Search NASA⌕ Search

SEARCH · Search NASA

Results for “Friction stir processing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Behavioral simulations and experimental evaluations of stress induced spatial nonuniformity of dynamic bulk modulus in additive friction stir deposited AA 6061

Additive friction stir deposition (AFSD) is a rapidly developing solid-state additive manufacturing (AM) technology that enables the fabrication of customized products on a relatively large scale. The unique forge-liked process offers high quality products with refined equiaxed microstructure and exceptional mechanical performance. However, in AFSD, the spatially distributed mechanical properties within a deposited layer have not been established so far, due to the lack of a suitable large-scale mapping method. In the present work, an ultrasonic dynamic-elasticity mapping method was employed to map the distribution of physical properties in a AFSD 6061 Al. Strong spatial asymmetries in elastographies were mainly due to the residual stresses. The origin of the asymmetries was investigated through thermo-mechanical simulations of the AFSD process. It was observed that majority of the asymmetries were associated with the mechanical residual stresses instead of the symmetric thermal residual stresses during linear deposition of the AFSD process. However, the thermal residual stresses can be manipulated to become asymmetric with a 90° turn in the linear deposition path, due to the difference between the levels of cooling along the edges of the inner and outer corners. Hence, the mechanical and thermo-mechanical residual stresses can be additive or subtractive depending on the direction of the turns. Here, such numerically predicted behaviors were also experimentally observed on the AFSD fabricated samples by ultrasonic elastography. Furthermore, additional preliminary studies on multi-layer AFSD fabrications show the asymmetric mechanical stresses generated during the deposition process on different layers generate constructive or destructive interference which results to spatially variable dynamic bulk modulus depending on the deposition orientations of layers.

36 MATERIALS SCIENCE↗

Innovative Tools Advance Revolutionary Weld Technique

The iconic, orange external tank of the space shuttle launch system not only contains the fuel used by the shuttle s main engines during liftoff but also comprises the shuttle s backbone, supporting the space shuttle orbiter and solid rocket boosters. Given the tank s structural importance and the extreme forces (7.8 million pounds of thrust load) and temperatures it encounters during launch, the welds used to construct the tank must be highly reliable. Variable polarity plasma arc welding, developed for manufacturing the external tank and later employed for building the International Space Station, was until 1994 the best process for joining the aluminum alloys used during construction. That year, Marshall Space Flight Center engineers began experimenting with a relatively new welding technique called friction stir welding (FSW), developed in 1991 by The Welding Institute, of Cambridge, England. FSW differs from traditional fusion welding in that it is a solid-state welding technique, using frictional heat and motion to join structural components without actually melting any of the material. The weld is created by a shouldered pin tool that is plunged into the seam of the materials to be joined. The tool traverses the line while rotating at high speeds, generating friction that heats and softens but does not melt the metal. (The heat produced approaches about 80 percent of the metal s melting temperature.) The pin tool s rotation crushes and stirs the plasticized metal, extruding it along the seam as the tool moves forward. The material cools and consolidates, resulting in a weld with superior mechanical properties as compared to those weld properties of fusion welds. The innovative FSW technology promises a number of attractive benefits. Because the welded materials are not melted, many of the undesirables associated with fusion welding porosity, cracking, shrinkage, and distortion of the weld are minimized or avoided. The process is more energy efficient, safe (no toxic smoke or shielding gas, liquid metal splatter, arcing, dangerous voltage, or radiation), and environmentally sound (no consumables, fumes, or noise) than fusion welding. Under computer control, an automated FSW machine can create welds with high reproducibility, improving efficiency and overall quality of manufactured materials. The process also allows for welding dissimilar metals as well as those metals considered to be "unweldable" such as the 7xxx series aluminum alloys. Its effectiveness and versatility makes FSW useful for aerospace, rail, automotive, marine, and military applications. A downside to FSW, however, is the keyhole opening left in the weld when the FSW pin tool exits the weld joint. This is a significant problem when using the FSW process to join circumferential structures such as pipes and storage containers. Furthermore, weld joints that taper in material thickness also present problems when using the conventional FSW pin tool, because the threaded pin rotating within the weld joint material is a fixed length. There must be capability for the rotating pin to both increase and decrease in length in real time while welding the tapered material. (Both circumferential and tapered thickness weldments are found in the space shuttle external tank.) Marshall engineers addressed both the keyhole and tapered material thickness problems by developing the auto-adjustable pin tool. This unique piece of equipment automatically withdraws the pin into the tool s shoulder for keyhole closeout. In addition, the auto-adjustable pin tool retracts, or shortens, the rotating pin while welding a weld joint that tapers from one thickness to a thinner thickness. This year, the impact of the Marshall innovation was recognized with an "Excellence in Technology Transfer Award" from the Federal Laboratory Consortium.

Source record↗

Friction Stir Dovetailing of AA7099 to Steel with AA6061 Interlayer for Reduced Zn Embrittlement at Dissimilar Interface

Joining of high strength Al alloy (AA7099) to steel (rolled homogeneous armor) with and without AA6061 interlayer was achieved using a friction stir dovetailing (FSD) method. Detailed investigations were conducted to establish correlations between mechanical performance and microstructural evolution of FSD joints. Lap shear tensile testing revealed that incorporation of the AA6061 interlayer combined with tailored processing methodology significantly improved both mechanical interlocking and load transmission across the dovetail interface. Following incorporation of the interlayer, the maximum load carrying capacity and peak extension (of the AA7099/AA6061/steel joint) are 60% and 210% higher, respectively, than results obtained from an AA7099/steel joint without an interlayer. Without an AA6061 interlayer, formation of zinc rich intermetallic compounds led to brittle interfacial failure of the AA7099-steel FSD joint. Incorporation of novel tool and joint configuration eliminated asymmetric joint performance as a function of loading direction, which is generally observed in friction stir lap welding. The efficacy of the use of an AA6061 interlayer in joining AA7099 to steel was demonstrated through mechanical testing as well as high resolution analytical electron microscopy characterization.

Dissimilar metal joining, Friction stir dovetailin↗

Tool-workpiece stick-slip conditions and their effects on torque and heat generation rate in the friction stir welding

Friction stir welding (FSW) has found increased applications in automotive and aerospace industries due to its advantages of solid-state bonding, no fusion and melting, and versatility in various working conditions and material combinations. However, the relationship among processing parameters, material properties, and bonding extent and fidelity remains largely empirical, primarily because of the lack of the mechanistic understanding of the tool-workpiece frictional behavior that affects our subsequent understanding of microstructural evolution and interface bonding formation. While the tool-workpiece stick-slip condition is believed to dictate the resulting torque and heat generation rate during the welding process, it remains rare and elusive to conduct a quantitative experimental measurement of such interfacial field. On the other hand, numerical simulations based on Computational Fluid Dynamics (CFD) rely on ad hoc assumptions of interfacial pressure and shear-stress conditions, but predictions can only be validated via the medium- and far-range temperature field which is known to be insensitive to the interfacial frictional behavior. This work first presents a comparison among two CFD-based simulation methodologies and the Coupled Eulerian Lagrangian (CEL) model in finite element method, the last of which uses the Coulomb friction so that the stick-slip is naturally developed. Based on the Hill-Bower similarity relationship in the contact analysis, an analytical model is developed here to prove why a constant stick-slip fraction will be developed in the steady state, to correlate the stick-slip fraction to processing parameters such as the tool spin rate, and further to derive dimensionless functions for torque and heat-generation-rate predictions. Pros and cons of various numerical approaches in predicting stick-slip are discussed, and our analytical model has been found to agree well with our numerical simulation and literature experimental results. These analyses provide the critical strain-rate and temperature fields that are needed for the bonding analysis in our future work.

36 MATERIALS SCIENCE↗

Fatigue Crack Growth Rate Test Results for Al-Li 2195 Parent Metal, Variable Polarity Plasma Arc Welds and Friction Stir Welds

The fatigue crack growth rate of aluminum-lithium (Al-Li) alloy 2195 plate and weldments was determined at 200-F, ambient temperature and -320-F. The effects of stress ratio (R), welding process, orientation and thickness were studied. Results are compared with plate data from the Space Shuttle Super Lightweight Tank (SLWT) allowables program. Data from the current series of tests, both plate and weldment, falls within the range of data generated during the SLWT allowables program.

Hafley, Robert A.↗

Peak microhardness recovery via T6 heat treatment with extremely soft annealed Al7075 feedstock in additive friction stir deposition

With standard T6 heat treatments, precipitate-hardened alloys such as Al7075 and Al6061 fabricated using Additive Friction Stir Deposition (AFSD) method restore to noticeablely different peak mechanical properties. Previous research observed similar results but did not provide a viable solution. This study proposes a new processing strategy, namely enhanced plastic deformation by subjecting the Al7075 feedstock to annealed softening treatments. Specifically, by annealing the standard T651-Al7075 feedstock and deposition substrate (179 HV), their Microhardness were first degraded to its lowest state (80 HV), which is called a Soft-to-Soft system. For the Soft-to-Soft system subjected to AFSD, after undergoing appropriate T6 heat treatment, the microhardness of the AFSD 7075 alloy was restored to its peak value (183.1 ± 1.8 HV). The results indicate that this softening strategy can effectively reduce the non-strengthening phase in the AFSD matrix, thereby increasing the strengthening phase (η′ phase). This addresses the issue of traditional AFSD-prepared aluminum alloys being unable to achieve peak performance through T6 heat treatment.

36 MATERIALS SCIENCE↗

Characterization of Plastic flow and Resulting Micro-Textures in a Friction Stir Weld

The mechanically affected zone of a friction stir weld (FSW) cross section exhibits two distinct microstructural regions, possibly the residues of two distinct currents of metal in the FSW flow process. In this study the respective textures of these microstructural regions are investigated using orientation image mapping (OIM).

Schneider, J. A.↗

Friction Stir Welding: Standards and Specifications in Today's U.S. Manufacturing and Fabrication

New welding and technology advancements are reflected in the friction stir welding (FSW) specifications used in the manufacturing sector. A lack of publicly available specifications as one of the reasons that the FSW process has not propagate through the manufacturing sectors. FSW specifications are an integral supporting document to the legal agreement written between two entities for deliverable items. Understanding the process and supporting specifications is essential for a successful FSW manufacturing operation. This viewgraph presentation provides an overview of current FSW standards in the industry and discusses elements common to weld specifications.

Ding, Robert Jeffrey↗

Neutron Diffraction Residual Stress Study of a AA2219-T87 Self-Reacting Friction Stir Weld

2219-T87 is a precipitation hardenable aluminum-copper alloy which sees wide use in structural aerospace components. Thick panels of this alloy are joined via self-reacting friction welding (SRFSW); however, this thermomechanical process can result in significant loss of the alloy’s strengthening precipitates and large residual stresses which are detrimental to mechanical behavior and performance. High-resolution maps of the residual strain and stress states along the normal, transverse, and longitudinal directions of 2219-T87 SRFSW were obtained using neutron diffraction measurements. Residual stress had the highest tensile value in the heat-affected zone (HAZ) and the largest compressive stress in the base metal region of the normal and transverse directions. Line profile residual stress distributions displayed an “M”-shaped distribution in each direction with the longitudinal direction being the most pronounced while 2D residual stresses displayed an hourglass-shaped pattern. Further, average maximal longitudinal residual stress values ranged from 60.6 to 85.6% of yield. Microhardness testing across the transverse weld section produced a “V”-shaped curve with slight hardness recovery in the stir zone. Maximal and minimal microhardness values were observed in the base metal (154 HV) and thermomechanically affected zone (82 HV), respectively. Microstructural evolution was recorded using optical microscopy and showed decreasing grain size from the HAZ to the stir zone.

36 MATERIALS SCIENCE↗

Process-level cost analysis of hybrid manufacturing pathways for aerospace structural components

Hybrid manufacturing is a promising route for producing complex aerospace components, yet systematic cost benchmarking across multiple additive-subtractive pathways remains limited. This study presents a comprehensive process-based cost analysis of seven hybrid manufacturing routes, including laser powder bed fusion (L-PBF), powder- and wire-directed energy deposition (DED), wire arc additive manufacturing (WAAM), additive friction stir deposition (AFSD), metal binder jetting (MBJ), and agility forging, followed by scanning and finish machining. Parametric cost models incorporating direct material, labor, and energy costs were developed. L-PBF results are discussed in detail for a pickle fork component and directly compared with commercial pricing. Across all hybrid routes, labor emerged as the dominant cost driver, contributing more than 70% of total manufacturing cost in some cases. AFSD exhibited the lowest cost for aluminum components, with MBJ being its 316 L stainless steel counterpart, after accounting for geometric scaling. Benchmarking against industrial quotes suggests that hybrid manufacturing can achieve cost levels comparable to those of commercial services, although labor-intensive processes exhibit greater deviation. The analysis highlights automation of material handling, setup, and supervision as key opportunities for improving economic competitiveness. Overall, the proposed framework provides a quantitative basis for evaluating and optimizing hybrid manufacturing pathways for aerospace applications.

Baruah, Sweta [ORNL] (ORCID:0009000174256207)↗

THE ROLE OF FRACTURE PROPERTIES ON LAP JOINT STRENGTH OF FRICTION STIR WELDED AA7055-T6 SHEETS

Friction stir lap welded (FSLW) joints have weight-saving potential in aluminum-intensive automotive assembly. However, FSLW also modifies the material microstructure close to the joint. Optimizing the FSLW process requires understanding the relationship between the strength and the joint's microstructure. In previous studies, efforts have been dedicated to determining the effects of local softening, the shape of the oxide line, and porosity. However, the impact of changes to the fracture properties on the joint's strength has not been studied. In this work, strength testing, and simulations, aided by material characterization, were used to determine the role of fracture properties on the shear strength of a 3-sheet (aluminum alloys 7055-7055-6022) lap joint. Characterization involved testing for fracture properties in the weld region. This data was then implemented into finite element simulations. As a result, the joint strength was predicted with a deviation of less than 6% from the experimental value. Comparison with strength prediction using only the base metal properties indicates that fracture property in the nugget region determines the strength of AA7055 FSLW.

Finite element analysis, Friction stir welding, ma↗

A Decade of Friction Stir Welding R and D at NASA's Marshall Space Flight Center and a Glance into the Future

Welding at NASA's Marshall Space Flight Center (MSFC), Huntsville, Alabama, has taken a new direction through the last 10 years. Fusion welding processes, namely variable polarity plasma arc (VPPA) and tungsten inert gas (TIG) were once the corner stone of welding development in the Space Flight Center's welding laboratories, located in the part of MSFC know as National Center for Advanced Manufacturing (NCM). Developed specifically to support the Shuttle Program's External Tank and later International Space Station manufacturing programs, was viewed as the paragon of welding processes for joining aluminum alloys. Much has changed since 1994, however, when NASA's Jeff Ding brought the FSW process to the NASA agency. Although, at that time, FSW was little more than a "lab curiosity", NASA researchers started investigating where the FSW process would best fit NASA manufacturing programs. A laboratory FSW system was procured and the first welds were made in fall of 1995. The small initial investment NASA made into the first FSW system has certainly paid off for the NASA agency in terms of cost savings, hardware quality and notoriety. FSW is now a part of Shuttle External Tank (ET) production and the preferred weld process for the manufacturing of components for the new Crew Launch Vehicle (CLV) and Heavy Lift Launch Vehicle (HLLV) that will take this country back to the moon. It is one of the solid state welding processes being considered for on-orbit space welding and repair, and is of considerable interest for Department of Defense @OD) manufacturing programs. MSFC involvement in these and other programs makes NASA a driving force in this country's development of FSW and other solid state welding technologies. Now, a decade later, almost the entire on-going welding R&D at MSFC now focuses on FSW and other more advanced solid state welding processes.

Ding, Jeff↗

Computed Tomography 3-D Imaging of the Metal Deformation Flow Path in Friction Stir Welding

In friction stir welding (FSW), a rotating threaded pin tool is inserted into a weld seam and literally stirs the edges of the seam together. To determine optimal processing parameters for producing a defect free weld, a better understanding of the resulting metal deformation flow path is required. Marker studies are the principal method of studying the metal deformation flow path around the FSW pin tool. In our study, we have used computed tomography (CT) scans to reveal the flow pattern of a lead wire embedded in a FSW weld seam. At the welding temperature of aluminum, the lead becomes molten and is carried with the macro-flow of the weld metal. By using CT images, a 3-dimensional (3D) image of the lead flow pattern can be reconstructed. CT imaging was found to be a convenient and comprehensive way of collecting and displaying tracer data. It marks an advance over previous more tedious and ambiguous radiographic/metallographic data collection methods.

Schneider, Judy↗

Metal Flow During Friction Stir Welding

The flow of metal during Friction Stir Welding is clarified using a faying surface tracer and a nib frozen in place during welding. It is shown that material is transported by two processes. The first is a wiping of material from the advancing front side of the nib onto a plug of material that rotates and advances with the nib. The material undergoes a helical motion within the plug that both rotates and advances with the plug and descends in the wash of the threads on the nib and rises on the outer part of the plug. After one or more rotations, this material is sloughed off the plug in its wake, primarily on the advancing side. The second process is an entrainment of material from the front retreating side of the nib that fills in between the sloughed off pieces from the advancing side. These two processes produce material with different mechanical properties and the strength of a weld should depend on the relative importance of the processes.

Guerra, M.↗

Flow Patterns During Friction Stir Welding

Friction Stir Welding is a relatively new technique for welding that uses a cylindrical pin or nib inserted along the weld seam. The nib (usually threaded) and the shoulder in which it is mounted are rapidly rotated and advanced along the seam. Extreme deformation takes place leaving a fine equiaxed structure in the weld region., The flow of metal during Friction Stir Welding is investigated using a faying surface tracer and a nib frozen in place during welding. It is shown that material is transported by two processes. The first is a wiping of material from the advancing front side of the nib onto a zone of material that rotates and advances with the nib. The material undergoes a helical motion within the rotational zone that both rotates and advances and descends in the wash of the threads on the nib and rises on the outer part of the rotational zone. After one or more rotations, this material is sloughed off in its wake of the nib, primarily on the advancing side. The second process is an entrainment of material from the front retreating side of the nib that fills in between the sloughed off pieces from the advancing side.

Guerra, M.↗

Joining AA7099 to Ni-Cr-Mo Steel Using Single Pass Friction Stir Dovetailing and AA6061 Butter Layer

A novel single pass friction stir dovetailing (FSD) was developed to join thick plate AA7099 to Ni-Cr-Mo steel in a lap configuration through the use of an AA6061 butter layer. The butter layer approach can be shown to significantly reduce interfacial failures by inhibiting the formation of brittle Fe–Al intermetallic compounds (IMCs) which are typically formed during conventional friction stir welding (FSW) of AA7099 directly to steel. This study evaluates the strength and microstructural evolution of the aluminum/steel joint interface between single pass FSD of AA7099/AA6061(butter)/steel fabricated using three different FSD tool configurations. The butter layer was achieved by placement of a free-floating strip of AA6061 within the dovetail groove that was pre-machined in the steel substrate. Friction stir welding was then used to simultaneously join the thick plate AA7099, the AA6061 strip and the AA7099 in a single weld pass. To optimize the joining process, three different pin geometries (full thread, half smooth/half thread, no thread) were evaluated; it was demonstrated that the half smooth/half thread tool produced the strongest weld joint due to the absence of a Zn rich layer at the Al/steel interface. The efficacy of this unique processing technique was tested using lap shear tensile testing as well as high resolution transmission electron microscopy (TEM). A discussion of the new FSD technique, joint configurations, and process parameters are provided along with joint microstructural analyses and mechanical performance.

Olszta, Matthew J.↗

Manufacturing of 5.5 Meter Diameter Cryogenic Fuel Tank Domes for the NASA Ares I Rocket

The Ares I rocket is the first launch vehicle scheduled for manufacture under the National Aeronautic and Space Administration s (NASA s) Constellation program. A series of full-scale Ares I development articles have been constructed on the Robotic Weld Tool at the NASA George C. Marshall Space Flight Center in Huntsville, Alabama. The Robotic Weld Tool is a 100 ton, 7-axis, robotic manufacturing system capable of machining and friction stir welding large-scale space hardware. This presentation will focus on the friction stir welding of 5.5m diameter cryogenic fuel tank components; specifically, the liquid hydrogen forward dome (LH2 MDA) and the common bulkhead manufacturing development articles (CBMDA). The LH2 MDA was the first full-scale, flight-like Ares I hardware produced under the Constellation Program. It is a 5.5m diameter elliptical dome assembly consisting of eight gore panels, a y-ring stiffener and a manhole fitting. All components are made from aluminum-lithium alloy 2195. Conventional and self-reacting friction stir welding was used on this article. Manufacturing solutions will be discussed including the implementation of photogrammetry, an advanced metrology technique, as well as fixtureless welding. The LH2 MDA is the first known fully friction stir welded dome ever produced. The completion of four Common Bulkhead Manufacturing Development Articles (CBMDA) will also be highlighted. Each CBMDA consists of a 5.5m diameter spun-formed dome friction stir welded to a y-ring stiffener. The domes and y-rings are made of aluminum 2014 and 2219 respectively. An overview of CBMDA manufacturing processes and the effect of tooling on weld defect formation will be discussed.

Jones, Ronald E.↗