Replication Data for: Hydrogen migration at restructuring palladium-silver oxide boundaries dramatically enhances reduction rate of silver oxide

The data underlying this published work have been made publicly available in this repository as part of the IMASC Data Management Plan. This work was supported as part of the Integrated Mesoscale Architectures for Sustainable Catalysis (IMASC), an Energy Frontier Research Center funded by the U.S. Department of Energy, Office of Science, Basic Energy Sciences under Award # DE-SC0012573.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Replication Data for: Oxophilicity Drives Oxygen Transfer at a Palladium−Silver Interface for Increased CO Oxidation Activity

The data underlying this published work have been made publicly available in this repository as part of the IMASC Data Management Plan. This work was supported as part of the Integrated Mesoscale Architectures for Sustainable Catalysis (IMASC), an Energy Frontier Research Center funded by the U.S. Department of Energy, Office of Science, Basic Energy Sciences under Award # DE-SC0012573.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrical resistivity of some palladium-silver alloys containing hydrogen at 4.2 K

The electrical resistivities of the alloys 90at.%Pd - 10at.%Ag, 80at.%Pd - 20at.%Ag, 70at.%Pd - 30at.%Ag, 60at.%Pd - 40at.%Ag, and 50at.%Pd - 50at.%Ag were measured as functions of absorbed hydrogen x at 4.2 K. These results show a minimum in the resistivity for all the alloys except 90Pd-10Ag; they show a maximum for all the alloys except for 50Pd-Ag. We associate the shapes of the plots with a modification of the Pd D-band because of the substitutional alloying of Ag and the interstitial absorption of hydrogen.

Smith, R. J.↗

Tensile properties of palladium-silver alloys with absorbed hydrogen

The alloys 90Pd-10Ag, 80Pd-20Ag, 70Pd-30Ag, 60Pd-40Ag, and 50Pd-50Ag containing absorbed hydrogen were tested in tension. The results show the tensile properties to be independent of the phase transition. Also, hydrogen in the lattice does not necessarily cause embrittlement or poor elongation. The changes in the tensile properties appear dependent on the electron to atom site ratio.

Smith, R. J.↗

Superconductivity in the palladium-hydrogen system

Band theory and phonon measurements are used to calculate the electron-phonon coupling constant wavelength for Pd and PdD. The results indicate that superconductivity is absent in Pd metal because of the large value of the Coulomb pseudopotential, and that superconductivity occurs in PdD primarily because of coupling with the optic phonons. These results are consistent with superconducting transition-temperature measurements for these systems.

Papaconstantopoulos, D. A.↗

The 55 K specific heat anomaly in palladium hydride

A specific heat anomaly in PdH and PdD has been observed by Aston et al. (1957) close to 55 K. Its position was found to be independent of hydrogen concentration and its magnitude to be linear in hydrogen concentration. Ferguson's (1965) and Brodowsky's (1972) explanations of the anomaly are shown to be unsatisfactory. This is true also for the detailed mechanical statistical model proposed by Staford and McLellan (1974) for interstitial solid solutions of hydrogen in transition metals. It is shown that Gopal's (1966) simple Schottky model of specific heat anomaly, which considers a system of several levels with Boltzmann statistics, provides much better agreement with experiment than the more elaborate models, both in magnitude and in predicting a linear dependence on hydrogen concentration.

Jacobi, N.↗

Sulfur poisoning of hydrocarbon oxidation by palladium

Using a differential bed recycle reactor the oxidation of ethane and diethyl ketone by a Pd catalyst was studied at the 0-30 ppm level in air. In both cases first order kinetics were observed. The ethane oxidation rate was characterized n the Arrhenius form by a pre-exponential of 1.0 x 10 to the 8th power cm/sec and an E sub a of 27 kcal/mole. The diethyl ketone oxidation rate was characterized by a pre-exponential of 5.7 x -1000 cm/sec and E sub a of 14 kcal/mole. Poisoning of ethan oxidation was also investigated by hydrogen sulfide and to a smaller extent by the refrigerants Freon 22 and Gentron 142-B. Poisoning by Gentron 142-B was much more severe than by hydrogen sulfide. Kinetic experiments indicated that only the pre-exponential was changing.

Baumgartner, A. J.↗

Electrical conductivity and phase diagram of binary alloys. 21: The system palladium-chromium

Pd-Cr alloys were investigated by thermal analysis, hardness measurements, X-ray analysis, microscopic examination of etched pieces, and temperature-resistance curves of the solid alloys. Only one compound, Pd2Cr3, m, 1389 deg, is formed. It possesses a cubic face centered lattice and forms with excess Pd a series of solid solutions with a minimum m.p. at 45 atoms% Pd. Hardness maximum appears at the Pd2Cr3 point. Pd2Cr3 forms no solid solutions with Cr but eutectic point appears at 25 atoms% Pd, m. 1320 deg. The sp. resistance of pure Cr in an atom of H, indicates no allotropic forms. Cr2O3 is solid in molten Cr. Pure Cr melts at 1890 plus or minus 10 deg but Cr contg. Cr2O3 starts to melt at 1770 to 1790 deg.

Grube, G.↗

An inert marker study for palladium silicide formation - Si moves in polycrystalline Pd2Si

A novel use of Ti marker is introduced to investigate the moving species during Pd2Si formation on 111 and 100 line-type Si substrates. Silicide formed from amorphous Si is also studied using a W marker. Although these markers are observed to alter the silicide formation in the initial stage, the moving species can be identified once a normal growth rate is resumed. It is found that Si is the dominant moving species for all three types of Si crystallinity. However, Pd will participate in mass transport when Si motion becomes obstructed.

Ho, K. T.↗

Palladium silicide formation under the influence of nitrogen and oxygen impurities

The effect of impurities on the growth of the Pd2Si layer upon thermal annealing of a Pd film on 100 line-type and amorphous Si substrates is investigated. Nitrogen and oxygen impurities are introduced into either Pd or Si which are subsequently annealed to form Pd2Si. The complementary techniques of Rutherford backscattering spectrometry, and N-15(p, alpha)C-12 or O-18(p, alpha)N-15 nuclear reaction, are used to investigate the behavior of nitrogen or oxygen and the alterations each creates during silicide formation. Both nitrogen and oxygen retard the silicide growth rate if initially present in Si. When they are initially in Pd, there is no significant retardation; instead, an interesting snow-plowing effect of N or O by the reaction interface of Pd2Si is observed. By using N implanted into Si as a marker, Pd and Si appear to trade roles as the moving species when the silicide front reaches the nitrogen-rich region.

Ho, K. T.↗

Palladium-chromium static strain gage for high temperature propulsion systems

The present electrical strain gage for high temperature static strain measurements is in its fine-wire and thin-film forms designed to be temperature-compensated on any substrate material. The gage element is of Pd-Cr alloy, while the compensator is of Pt. Because the thermally-induced apparent strain of this compensated wire strain gage is sufficiently small, with good reproducibility between thermal cycles to 800 C, output figures can be corrected within a reasonable margin of error.

Lei, Jih-Fen↗

In Situ Remediation of Polychlorinated Bephenyls Using Palladium Coated Iron or Magnesium

The remediation of polychlorinated biphenyls (PCBs) and other chlorinated synthetic aromatic compounds are of great concern due to their toxicity and persistence in the environment. When released into the environment, PCBs are sorbed to particulate matter that can then disperse over large areas. Although the US Environmental Protection Agency (EPA) has banned the manufacture of PCBs since 1979, they are still present in the environment posing possible adverse health affects to both humans and animals. Thus, it is of utmost importance to develop a method that remediates PCB-contaminated soil, sediments, and water. The objective of our research was to develop an in-situ PCB remediation technique that is applicable for the treatment of soils and sediments. Previous research conducted at the University of Central Florida (UCF) proved the feasibility of using an emulsified system to dehalogenate a dense non-aqueous phase liquid (DNAPL) source, such as TCE, in the subsurface by means of an in-situ injection. The generation of a hydrophobic emulsion system drew the DNAPL TCE, through the oil membrane where it diffused to the iron particle and underwent degradation. TCE continued to enter, diffuse, degrade and exit the droplet maintaining a concentration gradient across the membrane, thus maintaining the driving force of the reaction.

Geiger, Cherie L.↗

The Palladium Isotopic Composition in Iron Meteorites

Ru, Mo and Pd are very useful indicators for the identification of nucleosynthetic components. We have developed techniques for Pd isotopes, in an effort to check the extent of isotopic effects in this mass region and for a Pt-group element which is less refractory than Ru. Stable Pd isotopes are produced by the process only (102Pd), the s-process only (104Pd), the process only (Pd-110) and by both the r- and s-processes (Pd-105, Pd-106, Pd-108). Kelly and Wasserburg reported a hint of a shift in 102Pd (approx. 25(epsilon)u; 1(epsilon)u (triple bonds) 0.01%) in Santa Clara. Earlier searches for Mo and Ru isotopic anomalies were either positive or negative.

Chen, J. H.↗