At least 253 records · Page 14

Electrochemical-driven green recovery of lithium, graphite and cathode from lithium-ion batteries using water

The expected exponential increase in consumption of lithium-ion batteries (LIBs) would pose a unique challenge to the availability of near-critical resources like lithium and graphite in the upcoming decade. In this work, we present a lithium recovery process that utilizes a degradation mechanism, i.e., lithium plating, as a tool to concentrate metallic lithium at the anode/separator interface for convenient extraction at room temperature – using only water. Electrochemical characterization of fast charged (1–6 C) LIBs yielded a maximum capacity fade of 50% over ten cycles. The lithium plating was confirmed via voltage plateau analysis, coulombic efficiency, and DC resistance measurements. A maximum lithium plating condition was observed to exist between 4C and 5C, thereby limiting the energy consumption in the extraction process. Post-mortem film thickness measurement showed an incrementing film deposition with a maximum of 35 µm thickness. SEM and XPS analysis confirmed increasing concentration of a dense dendritic metallic lithium deposition on the anode/separator interface with C-rate. A green recovery process was adopted to extract the concentrated metallic lithium using distilled water. The lithium from the plated film, solid/electrolyte interface (SEI), electrolyte, anode, and cathode, was extracted as salts. A 37% improvement in lithium recoverability was achieved with fast charging under ambient conditions. XPS analysis showed ~92% of lithium yield with no residual lithium in the graphite. In addition, the battery-grade graphite was recovered with 97% purity after heat treatment of the washed anode film, and concentrated transition metals oxides in the cathode to 93% purity for convenient extraction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Quantifying lithium loss in amorphous silicon thin-film anodes via titration-gas chromatography

Silicon with a high theoretical capacity (3,579 mAh/g) is a promising anode candidate for lithium-ion batteries. However, commercialization is still impeded by low Coulombic efficiency, caused by solid electrolyte interphase (SEI) formation and trapped lithium (Li)-silicon (Si) alloy during repeated volume change. Quantifying capacity losses from each factor is crucial to formulate rational design strategies for further improvement. In this work, titration-gas chromatography and cryogenic transmission electron microscopy are applied to characterize the evolution of trapped Li-Si alloy and SEI growth in a silicon thin-film anode. It is found that continuous growth of the SEI is the dominant factor for lithium inventory loss during cycling, with only a marginal increase in trapped Li-Si alloy. This study offers a quantitative approach to differentiate Li in the SEI from trapped Li in Li-Si alloy through a silicon thin-film anode, providing unique insights into identifying critical bottlenecks for developing Si anodes.

25 ENERGY STORAGE↗

Investigation of electrode-electrolyte interfaces to enable non-flammable Li-ion batteries operating up to 125°C with liquid electrolyte

Non-flammable and high-temperature stable ionic liquid (IL)-based electrolytes could eliminate catastrophic battery failures and improve battery safety, but their poor electrochemical interaction with the LiNi x Mn y Co z O 2 (NMC) family of cathodes is a long-standing problem due to severe parasitic reactions at high temperature. Understanding surface and bulk structural mechanisms of NMC-type cathodes at elevated operational temperature is of paramount importance to facilitate stable electrochemical performance. Here, we report a non-flammable phosphonium IL-based cell chemistry that offers stable electrode-electrolyte interfaces, leading to electrochemical performance up to 125°C and high-temperature safety. We combine electrochemistry with multimodal X-ray spectroscopy methods to understand interfaces at elevated temperature (100°C). This nanoscale understating enables a proof-of-concept high-temperature cylindrical cell (14500), and the design achieves an average Coulombic efficiency of ≈99.5% up to 300 cycles at 100°C. The results ascertain the significance of depth-dependent degradation at the interface, guiding room-temperature Li-ion technology toward extreme-temperature applications.

36 MATERIALS SCIENCE↗

Emerging Potassium Metal Anodes: Perspectives on Control of the Electrochemical Interfaces

Potassium metal acts as the anode in emerging potassium metal batteries (KMBs). It further serves as the counter-electrode for potassium ion battery (KIB) half-cells, with its reliable performance being critical for assessing the working electrode material. This first-of-its-kind critical review focuses on the dual challenge of controlling the potassium metal-substrate and the potassium metal-electrolyte interface so as to prevent dendrites. The discussion begins with a comparison of the physical and chemical properties of K metal anodes versus the much oft studied Li and Na metal anodes. Based on established descriptions for root causes of dendrites, the problem should be less severe for K than for Li or Na, while in fact the opposite is observed. The key reason that the K metal surface rapidly becomes dendritic in common electrolytes is its unstable solid electrolyte interphase (SEI). An unstable SEI layer is defined as being non self-passivating. No SEI is perfectly stable during cycling, and all SEI structures are heterogenous both vertically and horizontally relative to the electrolyte interface. The difference between a "stable" and an "unstable" SEI may be viewed as the relative degree to which during cycling it thickens and becomes further heterogeneous. The unstable SEI on K metal leads to a number of interrelated problems, such as low cycling Coulombic efficiency (CE), a severe impedance rise, large overpotentials, and possibly electrical shorting; all of which have been reported to occur as early as in the first ten plating/stripping cycles. Many of the traditional "interface fixes" employed for Li and Na metal anodes, such as various artificial SEIs, surface membranes, barrier layers, the secondary separators, etc. have not been attempted or optimized for the case of K. This is an important area for further exploration, with an understanding that success may come harder than with Li due to K-based SEI reactivity with both ether and ester solvents. The second critical problem with K metal anodes is that they do not thermally or electrochemically wet a standard (untreated) Cu foil current collector. Published experimental and modeling research directly highlights the weak bonding between the K atoms and a Cu surface. Existing surface treatment approaches that achieve improved K wetting are discussed, along with the general design rules for future studies. Also discussed are geometry-based methods to tune nucleation, as well dual approaches where nucleation and SEI structure are tuned through complementary schemes to achieve extended half-cell and full battery stability. We hypothesize that K metal never achieves a planar wetting morphology even at cycle one making the dendrites "baked-in". We propose that classical thin films growth models, Frank van der Merwe (F-M), Volmer Weber (V-W), and Stranski-Krastanov (S-K) can be employed to describe early stage plating behavior. It is demonstrated that island-like V-W growth is the applicable description for the natural plating behavior of K on pristine Cu. Moving forward, there are three inter-related thrusts to be pursued: First, K salt - based electrolyte formulations have to mature and become further tailored to handle the increased reactivity of a metal rather than an ion anode. Second, the K-based SEI structure needs to be further understood and ultimately tuned to be less reactive. Third, the energetics of the K metal - current collector interface must be controlled to promote planar wetting/dewetting throughout cycling.

25 ENERGY STORAGE↗

Excitonic Effects in X-ray Absorption Spectra of Fluoride Salts and Their Surfaces

Given their natural abundance and thermodynamic stability, fluoride salts may appear as evolving components of electrochemical interfaces in Li-ion batteries and emergent multivalent ion cells. This is due to the practice of employing electrolytes with fluorine-containing species (salt, solvent, or additives) that electrochemically decompose and deposit on the electrodes. Operando X-ray absorption spectroscopy (XAS) can probe the electrode–electrolyte interface with a single-digit nanometer depth resolution and offers a wealth of insights into the evolution and Coulombic efficiency or degradation of prototype cells, provided that the spectra can be reliably interpreted in terms of local oxidation state, atomic coordination, and electronic structure about the excited atoms. Here we explore fluorine K-edge XAS of mono- (Li, Na, and K) and di-valent (Mg, Ca, and Zn) fluoride salts from a theoretical standpoint and discover a surprising level of detailed electronic structure information about these materials despite the relatively predictable oxidation state and ionicity of the fluoride anion and the metal cation. Utilizing a recently developed many-body approach based on the ΔSCF method, we calculate the XAS using density functional theory and experimental spectral profiles are well reproduced despite some experimental discrepancies in energy alignment within the literature, which we can correct for in our simulations. We outline a general methodology to explain shifts in the main XAS peak energies in terms of a simple exciton model and explain line-shape differences resulting from the mixing of core-excited states with metal d character (for K and Ca specifically). Given ultimate applications to evolving interfaces, some understanding of the role of surfaces and their terminations in defining new spectral features is provided to indicate the sensitivity of such measurements to changes in interfacial chemistry.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Semiconducting Zn x Mo 3 S 13 -GO Chalcocarbogel: A High-Capacity and Stable Sulfur-Equivalent Conversion-Based Electrode for Lithium-Ion Batteries

Lithium–sulfur batteries with a sulfur electrode offer a theoretical capacity of ∼1672 mAh g –1 , but rapid capacity loss mainly constrains their practical application. This work introduces a semiconducting and amorphous Zn x Mo 3 S 13 -GO (x = 0.5) chalcocarbogel sulfur-equivalent electrode with superior capacity and stability for lithium-ion batteries (LIBs). The Zn x Mo 3 S 13 -GO is synthesized in solution under ambient conditions, and its local structure contains S–S, M-Q (M = Mo, Zn; Q = S, O), C–S, and Mo–Mo bonding motifs with Mo coordination environment closely related to Mo 3 S 13 anions, as determined by X-ray photoelectron spectroscopy, synchrotron X-ray scattering, X-ray absorption spectroscopy, and ab initio molecular dynamics simulations. The Li/Zn x Mo 3 S 13 -GO cell offers an initial discharge capacity of 1019 mAh g –1 at a rate of C/3. After the activation cycles, the Li/Zn x Mo 3 S 13 -GO cell demonstrates good cycling stability, retaining a discharge capacity of 519.4 mAh g –1 after 250 cycles with ∼99.98% Coulombic efficiency and excellent rate capabilities. Moreover, it provides an initial discharge capacity of ∼574 mAh g –1 and maintains a retention capacity of 279 mAh g –1 at 1C after 625 cycles. The Lewis acidic Zn 2+ ion enhances the Lewis basic polysulfide anchoring ability and reduces the dissolution of polysulfides produced during the redox process through Zn–S covalent interaction, while the semiconducting and amorphous structure of the chalcocarbogel increases the electrical and ionic conductivity. Furthermore, this work highlights chalcocarbogels’ potential for developing high-capacity and stable electrodes for LIBs.

25 ENERGY STORAGE↗

On the Structural Origin of Fast Li-Ion Cycling in Tetragonal Bronze-Type Nb 8 W 9 O 47

Bronze and bronze-derived, mixed metal oxides are materials of growing interest for lithium-ion battery anodes due to their high-rate capabilities and the potential for high energy densities via multielectron redox. We report on the synthesis and electrochemical properties of the tetragonal tungsten bronzetype phase Nb 8 W 9 O 47 and our investigation into the structural evolution of this phase upon lithium (de)intercalation, with particular attention to how it relates to the fast-cycling capabilities. Electrochemical cycling shows Nb 8 W 9 O 47 can achieve greater than one Li + per transition metal at rates of C/2 or slower and maintains a capacity equivalent to 0.65 Li + per transition metal at a rate of 20C. Sequential Rietveld analysis of operando X-ray diffraction data reveals anisotropic changes to the unit cell parameters during discharge, accompanied by an off-centering of the transition metals within their octahedral environments. While higher capacities can be accessed below 1.2 V, cells discharged to 1.0 V exhibit a significant expansion of the unit cell volume and reduced Coulombic efficiencies. This report suggests that rigid crystal structures incapable of undergoing polyhedral rotational deformations can instead exploit displacive distortions of the transition metal redox center to enable fast Li-ion cycling with minimal atomic rearrangements.

25 ENERGY STORAGE↗

Low-Temperature Processing of Pyrolysis Bio-Oil for Sustainable Biographite Production

Catalytic graphitization of pyrolysis bio-oil with iron (Fe) can produce an anode material for lithium-ion batteries (LIBs) at a moderate temperature. The key challenge to scaling up the process is foaming, which occurs due to the oxidation of Fe by the organic acids present in bio-oil. This study explored five different pathways to control foaming in bio-oil upon Fe addition, including (i) defoamers use, (ii) use of iron oxide (Fe2O3) as graphitization catalyst, (iii) pH adjustment of bio-oil, (iv) bio-oil coking (300-500 degrees C), and (v) low-temperature pretreatment of bio-oil (150-200 degrees C). The low-temperature pretreatment successfully avoided foaming by removing the volatile acids in bio-oil. The bio-oil was solidified and powdered for even mixing with the Fe catalyst. The biographite catalytically prepared at 1500 degrees C following this pathway demonstrated nearly theoretical specific gravimetric capacity (~370 mAh/g), high initial Coulombic efficiency (90.03%), and minimal capacity fading after 50 cycles in LIB half-cells. The low-temperature pretreatment pathway also addressed the viscosity, swelling, and aging issues associated with bio-oil processing and will make scale-up endeavors more attainable.

09 BIOMASS FUELS↗

Efficacy of Stabilizing Calcium Battery Electrolytes through Salt-Directed Coordination Change

Achieving practical, high-energy-density calcium batteries requires controlling the stability of Ca 2+ electrolytes during calcium metal cycling. Because of the highly reactive nature of calcium, most typical electrolyte constituents are unstable, leading to electrode passivation and low Coulombic efficiency. Among various commercially available salts, calcium bis(trifluoromethylsulfonyl)imide (Ca(TFSI) 2 ) is attractive because of its oxidative stability and high solubility in a variety of solvents. However, this salt does not allow for calcium metal plating, and it has been proposed that TFSI – instability induced by Ca 2+ coordination is to blame. In this work, we test the ability of strongly coordinating Ca 2+ cosalts such as halides and borohydrides to displace TFSI – from the first coordination shell of Ca 2+ and thereby stabilize TFSI-based electrolytes to enable calcium plating. Through spectroscopic analysis, we find that the effectiveness of these cosalts at displacing the TFSI – anion is dependent on the solvent’s coordination strength toward Ca 2+ . Surprisingly, electrochemical calcium deposition behavior is not correlated to the population of bound or free TFSI – . Instead, the nature of the coordination interaction between Ca 2+ and the cosalt anion is more important for determining stability. Our findings indicate that TFSI – anions are inherently unstable during calcium deposition even in the nominally free state. Furthermore, strategies aimed at eliminating the interactions of these anions with the electrode surface via interface/interphase design are required.

25 ENERGY STORAGE↗

Room-Temperature Calcium Plating and Stripping Using a Perfluoroalkoxyaluminate Anion Electrolyte

Multivalent ion chemistries, like Ca 2+ , used in energy storage boast the potential to utilize solid metallic anodes and provide high volumetric energy density. The promise of such systems relies on the ability to incorporate high-voltage cathode materials while sustaining robust plating and stripping at the anode. These processes are dependent on an electrochemically stable electrolyte for ion transport and storage. In this work, we report an addition to the limited pool of nonaqueous electrolytes capable of plating and stripping calcium at room temperature. The synthesis and structural properties of calcium tetrakis(perfluoro-tert-butoxy) aluminate (Ca[TPFA] 2 ) are described along with the electrochemical performance during plating and stripping (up to 55% Coulombic efficiency) and a proof of concept for full cell viability with a CuS cathode material. X-ray experiments were used to study both the bulk solvation structure around calcium and possible decomposition pathways of the weakly coordinating TPFA anion.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Failure Process During Fast Charging of Lithium Metal Batteries with Weakly Solvating Fluoroether Electrolytes

While improving the lithium metal (Li) Coulombic efficiency has been a focus for electrolyte design, the performance under high current densities is less studied yet highly relevant for practical applications. Here, we evaluate the charge-rate-dependent cycling stability using three types of weakly solvating fluoroether electrolytes. Although good cycle life was achieved in all three electrolytes under low current densities, they all exhibited a soft shorting behavior above various threshold current densities (between 2 and 5.2 mA cm –2 ). In this study, we attributed the current-dependent electrode morphology to both Li growth and residual solid electrolyte interface (rSEI) growth processes. In early cycles, Li morphology guided the formation of rSEI structures. In later cycles, the rSEI structure partially impacted Li growth. Under low current densities, the rSEI was inhomogeneous with large voids for subsequent bulky lithium growth. Under high current densities, the rSEI became more dense, which aggravated the high-surface/volume-ratio Li growth through and on the top of the rSEI. Among the three weakly solvating fluoroether electrolytes, the ones with lower ionic conductivity were observed to short within fewer cycles and at lower charge current densities. Our work suggests that fast ion transport in electrolytes may be a desirable feature for the stable operation at >1C charging in high-energy-density lithium metal batteries.

25 ENERGY STORAGE↗

Evolution and Degradation Patterns of Electrochemical Cells Based on the Analysis of Interfacial Phenomena at Li Metal Anode/Electrolyte Interfaces

In this work, we report the results of a theoretical–computational analysis of the solid electrolyte interphase (SEI) growth and degradation dynamics occurring in lithium metal batteries during cycling. We use ab initio-kinetic Monte Carlo simulations to generate a synthetic data set, which is analyzed by machine learning methods. We aim to determine: (i) how modifications in interfacial interaction energies between solid electrolyte interphase (SEI) blocks and between Li ions and SEI facets impact the Coulombic efficiency (CE) of the battery and (ii) what factors, including reactions, microscopic transport, and other interfacial events, may lead to cell performance “failure” during prolonged charge and discharge cycles, signaled as a sharp decay in the CE over cycling. The demonstration of our approach is done on a cell including a Li metal surface interfacing with a previously introduced state-of-the-art electrolyte, and the idea can be applied to any electrochemical system. Outcomes include the identification of the leading chemical, physical, and structural variables causing cell failure and relating them to the electrolyte formulation, thus paving the way to future more refined analysis and electrolyte design.

batteries↗

Design Principles and Routes for Calcium Alkoxyaluminate Electrolytes

Multivalent-ion battery technologies are increasingly attractive options for meeting diverse energy storage needs. Calcium ion batteries (CIB) are particularly appealing candidates for their earthly abundance, high theoretical volumetric energy density, and relative safety advantages. Here, at present, only a few Ca-ion electrolyte systems are reported to reversibly plate at room temperature: for example, aluminates and borates, including Ca[TPFA] 2 , where [TPFA] - = [Al(OC(CF 3 ) 3 ) 4 ] - and Ca[B(hfip) 4 ] 2 , [B(hfip) 4 ] 2 – = [B(OCH(CF 3 ) 2 ) 4 ] - . Analyzing the structure of these salts reveals a common theme: the prevalent use of a weakly coordinating anion (WCA) consisting of a tetracoordinate aluminum/boron (Al/B) center with fluorinated alkoxides. Leveraging the concept of theory-aided design, we report an innovative, one-pot synthesis of two new calcium-ion electrolyte salts (Ca[Al(tftb) 4 ] 2 , Ca[Al(hftb) 4 ] 2 ) and two reported salts (Ca[Al(hfip) 4 ] 2 and Ca[TPFA] 2 ) where hfip = (-OCH(CF 3 ) 2 ), tftb = (-OC(CF 3 )(Me) 2 ), hftb = (-OC(CF 3 ) 2 (Me)), [TPFA] - = [Al(OC(CF 3 ) 3 ) 4 ] - . We also reveal the dependence of Coulombic efficiency on their inherent propensity for cation–anion coordination.

25 ENERGY STORAGE↗

Complexing Agent-Assisted Membraneless Zinc–Iodine Aqueous Batteries

A membrane is required for conventional zinc–iodine aqueous batteries, since soluble polyiodides cross over to the anode side and react with zinc metal spontaneously. Making the battery membraneless increases ion transport and reduces its cost and overall footprint. In this paper, a membraneless Zn–I 2 aqueous battery is demonstrated, employing a complexing agent, 1-butyl-1-methylpyrrolidinium iodide (MBPI), to promote the formation of I 5 – -containing, phase-separated polyiodides upon charging, to minimize self-discharge and suppress Zn dendrite growth. With an additional 0.3 M MBPI in 4 M ZnI 2 electrolyte, the membraneless battery achieved 65 cycles with >85% Coulombic efficiency, whereas the MBPI-free control failed immediately. Additionally, a volumetric capacity of 14.3 Ah L –1 was achieved, surpassing those of most membraneless batteries reported to date regardless of redox chemistry, and underscores the potential of complexing agents in simplifying the architecture of conventional Zn–I 2 flow batteries.

25 ENERGY STORAGE↗

A High-Rate Lithium Manganese Oxide-Hydrogen Battery

Rechargeable hydrogen gas batteries show promises for the integration of renewable yet intermittent solar and wind electricity into the grid energy storage. Here, we describe a rechargeable, high-rate, and long-life hydrogen gas battery that exploits a nanostructured lithium manganese oxide cathode and a hydrogen gas anode in an aqueous electrolyte. The proposed lithium manganese oxide-hydrogen battery shows a discharge potential of ~1.3 V, a remarkable rate of 50 C with Coulombic efficiency of ~99.8%, and a robust cycle life. A systematic electrochemical study demonstrates the significance of the electrocatalytic hydrogen gas anode and reveals the charge storage mechanism of the lithium manganese oxide-hydrogen battery. This work provides opportunities for the development of new rechargeable hydrogen batteries for the future grid-scale energy storage.

25 ENERGY STORAGE↗

Elucidating Interfacial Stability between Lithium Metal Anode and Li Phosphorus Oxynitride via In Situ Electron Microscopy

Li phosphorus oxynitride (LiPON) is one of a very few solid electrolytes that have demonstrated high stability against Li metal and extended cyclability with high Coulombic efficiency for all solid-state batteries (ASSBs). However, theoretical calculations show that LiPON reacts with Li metal. Here, we utilize in situ electron microscopy to observe the dynamic evolutions at the LiPON–Li interface upon contacting and under biasing. We reveal that a thin interface layer (~60 nm) develops at the LiPON–Li interface upon contact. This layer is composed of conductive binary compounds that show a unique spatial distribution that warrants an electrochemical stability of the interface, serving as an effective passivation layer. Our results explicate the excellent cyclability of LiPON and reconcile the existing debates regarding the stability of the LiPON–Li interface, demonstrating that, though glassy solid electrolytes may not have a perfect initial electrochemical window with Li metal, they may excel in future applications for ASSBs.

25 ENERGY STORAGE↗

In Situ Formation of Polycyclic Aromatic Hydrocarbons as an Artificial Hybrid Layer for Lithium Metal Anodes

Nonuniform Li deposition causes dendrites and low Coulombic efficiency (CE), seriously hindering the practical applications of Li metal. Herein, we developed an artificial solid-state interphase (SEI) with planar polycyclic aromatic hydrocarbons (PAHs) on the surface of Li metal anodes by a facile in situ formation technology. The resultant dihydroxyviolanthron (DHV) layers serve as the protective layer to stabilize the SEI. In addition, the oxygen-containing functional groups in the soft and conformal SEI film can regulate the diffusion and transport of Li ions to homogenize the deposition of Li metal. The artificial SEI significantly improves the CEs and shows superior cyclability of over 1000 h at 4 mAh cm –2 . The LiFePO 4 /Li cell (2.8 mAh cm –2 ) enables a long cyclability for 300 cycles and high CEs of 99.8%. Furthermore, this work offers a new strategy to inhibit Li dendrite growth and enlightens the design on stable SEI for metal anodes.

25 ENERGY STORAGE↗