Search NASA⌕ Search

SEARCH · Search NASA

Results for “Powder”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Microstructural Characteristics of U-Zr Ingot Slug and Atomized Powder for SFR metal Fuel

Rod-type fuel slugs and spherical powder of U- 10wt.%Zr alloy was also fabricated and characterized in microstructure by injection casting, gravity casting and centrifugal atomization process. U grains became finer from ∼30μm in conventionally ingot rod to ∼2μm in atomized powder. Laminar structure became so fine from ∼0.2μm in conventionally cast ingot rod to 0.05∼0.1μm in atomized powder. Metallic fuels such as U-Zr and U-Pu-Zr alloys have been considered as a nuclear fuel for a sodium-cooled fast reactor (SFR), related to the closed fuel cycle for managing minor actinides and reducing a high radioactivity levels since the 1980's. Metallic fuel slugs of U-Pu-Zr alloys for SFR have conventionally been fabricated by an injection casting method. U-Pu-Zr alloy melts are injected and cast into quartz tube molds during injection casting. Metallic fuel slugs are collected by fracturing quartz tubes from the molds. Demolded quartz tubes are treated with radioactive wastes. Recently, management of minor actinides (MA) became an important issue because direct disposal of the long-lived MA can be a long-term burden for a tentative repository up to several hundreds of thousand years. The metallic fuel for SFR should be remotely fabricated under a radiation shielded environment such as a hot cell, because it contains highly radioactive MA such as Np, Am and Cm. The addition of MA in the fuel composition introduces new challenges in the manufacturing of a metallic fuel slug. Am has a high vapor pressure under a vacuum atmosphere at above a melting temperature of U-Zr or U-Pu-Zr. Used graphite crucibles and quartz molds cannot be recycled easily because of difficult decontamination of radioactive residues on their surfaces. It is necessary to minimize the vaporization of Am and volume of radioactive wastes. Atomized metallic fuel does not need these quartz molds during fabrication, as uranium alloys are prepared as a particle form. It is possible to reduce the formation of radioactive wastes by applying the fabrication process of a particulate metallic fuel. Metallic fuel having a fine microstructure, which originates from a rapid solidification effect during atomization process, results in a higher FG release rate during irradiation. In the case of applying a new forming method such as vibrocompaction in Zr sheath, the sheath can act as a reliable FCCI (fuel/cladding chemical interaction) barrier and a re-constraint for external elongation. In addition, atomized fuel powder, dispersed in a Na liquid metal having a high thermal conductivity, may have a lower temperature distribution during irradiation. In order to develop an efficient fabrication process of metallic fuel for SFR, U-Zr ingot rods were fabricated in a lab-scale with various casting methods. Rod-type U-Zr fuel slugs were fabricated by gravity casting and injection casting. Spherical powder of U-Zr alloy was also fabricated by centrifugal atomization. And then, the microstructural characteristics were investigated by using electron microscopes and energy-dispersive electron X-ray spectroscopy. Atomized U-10Zr powder generally showed spherical morphology of below 200 μm in particle size. U grains became finer from ∼30 μm in conventionally ingot rod to ∼2 μm in atomized powder. Laminar structure became so fine from ∼0.2 μm in conventionally cast ingot rod to 0.05∼0.1 μm in atomized powder. Atomized particulate metallic fuel for SFR has a fine microstructure, resulting in a higher fission gas release rate during irradiation. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The origin and formation of oxygen inclusions in austenitic stainless steels manufactured by laser powder bed fusion

The origins of nano-scale oxide inclusions in 316L austenitic stainless steel (SS) manufactured by laser powder bed fusion (L-PBF) was investigated by quantifying the possible intrusion pathways of oxygen contained in the precursor powder, extraneous oxygen from the process environment during laser processing, and moisture contamination during powder handling and storage. When processing the fresh, as-received powder in a wellcontrolled environment, the oxide inclusions contained in the precursor powder were the primary contributors to the formation of nano-scale oxides in the final additive manufactured (AM) product. These oxide inclusions were found to be enriched with oxygen getter elements like Si and Mn. By controlling the extraneous oxygen level in the process environment, the oxygen level in AM produced parts was found to increase with the extraneous oxygen level. The intrusion pathway of this extra oxygen was found to be dominated by the incorporation of spatter particles into the build during processing. Moisture induced oxidation during powder storage was also found to result in a higher oxide density in the AM produced parts. SS 316L powder free of Si and Mn oxygen getters was processed in a well-controlled environment and resulted in a similar level of oxygen intrusion. Finally, microhardness testing indicated that the oxide volume fraction increase from extraneous oxygen did not influence hardness values. However, a marked decrease in hardness was found for the humidified and Si-Mn free AM processed parts.

36 MATERIALS SCIENCE↗

Thermal evolution behavior of carbides and {gamma} Prime precipitates in FGH96 superalloy powder

The characteristics of rapidly solidified FGH96 superalloy powder and the thermal evolution behavior of carbides and {gamma} Prime precipitates within powder particles were investigated. It was observed that the reduction of powder size and the increase of cooling rate had transformed the solidification morphologies of atomized powder from dendrite in major to cellular structure. The secondary dendritic spacing was measured to be 1.02-2.55 {mu}m and the corresponding cooling rates were estimated to be in the range of 1.4 Multiplication-Sign 10{sup 4}-4.7 Multiplication-Sign 10{sup 5} K{center_dot}s{sup -1}. An increase in the annealing temperature had rendered the phase transformation of carbides evolving from non-equilibrium MC Prime carbides to intermediate transition stage of M{sub 23}C{sub 6} carbides, and finally to thermodynamically stable MC carbides. The superfine {gamma} Prime precipitates were formed at the dendritic boundaries of rapidly solidified superalloy powder. The coalescence, growth, and homogenization of {gamma}' precipitates occurred with increasing annealing temperature. With decreasing cooling rate from 650 Degree-Sign C{center_dot}K{sup -1} to 5 Degree-Sign C{center_dot}K{sup -1}, the morphological development of {gamma} Prime precipitates had been shown to proceed from spheroidal to cuboidal and finally to solid state dendrites. Meanwhile, a shift had been observed from dendritic morphology to recrystallized structure between 900 Degree-Sign C and 1050 Degree-Sign C. Moreover, accelerated evolution of carbides and {gamma}' precipitates had been facilitated by the formation of new grain boundaries which provide fast diffusion path for atomic elements. - Highlights: Black-Right-Pointing-Pointer Microstructural characteristic of FGH96 superalloy powder was investigated. Black-Right-Pointing-Pointer The relation between microstructure, particle size, and cooling rate was studied. Black-Right-Pointing-Pointer Thermal evolution behavior of {gamma} Prime and carbides in loose FGH96 powder was studied.

36 MATERIALS SCIENCE↗

A detailed study of pre-heating effects in electron beam melting powder bed fusion process

Metal-based additive manufacturing processes, such as powder bed fusion with electron beam (PBF-EB) process, also referred to as electron beam melting (EBM), can produce high-density parts with minimal residual stresses due to the uniform and coherent preheating of the powder bed. However, understanding and controlling the multiple stages of preheating is required to enable the production of high-quality, consistent parts of various materials. This work presents a large-scale, multi-layer, three-dimensional numerical analysis focused on studying the preheating stages for predicting thermal history during the PBF-EB process. The model follows a continuous multi-stage cyclic process, that incorporates all the main stages of the PBF-EB process for 316 L stainless steel. This includes the gradual deposition of a new powder layer, the first and second preheating levels of the powder bed, and the energy deposition during melting (excluding the actual melt-pool behavior simulation). The model employs an adaptive time-scaling approach that automatically adjusts the energy deposition for each solution time-increment. This allows for localized changes in time-resolution over an otherwise computationally expensive multi-layer procedure. The material property variations are also taken into account, with an emphasis on the subtle irreversible changes in powder effective thermal conductivity after the two requisite preheating stages of the powder bed. This effect is studied using simplified conductivity models from the literature for partially sintered powder, validated by a dedicated experiment and numerical simulation. The large-scale model is then used to estimate the actual temperatures during first and second preheating levels for 316 L steel, which is not yet fully supported commercially for PBF-EB. Model predictions are corroborated by experiments, using and analyzing IR images, taken at the completion of each layer by the machine’s built-in infrared camera. The current model also incorporates a qualitative assessment for the effects of conductivity change during pre-heating, as well as evaluates the applicability of the time-scaling approach.

36 MATERIALS SCIENCE↗

A horizontal powder injector for W7-X

We report that injection of low-Z powders into fusion plasma has been used to improve wall conditions, similar to the standard boronization process using diborane. Powder injection has the advantage of being much simpler, non-toxic, and efficient. The W7-X stellarator is planning on utilizing powder injection in long pulse discharges; a proof-of-principle test for horizontal injection into the plasma was conceived, a Probe Mounted Particle Injector (PMPI). The PMPI concept is developed using a polyetheretherketone (PEEK) paddle wheel hub that is driven by a piezo motor, due to the high magnetic fields, that rotates at 100 deg/s. This small PMPI fits into an envelope of 120 mm diameter × 150 mm long, a standard size for Multi-Purpose Manipulator (MPM). The device is housed in a carbon cup mounted on a retractable probe that can be placed near the plasma edge, enabling powder injection ˜4–8 cm radially into the boundary plasma. The feed for the paddle is via piezo electric actuator that vibrates a funnel filled with powder into a trough for the paddle to push. The 8 paddle arms, 35 mm long and 10 mm wide, are made from 0.38 mm thick PEEK which drag slightly along the powder-filled trough bottom, becoming a spring-loaded paddle which accelerates the powder upon release. Finally, design challenges are the high ambient magnetic field, vacuum compatible materials, high temperature environment, limited rotary-drive options, and compact space. The design and testing of this new device will be presented.

36 MATERIALS SCIENCE↗

Cold spray manufacturing of oxide-dispersion strengthened (ODS) steels using gas-atomized and ball-milled 14YWT powders

The cold spray deposition process has been investigated for the manufacture of 14YWT oxide-dispersion strengthened (ODS) steel, a nanostructured ferritic alloy (NFA), using gas-atomized and ball-milled feedstock powders. Cold spraying of the gas-atomized powder resulted in a thick dense deposit, but annealing them above 900 °C induced grain growth and heterogeneous precipitation of nanoparticles, thus resulting in lower hardness (~ 170 HV) compared to 14YWT ODS steel manufactured by the conventional method. The ball-milled powder (Fe-14Cr-3W-0.4Ti-0.2Y-0.125O) was cryomilled in liquid N 2 to achieve small particle sizes followed by annealing in a H 2 /Ar environment at 1000 °C and 1100 °C to reduce the hardness from ~ 8 GPa to ~ 5 GPa. Both smaller particle sizes and lower hardness of annealed powders made them amenable to the cold spray deposition process, resulting in thick and dense deposits, while retaining the favorable fully solutionized microstructure of the ball-milled powders. The microstructure of the as-deposited ODS exhibited very fine grain sizes (50–250 nm) with a uniform dispersion of Y-Ti-O nanoprecipitates in the ferritic steel matrix. The hardness values of the cold spray deposits using the powders annealed at 1000 °C and 1100 °C was 770 HV and 496 HV, respectively. Post-heat treatment of the as-deposited material up to 1100 °C showed a high-density microstructure with uniformly dispersed nanoscale oxide particles. The hardness of the annealed deposits up to 1000 °C had a notably higher hardness than bulk 14YWT ODS steel manufactured by conventional methods. The study demonstrates that cold spray deposition of the microstructurally-tailored feedstock powders can be used to successfully manufacture ODS steel with microstructure and properties comparable to those produced by the conventional methods, while providing for an attractive option for the more rapid and cost-effective manufacturing of ODS steel cladding tubes.

14YWT↗

Morphology and mechanism study for the synthesis of ZrB{sub 2}–SiC powders by different methods

ZrB{sub 2}–SiC ceramics, whose SiC is generally incorporated into the system by mechanical mixing, are known to have better performance than monolithic ZrB{sub 2}. Therefore, synthesis of duplex ZrB{sub 2}–SiC powders is beneficial for improving sinterability and mechanical properties of ZrB{sub 2}–SiC composites. In the present work, ZrB{sub 2}–SiC duplex powders with different morphologies were synthesized at 1550 °C for 2 h using as-synthesized amorphous hydrous ZrO{sub 2}–SiO{sub 2}. Both precipitation and sol–gel methods were used to prepare ZrO{sub 2}–SiO{sub 2} precursors. ZrB{sub 2}–SiC powder derived from precipitation method presented a rod-like morphology with smaller irregular particles adhering to them. And the morphology from sol–gel method was equiaxed shape with a very uniform distribution for principal components of Zr and Si. - Graphical abstract: SEM images of the ZrB2-SiC powders obtained by different methods. Display Omitted - Highlights: • ZrB{sub 2}–SiC powders with different morphologies were synthesized. • Precipitation and sol–gel methods were used to prepare ZrO{sub 2}–SiO{sub 2} precursors. • Possible mechanisms of morphology formation were investigated. • This work provided a potential way of morphology control for raw powders. • The synthesized duplex powders achieved a uniform distribution of SiC in ZrB{sub 2}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructures of the silicon carbide nanowires obtained by annealing the mechanically-alloyed amorphous powders

Silicon, graphite and boron nitride powders were mechanically alloyed for 40 h in argon. The as-milled powders were annealed at 1700 °C in nitrogen for 30 min. The annealed powders are covered by a thick layer of gray–green SiC nanowires, which are 300 nm to 1000 nm in diameter and several hundred microns in length. Trace iron in the raw powders acts as a catalyst, promoting the V–L–S process. It follows that the actual substances contributing to the growth of the SiC nanowires may be silicon, graphite and the metal impurities in the raw powders. The results from HRTEM and XRD reveal that the products contain both straight α/β-SiC nanowires and nodular α/β-SiC nanochains. It is interestingly found that 6H–SiC coexists with 3C–SiC in one nodular nanowire. This novel structure may introduce periodic potential field along the longitudinal direction of the nanowires, and may find applications in the highly integrated optoelectronic devices. - Graphical abstract: Display Omitted - Highlights: • SiC nanowires were prepared by annealing the mechanically alloyed amorphous powders. • SiC nanowires are 300 nm to 1000 nm in diameter and several hundred microns in length. • The products contain both straight α/β-SiC nanowires and nodular α/β-SiC nanochains. • Trace Fe in the raw powders acts as a catalyst, promoting the V–L–S process. • 6H–SiC coexists with 3C–SiC in one nodular SiC nanowire.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Magnetic properties of nano-clusters lanthanum chromite powders doped with samarium and strontium ions synthesized via a novel combustion method

Graphical abstract: Nanocrystalline Sm{sup 3+} and Sr{sup 2+} doped LaCrO{sub 3} powders have been synthesized through a novel gel combustion synthesis using triethanol amine (TEA). The saturation magnetization of the LaCrO{sub 3} increased with an increase Sm{sup 3+} ion and it decreased with an increase in the Sr{sup 3+} ion to 0.3 at temperature 1000 {sup o}C for 2 h due to the formation of a monodispersed uniform octahedral structure as shown in the Fig. Research highlights: {yields} Single-phase orthorhombic lanthanum chromite LaCrO{sub 3} nanoclusters have been successfully synthesized through a novel gel combustion synthesis using triethanol amine (TEA). {yields} Sr{sup 2+} ions doped LaCrO{sub 3} increased the unit cell volume and the crystallite size whereas Sm{sup 3+} ions doped LaCrO{sub 3} decreased the unit cell volume and the crystallite size. {yields} The saturation magnetization of the LaCrO{sub 3} powders increased continuously with an increase in the Sm concentration and it decreased with an increase in the Sr ion up to 0.3 at annealing temperature of 1000 {sup o}C for 2 h. -- Abstract: A novel approach to synthesize a single-phase orthorhombic perovskite lanthanum chromite LaCrO{sub 3} clusters doped with Sm{sup 3+} and Sr{sup 2+} ions via gel combustion route was reported. The producing materials were synthesized using metal nitrates as oxidizers and triethanol amine (TEA), N-butyl amine (NBA) or ethylene diamine (EDA) as a fuel. The effect of the annealing temperature, type of organic fuel and the variation of the samarium and/or strontium substitution and its impact on crystal structure, crystallite size, microstructure and magnetic properties of the LaCrO{sub 3} powders formed was systematically studied. The results revealed that a well crystalline single phase of pure LaCrO{sub 3} can be achieved at annealing temperature from 800 to 1000 {sup o}C for 2 h. Moreover, each organic carrier materials exhibited a different degree of effectiveness in the synthesis of the mixed oxide powders. The crystal structure was influenced by doped Sm{sup 3+} and/or Sr{sup 2+} ions. The crystallite size of the produced powders was increased with the increase the annealing temperature, increasing the Sm{sup 3+} ion and the decrease of Sr{sup 2+} ion substitution. The microstructures of the produced powders were found to be nanoclusters octahedra-like shaped. The saturation magnetization of the LaCrO{sub 3} powders increased continuously with an increase in the Sm{sup 3+} ion concentration and it decreased with an increase in the Sr{sup 2+} ion up to 0.3 at annealing temperature of 1000 {sup o}C for 2 h. The maximum saturation magnetization (0.279 emu/g) was achieved at the Sm{sup 3+} ion molar ratio 0.3 and annealing temperature 1000 {sup o}C. Moreover, wide coercivities can be obtained at different synthesis conditions (49.25 to 522 Oe).

36 MATERIALS SCIENCE↗

Synthesis and photochromic properties of EDTA-induced MoO{sub 3} powder

Graphical abstract: The MoO{sub 3} powder, which exhibits highly dispersed floral aggregated-like structure built up by superimposed and staggered nanoflakes with a diameter of 1-1.5 {mu}m and a thickness of 0.1-0.2 {mu}m, has been successfully obtained when the molar ratio of EDTA/Mo{sup 6+} is 0.05:1. The EDTA inducer obviously enlarges the surface area and apparently enhances the reactivity of MoO{sub 3} powders, making it show greater absorptive capacity to the excitation light and better photochromic properties than the pure MoO{sub 3} powder. Highlights: {yields} EDTA as organic inducing agent. {yields} EDTA inducer at EDTA/Mo{sup 6+} molar ratio of 0.05:1 enables growth of flower-like microspheres. {yields} The formation of flower-like MoO{sub 3} makes its photochromic properties strongly enhanced. -- Abstract: In this study, the photochromic MoO{sub 3} powder with novel morphology has been synthesized via hydrothermal method, using ethylene diamine tetraacetice acid (EDTA) as organic inducing agent. The influence of EDTA on the morphology, structure and photochromic properties of MoO{sub 3} powder has been characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), as well as ultraviolet and visible spectroscopy (UV-vis) and color difference meter. When the molar ratio of EDTA/Mo{sup 6+} is 0.05:1, the EDTA-induced MoO{sub 3} powder is found to have 3D flower-like morphologies and excellent photochromic properties. Furthermore, the possible growth mechanism of the flower-like structure and the photochromic mechanism of MoO{sub 3} powder are also discussed in detail.

36 MATERIALS SCIENCE↗

Large-scale and shape-controlled synthesis and characterization of nanorod-like nickel powders under microwave radiation

Graphical abstract: The nanorod-like pure nickel were fabricated via hydrothermal liquid phase reduction route under microwave irradiation with hydrazine hydrate as a reducing agent as well as polyvinyl alcohol as a dispersant and/or structure directing agent. The materials were characterized by XRD, SEM, EDS, HRTEM, and selected-area electron diffraction, etc. The lattice expansion for Ni powders was explained in detail. As-prepared Ni sample was of obvious shape anisotropy with length diameter ratio of 5. Magnetic measurements shown that the magnetic properties of Ni nanorod-like (fcc) were quite different from those of hexagonal closed-packed (hcp) Ni nanoparticles. Highlights: Black-Right-Pointing-Pointer The synthesis of nanorod-like nickel under microwave irradiation. Black-Right-Pointing-Pointer Nitrogen generated in reaction as a shielding gas. Black-Right-Pointing-Pointer The lattice expansion for Ni powders was explained in detail. Black-Right-Pointing-Pointer Magnetic properties of Ni were quite different from those of Ni nanoparticles. -- Abstract: The nanorod-like nickel powders were fabricated via hydrothermal liquid phase reduction route under microwave irradiation with hydrazine hydrate as a reducing agent as well as polyvinyl alcohol as a dispersant and/or structure directing agent. The morphology and structure of as-prepared products could be easily tuned by adjusting process parameters such as pH value and microwave irradiation time. The resulting materials were characterized by X-ray diffraction (XRD), scanning electron microscope, transmission electron microscopy and selected-area electron diffraction (SAED). The results demonstrated that pure nickel powders with face-centered cubic (fcc) structure were prepared at relatively mild condition and no characteristic peaks of nickel oxide in the XRD pattern were found. The phenomenon of lattice expansion for Ni powders was explained in details according to the XRD theory. As-prepared Ni sample was of obvious shape anisotropy with length diameter ratio of 5. Magnetic measurements shown that the magnetic properties of nanorod-like (fcc) Ni powders were quite different from those of hexagonal closed-packed (hcp) Ni nanoparticles. Furthermore, it had more strong ferromagnetic properties than that of Ni powders both bulk and nanoparticles.

36 MATERIALS SCIENCE↗

A study on in situ growth of TaC whiskers in Al{sub 2}O{sub 3} matrix powder for ceramic cutting tools

Graphical abstract: In situ growth of TaC whiskers (TaC{sub w}) was synthesized in an α-Al{sub 2}O{sub 3} matrix powder via a carbothermal reduction technique. The whiskers were 0.2–0.5 μm in diameter and 5–15 μm in length; they were straight and had smooth surfaces. Highlights: ► In situ growth of TaC whiskers was synthesized in an α-Al{sub 2}O{sub 3} matrix powder. ► The wet mixing method and 1450 °C were suitable for whiskers growth. ► The growth of TaC whiskers is not influenced by the Al{sub 2}O{sub 3} powder. ► The major impurities were TaC particles, nickel and unreacted carbon. -- Abstract: In situ growth of tantalum carbide (TaC) whiskers was synthesized in an α-Al{sub 2}O{sub 3} matrix powder via a carbothermal reduction technique within a temperature range of 1350–1500 °C in an argon atmosphere. The starting materials consisted of Ta{sub 2}O{sub 5}, C, Ni and NaCl powders. Different mixing methods and various reaction temperatures were employed. Most of the prepared whiskers were 0.2–0.5 μm in diameter and 5–15 μm in length. The reaction temperature of 1400–1450 °C was suitable for the growth of TaC whiskers and a wet mixing method was beneficial to increase the whisker yield. Some of the whiskers exhibited the needle shape while others exhibited the screw shape. The growth mechanism of the whiskers was a complex mechanism involving a helical screw dislocation mechanism and a vapor–liquid–solid process. No obvious influences of the Al{sub 2}O{sub 3} matrix powder on the growth of TaC whiskers were found and the major impurities in the obtained powder were TaC particles, nickel and unreacted carbon.

36 MATERIALS SCIENCE↗

Corrosion inhibitor storage and release property of TiO{sub 2} nanotube powder synthesized by rapid breakdown anodization method

Graphical abstract: Display Omitted Highlights: ► TiO{sub 2} nanotube powders were synthesized by rapid breakdown anodization method. ► Benzotriazole was loaded into the TiO{sub 2} nanotube powders. ► Low pH induced release of benzotriazole from TiO{sub 2} nanotube powders was proved. -- Abstract: Titanium dioxide (TiO{sub 2}) is one of the most studied substances in material science due to its versatile properties and diverse applications. In this study titanium dioxide nanotube powder were synthesized by rapid breakdown anodization (RBA) method. The synthesis involved potentiostatic anodization of titanium foil in 0.1 M HClO{sub 4} electrolyte under an applied voltage of 20 V and rapid stirring. The morphology and the phase of titanium dioxide nanotube powder were studied using field emission scanning electron microscopy, laser Raman spectroscopy and high resolution transmission electron microscopy. Benzotriazole was chosen as model inhibitor to evaluate TiO{sub 2} nanotube powder's corrosion inhibitor loading and releasing properties. The storage and release properties of TiO{sub 2} nanotube powder were studied using UV–visible spectroscopy and thermogravimetric analysis.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synthesis of nano-sized amorphous boron powders through active dilution self-propagating high-temperature synthesis method

Graphical abstract: Nano-sized amorphous boron powders were synthesized by active dilution self-propagating high-temperature synthesis (SHS) method. The effects of endothermic reaction rate, the possible chemical reaction mechanism and active dilution model for synthesis of the product were also discussed. Highlights: ► Nano-sized amorphous boron powders were synthesized by active dilution self-propagating high-temperature synthesis method. ► The morphology, particle size and purity of the samples could be effectively controlled via changing the endothermic rate. ► The diluter KBH{sub 4} played an important role in active dilution synthesis of amorphous nano-sized boron powders. ► The active dilution method could be further popularized and become a common approach to prepare various inorganic materials. - Abstract: Nano-sized amorphous boron powders were synthesized by active dilution self-propagating high-temperature synthesis (SHS) method at temperatures ranging from 700 °C to 850 °C in a SHS furnace using Mg, B{sub 2}O{sub 3} and KBH{sub 4} as raw materials. Samples were characterized by X-ray powder diffraction (XRD), Laser particle size analyzer, Fourier transform infrared spectra (FTIR), X-ray energy dispersive spectroscopy (EDX), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and high-resolution transmission TEM (HRTEM). The boron powders demonstrated an average particle size of 50 nm with a purity of 95.64 wt.%. The diluter KBH{sub 4} played an important role in the active dilution synthesis of amorphous nano-sized boron powders. The effects of endothermic reaction rate, the possible chemical reaction mechanism and active dilution model for synthesis of the product were also discussed.

36 MATERIALS SCIENCE↗

Radiation transfer in metallic-powder beds during laser forming

This paper presents numerical simulations of two-dimensional radiation transfer in a powder layer that resides on a substrate of the same material and is exposed to a normally incident laser beam with an axisymmetric bell-shaped or top-hat intensity profile. The powder layer is treated as an equivalent homogeneous absorbing/scattering medium with radiative properties defined by the reflectance of the solid phase, the porosity of the powder and its surface area. The model used is applicable when the laser beam diameter far exceeds the particle size of the powder. It is shown that the absorptance of an optically thick layer of opaque powder particles is a universal function of the absorptance of the solid phase and is independent of surface area and porosity, in agreement with experimental data in the literature. The fraction of laser energy absorbed in the powder-substrate system and that absorbed in the substrate decrease with an increase in the reflectance of the material, but the powder bed is then more uniformly heated. (laser technologies)

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of Preliminary Powder Production and Consolidation for Advanced LEU Fuel Concepts

A set of novel uranium-based alloys has been proposed for use in advanced LEU fuel systems that utilize powder metallurgical methods for fabrication of the fuel forms. This study seeks to evaluate the effectiveness of current fabrication methods to produce powder of each of the candidate alloys and consolidate composite systems. Powder samples were produced via atomization and analyzed for particle size, shape, and microstructure utilizing sieving methods and scanning electron microscopy (SEM). Preliminary pellet consolidation tests were conducted with the atomized powder using a press and sinter method. The resulting pellets were analyzed via SEM to evaluate the morphology of the composite system. These preliminary tests demonstrate the ability to produce powder but did not yield the desired quality of powder and impacted the ability to fabricate a fully dense pellet. A refined process is under development to produce a higher yield of small (<250 µm) spherical powder.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of Inconel 625 fabricated using powder-bed-based additive manufacturing technologies

The purpose of this study was to perform a comparative analysis of powder-bed-based additive manufacturing (AM) technologies during the production of metallic components using Inconel 625 powder material. The AM technologies explored in this study include electron beam powder bed fusion (EPBF), laser powder bed fusion (LPBF), and binder jetting technology. Samples were fabricated in two build directions (X and Z build orientations) for this evaluation process, where all specimens underwent a hot isostatic pressing (HIP) post-process. The comparison was made in terms of microstructure and mechanical properties including ultimate tensile strength (UTS), yield strength (YS), percent elongation, and modulus of elasticity (E). Microstructural characterization showed evidence of equiaxed grain formation for binder jetting and LPBF parts, whereas EPBF parts displayed a more columnar grain formation parallel to the build direction. Six specimens were tested per technology, three built in the X orientation and three built in the Z orientation. All six specimens were built in a single run of each AM machine. Results indicated that all three technologies are capable of meeting the minimum requirements of the ASTM F3056-14 standard for parts produced in the X orientation, with properties that are similar to wrought Inconel 625. In the Z orientation, however, only LPBF was able to meet the minimum standard requirements. Through the comparative analysis of the mechanical properties, here this work showed that LPBF outperformed the other technologies in a majority of the evaluated properties, followed by EPBF and binder jetting. An analysis of the fracture surfaces of tensile specimens was also performed, and it indicated ductile fracture (dimple rupture) for the specimens produced with all three of the AM technologies studied. Nevertheless, the characterization also showed certain differences in the fractured surfaces, such as the presence of un-sintered powder particles for the binder jetting processed Inconel 625, or the development of the so called woody structure for the EPBF processed material. This study can be used to determine distinct characteristics between the three powder-bed-based technologies for the fabrication of Inconel 625 that can further include other technologies and materials using similar approaches.

36 MATERIALS SCIENCE↗

Investigation of the Surface Chemistry of Magnesium and Magnesium Alloy Powders

Magnesium (Mg) and Mg alloy powders are generally difficult to sinter at atmospheric pressure in inert atmospheres purportedly due to the presence of powder particle surface oxide layers. To better understand sintering of Mg and Mg alloy powders, x-ray photoelectron spectroscopy (XPS) was performed to characterize the surface chemistry of gas atomized pure Mg and Mg alloys AZ91D and WE43 powders. These results are used to quantitatively determine the surface chemistry of these powders. Additionally, equilibrium thermodynamic modeling of these Mg/Mg alloys materials exposed to oxygen down to part per billion concentrations are presented for relative comparison to experimental XPS results. Analysis of these results are intended to improve sintering of Mg and Mg alloy powder materials through more quantitative knowledge of powder surface chemistry.

25 ENERGY STORAGE↗