The bonding of FeN2, FeCO, and Fe2N2 - Model systems for side-on bonding of CO and N2

Qualitative calculations are performed to elucidate the nature of the side-on interaction of both N2 and CO with a single Fe atom. The systems are found to be quite similar, with bonding leading to an increase in the CO or N2 bond length and a decrease in the vibrational frequency. The CO or N2 stretching modes lead to a large dipole derivative along the metal-ligand bond axis. The populations show an almost identical, large donation from the Fe 3d orbitals into the CO or N2 Pi-asterisk. The larger system Fe2N2 is then considered, with the N2 bridging the Fe2, both parallel and perpendicular to the Fe2 bond axis for two different Fe-Fe distances. For FeN2, the shift in the observed N2 frequency is smaller than observed for the alpha state of N2/Fe(111). The shift in the N2 vibrational frequency increases when the N2 interacts with two Fe atoms, either at the Fe-Fe nearest neighbor distance or at the first layer Fe-Fe distance, when the side-on N2 axis is oriented perpendicular to an Fe-Fe bond.

Bauschlicher, Charles W., Jr.↗

Metal-dielectric interactions

There is a wide variety of situations wherein metals are in solid state contact with dielectric materials. The paper reviews some of the factors that influence solid state interactions for metals in contact with dielectric surfaces. Since surfaces play an important part in these reactions, the use of analytical tools in characterizing surfaces is discussed. Adhesion, friction, and wear are utilized as indicators of the nature of interfacial bonding between metals and dielectrics can be effectively determined with adhesion and friction force measurements. Films present on the surface, such as oxygen or water vapor, markedly alter adhesive bond strength which in turn affects friction force and interfacial fracture when attempts are made to separate the contact regions. Analytical surface tools such as the field ion microscope, Auger emission spectroscopy, and X-ray photoelectron spectroscopy are very effective in providing insight into the effect of contact on the surfaces of metals and dielectrics.

Buckley, D. H.↗

Joining of Silicon Carbide-Based Ceramics by Reaction Forming Method

Recently, there has been a surge of interest in the development and testing of silicon-based ceramics and composite components for a number of aerospace and ground based systems. The designs often require fabrication of complex shaped parts which can be quite expensive. One attractive way of achieving this goal is to build up complex shapes by joining together geometrically simple shapes. However, the joints should have good mechanical strength and environmental stability comparable to the bulk materials. These joints should also be able to maintain their structural integrity at high temperatures. In addition, the joining technique should be practical, reliable, and affordable. Thus, joining has been recognized as one of the enabling technologies for the successful utilization of silicon carbide based ceramic components in high temperature applications. Overviews of various joining techniques, i.e., mechanical fastening, adhesive bonding, welding, brazing, and soldering have been provided in recent publications. The majority of the techniques used today are based on the joining of monolithic ceramics with metals either by diffusion bonding, metal brazing, brazing with oxides and oxynitrides, or diffusion welding. These techniques need either very high temperatures for processing or hot pressing (high pressures). The joints produced by these techniques have different thermal expansion coefficients than the ceramic materials, which creates a stress concentration in the joint area. The use temperatures for these joints are around 700 C. Ceramic joint interlayers have been developed as a means of obtaining high temperature joints. These joint interlayers have been produced via pre-ceramic polymers, in-situ displacement reactions, and reaction bonding techniques. Joints produced by the pre-ceramic polymer approach exhibit a large amounts of porosity and poor mechanical properties. On the other hand, hot pressing or high pressures are needed for in-situ displacement reactions and reaction bonding techniques. Due to the equipment required, these techniques are impractical for joining large or complex shaped components.

Singh, M.↗

Fabrication of large tungsten structures by chemical vapor deposition

Process is accomplished by reducing tungsten hexafluoride with hydrogen. Metallic tungsten of essentially 100 percent purity and density is produced and built up as dense deposit on heated mandrel assembly. Process variations are building up, sealing or bonding refractory metals at temperatures below transition temperatures of base metal substrates.

Kahle, V. E.↗

Bonded Lubricants

Another spinoff to the food processing industry involves a dry lubricant developed by General Magnaplate Corp. of Linden, N.J. Used in such spacecraft as Apollo, Skylab and Viking, the lubricant is a coating bonded to metal surfaces providing permanent lubrication and corrosion resistance. The coating lengthens equipment life and permits machinery to be operated at greater speed, thus increasing productivity and reducing costs. Bonded lubricants are used in scores of commercia1 applications. They have proved particularly valuable to food processing firms because, while increasing production efficiency, they also help meet the stringent USDA sanitation codes for food-handling equipment. For example, a cookie manufacturer plagued production interruptions because sticky batter was clogging the cookie molds had the brass molds coated to solve the problem. Similarly, a pasta producer faced USDA action on a sanitation violation because dough was clinging to an automatic ravioli-forming machine; use of the anti-stick coating on the steel forming plates solved the dual problem of sanitation deficiency and production line downtime.

Source record↗

Through-Thickness Tensile Properties of Triaxial Braided Composites

The through-thickness strength of triaxial braided composites was measured using thin specimens bonded to metallic tabs. Despite providing reasonable engineering estimates of the bulk properties, some test specimen limitations were noted: For strong epoxies, significant shear and tensile stresses occur and induce failure between the first layer and bond-line; the strains over much of the exterior are ~10% lower than interior strains, which are representative of the nominal state; and failure often occurred near or along the adhesive bond line. These interference were partially overcome by adding a large radius to the gage section. Based on the finite element analysis and experimental measurements, the nominal elastic modulus and Poisson's ratio are E(sub 33) = 10.7 GPa and v(sub 31) = 0.08 for the three triaxial braided composites tested. Strengths vary from 14 to 40 MPa depending on the resin. Relative to the in-plane properties, the through thickness modulus, fracture strength, failure strain, and Poisson's ratio are 1/5th, 1/30th, 1/6th, and 1/4th. Interlaminar failure occurred with varying degrees of fiber tear out along with little damage to axial tows, resulting is a smooth undulating fracture surface. Post cure temperature excursions to 177 deg C (350 deg F) had little effect on elastic constants but reduced the strength E862 based composites severely. The strength of PR520 and 5208 based composites increased.

composite↗

Production and Characterization of Additively Manufactured Radiator Panels with Integral Branching Heat Pipes for High-Temperature Heat Rejection

Emerging concepts for fission surface power and nuclear electric propulsion necessitate lightweight, mechanically robust, and thermally efficient heat rejection radiators. State-of-the-art intermediate-temperature (~400 K) composite radiator assemblies have been developed based on titanium-water heat pipes bonded to metal, graphite, and carbon-fiber-based panels. NASA has identified a need for new radiator concepts that can operate at even higher temperatures (500 – 600 K), minimize thermal resistances and thermal stress failures at bond interfaces, and approach areal densities of 2 – 3 kg m -2 . To meet these needs, our team is developing additively manufactured (AM) radiator panels with integral branching wicking heat pipe networks. Water is selected as the working fluid for this temperature range. Based on simulations and thermal vacuum experiments, these branching embedded heat pipe networks can efficiently distribute heat over panels for finned surface efficiencies of η f >70% at T H = 500 K input heat. This paper first presents laser powder-bed fusion AM strategies to produce embedded porous structures for wicking heat pipes in Inconel 718 and titanium alloys (commercially pure and Ti-6Al-4V alloys). Post-build chemical and thermal treatments are described that yield hydrophilic wicking surfaces for operation with water. Transient rate-of-rise experiments with water and acetone are reported that yield estimates for AM wick porosity (ϵ), permeability (K), and effective pore radius (r pore ). Based on the wick characterization results, small prototype radiator panels (75 × 125 mm) with integrated heat pipe networks were manufactured. Heat rejection performance data are presented from cold thermal vacuum testing, with heat input temperatures up to ~510 K. Future efforts will focus on improving heat pipe performance, optimizing radiator mass, and evaluating larger panels to assess scalability.

thermal management↗

Production and Characterization of Additively Manufactured Radiator Panels With Integral Branching Heat Pipes for High-Temperature Heat Rejection

Emerging concepts for fission surface power and nuclear electric propulsion necessitate lightweight, mechanically robust, and thermally efficient heat rejection radiators. State-of-the-art intermediate-temperature (~400 K) composite radiator assemblies have been developed based on titanium-water heat pipes bonded to metal, graphite, and carbon-fiber-based panels. NASA has identified a need for new radiator concepts that can operate at even higher temperatures (500 – 600 K), minimize thermal resistances and thermal stress failures at bond interfaces, and approach areal densities of 2 – 3 kg m -2 . To meet these needs, our team is developing additively manufactured (AM) radiator panels with integral branching wicking heat pipe networks. Water is selected as the working fluid for this temperature range. Based on simulations and thermal vacuum experiments, these branching embedded heat pipe networks can efficiently distribute heat over panels for finned surface efficiencies of η f >70% at T H = 500 K input heat. This paper first presents laser powder-bed fusion AM strategies to produce embedded porous structures for wicking heat pipes in Inconel 718 and titanium alloys (commercially pure and Ti-6Al-4V alloys). Post-build chemical and thermal treatments are described that yield hydrophilic wicking surfaces for operation with water. Transient rate-of-rise experiments with water and acetone are reported that yield estimates for AM wick porosity (ϵ), permeability (K), and effective pore radius ( r pore ). Based on the wick characterization results, small prototype radiator panels (75 × 125 mm) with integrated heat pipe networks were manufactured. Heat rejection performance data are presented from cold thermal vacuum testing, with heat input temperatures up to ~510 K. Future efforts will focus on improving heat pipe performance, optimizing radiator mass, and evaluating larger panels to assess scalability.

nuclear electric propulsion↗

Brazing SiC/SiC Composites to Metals

Experiments have shown that active brazing alloys (ABAs) can be used to join SiC/SiC composite materials to metals, with bond strengths sufficient for some structural applications. The SiC/SiC composite coupons used in the experiments were made from polymerbased SiC fiber preforms that were chemical-vapor-infiltrated with SiC to form SiC matrices. Some of the metal coupons used in the experiments were made from 304 stainless steel; others were made from oxygen-free, high-conductivity copper. Three ABAs were chosen for the experiments: two were chosen randomly from among a number of ABAs that were on hand at the time; the third ABA was chosen because its titanium content (1.25 percent) is less than those of the other two ABAs (1.75 and 4.5 percent, respectively) and it was desired to evaluate the effect of reducing the titanium content, as described below. The characteristics of ABAs that are considered to be beneficial for the purpose of joining SiC/SiC to metal include wettability, reactivity, and adhesion to SiC-based ceramics. Prior to further development, it was verified that the three chosen ABAs have these characteristics. For each ABA, suitable vacuum brazing process conditions were established empirically by producing a series of (SiC/SiC)/ABA wetting samples. These samples were then sectioned and subjected to scanning electron microscopy (SEM) and energy-dispersive x-ray spectrometry (EDS) for analysis of their microstructures and compositions. Specimens for destructive mechanical tests were fabricated by brazing of lap joints between SiC/SiC coupons 1/8-in. (.3.2- mm) thick and, variously, stainless steel or copper tabs. The results of destructive mechanical tests and the SEM/EDS analysis were used to guide the development of a viable method of brazing the affected materials.

Steffier, Wayne S.↗