Search NASA⌕ Search

SEARCH · Search NASA

Results for “STEELS - FRICTION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

Understanding failure in austenitic steels: Key considerations for molten salt storage in CSP applications

Owing to their excellent properties, austenitic stainless steels are extensively used in boilers, furnaces, molten salt tanks, and other applications that are subjected to extreme mechanical loads and high-temperature conditions. Their high corrosion and creep resistance make them suitable for high-temperature operating environments. Additionally, good fatigue resistance and favorable mechanical and visual properties are essential. However, the premature failure of several components at elevated temperatures has been previously reported. Although the failure analysis of components in service is complex, processes such as cold work and welding have been identified as contributing factors to the performance degradation of these steels. This study aims to analyze the various documented failure modes and mechanisms in austenitic steels, including creep, cracking, stress relaxation cracking, and fatigue, to better understand the multi-objective design requirements for these alloys as structural materials for high-temperature molten salt tanks in Concentrating Solar Power (CSP) plants. Stabilized austenitic grades, such as AISI 347H, demonstrate superior resistance to creep and corrosion-related degradation when compared to non-stabilized grades like AISI 316L at temperatures relevant to concentrated solar power (CSP) applications. In contrast, nickel-based alloys offer enhanced corrosion resistance, albeit at a higher cost. This review underscores that creep, stress relaxation cracking, and thermo-mechanical fatigue are the predominant long-term failure risks in CSP hot tanks.

14 SOLAR ENERGY↗

Binder-jetted AISI M2 tool steel during hot isostatic pressing: Densification and carbide transformation

Binder jetting (BJ) enables fabrication of complex components from high-alloy steels such as AISI M2; however, residual porosity after sintering limits mechanical performance. This study investigates the coupled effects of binder chemistry, sintering conditions, cooling rate, and subsequent hot isostatic pressing (HIP) on densification, microstructure, and mechanical response in binder-jetted M2 tool steel. HIP increased relative density from ∼93 to 95% to >99% and improved compressive strength by ∼40-70%. Densification was governed by initial pore morphology, where closed porosity was effectively eliminated, while interconnected porosity limited full consolidation. Microstructural analysis (XRD, EBSD, SEM) shows that HIP promotes dissolution of metastable carbides and redistribution of alloying elements (W, Mo, V), transforming heterogeneous carbide networks into finer and more uniformly distributed M 2 C, MC, and M 6 C phases through diffusion-assisted homogenization. Among the investigated conditions, the FluidFuse binder combined with sintering at 1270 °C for 60 min and furnace cooling produced the most balanced response, achieving ∼99.7% density, ∼855 HV hardness, ∼4130 MPa compressive strength, and ∼24% strain. In contrast, higher sintering temperatures promoted carbide coarsening, reducing ductility despite high density. HIP reduces microstructural heterogeneity and drives the system toward a near-equilibrium state with reduced sensitivity to prior processing history. A comparative assessment with conventional and additive manufacturing routes (LPBF, DED, EBM, FFF) shows that the BJ-HIP approach achieves competitive densification and mechanical performance. These findings provide a mechanistic basis for controlling densification and microstructure in high-alloy steels processed via BJAM.

AISI M2 tool steel↗

Microstructure and fracture toughness characterization of three 9Cr ODS EUROFER steels with different thermo-mechanical treatments

Ferritic martensitic ODS steels are one of the candidate structural materials for future Gen-IV nuclear fission and fusion reactors. Here, the dependence of fracture toughness on microstructure was investigated by comparing three 9Cr ODS EUROFER steels manufactured through different thermo-mechanical processing routes. Quasi-static fracture toughness testing was performed with sub-sized C(T) specimens and microstructural characterization was carried out using scanning electron microscopy, electron backscatter diffraction, and transmission electron microscopy. It was found that at lower test temperatures (-100 – 22 °C), the fracture toughness was primarily controlled by crack initiation at sub-micron particles and by production of secondary cracks during fracture. At higher temperatures (above 100 °C), fracture toughness was predominantly controlled by the matrix ductility and the grain boundary strength with a relatively ductile coarse-grained alloy demonstrating higher fracture toughness compared to high-strength fine-grained alloys. These results and discussion show that variations in thermomechanical treatments can produce significant differences in microstructure and fracture toughness behavior of ferritic martensitic ODS steels.

36 MATERIALS SCIENCE↗

Mechanical behavior of additively manufactured and wrought 316L stainless steels before and after neutron irradiation

Fabrication of nuclear reactor components using additive manufacturing (AM) methods is now a practical option since the AM technologies have advanced to allow for building of complex parts with high quality materials. To assess the mechanical performance of printed components in reactor-relevant conditions and to build a property database for the AM 316L stainless steel (SS), mechanical testing and characterization were performed before and after neutron irradiation. In this work, miniature tensile specimens were irradiated at the High Flux Isotope Reactor (HFIR) to 0.2 and 2 displacements per atom (dpa) at 300 and 600°C. The AM 316L SS was tested in the as-built, stress-relieved, and solution-annealed conditions, and the wrought (WT) 316L SS in solution-annealed condition as a reference alloy. The baseline test result showed that the AM 316L SS, regardless of the post-build heat treatment, had higher strength than the WT 316L SS, but similar ductility. Post-irradiation tensile testing was conducted at RT, 300°C, and 500°C for selected irradiation conditions. Neutron irradiation induced significant changes in the mechanical behavior of the AM stainless steels, including both hardening and softening. Although the as-built 316L steel after 300°C irradiation showed necking just after yielding, the overall property changes of the as-printed alloy became less significant after 600°C irradiation. Irradiation-induced ductilization was also observed after the higher temperature irradiation. In general, the strength change was smaller in the relatively stronger as-built and stress-relieved AM SSs than in the solution-annealed AM and WT SSs. These relatively lower strength 316L SSs overall retained higher ductility in the irradiation conditions tested, but the stronger 316L SSs demonstrated a similar level of ductility after the higher temperature (600°C) irradiation. It is a positive assessment for the AM 316L materials that no embrittlement was observed within the test and irradiation conditions of the experiment.

36 MATERIALS SCIENCE↗

Impact of neutron irradiation on the thermophysical properties of additively manufactured stainless steel and inconel

The deployment of additive manufacturing (AM) technologies to support the nuclear energy industry is limited by the current lack of data related to the irradiation performance of AM parts. The Colorado School of Mines is conducting a multi-year irradiation and post irradiation examination project to study the impacts of neutron irradiation on stainless steel 316L and Inconel 718 and 625 specimens produced by several commercially available AM techniques and irradiated in the Advanced Test Reactor (ATR) at the Idaho National Laboratory (INL). This paper presents initial results on the impact of neutron irradiation on the heat capacity, the thermal diffusivity, and the thermal conductivity of the specimens at temperatures between 100 oC and 400 oC. The unirradiated AM specimens have heat capacity values similar to, or lower than, the reference values, regardless of manufacturing method or material. The irradiated AM specimens have average heat capacities greater than the unirradiated specimens and reference values in every case. Additionally, the thermal diffusivities of the unirradiated AM specimens are either larger or statistically similar to the reference values. The irradiated AM specimens exhibit lower thermal diffusivities compared to the reference thermal diffusivity values. One of the stainless steel 316L laser powder bed fusion samples exhibited thermal diffusivity values with statistically significant anisotropy prior to and after irradiation. The thermal conductivities of the unirradiated AM stainless steel 316L specimens and the unirradiated Inconel 718 specimens are lower or statistically similar to the reference values. The unirradiated Inconel 625 specimens exhibit slightly higher thermal conductivity values than the reference values. The irradiated specimens show a significant increase in thermal conductivity compared to the unirradiated specimens and the reference values for all materials.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Revealing the chemical environment of Cr, Fe, and Ni in high temperature-ultrafine precipitate strengthened steel subjected to low fluence neutron irradiation

High-temperature ultrafine-precipitate-strengthened (HT-UPS) steel has potential applications in advanced nuclear reactors as a structural material. However, little is currently known about its response to neutron irradiation. This research provides insight into the neutron irradiation-induced physicochemical changes of the major constituents in HT-UPS steels, including Fe, Cr, and Ni, using synchrotron X-ray absorption near edge structure (XANES) and diffraction. This study is the first known investigation using XANES to characterize HT-UPS steel to analyze the evolution of the atomic level chemistry. It was found that following irradiation, nucleation, ballistic dispersion, and/or coarsening of Cr 23 C 6 precipitates occurred at very low neutron irradiation fluences, from 0.003 displacements per atom (dpa) up to 0.3 dpa, at ~600°C, which were at least an order of magnitude lower than previous studies. Calculations of the angular momentum projections, partial density of states, and the XANES spectra confirmed the experimental findings of the Cr 23 C 6 precipitate evolution. In contrast, the local atomic structure around Fe and Ni atoms demonstrated irradiation resistance.

36 MATERIALS SCIENCE↗

Evolution of the role of molybdenum in duplex stainless steels during thermal aging: From enhancing spinodal decomposition to forming heterogeneous precipitates

Thermal aging of ferrite in duplex stainless steels leads to a complex microstructural evolution that can give way to large deleterious changes in mechanical properties. The microstructural evolution mechanisms that happen concurrently are strongly linked to minor changes in composition. By characterizing duplex stainless steels with various compositions over a range of aging conditions, it was revealed that adding a modest amount of Mo to cast austenitic stainless steel (such as changing from grade CF3 to grade CF3M) not only increases the kinetics of spinodal decomposition and Ni-Si-Mn-rich G-phase precipitation, but it also forms a separate Mo-rich phase. At shorter equivalent aging times, Mo segregates from Fe and towards Cr accelerating spinodal decomposition. At longer aging times, Mo enriches in the Ni-Si-Mn clusters before phase separating into an adjoined Mo-rich cluster. We found that these phase changes and precipitation events result in a rather steep drop in fracture and impact toughness. These results will inform the design of similar alloys for use at high temperatures.

36 MATERIALS SCIENCE↗

The influence of nitrogen and nitrides on the structure and properties of proton irradiated ferritic/martensitic steel

The 12Cr1MoWV (wt%) ferritic/martensitic steel HT9 is a candidate material for fuel cladding in advanced nuclear reactors, such as the Versatile Test Reactor currently under development. As such, understanding the relationship between microstructure and mechanical properties in the context of irradiation environments for these steels is critical. N content, and more specifically interstitial N, has been hypothesized to be detrimental to irradiated properties at lower temperatures (less than 0.3T m ) to a total of 6 dpa; however, in this work at a dose of 1 dpa the irradiated microstructure was improved with added N, leading to less irradiation hardening. Three variants of HT9 were irradiated with 1.5 MeV protons to a dose of 1 dpa at 300°C. The HT9 variants included Low (10 ppm), Mid (190 ppm), and High (440 ppm) N alloys that were otherwise nearly identical. Changing the N content had a variety of effects on the irradiated defect structures. As N content increased, the average dislocation loop diameter decreased, while the number density of loops increased. Additionally, extensive Ni clustering was observed on dislocations and interfaces. The Mid and High N specimens exhibited significantly less hardening (ΔHV≃100) relative to the Low N specimen (ΔHV≃160). The decrease in hardening is attributed to vanadium carbonitride acting as a sink for Ni clusters that would otherwise form on dislocations. Under the irradiation conditions used, these results suggest increasing the N content in HT9 may have a desirable effect on the irradiated structure and properties at the dose studied, as well as the swelling resistance at higher doses. In other words, N content appears to be a powerful tool for tailoring the self-interstitial atom cluster mobility in F/M steels for different temperature and dose applications.

36 MATERIALS SCIENCE↗

Compatibility of Fe-Cr-Al and Fe-Cr-Al-Mo oxide dispersion strengthened steels with static liquid sodium at 700 °C

We report the corrosion behavior and tensile properties of oxide dispersion strengthened (ODS) FeCr, FeCrAl, FeCrAlMo steels and 316H stainless steel were evaluated after 1000 h at 700 °C in static sodium with and without an oxygen getter (Zr foil). Without Zr foil to getter the dissolved oxygen in the liquid sodium, combined oxidation (formation of Cr, Fe-rich or Al-rich oxides) and dissolution of the studied materials was observed. For the ODS FeCr, Cr- and Fe-rich oxide formation and dissolution induced Cr depletion in the underlying alloy and led to the formation of laves phases that were observed to be detrimental to the room temperature tensile properties. For ODS FeCrAlMo and FeCrAl Al-rich oxide formation and dissolution resulted in Al depletion in the underlying alloys but did not impact tensile properties at room temperature. For 316H temperature induced sensitization combined with oxidation decreased room temperature tensile properties. With Zr foil added as oxygen getter, roughened surfaces and Al depletion profiles suggested the dissolution of ODS FeCr and FeCrAl into the liquid sodium while limited dissolution was observed for ODS FeCrAlMo and 316H. For the 316H and ODS FeCrAlMo steels, precipitates were formed at the grain boundaries after exposure. Tensile properties of ODS FeCr, FeCrAl and FeCrAlMo were not affected by the 1000 h corrosion exposure with Zr foil added to the sodium but for 316H temperature-induced grain boundary sensitization negatively affected the tensile properties.

36 MATERIALS SCIENCE↗

Suppression of irradiation hardening in tungsten-coated ferritic steel for fusion reactor blanket applications

W-coated reduced activation ferritic steels have been developed for use as plasma facing components in fusion reactor blankets, offering excellent sputtering resistance and structural strength. Previous high-temperature coating methods, such as diffusion bonding and brazing, caused interfacial deterioration due to thermal stress from mismatched thermal expansion between W and reduced activation ferritic steel. To address this, underwater explosive welding was introduced as a high-velocity cold process that joins dissimilar materials while maintaining a strong, thin interface without the thermal issues associated with traditional methods. In this study, the effects of neutron irradiation on the hardness and microstructure in W-coated F82H reduced activation ferritic steel (W/F82H) joined by underwater explosive welding are investigated. Following neutron irradiation at 290 °C, irradiation hardening is suppressed in W, F82H, and their interface within the W/F82H material. Furthermore, microstructural observations indicate that the recovery of work hardening and relaxation of elastic strain introduced during coating significantly contribute to the suppression of irradiation hardening in W/F82H. In conclusion, W/F82H exhibits significantly suppressed irradiation hardening compared with those in stand-alone materials. This suppression is explained by residual stress from thermal expansion mismatch and the unique microstructure at the interface. These results provide valuable insights for the development of more durable materials in nuclear fusion applications.

36 MATERIALS SCIENCE↗

Gas tungsten arc welding and post weld heat treatment effects on microstructure and mechanical property of castable nanostructured alloy steel

Here, this paper details the first study of castable nanostructured alloy (CNA) steel gas tungsten arc weldability and the post-weld heat treatment (PWHT) effects. Effects of welding heat input, thermal cycles, and PWHT on microstructures, microhardness distributions, room temperature tensile properties, and fracture characteristics are discussed. Results show that CNA steel exhibits excellent weldability (i.e., no indication of welding defects and reasonable tensile properties). The welded joint exhibited heterogeneous microstructures with δ-ferrite as well as large microhardness variation and fluctuation. The welded joint yield and ultimate tensile strengths were similar to those of the base metal, but the elongations decreased by 30 %. However, with normalization and tempering PWHT, the δ-ferrite was eliminated, microstructure was modified, hardness was unified, and joint ductility was restored. The study indicated that the CNA reduced-activation ferritic-martensitic steel owns excellent weldability, and PWHT is needed for the industrial application of welded structures.

36 MATERIALS SCIENCE↗

Influence of defect characteristics on tensile deformation of an additively manufactured stainless steel: Evolutions of texture and intergranular strain

The micromechanics of plastic deformation behavior of a selective laser melt processed austenitic stainless steel were studied by investigating the evolutions of texture and intergranular strain using in situ high-energy synchrotron x-ray diffraction (sXRD). The effects of defect characteristics on tensile behavior were studied using three different samples: a near full-density sample with elliptical closed voids and two samples with lack-of-fusion (LOF) defects tensile loaded either perpendicular or parallel to their major axes. The evolutions of pole figures and inverse pole figures show that the full-density specimen develops a strong (111)/(200) fiber texture along the loading direction. For both LOF specimens, the evolution of texture is qualitatively similar to the full-density counterpart, but the development of the fiber texture was much slower, indicating a limited plasticity at a given macroscopic strain. The intergranular strain evolution in the full-density specimen is similar to that of a wrought 316L stainless steel. Conversely, a significantly different intergranular strain development was observed in a LOF specimen, where tensile strain development was observed in both the axial and transverse directions. Finally, the influence of defect type, density, and orientation on the local stress states in the steel matrix and the evolutions of intergranular strains is discussed.

36 MATERIALS SCIENCE↗

Creep of MARBN-type 9Cr martensitic steel in gaseous CO 2 environment

Here, with an interest in moving from steam to supercritical CO 2 as the working fluid in advanced energy systems, it is important to study the mechanical response of structural alloys to CO 2 -containing environments. MARBN-type 9Cr martensitic steel was originally developed for application in boilers for supercritical and ultra-supercritical power plants where the steam temperature reaches 650 °C. In this research, a MARBN-type 9Cr martensitic steel designed and manufactured at NETL was creep tested in a gaseous CO 2 environment (i.e., 0.1 MPa at 650 °C), and the results are directly compared to creep tests conducted in air. It was found that environmentally-assisted cracking facilitated by carbide formation beneath the growing oxide accelerated failure in gaseous CO 2 . This work indicates that creep-oxidation interactions in advanced martensitic steels represent an important consideration for materials selection in supercritical CO 2 power cycles. Furthermore, this work confirms that more oxidation-resistant alloys will be required for the highest temperature portions of these systems.

36 MATERIALS SCIENCE↗

The mechanism of twin thickening and the elastic strain state of TWIP steel nanotwins

A Twinning Induced Plasticity (TWIP) steel with a nominal composition of Fe-16.4Mn-0.9C-0.5Si-0.05Nb-0.05V was deformed to an engineering strain of 6%. The strain around the deformation twins were mapped using the 4D-STEM technique. Strain mapping showed a large average elastic strain of approximately 6% in the directions parallel and perpendicular to the twinning direction. However, the large average strain comprised of several hot spots of even larger strains of up to 12%. These hot spots could be attributed to a high density of sessile Frank dislocations on the twin boundary and correspond to shear stresses of 1–1.5 GPa. The strain and therefore stress fields are significantly larger than other materials known to twin and are speculated to be responsible for the early thickness saturation of TWIP steel nanotwins. The ability to keep twins extremely thin helps improve grain fragmentation, i.e. the dynamic Hall–Petch effect, and underpins the large elongations and strain hardening rates in TWIP steels.

36 MATERIALS SCIENCE↗

Influence of fatigue precracking and specimen size on Master Curve fracture toughness measurements of EUROFER97 and F82H steels

EUROFER97 and F82H steels are two leading reduced-activation ferritic-martensitic (RAFM) steels for fusion first wall and blanket applications. Exposure to the harsh environment of fusion reactors can result in severe degradation of fracture toughness. Thus, the post-irradiation evaluation of fracture toughness is critical for understanding the material behavior. Due to the space constraints of irradiation facilities and challenges in controlling a uniform irradiation condition for large size specimens, the development of small specimen test techniques (SSTT) is indispensable to evaluate the performance of irradiated materials. In this study, we evaluated specimen size effects on the Master Curve fracture toughness of EUROFER97 and F82H steels. A wide variety of specimens, including 0.5 T compact tension (C(T)) specimens, 0.16 T mini-compact tension (miniC(T)) specimens, and 1.65 mm miniature bend bar specimens, were tested. The testing methodology was based on the Master Curve method in the ASTM E1921 standard. No specimen size effect was observed in 0.5 T C(T) and 0.16 T miniC(T) specimens on the Master Curve reference temperature T0, while 1.65 mm miniature bend bar specimens yielded a higher T 0Q . A strong effect of fatigue precracking on T 0 for 0.5 T C(T) and 0.16 T miniC(T) specimens was observed, such that testing on specimens with skewed fatigue precrack fronts resulted in lower T 0 than for specimens with ASTM standard qualified straight fatigue precrack fronts. The results highlight the importance of experimental quality control in developing SSTT for Master Curve fracture toughness testing. Lastly, we also evaluated and provided recommendations on the minimum number of specimens needed for each specimen type for yielding reliable T 0Q values.

36 MATERIALS SCIENCE↗

Morphology and elemental composition of a new iron-rich ferrite phase in highly irradiated austenitic steel

Here, elemental composition and morphology of a previously unidentified radiation-induced ferrite phase were investigated in a 300-series steel irradiated by neutrons in-service up to 57.6 dpa. Specimens of 18Cr-10Ni-Ti stainless steel (AISI 321 analog) were cut from a hexagonal wrapper of a fuel assembly irradiated in the BN-350 sodium-cooled fast reactor. An Fe-rich bcc-phase was observed primarily on grain boundaries. In this phase, the concentration of Cr is ~8–12% (compared to ~19% in the matrix), the concentration of Ni is ~1.5–3% (~9% in the bulk material), and the concentration of Mn is ~0.23% (1.3% in the matrix). This Fe-rich phase is distinctly different from the retained-ferrite phase, commonly found in commercial austenitic steels. The extensive appearance of this Fe-rich ferrite on grain boundaries suggests that enhanced surface–intergranular corrosion may occur in water-cooled power reactors, arising from the low Ni, Mn, and Cr concentrations in this phase.

36 MATERIALS SCIENCE↗

The role of excess vacancies in stabilizing solute clusters in low-alloy steels

The formation of solute clusters in irradiated low-alloy steels, such as reactor pressure vessel steels, is a critical cause of radiation hardening and embrittlement. However, the chemical interactions among solute elements and excess vacancies remain to be fully understood. This study employs density functional theory, cluster expansion, and lattice-based Monte Carlo simulations to examine the stability and morphology of nano-size coherent solute clusters with excess vacancies. The findings reveal that excess vacancies are crucial in stabilizing and promoting the growth of Mn-Ni-Si-vacancy clusters. A minimum of seven vacancies is required for stable nucleation and growth of these clusters. These Mn-Ni-Si clusters act as defect sinks, effectively trapping and absorbing mobile vacancies generated under irradiation. Furthermore, phosphorus (P) preferentially dissolves in Mn-Ni-Si clusters due to chemical coupling with vacancies. In conclusion, this study offers new insights into solute-vacancy interactions, enhancing our understanding of solute-defect cluster formation and embrittlement in low-alloy steels.

36 - MATERIALS SCIENCE↗

Rapid tempering to enhance dynamic performance of high and ultra-high strength steels

This study employed rapid, short-time duration (1 s) tempering to improve the dynamic performance of high-strength steel (HSS) and ultra-high-strength steel (UHSS), compared to quenched and conventionally (1800 s) tempered microstructures. Rapid tempering significantly improved the Charpy toughness of both steels compared to the conventionally tempered condition at an equivalent tempering parameter (TP) or hardness level. For conventionally tempered conditions, tempered martensite embrittlement was observed within the tempering temperature range of 200–400 °C, whereas rapid tempering exhibited increased Charpy toughness with increasing tempering temperature across all tempering conditions. Dynamic compression experiments indicated that rapid tempering led to improved ductility compared to the conventionally tempered condition at an equivalent TP. This work shows that the same rapid tempering strategy used for HSS is directly transferable to a higher-carbon UHSS and provides the first systematic evidence of improved strength-ductility combinations and cracking resistance under dynamic compression, supported by Kolsky bar experiments.

36 MATERIALS SCIENCE↗