The influence of temperature on fatigue-crack growth in a mill annealed Ti-6Al-4V alloy

To understand the influence temperature on the rate of fatigue crack growth in high strength metal alloys, constant load amplitude, fatigue crack growth experiments were carried out using a 1/4-inch-thick (6.35 mm) mill annealed Ti-6Al-4V alloy plate as a model material. The rates of fatigue crack growth were determined as a function of temperature, ranging from room temperature to about 290 C (or, about 550 F/563K) and as a function of the crack tip stress intensity factor in a dehumidified high purity argon environment. Limited correlative experiments indicate that dehumidified oxygen and hydrogen have no effect on the rate of fatigue crack growth in this alloy, while distilled water increased the rate of crack growth slightly in the range tested. Companion fractographic examinations suggest that the mechanisms for fatigue crack growth in the various environments are essentially the same.

Wei, R. P.↗

Annealing effects in plated-wire memory elements. I - Interdiffusion of copper and Permalloy.

Results of investigations using X-ray diffraction and electron-beam microprobe techniques have shown that copper and Permalloy platings interdiffuse at low temperatures when plated-wire memory elements are annealed for times as short as 50 hr. Measurable interdiffusion between Permalloy platings and gold substrates does not occur in similar conditions. Both magnetic and compositional changes during aging are found to occur by a thermally activated process with activation energies around 38 kcal/mol. It is shown, however, that copper-diffusion and magnetic-dispersion changes during aging are merely concurrent processes, neither being the other's cause.

Knudson, C. I.↗

The influence of temperature on fatigue crack growth in a mill annealed Ti-6Al-4V alloy.

To study the influence of temperature on the rate of fatigue crack growth in high strength metal alloys, constant load amplitude fatigue crack growth experiments were carried out using a .25-in.-thick mill annealed Ti-6Al-4V alloy plate. The rates of fatigue crack growth were determined as a function of temperature, ranging from room temperature to about 290 C, and as a function of the crack tip stress intensity factor in a dehumidified high purity argon environment. Limited correlative experiments were carried out in distilled water, dehumidified oxygen and hydrogen, and in vacuum. The results indicate that the rate of fatigue crack growth is essentially independent of test temperature in this alloy, and is affected by residual moisture in very small concentrations. Companion fractographic examinations suggest that the mechanims for fatigue crack growth in the various environments are essentially the same.

Wei, R. P.↗

The influence of temperature on fatigue-crack growth in a mill-annealed Ti-6Al-4V alloy

To understand the influence of temperature on the rate of fatigue crack growth in high strength metal alloys, constant load amplitude fatigue crack growth experiments were carried out using a 1/4 inch thick (6.35 mm) mill-annealed Ti-6Al-4V alloy plate as a model material. The rates of fatigue crack growth were determined as a function of temperature, ranging from room temperature to about 290 C and as a function of the crack tip, stress intensity factor K, in dehumidified high purity argon environment. The dependence of the rate of fatigue crack growth on K appears to be separable into two regions. The transition correlates with changes in both the microscopic and macroscopic appearances of the fracture surfaces, and suggests a change in the mechanism and the influence of microstructure on fatigue crack growth.

Wei, R. P.↗

Growth of surface and corner cracks in beta-processed and mill-annealed Ti-6Al-4V

Empirical stress-intensity expressions were developed to relate the growth of cracks from corner flaws to the growth of cracks from surface flaws. An experimental program using beta-processed Ti-6Al-4V verified these expressions for stress ratios, R greater than or equal to 0. An empirical crack growth-rate expression which included stress-ratio and stress-level effects was also developed. Cracks grew approximately 10 percent faster in transverse-grain material than in longitudinal-grain material and at approximately the same rate in longitudinal-grain mill-annealed Ti-6Al-4V. Specimens having surface and corner cracks and made of longitudinal-grain, beta-processed material were tested with block loads, and increasing the stresses in a block did not significantly change the crack growth rates. Truncation of the basic ascending stress sequence within a block caused more rapid crack growth, whereas both the descending and low-to-high stress sequences slowed crack growth.

Bell, P. D.↗

Alteration of an annealed and irradiated lunar fines sample by adsorbed water

Apollo 12 lunar fines sample 12070,403 was annealed at 1000 C and subsequently irradiated with a beam of 130 MeV Fe(9+) ions. Adsorptions of nitrogen and water were measured before and after the irradiation. Prior to the irradiation, the fines were nonporous and water had no effect on the physical characteristics of the lunar fines. In contrast, after the irradiation, the interaction with water caused an increase in the specific surface area and created a pore system. These results are definitive evidence that the interaction of water with damage tracks is the prime factor involved in the alteration of lunar fines by adsorbed water.

Holmes, H. F.↗

The stress corrosion resistance and the cryogenic temperature mechanical properties of annealed Nitronic 60 bar material

Ambient and cryogenic temperature mechanical properties and the ambient temperature stress corrosion properties of annealed, straightened, and centerless ground Nitronic 60 stainless steel alloy bar material are presented. The mechanical properties of longitudinal specimens were evaluated at test temperatures from ambient to liquid hydrogen. The tensile test data indicated increasing strength with decreasing temperature to -196 C. Below liquid nitrogen temperature the smooth tensile and notched tensile strengths decreased slightly while the elongation and reduction of area decreased drastically. The Charpy V-notched impact energy decreased steadily with decreasing test temperature. Stress corrosion tests were performed on longitudinal tensile specimens and transverse C-ring specimens exposed to: alternate immersion in a 3.5% NaCl bath; humidity cabinet; and a 5% salt spray atmosphere. The longitudinal tensile specimens experienced no corrosive attack. Approximately 3/4 of the transverse C-rings exposed to alternate immersion and to salt spray experienced a pitting attack on the top and bottom ends. Additional stress corrosion tests were performed on transverse tensile specimens. No failures occurred in the 90% stressed specimens exposed for 90 days in the alternate immersion and salt spray environments

Montano, J. W. L.↗

The influence of composition, annealing treatment, and texture on the fracture toughness of Ti-5Al-2.5Sn plate at cryogenic temperatures

The plane strain fracture toughness K sub Ic and conventional tensile properties of two commercially produced one-inch thick Ti-5Al-2.5Sn plates were determined at cryogenic temperatures. One plate was extra-low interstitial (ELI) grade, the other normal interstitial. Portions of each plate were mill annealed at 1088 K (1500 F) followed by either air cooling or furnace cooling. The tensile properties, flow curves, and K sub Ic of these plates were determined at 295 K (room temperature), 77 K (liquid nitrogen temperature), and 20 K (liquid hydrogen temperature).

Vanstone, R. H.↗

Reverse annealing in radiation-damaged, silicon solar cells

In order to understand the results in terms of properties of the radiation induced defects, a combination of diffusion length measurements and defect data obtained from Deep Level Transient Spectroscopy were used. The results indicate that the defect at E sub v + 0.30 eV is responsible for the observed reversed annealing. The defect was identified as a boron-oxygen vacancy complex. This identification is a guide to processing efforts aimed at increasing the concentration of these radiation induced defects.

Weinberg, I.↗

Magnetic and metallurgical properties of directionally solidified eutectic Bi/MnBi composites - The effects of annealing

Eutectic Bi/MnBi (97.8 a/o Bi) samples have been plane-front directionally solidified. The resultant microstructures consist of elongated, aligned particles of MnBi dispersed in a Bi-matrix. Magnetization as a function of temperature (4.2 to 300 K) and applied field (up to 220 kG) has been used to evaluate solidification parameters and magnetic properties. At room temperature, in addition to the diamagnetic contribution of Bi, one finds a superposition of the ferromagnetic, low temperature (LTP) MnBi phase and paramagnetic phases. At cryogenic temperatures, one of the room temperature paramagnetic phases is ferromagnetic with an intrinsic coercivity of 120 kOe while the other remains paramagnetic for low fields and orders ferromagnetically at high fields in a complicated way. Annealing of as-grown samples was found to produce significant changes in magnetic properties. The origins of the paramagnetic phases and their relation to the mechanisms which control the coercive field of the hard magnetic LTP MnBi phase are discussed.

Pirich, R. G.↗

Solar power satellite system definition study. Volume 4: Silicon solar cell annealing test, phase 1

Laser annealing tests were conducted on ten 50 micron cells. Two were control cells that were not irradiated. These showed no loss in output due to exposure to the laser. Two cells were broken in handling. Six cells were successfully tested. All cells tested without breakage showed some recovery. One cell was subjected to two cycles and showed recovery on both cycles. Cells that were moderately degraded appeared to recover more completely than those more severly degraded. Exposure times ranged from two to ten seconds at 500 degrees centigrade. There was some indication that longer exposure was beneficial.

Walker, F.↗

Annealing radiation damaged silicon solar cells with a copper halide laser

The use of a multiply pulsed copper halide laser to significantly anneal out the damage to silicon solar cells caused by a simulated space radiation environment is investigated. Preliminary experiments demonstrate that the amount of damage can be decreased by 41% as measured by the maximum power generated.

Pivirotto, T. J.↗

The influence of isothermal annealing on the molybdenum fibers of a directed solid gamma/gamma prime - alpha alloy

The mechanical characteristics of the directed solid eutectic Ni-Al-Mo (gamma/gamma prime)-alpha alloy at high temperatures make it useful in the blades of gas turbines. Structural changes are observed for the alloy under isothermal annealing, particularly the formation of molybdenum plates at the grain boundary and an increase of the gamma phase in relation to the gamma prime phase. Molybdenum lamellas appear at the grain boundary above 1100 C which can have a negative influence on the mechanical properties. The change in the structure near the grain boundary with the increase in temperature is illustrated through a sequence of pictures.

Whittenberger, J. D.↗

Study of radiation induced deep-level defects and annealing effects in the proton irradiated AlGaAs-GaAs solar cells

The radiation induced deep-level defects and the recombination parameters in the proton irradiated AlGaAs-GaAs p-n junction solar cells were investigated over a wide range of proton energies (from 50 KeV to 10 MeV) and proton fluences (from 10 to the 10th to 10 to the 13th P/sq cm), using DLTS, I-V, C-V, and SEM-EMIC measurement techniques. The measurements were used to determine the defect and recombination parameters such as defect density and energy level, carrier lifetimes, and the hole diffusion lengths in the GaAs LPE layers. Results show that a good correlation was obtained between the measured defect parameters and the dark recombination current as well as the performance parameters of the solar cells. The most damages to the cell were produced by the 200 KeV protons. In addition, the effects of low temperatures (200 to 400 C) thermal annealing on the deep-level defects and the dark current of the 200 KeV proton irradiated samples were examined.

Li, S. S.↗

A thermochemical model of radiation damage and annealing applied to GaAs solar cells

Calculations of the equilibrium conditions for continuous radiation damage and thermal annealing are reported. The calculations are based on a thermochemical model developed to analyze the incorporation of point imperfections in GaAs, and modified by introducing the radiation to produce native lattice defects rather than high-temperature and arsenic atmospheric pressure. The concentration of a set of defects, including vacancies, divacancies, and impurity vacancy complexes, are calculated as a function of temperature. Minority carrier lifetimes, short circuit current, and efficiency are deduced for a range of equilibrium temperatures. The results indicate that GaAs solar cells could have a mission life which is not greatly limited by radiation damage.

Conway, E. J.↗

Annealing Solar Cells With Lasers

Laser anneals silicon solar cells rapidly enough for use in production. Laser frequently doubled neoduyminum: yttrium-aluminum-garnet (Nd:YAG) device. 30-m-diameter spot formed by lasers covers enough area to process silicon wafers rapidly. Laser anealed cells have efficiencies greater than 15 percent.

Katzeff, J. S.↗

Radiation damage and annealing of amorphous silicon solar cells

Amorphous silicon solar cells were irradiated with 1 MeV electrons at the Space Environmental Effects Laboratory of the NASA Langley Research Center. The cells accumulated a total fluence of 10 to the 14th, 10 to the 15th, and 10 to the 16th electrons per square centimeter and exhibited increasing degradation with each irradiation. This degradation was tracked by evaluating the I-V curves for AM0 illumination and the relative spectral response. The observed radiation damage was reversed following an anneal of the cells under vacuum at 200 C for 2 hours.

Byvik, C. E.↗