh g -1 with a capacity retention of 71% after 200 cycles. Furthermore, the rational design of PSAs and investigation of their dual role for stable and safe Li-metal batteries may shed a light on adhesive polymers for battery applications.

25 ENERGY STORAGE↗

Minimizing Inter‐Lattice Strain to Stabilize Li‐Rich Cathode by Order–Disorder Control

Li-rich Mn-based layered (LMR) cathodes with anionic redox chemistry show great potential for next-generation sustainable Li-ion battery (LIB) applications due to the low cost and high energy density. However, the asynchronous structural evolutions with cycling in the heterogeneous composite structure of LMR lead to serious lattice strain and thus fast electrochemical decay, which hinders the commercialization of LMR cathodes. Here, in this study, an order–disorder coherent LMR cathode is demonstrated that exhibits a higher average voltage (by 0.25 V), negligible voltage decay (97.6% voltage retention after 100 cycles at 100 mA g −1 ), and enhanced cycling stability (98% capacity retention after 200 cycles at 100 mA g −1 ) compared to its layered oxide counterparts. It is proposed that this order–disorder coherent structure design can promote a more synchronous and homogeneous structure evolution during charge and discharge, thus minimizing lattice strain, which significantly prevents layer collapse and collective degradation at high voltage, improving the electrochemical stability. The study displays the feasibility of optimizing the performance of Li-rich cathode materials through a dedicated order–disorder structure control for sustainable energy storage.

Xu, Shenyang [Peking University, Shenzhen (China)]↗

Reaction inhomogeneity coupling with metal rearrangement triggers electrochemical degradation in lithium-rich layered cathode

High-energy density lithium-rich layered oxides are among the most promising candidates for next-generation energy storage. Unfortunately, these materials suffer from severe electrochemical degradation that includes capacity loss and voltage decay during long-term cycling. Present research efforts are primarily focused on understanding voltage decay phenomena while origins for capacity degradation have been largely ignored. Here, we thoroughly investigate causes for electrochemical performance decline with an emphasis on capacity loss in the lithium-rich layered oxides, as well as reaction pathways and kinetics. Advanced synchrotron-based X-ray two-dimensional and three-dimensional imaging techniques are combined with spectroscopic and scattering techniques to spatially visualize the reactivity at multiple length-scales on lithium- and manganese-rich layered oxides. These methods provide direct evidence for inhomogeneous manganese reactivity and ionic nickel rearrangement. Coupling deactivated manganese with nickel migration provides sluggish reaction kinetics and induces serious structural instability in the material. Our findings provide new insights and further understanding of electrochemical degradation, which serve to facilitate cathode material design improvements.

25 ENERGY STORAGE↗

Origin of Capacity Degradation of High-Voltage KVPO 4 F Cathode

Potassium vanadium fluorophosphate (KVPO 4 F) is one of the most promising cathode candidates for K-ion batteries because of its high specific capacity, voltage, and energy density. However, reducing its capacity fade remains an important challenge. This work leverages structure and electrochemical analysis to understand the capacity degradation mechanism of the KVPO 4 F cathode. Interestingly, no structural degradation of the KVPO4F cathode is detected after 200 cycles in the wide voltage window of 5.0-2.5 V (vs K/K + ). Instead, the capacity degradation is attributed to electrolyte decomposition at high voltage ( > 4.5 V vs K/K + ), which causes drying of the electrolyte and the formation of insulating layers on the cathode surface, significantly increasing the polarization. The properties of four KPF 6 - A nd carbonate-based K electrolytes are compared, and 0.7 M KPF 6 in ethylene carbonate/propylene carbonate exhibits the highest oxidation stability and results in the best cycling stability for the KVPO 4 cathode. These findings suggest that the key to improving the cycling stability of KVPO 4 F is to develop novel K electrolytes with even higher oxidation stability.

25 ENERGY STORAGE↗

Additive engineering for robust interphases to stabilize high-Ni layered structures at ultra-high voltage of 4.8 V

Nickel-rich layered cathode materials promise high energy density for next-generation batteries when coupled with lithium metal anodes. However, the practical capacities accessible are far less than the theoretical values due to their structural instability during cycling, especially when charged at high voltages. Here we demonstrate that stable cycling with an ultra-high cut-off voltage of 4.8 V can be realized by using an appropriate amount of lithium difluorophosphate in a common commercial electrolyte. The Li||LiNi 0.76 Mn 0.14 Co 0.10 O 2 cell retains 97% of the initial capacity (235 mAh g -1 ) after 200 cycles. The cycling stability is ascribed to the robust interphase on the cathode. It is formed by lithium difluorophosphate decomposition, which is facilitated by the catalytic effect of transition metals. The decomposition products (Li 3 PO 4 and LiF) form a protective interphase. This suppresses transition metal dissolution and cathode surface reconstruction. It also facilitates uniform Li distribution within the cathode, effectively mitigating the strain and crack formation.

25 ENERGY STORAGE↗

Scale-Up of Lithium Iron & Aluminum Nickelate Advanced Cathode and Fabrication of A Battery Pack Comprising The Same

Global battery manufacturers are increasingly worried about the serious supply chain constraint caused by rapid fluctuations in cobalt prices over the years. We present a novel cobalt-free, nickel-rich layered cathode material called NFA class (LiNixFeyAlzO2) to tackle this challenge. Spherical NFA(OH)2 precursors were successfully synthesized by incorporating Ni, Fe, and Al elements using a co-precipitation reaction in a continuous stirred tank reactor. The LiNFAO2 cathode, composed of LiNi0.85Fe0.05Al0.1O2, was synthesized and analyzed using X-Ray diffraction, Mössbauer spectroscopy, and scanning electron microscopy (SEM). The material's electrochemical behavior was evaluated through various techniques at different lithiation/delithiation states in two voltage ranges. The cobalt-free material exhibits a high capacity of 190 mAh/g at 0.1C within the voltage range of 3V-4.5V, as demonstrated by electrochemical performance evaluations. Rate and cycling evaluations showed good rate capability and cycling stability, with 88% capacity retention after 100 cycles at C/3 within the voltage range of 3V-4.3V. Our research shows the great potential of cobalt-free NFA cathodes as a feasible option for developing cost-effective lithium-ion batteries.

25 ENERGY STORAGE↗