Covalent Organic Framework as an Efficient Protection Layer for a Stable Lithium-Metal Anode

We report Lithium (Li) metal shows great potential for achieving high-energy-density rechargeable batteries. However, the practical applications of Li-metal batteries are still challenged by the formation of Li dendrites and unstable solid-electrolyte interphase (SEI) on metallic Li. Herein, a thin covalent organic framework layer is in situ fabricated on Li (COF-Li) to suppress Li dendrite growth and mitigate the side reaction on the Li anode. The COF has a periodic and uniform porosity, allowing for selectively sieving Li ions and guiding a uniform Li deposition. As a result, the COF-Li exhibits a non-dendrite morphology during repeated Li plating/stripping and demonstrates a remarkable cycle life over 13 200 h with an extremely low overpotential of only 16 mV at a high current density of 10 mA cm -2 and a high areal capacity of 10 mAh cm -2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of Laser Fluence on Microstructure and Bonding Characteristics of Wideband Laser-Deposited Nickel Composite Coatings

The wideband laser has shown great potential in metal–ceramic coatings deposition due to the high efficiency and low dilution rate. However, the effects of wideband laser process on microstructure evolution and bonding mechanism at the coatings/substrate interface are still a critical problem and need further investigation. In this work, nickel composite coatings are fabricated on the surface high-strength low-alloy steel. The effects of laser fluence on microstructure evolution, shear strength and fracture mechanism are studied. Results indicated the added WC particles were partly dissolved due to the high-power laser irradiation. Many block precipitates and dense eutectic were synthesized in composite coatings. Reinforced phases mainly consist of Cr{sub 5}B{sub 3}, Cr{sub 23}C{sub 6}, W{sub 2}C and Cr{sub 3}Ni{sub 2}. The dilution of Q550 steel contributed to the formation of nickel dendrites and facilitated a dense metallurgical bonding at coating/substrate interface when laser fluence was high. Shear strength tests indicated the laser fluence and shear strength had a positive correlation. For Ni60/WC composite coatings designed in these experiments, the recommend laser fluence should be higher than 55 J/mm{sup 2}, above which the shear strength could be greater than 200 MPa. Fracture surfaces indicated the failure mechanism of composite coatings was quasi-cleavage fracture.

36 MATERIALS SCIENCE↗

Laser 3D Printing of Fe-Based Bulk Metallic Glass: Microstructure Evolution and Crack Propagation

This work presents a comprehensive study of microstructure evolution, crack development and hardness performance of Fe-based bulk metallic glass parts processed by laser 3D printing. The combination of a low scan speed and high energy density generates a low temperature gradient, leading to supercooling and the formation of coarse dendrite and cellular crystal microstructure. Columnar dendrites grow in a single direction with large stress, and cracks are easily formed between the dendrites. The stress intensity factor (SIF) caused by the crack surface tension is small, the crack healing effect is weak, and it is difficult to prevent crack propagation. Cellular grain growth is uniform and more easily accommodates the strain, preventing crack initiation and propagation. In contrast, use of a high scan speed with low energy input produces a fine and uniform dendrite or even nanocrystalline, microstructure with microcracks. The SIF caused by the crack surface tension is large, and the crack healing effect is strong and prevents crack initiation and propagation. For low energy density, the hardness of the sample is similar to the hardness of the cast amorphous. This result indicates that the printing sample retained some amorphous characteristics.

36 MATERIALS SCIENCE↗

Tailoring copper current collector roughness and crystallographic orientation to improve lithium plating

Secondary lithium metal batteries are of great interest due to a high theoretical energy density, but rechargeability is limited by the formation of lithium dendrites that lead to internal short circuits and catastrophic cell failure. Mitigating dendrites through uniform current distribution at the current collector is a promising solution to enabling long cycle life of lithium metal electrodes. Here, the impact of copper crystal orientation and roughness on electrochemically deposited lithium morphology is studied. For 50 cycles, the capacity retention from greatest to least followed polycrystalline copper 95 ± 1 % (MC-PC) ≥ 94.55 ± 0.01 % Cu (110) > 93.0 ± 0.4 % Cu(111) > 75.8 ± 0.1 % Cu(100). Cu(100) performed the worst in all cases with shorts occurring frequently before reaching 50 cycles. Cryo-scanning electron microscopy images showed that after 50 cycles, MC-PC Cu had the best lithium morphology, but at early cycles, Cu(111) formed the densest lithium layer. MC-PC Cu had the most uniform lithium nucleation which may have been caused by increased roughness relative to the single crystal samples. When polycrystalline Cu (F-PC) roughness was systematically controlled, the cumulative Coulombic efficiency increased from about 0.3–0.5 with increasing roughness from an Ra of about 10–40 nm. Lastly, plating rates were studied. Slower rates of 0.25 mA/cm 2 exhibited denser lithium morphology in all cases as compared to 0.5 and 1.0 mA/cm 2 , but the relative porosity of Li deposited on the different current collectors depended on the rate applied.

Copper↗

Complementary Electrolyte Design for Li Metal Batteries in Electric Vehicle Applications

In this report a complementary electrolyte system with 0.8 M lithium bis(fluorosulfonylimide) (LiFSI) salt and 2 wt % lithium perchlorate (LiCLO4) additive in fluoroethylene carbonate (FEC)/ethyl methyl carbonate (EMC) solution enables not only stable cycling of lithium metal batteries (LMBs) with practical loading (<30 μm lithium anode, cathode loading > 4 mAh/cm 2 ) but also outstanding degradation stability toward the end of cycle life when compared to the conventional electrolyte. Although the use of LiFSI salt can increase the electrolyte conductivity and lengthen the cycle life of LMBs, the aged lithium anode morphology formed by the sacrificial decomposition of LiFSI is highly porous, leading to an abrupt cell capacity drop toward the end of cycling. Moreover, the inability to stop aluminum corrosion by the LiFSI-based electrolyte also causes cracking of the cathode tab during prolonged cycling. It is observed that a highly porous aged lithium consumed electrolyte at a higher rate, leading to the dry-out of electrolyte solvents. On the contrary, dense aged lithium anode morphology increased the localized current applied on the lithium, causing the formation of lithium dendrite. Thus, porosity control is the key to enhance battery performance. In this complementary system, LiClO 4 was introduced as an advanced additive to not only improve the capacity retention rate but also mitigate the abrupt capacity drop toward the end of cycle life because LiClO 4 acted as a pore astringent reducing the porosity of the aged lithium metal anode to the desired level. Moreover, the addition of LiClO 4 can also suppress the AI corrosion, allowing stable high-voltage cycling of LMBs. The synergistic effect of combining LiFSI salt and a LiClO 4 additive leads to an electrolyte system that can facilitate the application of high-energy LMBs with practical electrode loading.

25 ENERGY STORAGE↗

Organosulfide-plasticized solid-electrolyte interphase layer enables stable lithium metal anodes for long-cycle lithium-sulfur batteries

Lithium metal is a promising anode candidate for the next-generation rechargeable battery due to its highest specific capacity (3860 mA h g -1 ) and lowest potential, but low Coulombic efficiency and formation of lithium dendrites hinder its practical application. Here, we report a self-formed flexible hybrid solid-electrolyte interphase layer through co-deposition of organosulfides/organopolysulfides and inorganic lithium salts using sulfur-containing polymers as an additive in the electrolyte. The organosulfides/organopolysulfides serve as “plasticizer” in the solid-electrolyte interphase layer to improve its mechanical flexibility and toughness. The as-formed robust solid-electrolyte interphase layers enable dendrite-free lithium deposition and significantly improve Coulombic efficiency (99% over 400 cycles at a current density of 2mAcm -2 ). A lithium-sulfur battery based on this strategy exhibits long cycling life (1000 cycles) and good capacity retention. This study reveals an avenue to effectively fabricate stable solid-electrolyte interphase layer for solving the issues associated with lithium metal anodes.

25 ENERGY STORAGE↗

Visualization of clustered protocadherin neuronal self-recognition complexes

Neurite self-recognition and avoidance are fundamental properties of all nervous systems. These processes facilitate dendritic arborization, prevent formation of autapses and allow free interaction among non-self neurons. Avoidance among self neurites is mediated by stochastic cell-surface expression of combinations of about 60 isoforms of α-, β- and γ-clustered protocadherin that provide mammalian neurons with single-cell identities. Avoidance is observed between neurons that express identical protocadherin repertoires, and single-isoform differences are sufficient to prevent self-recognition. Protocadherins form isoform-promiscuous cis dimers and isoform-specific homophilic trans dimers. Although these interactions have previously been characterized in isolation, structures of full-length protocadherin ectodomains have not been determined, and how these two interfaces engage in self-recognition between neuronal surfaces remains unknown. Here we determine the molecular arrangement of full-length clustered protocadherin ectodomains in single-isoform self-recognition complexes, using X-ray crystallography and cryo-electron tomography. We determine the crystal structure of the clustered protocadherin γB4 ectodomain, which reveals a zipper-like lattice that is formed by alternating cis and trans interactions. Using cryo-electron tomography, we show that clustered protocadherin γB6 ectodomains tethered to liposomes spontaneously assemble into linear arrays at membrane contact sites, in a configuration that is consistent with the assembly observed in the crystal structure. These linear assemblies pack against each other as parallel arrays to form larger two-dimensional structures between membranes. Furthermore, our results suggest that the formation of ordered linear assemblies by clustered protocadherins represents the initial self-recognition step in neuronal avoidance, and thus provide support for the isoform-mismatch chain-termination model of protocadherin-mediated self-recognition, which depends on these linear chains.

59 BASIC BIOLOGICAL SCIENCES↗

Effect of nanopatterning on mechanical properties of Lithium anode

One of the challenges in developing Lithium anodes for Lithium ion batteries (LIB) is controlling the formation of Li dendrites during cycling of the battery. Nanostructuring and nanopatterning of electrodes shows a promising way to suppress the growth of Li dendrites. However, in order to control this behavior, a fundamental understanding of the effect of nanopatterning on the electromechanical properties of Li metal is necessary. In this paper, we have investigated the mechanical and wear properties of Li metal using Atomic Force Microscopy (AFM) in an airtight cell. By using different load regimes, we determined the mechanical properties of Li metal. Here, we show that as a result of nanopatterning, Li metal surface underwent work hardening due to residual compressive stress. The presence of such stresses can help to improve cycle lifetime of LIBs with Li anodes and obtain very high energy densities.

25 ENERGY STORAGE↗

Mechanical and electrical changes in electrochemically active polyimide binders for Li-ion batteries

Polyimide binders are often used in electrodes made with silicon for lithium-ion batteries for their mechanical strength and adhesion, which help mitigate mechanical issues associated with large volumetric expansion. These binders can be electrochemically active, but it is difficult to characterize what physical and chemical changes occur due to a composite electrode with multiple components and processes at play. Here, in this work, we study electrodes consisting only of polyimide binder and conductive carbon, using scanning probe-based techniques—contact resonance, force volume, and scanning spreading resistance microscopy—along with cryo-scanning transmission electron microscopy, electron energy loss spectroscopy, and energy dispersive X-ray spectroscopy. We show that lithium becomes trapped in the binder during cycling and results in large initial capacity losses, the formation of dendrite-like features, column-like domains of significantly increased mechanical modulus, and a slight increase in electronic resistivity.

25 ENERGY STORAGE↗

Influence of laser cladding regimes on structural features and mechanical properties of coatings on titanium substrates

In this paper an influence of the tantalum content on the structure and properties of surface layers of the titanium alloy doped using a laser treatment technology was investigated. It was found that an increase of a quantity of filler powder per one millimeter of a track length contributed to a rise of the content of undissolved particles in coatings. The maximum thickness of a cladded layer was reached at the mass of powder per the length unit equaled to 5.5 g/cm. Coatings were characterized by the formation of a dendrite structure with attributes of segregation. The width of a quenched fusion zone grew with an increase in the rate of powder feed to the treated area. Significant strengthening of the titanium surface layer alloyed with tantalum was not observed; however, the presence of undissolved tantalum particles can decrease the hardness of titanium surface layers.

36 MATERIALS SCIENCE↗

In-situ visualization of the transition metal dissolution in layered cathodes

Transition metal dissolution in layered cathodes is one of the most intractable issues that deteriorates the battery performance and lifetime. It not only aggravates the structure degradation in cathode, but also damages the solid electrolyte interphase in anode and even induce the formation of lithium dendrites. In this work, we investigate the dissolution behaviors of polycrystalline and single-crystalline layered cathode via operando X-ray imaging techniques. The described cathode particle morphology appears to have a significant impact on the evolution of the dissolution dynamics. As a mitigation strategy, we reveal that doping with trace amount of Zr in the layered cathode could improve its robustness against the transition metal dissolution. Our finding provides valuable insights for designing the next-generation highly-stable layered battery cathodes.

25 ENERGY STORAGE↗

Perspective—Lithium Metal Nucleation and Growth on Conductive Substrates: A Multi-Scale Understanding from Atomistic, Nano-, Meso-, to Micro-Scales

Reversible lithium (Li) deposition and stripping on conductive substrates like copper is vital for long-life high-energy rechargeable Li batteries. The reversibility is believed hindered by solid electrolyte interphase (SEI) formation and Li dendritic growth. Via in situ, operando cryo-microscopy and molecular dynamics simulation, we discovered amorphous Li before a disorder-order phase transition to bcc phase. The kinetics plays a significant role in Li nucleation and morphology evolution. This perspective on Li nucleation and growth from atomistic to nano- (<20 nm), meso- (20–100 nm), and micro-scales (>100 nm) provides a practical guidance on regulating dense Li deposits reversibly for long life performance.

25 ENERGY STORAGE↗

Molecular Layer Deposition of Crosslinked Polymeric Lithicone for Superior Lithium Metal Anodes

In this work, we for the first time developed a novel lithium-containing crosslinked polymeric material, a lithicone that enables excellent protection effects over lithium (Li) metal anodes. This new lithicone was synthesized via an accurately controllable molecular layer deposition (MLD) process, in which lithium tert -butoxide (LTB) and glycerol (GL) were used as precursors. The resultant LiGL lithicone was analyzed using a suite of characterizations. Furthermore, we found that the LiGL thichicone could serve as an exceptional polymeric protection film over Li metal anodes. Our experimental data revealed that the Li electrodes coated by this LiGL lithicone can achieve a superior cycling stability, accounting for an extremely long cyclability of >13,600 Li-stripping/plating cycles and having no failures so far in Li/Li symmetric cells at a current density of 5 mA/cm 2 and an areal capacity of 1 mAh/cm 2 . We found that, with a sufficient protection by this LiGL coating, Li electrodes could realize long-term stable cyclability with little formation of Li dendrites and solid electrolyte interphase. This novel LiGL represents a facile and effective solution to the existing issues of Li anodes and potentially paves a technically feasible route for lithium metal batteries.

Meng, Xiangbo↗

Effect of undercooling on the microstructure of Ni-35 at. pct Mo (eutectic) and Ni-38 at. pct Mo (hypereutectic) alloys

Ni-35 at. pct Mo and Ni-38 at. pct Mo alloy specimens have been solidified from various levels of undercooling in the differential thermal analysis and the electromagnetic levitation units in a pyrex/vycor bed. The evolution of the microstructure in the solified specimens has been examined in terms of the degree of undercooling, the nature of the first phase to nucleate from the melt, and the specimen cooling rate. The melt has been observed to undercool more in the presence of intermetallic NiMo (beta) phase as compared to that in the presence of nickel-rich solid solution (gamma). The 'anomalous eutectic' type of microstructure has been shown to result from the initial formation of the dendritic skeleton of either of the two phases, its segmentation due to convection and ripening, and the subsequent nucleation of the other phase in the interdendritic liquid regions. The recalescence behavior has been examined as a function of undercooling and the nature of the phase nucleating first in the melt.

Tewari, S. N.↗

Local convective flows in partly solidified alloys

Channel formation in a dendritic mushy zone is examined with reference to experimental results obtained for an acqueous system, NH4Cl-H2O, and a low-melting metallic system, Pb-Sn. The problems of channel nucleation, propagation, and prevention are considered for a configuration in which heat flow is directed downwards and growth occurs upwards into a positive temperature gradient. It is found that channels nucleate at the growth front by double diffusive perturbations into the quiescent bulk liquid, and not by perturbations within the dendritic framework of the mushy zone.

Hellawell, A.↗

The Martian valley networks: Origin by niveo-fluvial processes

The valley networks may hold the key to unlocking the paleoclimatic history of Mars. These enigmatic landforms may be regarded as the Martian equivalent of the Rosetta Stone. Therefore, a more thorough understanding of their origin and evolution is required. However, there is still no consensus among investigators regarding the formation (runoff vs. sapping) of these features. Recent climatic modeling precludes warm (0 degrees C) globally averaged surface temperatures prior to 2 b.y. when solar luminosity was 25-30 percent less than present levels. This paper advocates snowmelt as the dominant process responsible for the formation of the dendritic valley networks. Evidence for Martian snowfall and subsequent melt has been discussed in previous studies.

Rice, J. W., Jr.↗

A Dual Stage Sodium Thermo-Electro-Chemical Converter

The need for reliable and distributable energy sources is evident given the current forecasting of the world’s energy demand [1]. One prominent obstacle is the lack of an efficient direct heat-to-electricity conversion technology. The sodium thermo-electro-chemical converter (Na-TECC) is a highly efficient thermally regenerative electrochemical system (TRES) that can fill this void. The advantage of the Na-TECC over other direct conversion technologies is that it is a closed device (unlike fuel cells) requiring nothing more than a heat input (similar to thermoelectrics). It also has a high power density (> 1 W/cm2) and specific power up to 0.5 kW/kg , with the potential to achieve > 45% heat to electricity conversion efficiencies [2]. Furthermore, the converter rejects heat at a temperature hot enough to make it amenable for cogeneration, potentially under air-cooled operation. This electrochemical technology uses a special ion-selective solid-electrolyte called beta-alumina (Na2O•11Al2O3), that is highly conductive to sodium cations. A more conducting variation of this compound is beta”-alumina (Na2O•MgO•5Al2O3), where the magnesium acts as a stabilizer [3]. In the device, liquid sodium enters an evaporator where it is heated isobarically and vaporizes. The vapor is then oxidized at the interface between the anode and the solid-electrolyte. The Na-TECC generates electric power by allowing the high pressure oxidized sodium vapor ions to expand isothermally through the solid-electrolyte from the anode to the cathode. The liberated electrons are simultaneously conducted through an external load and recombine with the cations at the cathode. The low pressure sodium vapor is subsequently condensed and a wick pumps the liquid into the high pressure plenum to complete the cycle. Previous Na-TECCs have achieved efficiencies of 18% due to practical losses, whereas the potential efficiencies are above 45% [4]. Thermodynamic limitations and design constraints have limited previous devices from attaining these record efficiencies. Specifically, the maximum potential voltage in these previous devices was substantially reduced by the kinetic limitations of the charge transfer in the cathode (referred to as the overpotential) and by Joule heating losses due to the solid-electrolyte resistance, electrode resistance, and current collector resistance. Moreover, previous devices experienced a steady loss in performance throughout their lifetime. The drop in performance has been attributed to the electrolyte undergoing thermal and chemical breakdown due to crack propagation, loss of sodium oxide, and the formation of molten dendrites that create electrical shorts [5]. Finally, previous designs have also had a substantial problem with proper thermal management, with some showing thermal losses as great as 50% of the heat input. To improve the efficiency, a dual stage conversion process is being explored. Rather than using one isothermal expansion step, the dual cycle will employ two separate electrolytes to allow two separate expansion steps: one at the high temperature, and another at an intermediate temperature. This new cycle is thermodynamically favorable as it allows for regeneration from the isobaric cooling of the first expansion step, and reheat to complete the expansion in the second step. This allows the engine to reach a lower condenser temperature than its single stage counterpart, thus increasing the overall efficiency. The temperature drop across each electrolyte in the dual stage device (e.g., ~ 400 K) is smaller than the temperature drop across a comparable single stage device (e.g., ~ 800 K). This is amenable for better thermal management and allows for less heat loss. This will also mitigate the thermal shock across the very thin (< 1 mm) solid electrolytes, reduce crack propagation and limit the percolation of the molten dendrites, and ultimately increase the lifetime of the device. As an additional benefit the dual stage can be designed using planer geometries, rather than tubular geometries used in previous single stage models, which can be manufactured less expensively. This modified geometry can be tailored to improve the thermal management by reducing the radiation losses, which has been the biggest source of thermal losses [2]. A dual stage concept for the Na-TECC has never been demonstrated in literature. In this presentation, the operation of a single stage device will be revisited and, by adopting concepts used for similar converters, the thermodynamic operation of the dual stage will be developed [6]. Using the dual stage approach, the efficiency and power equations have been redefined to include regeneration and reheat. Questions such as what current densities optimize the power output or which intermediate temperature maximizes the efficiency will also be answered. Initial calculations of the dual stage show that the thermal management is the most sensitive parameter. Although the ideal voltage produced by the dual stage can be higher, there are potential drawbacks. For example, by using a lower condenser temperature the dual stage device will have a higher open circuit voltage, but it will also have a larger overpotential due to the limited cathodic kinetics that occur at a lower temperature. In short, there are several trade-offs in this device that need to be balanced. It will be demonstrated that the dual stage device must have lower thermal losses than a single stage device if it is to have a higher efficiency.

14 SOLAR ENERGY↗

Electrode Edge Effects and the Failure Mechanism of Lithium-Metal Batteries

Lithium (Li) metal with very high specific capacity makes it one of the ideal anode for high energy batteries. However, Li dendrite growth and the formation of isolated (or “dead”) Li during repeated Li plating/stripping processes lead to its low Coulombic efficiency (CE). In this work, we discovered for the first time that part of Li CE loss can be attributed to the edge effect of the copper (Cu) substrate electrode in a conventional Li||Cu cell configuration. The “dead” Li formed on the edge of Cu substrate was systematically investigated through scanning electron microscopy, energy dispersive X-ray spectroscopy, and two-dimensional X-ray photoelectron spectroscopy. In order to minimize the Li loss at the edge of the Cu exposed to pressure-free space, modified Li||Cu cell configuration with a Cu electrode smaller than Li metal is preferred. It was clearly demonstrated that using an electrode configuration with minimal open space or “pressure-free space” across electrodes can reduce “dead” Li accumulated during cycling and increase Li CE. This phenomena was also verified in Li metal batteries (Li||LiNi1/3Mn1/3Co1/3O2) and should be considered in the design of practical Li metal batteries.

Lee, Hongkyung↗