Search NASA⌕ Search

SEARCH · Search NASA

Results for “Ductile material”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Ductile fracture of cylindrical vessels containing a large flaw

The fracture process in pressurized cylindrical vessels containing a relatively large flaw is considered. The flaw is assumed to be a part-through or through meridional crack. The flaw geometry, the yield behavior of the material, and the internal pressure are assumed to be such that in the neighborhood of the flaw the cylinder wall undergoes large-scale plastic deformations. Thus, the problem falls outside the range of applicability of conventional brittle fracture theories. To study the problem, plasticity considerations are introduced into the shell theory through the assumptions of fully-yielded net ligaments using a plastic strip model. Then a ductile fracture criterion is developed which is based on the concept of net ligament plastic instability. A limited verification is attempted by comparing the theoretical predictions with some existing experimental results.

Erdogan, F.↗

Prediction and Verification of Ductile Crack Growth from Simulated Defects in Strength Overmatched Butt Welds

Defects that develop in welds during the fabrication process are frequently manifested as embedded flaws from lack of fusion or lack of penetration. Fracture analyses of welded structures must be able to assess the effect of such defects on the structural integrity of weldments; however, the transferability of R-curves measured in laboratory specimens to defective structural welds has not been fully examined. In the current study, the fracture behavior of an overmatched butt weld containing a simulated buried, lack-of-penetration defect is studied. A specimen designed to simulate pressure vessel butt welds is considered; namely, a center crack panel specimen, of 1.25 inch by 1.25 inch cross section, loaded in tension. The stress-relieved double-V weld has a yield strength 50% higher than that of the plate material, and displays upper shelf fracture behavior at room temperature. Specimens are precracked, loaded monotonically while load-CMOD measurements are made, then stopped and heat tinted to mark the extent of ductile crack growth. These measurements are compared to predictions made using finite element analysis of the specimens using the fracture mechanics code Warp3D, which models void growth using the Gurson-Tvergaard dilitant plasticity formulation within fixed sized computational cells ahead of the crack front. Calibrating data for the finite element analyses, namely cell size and initial material porosities are obtained by matching computational predictions to experimental results from tests of welded compact tension specimens. The R-curves measured in compact tension specimens are compared to those obtained from multi-specimen weld tests, and conclusions as to the transferability of R-curves is discussed.

Nishioka, Owen S.↗

Effects of fine porosity on the fatigue behavior of a powder metallurgy superalloy

Hot-isostatically-pressed powder-metallurgy Astroloy was obtained which contained 1.4 percent porosity at the grain boundaries produced by argon entering the powder container during pressing. This material was tested at 650 C in fatigue, creep-fatigue, tension, and stress-rupture and the results compared with data on sound Astroloy. They influenced fatigue crack initiation and produced a more intergranular mode of propagation but fatigue life was not drastically reduced. Fatigue behavior of the porous material showed typical correlation with tensile behavior. The plastic strain range-life relation was reduced proportionately with the reduction in tensile ductility, but the elastic strain range-life relation was changed little.

Miner, R. V.↗

Characterization of solid particle erosion resistance of ductile metals based on their properties

This paper presents experimental results pertaining to spherical glass bead and angular crushed glass particle impingement. A concept of energy absorption to explain the failure of material is proposed and is correlated with the erosion characteristics of several pure metals. Analyses of extensive erosion data indicate that the properties - surface energy, specific melting energy, strain energy, melting point, bulk modulus, hardness, atomic volume - and the product of the parameters - linear coefficient of thermal expansion x bulk modulus x temperature rise required for melting, and ultimate resilience x hardness - exhibit the best correlations. The properties of surface energy and atomic volume are suggested for the first time for correlation purposes and are found to correlate well with erosion rates at different angles of impingement. It further appears that both energy and thermal properties contribute to the total erosion.

Rao, P. V.↗

A Theoretical and Experimental Investigation of the Influence of Temperature Gradients on the Deformation and Burst Speeds of Rotating Disks

The purposes of this investigation were to evaluate the influence of temperature gradients and to test the validity of a recently developed method of calculating plastic flow in disks by comparing the calculated results with experimental observations. Short-time spin tests on parallel-sided, 10-inch-diameter disks were conducted under conditions that subject the disks to a range of temperatures from 70 to 1440 F. The agreement between the theoretical and experimental results was good over the range of temperature conditions investigated. Temperature gradients produced little reduction in the burst speed of the disks which had a high ductility..

LOADS AND STRESSES, STRUCTURAL↗

The effect of hydrogen and microstructure on the deformation and fracture behavior of a single crystal nickel-base superalloy

A study was conducted on the effects of internal hydrogen and microstructure on the deformation and fracture of a single crystal nickel-base superalloy. In particular, room temperature plane strain fracture toughness and tensile tests were performed on hydrogen-free and hydrogen charged samples of PWA 1480. The role of microstructure was incorporated by varying the levels of porosity and eutectic gamma/gamma prime through hot isostatic pressing and heat treatment. The room temperature behavior of PWA 1480 was unusual because precipitate shearing was not the primary deformation mechanism at all strains. At strains over 1 percent, dislocations were trapped in the gamma matrix and an attempt was made to relate this behavior to compositional differences between PWA 1480 and other superalloys. Another unique feature of the tensile behavior was cleavage of the eutectic gamma/gamma prime, which is believed to initiate the failure process. Fracture occurred on (111) planes and is likely a result of shear localization along these planes. Elimination of the eutectic gamma/gamma prime greatly improved the tensile ductility, but pososity had no effect on tensile properties. Large quantities of hydrogen (1.74 at. percent) were gas-phase charged into the material, but surprisingly this was not a function of the amount of porosity or eutectic gamma/gamma prime present. Desorption experiments suggest that the vast majority of hydrogen is at reversible lattice trapping sites. This large, uniform concentration of hydrogen dramatically reduced the tensile strain to failure, but only slightly affected the reduction in area. Available hydrogen embrittlement models were examined in light of these results and it was found that the hydrogen enhanced localized plasticity model can explain much of the tensile behavior. K(IC) fracture toughness tests were conducted, but it was necessary to also perform J(IC) tests to provide valid data.

Walston, William S.↗

Self-healing polymers

A three dimensional structure fabricated from a self-healing polymeric material, comprising poly(ester amides) obtained from ethylene glycol, azelaic acid and 1,1-aminoundecanoic acid, wherein polymeric material has a melt index above 2.5 g/10 min. as determined by ASTM D1238 at 190.degree. C. and 2.16kg, impact resistance and ductility sufficient to resist cracking and brittle fracture upon impact by a 9 mm bullet fired at a temperature of about 29.degree. C. at subsonic speed in a range from about 800 feet/sec to about 1000 feet/sec. It has been determined that the important factors necessary for self-healing behavior of polymers include sufficient impact strength, control of the degree of crystallinity, low melting point and the ability to instantly melt at impacted area.

Klein, Daniel J.↗

Correlation of deformation mechanisms with the tensile and compressive behavior of NiAl and NiAl(Zr) intermetallic alloys

To identify the mechanisms controlling strength and ductility in powder-extruded NiAl and NiAl + 0.05 at. pct Zr, tensile and compressive testing was performed from 300 to 1300 K for several grain sizes. Grain size refinement significantly increased yield stress in both alloys and, in some cases, slightly lowered the ductile-to-brittle transition temperature (DBTT), although no room-temperature tensile ductility was observed even in the finest grain size specimens. The small Zr addition increased the DBTT and changed the low-temperature fracture mode from intergranular in NiAl to a combination of intergranular and transgranular in the Zr-doped alloy. Scanning electron microscopy of compression specimens deformed at room temperature revealed the presence of grain-boundary cracks in both alloys. These cracks were due to the incompatibility of strain in the polycrystalline material, owing to the lack of five independent slip systems. The tendency to form grain-boundary cracks, in addition to the low fracture stress of these alloys, contributed to the lack of tensile ductility at low temperatures.

Bowman, R. R.↗

Cyclic plasticity and failure of structural components

An analytical approach for low-cycle fatigue prediction is presented. The approach combines a cyclic plasticity model with the finite element method and a damage accumulation criterion for ductile metals. The cyclic plasticity model is based on the concept of the combination of several yield surfaces. The surfaces are related to the material uniaxial stress-strain curve idealized by piecewise linear segments. The damage criterion is based on the Coffin-Manson formulae modified for the mean stress variation effect. It is extended to the multiaxial varying stress-strain field and applied for both the crack initiation and the crack growth processes. The stable slow crack growth rate is approximated by the damage accumulation gradient computed from the cracked finite element models. This procedure requires fatigue testing data of only smooth specimens under constant strain amplitudes. The present approach is illustrated by numerical examples of an aircraft wing stiffened panel subjected to compression, which causes material yielding and residual tension.

Kalev, I.↗

Deformation behavior of NiAl-based alloys containing iron, cobalt, and hafnium

The effects of alloying additions on the mechanical properties of the B2 intermetallic NiAl have been investigated in both the melt-spun ribbon and consolidated, bulk form. The study is based on a matrix of NiAl-based alloys with up to 20 at. pct Co and Fe additions and with reduced Al levels in the range of 30-40 at. pct. Characterization of the melt-spun ribbon by optical and scanning electron microscopy indicates a range of microstructures, including single-phase beta, gamma-prime necklace phase surrounding either martensitic or beta grains, and a mixture of equiaxed martensitic and gamma-prime grains. Bend ductility is present in melt-spun and annealed ribbons exhibiting the gamma-prime necklace structure and in a single-phase beta material containing 20 at. pct Fe. The analysis of compressive flow behavior on consolidated, bulk specimens indicates that the single-phase beta alloys exhibit a continuous decrease in yield stress with increasing temperature and profuse microcracking at grain boundaries. In contrast, multiphase (gamma-prime + either martensite or beta) alloys tend to display a peak in flow stress between 600 and 800 K, with little or no signs of microcracking. In general, heat treatments which convert the martensitic grains to beta + gamma-prime result in improved strength at temperatures above 600 K and better resistance to crack initiation.

Pank, D. R.↗

Ductility enhancement from interface dislocation sources in a directionally solidified beta + gamma + gamma-prime Ni-Fe-Al composite alloy

A directionally solidified beta + gamma + gamma-prime Ni-Fe-Al in situ composite alloy of composition Ni50Fe30Al20 has been used to investigate the effect of a plastically soft second phase on the mechanical behavior of a B2 ordered intermetallic alloy. This material exhibits extensive plasticity during compressive deformation at room temperature and fails in shear with extensive gamma + gamma-prime lamellar or rod pullout. The material also exhibits about 10 percent tensile elongation to fracture at room temperature, with final fracture that includes substantial necking of the gamma + gamma-prime lamellae or rods. Observation of slip lines and dislocation substructures discloses that the normally brittle beta matrix undergoes extensive plasticity in order to deform compatibly with the more ductile gamma phase. The plasticity of the beta matrix is accomplished by the generation of glissile dislocations into the beta matrix from the beta/gamma interface region and is enhanced because of a favorable beta-gamma orientation relationship for slip transfer. Ductility enhancement from interface-generated mobile dislocations generated from beta-gamma interfaces is compared to that observed in film-coated beta-NiAl single crystals and FeAl polycrystals.

Larsen, M.↗

Erosion and the gas turbine engine, part 2

Procedures for protecting aircraft engines from impact damage due to sand and dust particles are discussed. One system is to develop a filtration system to remove most of the solid particles. Another method is to design blade materials and blade protection coatings. The concepts of erosion within aircraft engines are explained. Curves are presented to show the effect of impingement angle on ductile and elastic modes of erosion. Engine sand and dust ingestion tests were conducted on T63-A-5A engines and the results are produced in graph form. The results of tests conducted in a dynamic erosion facility are analyzed.

Newhart, J. E.↗

Elevated temperature crack growth in advanced powder metallurgy aluminum alloys

Rapidly solidified Al-Fe-V-Si powder metallurgy alloy FVS0812 is among the most promising of the elevated temperature aluminum alloys developed in recent years. The ultra fine grain size and high volume fraction of thermally stable dispersoids enable the alloy to maintain tensile properties at elevated temperatures. In contrast, this alloy displays complex and potentially deleterious damage tolerant and time dependent fracture behavior that varies with temperature. J-Integral fracture mechanics were used to determine fracture toughness (K sub IC) and crack growth resistance (tearing modulus, T) of extruded FVS0812 as a function of temperature. The alloy exhibits high fracture properties at room temperature when tested in the LT orientation, due to extensive delamination of prior ribbon particle boundaries perpendicular to the crack front. Delamination results in a loss of through thickness constraint along the crack front, raising the critical stress intensity necessary for precrack initiation. The fracture toughness and tensile ductility of this alloy decrease with increasing temperature, with minima observed at 200 C. This behavior results from minima in the intrinsic toughness of the material, due to dynamic strain aging, and in the extent of prior particle boundary delaminations. At 200 C FVS0812 fails at K levels that are insufficient to cause through thickness delamination. As temperature increases beyond the minimum, strain aging is reduced and delamination returns. For the TL orientation, K (sub IC) decreased and T increased slightly with increasing temperature from 25 to 316 C. Fracture in the TL orientation is governed by prior particle boundary toughness; increased strain localization at these boundaries may result in lower toughness with increasing temperature. Preliminary results demonstrate a complex effect of loading rate on K (sub IC) and T at 175 C, and indicate that the combined effects of time dependent deformation, environment, and strain aging may play a role. Fractography showed that microvoid coalescence was the microscopic mode of fracture in FVS0812 under all testing conditions. However, the nature of the microvoids varied with test temperature and loading rate, and is complex for the fine grain and dipersoid sizes of FVS0812.

Porr, William C., Jr.↗

The Role of the Interface in Refractory Metal Alloy Composites

Creep-rupture and tensile tests have been used to evaluate thoriated W-wire reinforced Nb-1 percent Zr alloy matrix composites fabricated via arc-spray monotape technique. A significant creep strength enhancement was observed over the unreinforced matrix alloy while matrix integrity was maintained; the fiber/matrix interface phase is noted to be a strong and ductile W/Nb alloy, which is formed due to the mutual solubility of the constituent metals. High strength, toughness, and thermal stability are demonstrated by this material system, which is also resistant to liquid alkali metal corrosion.

Grobstein, Toni↗

Dynamic Fracture Initiation Toughness at Elevated Temperatures With Application to the New Generation of Titanium Aluminide Alloys

Recently, a new generation of titanium aluminide alloy, named Gamma-Met PX, has been developed with better rolling and post-rolling characteristics. I'revious work on this alloy has shown the material to have higher strengths at room and elevated temperatures when compared with other gamma titanium aluminides. In particular, this new alloy has shown increased ductility at elevated temperatures under both quasi-static and high strain rate uniaxial compressive loading. However, its high strain rate tensile ductility at room and elevated temperatures is limited to approx. 1%. In the present chapter, results of a study to investigate the effects of loading rate and test temperature on the dynamic fracture initiation toughness in Gamma-Met PX are presented. Modified split Hopkinson pressure bar was used along with high-speed photography to determine the crack initiation time. Three-point bend dynamic fracture experiments were conducted at impact speeds of approx. 1 m/s and tests temperatures of up-to 1200 C. The results show that thc dynamic fracture initiation toughness decreases with increasing test temperatures beyond 600 C. Furthermore, thc effect of long time high temperature air exposure on the fracture toughness was investigated. The dynamic fracture initiation toughness was found to decrease with increasing exposure time. The reasons behind this drop are analyzed and discussed.

Shazly, Mostafa↗

Risk Assessment for Titanium Pressure Vessels Operating Inside the ARES I's Liquid Hydrogen Tank Environment

Titanium alloy (Ti-6-4) is currently being proposed for the manufacturing of pressure vessels (PV) for storage of compressed helium gas, which are mounted inside the ARES I's liquid hydrogen (LH2) tank. At cryogenic temperature, titanium alloys usually have the highest strength-to-weight ratio property and have been considered as the metallic materials of choice for lightweight PV operating in LH2 environment. Titanium PV s are also considered as heritage hardware because they have been used by NASA for the Saturn IV-B rocket s LH2 tank in the mid 1960 s. However, hydrogen embrittlement is possible if Ti-6-4 alloy is exposed to gaseous hydrogen at certain pressure and temperature during the LH2 tank filling and draining operations on the launch pad, and during the J2X engine burn period for the ARES I s upper stage. Additionally, the fracture toughness and ductility properties of Ti-6-4 are significantly decreased at cryogenic temperature. These factors do not necessary preclude the use of titanium PV in hydrogen or at cryogenic applications; however, their synergistic effects and the material damage tolerance must be accounted for in the mission life assessment for PV s, which are considered as fracture critical hardware. In this paper, an overview of the risk assessment for Ti-6-4 alloy, strategy to control hydrogen embrittlement and brief metallic material trade study for PV operating in LH2 tank will be presented.

Lee, Jonathan A.↗

Bending Performance of Tungsten Printed Via Laser Powder Bed Fusion With Ceramic Dispersion Modified Powder Feedstock

Additively manufactured tungsten is a candidate refractory material for high-temperature aerospace and nuclear fusion/fission applications. The printability of pure tungsten is challenged by cracking defects arising from the metal’s high brittle-to-ductile transition temperature and low solubility of interstitial impurities. Furthermore, the cast microstructure inherent to the laser powder bed fusion (L-PBF) process has limited strength compared to worked microstructures common in wrought tungsten. Aside from process-related techniques to mitigate defects and increase strength (e.g., heated build chambers, multi-laser systems, low oxygen environmental control, etc.), micro-alloying additions can positively influence tungsten printability and strength. In this work, pure tungsten L-PBF feedstock was modified with 1 wt% additions of ceramic compound nano-powders. Wrought and printed bars were evaluated in four-point bending. Flexural strength and fractography were primary means of comparison to assess the effect of the feedstock modification on printed tungsten mechanical performance.

Additive Manufacturing↗