Hydrogen environment embrittlement of astroloy and Udimet 700 (nickel-base) and V-57 (iron-base) superalloys

The sensitivity to hydrogen environment embrittlement of three superalloys was determined. Astroloy forgings were resistant to embrittlement during smooth tensile, notched tensile, and creep testing in 3.5-MN/sq m hydrogen over the range 23 to 760 C. The notched tensile strength of Udimet 700 bar stock in hydrogen at 23 C was only 50 percent of the baseline value in helium. Forgings of V-57 were not significantly embrittled by hydrogen during smooth tensile testing over the range 23 to 675 C; creep and rupture lives of V-57 were degraded by hydrogen. Postcreep tensile ductility of V-57 was reduced by 40 percent after creep exposure in hydrogen.

Gray, H. R.↗

Effect of casting geometry on mechanical properties of two nickel-base superalloys

An investigation was performed to determine mechanical properties of two rhenium-free modifications of alloy TRW, and to evaluate the suitability of the alloy for use in a small integrally cast turbine rotor. The two alloys were initially developed using stress rupture properties of specimens machined from solid gas turbine blades. Properties in this investigation were determined from cast to size bars and bars cut from 3.8 by 7.6 by 17.8 cm blocks. Specimens machined from blocks had inferior tensile strength and always had markedly poorer rupture lives than cast to size bars. At 1,000 C the cast to size bars had shorter rupture lives than those machined from blades. Alloy R generally had better properties than alloy S in the conditions evaluated. The results show the importance of casting geometry on mechanical properties of nickel base superalloys and suggest that the geometry of a component can be simulated when developing alloys for that component.

Johnston, J. R.↗

Volume Fraction Determination in Cast Superalloys and DS Eutectic Alloys by a New Practice for Manual Point Counting

Volume fraction of a constituent or phase was estimated in six specimens of conventional and DS-eutectic superalloys, using ASTM E562-76, a new standard recommended practice for determining volume fraction by systematic manual point count. Volume fractions determined ranged from 0.086 to 0.36, and with one exception, the 95 percent relative confidence limits were approximately 10 percent of the determined volume fractions. Since the confidence-limit goal of 10 percent, which had been arbitrarily chosen previously, was achieved in all but one case, this application of the new practice was considered successful.

Andrews, C. W.↗

Preparation of eutectic superalloys by EFG

An attempt was made to produce airfoil shaped bars of three different eutectic superalloys by means of the edge-defined, film-fed growth (EFG) method. The alloys used were a gamma + delta Ni-Cb alloy, a gamma/gamma prime + delta Ni-Cb-Al alloy and a Co-TaC alloy containing Ni and Cr. The development of a new die material was essential in the investigation since these alloys are reactive toward known die materials. Tantalum carbide was selected as a die material because it exhibited spontaneous capillary rise and slow rate of degradation in the liquid metals. Eutectic bars up to 1 mm thick and 6 mm wide were grown from TaC dies in order to determine the growth characteristics and the thermal gradient. Large bars of the gamma/gamma prime + delta alloy were grown and tensile tested. A die with a blind central cavity was designed and several hollow, tear-shaped bars were grown.

Hurley, G. F.↗

Hot corrosion studies of four nickel-base superalloys: B-1900, NASA-TRW VIA, 713C and IN738

The susceptibility to hot corrosion of four nickel base superalloys has been studied at 900 deg and 1000 deg C in one atmosphere of slowly flowing oxygen. Hot corrosion was induced by coating the samples with known doses of NaSO4 and oxidizing the coated samples isothermally on a sensitive microbalance. In general, the order of susceptibility found was: B-1900 is greater than 713C is greater than NASA-TRW VIA and is greater than IN738. This order corresponds to the order of decreasing molybdenum content of the alloys. Chemical evidence for B-1900 indicates that hot corrosion is instigated by acid fluxing of the protective Al2O3 coating by MoO3.

Fryburg, G. C.↗

Oxidation in oxygen at 900 deg and 1000 deg C of four nickel-base cast superalloys: NASA-TRW VIA, B-1900, alloy 713C, and IN-738

The oxidation at 900 and 1,000 C of four nickel-base superalloys in 1 atmosphere of slowly flowing oxygen was investigated. Thermogravimetric rate data were obtained for periods to 100 hours. The morphology and composition of the oxide scales formed after 100 hours were studied by optical microscopy, X-ray diffraction, electron microprobe, scanning electron microscopy, and X-ray photoelectron spectroscopy (ESCA). Alloys B-1900 and VIA were found to be primarily alumina formers, though probably 25 percent of their surface was covered by CR2O3-containing oxides at 900 C. Alloys 713C and IN-738 were primarily chromia formers, though the surface of 713C at 1,000 C was covered with NiO, and the surface of IN-738 at both temperatures was covered with a thin layer of TiO2.

Fryburg, G. C.↗

Estimate of conjugate gamma and gamma prime compositions in Ni-base superalloys

Approaches for estimating the composition of the matrix phase of alloys from the melt composition are reviewed. The first method is based on assigning essentially fixed stoichiometry to precipitating phases and is typified by PHACOMP. The second method uses analytical geometry to interpret phase diagrams and is applicable to a two-phase region of a six-component Ni-base system. The geometric method is also applicable to commercial Ni-base superalloys.

Dreshfield, R. L.↗

Susceptibility to hot corrosion of four nickel-base superalloys, NASA-TRW VIA, B-1900, 713C and IN-738

The susceptibility to hot corrosion of four nickel-base, cast superalloys has been studied at 900 and 1000 C. The test consisted of coating alloy samples with known amounts of Na2SO4 and oxidizing the coated samples isothermally in 1 atmosphere of slowly flowing oxygen, the weight-gain being monitored on a sensitive recording microbalance. Susceptibility to hot corrosion decreased in the order of decreasing molybdenum content of the alloys. Preoxidation of samples before hot-corrosion testing markedly increased the induction period observed prior to the inception of hot corrosion for all alloys tested. X-ray diffraction analyses of the oxide scales were made. All samples that underwent hot corrosion showed the presence of a (Ni,Co)MoO4 layer near the alloy-oxide interface. Several specimens displayed resistance to hot corrosion and these showed NaTaO3 as a prominent feature in their oxide scale. Our results may be interpreted as indicating that molybdenum in an alloy is detrimental, with respect to hot corrosion, while tantalum is beneficial.

Stearns, C. A.↗

Effect of simulated Earth reentry exposure on mechanical properties of several oxide dispersion strengthened and superalloy sheet materials

The effects of simulated multiple reentry into the earth's atmosphere on the mechanical properties of several high temperature metallic sheet materials were evaluated. The materials included five tin-gage (nominally 0.025- or 0.037-cm) oxide dispersion strengthened (ODS) alloys and two thin-gage (nominally 0.037-cm) superalloys. Multiple reentry conditions were simulated through cyclic Plasma Arc Tunnel (PAT) exposure. PAT exposure generally consisted of 100 cycles of 600 second duration at 1255, 1366, or 1477 K in a Mach 4.6 airstream with an impact pressure of nominally 800 N/m2. PAT exposure generally produced a uniform oxide scale, oxide pits or intergranular oxidation, Kirkendall porosity, and alloy depletion zones except for the aluminum-containing ODS alloys. Only a uniform oxide scale was formed on the aluminum-containing ODS alloys. PAT exposure did not significantly affect the mechanical properties of the thin-gage (nominally 0.025- or 0.037-cm) alloys evaluated. Thus it appears that the microstructural changes produced by Plasma Arc Tunnel exposure has little influence on mechanical properties.

Whittenberger, J. D.↗

Directionally solidified eutectic gamma plus beta nickel-base superalloys

A directionally solidified multivariant eutectic gamma + beta nickel-base superalloy casting having improved high temperature strength and oxidation resistance properties is provided. This comprises a two phase eutectic structure containing, on a weight percent basis, 5.0-15.0 tungsten, 8.5-14.5 aluminum, 0.0-35.0 cobalt and the balance being nickel. Embedded within the gamma phase nickel-base matrix are aligned eutectic beta phase (primarily (NiCo)Al reinforcing lamellae.

Jackson, M. R.↗

Mechanism of beneficial effect of tantalum in hot corrosion of nickel-base superalloys

X-ray diffraction and electron microprobe analyses were used to examine a prominent NaTaO3 pattern formed in a number of nickel-base superalloys. It is found that a beneficial effect of tantalum with respect to hot corrosion attack arises from the ability of Ta2O5 to tie up Na2O and prevent the formation of a molten Na2MoO4 phase.

Fryburg, G. C.↗

Hot corrosion studies of four nickel-base superalloys - B-1900, NASA-TRW VIA, 713C and IN738

The susceptibility to hot corrosion of four nickel-base superalloys has been studied at 900 and 1000 C in one atmosphere of slowly flowing oxygen. Hot corrosion was induced by coating the samples with known doses of Na2SO4 and oxidizing the coated samples isothermally on a sensitive microbalance. In order of decending susceptibility to hot corrosion, these alloys were ranked: B-1900, 713C, NASA-TRW VIA, IN738. This order corresponds to the order of decreasing molybdenum content of the alloys. Chemical evidence for B-1900 indicates that hot corrosion is instigated by acid fluxing of the protective Al2O3 coating by MoO3.

Fryburg, G. C.↗

High temperature oxidation resistant coatings for the directionally solidified Ni-Nb-Cr-Al eutectic superalloy

Protective coatings required for the Ni-Nb-Cr-Al directionally solidified eutectic superalloy were developed and evaluated on the basis of oxidation resistance, diffusional stability, thermal fatigue, and creep resistance. NiCrAlY+Pt and NiCrAlY physical vapor-deposition coating systems exhibited the best combination of properties. Burner-rig testing indicated that the useful life of a 127-micron-thick NiCrAlY+Pt coating exceeds 1000 h at 1366 K. Eutectic-alloy creep lives at 1311 K and a stress of 151.7 MN/sq m were greater for NiCrAlY+Pt-coated specimens than for uncoated specimens by a factor of two.

Strangman, T. E.↗

Wrought nickel-base superalloy

Superalloy for advanced temperature use is suited to cost-saving powder-metallurgy manufacturing methods and has improved phase stability during longtime heating. Wide variety of applications exists where stainless steels are used for oxidation and/or corrosion resistance.

Miner, R. V.↗

Directionally solidified eutectic gamma-gamma nickel-base superalloys

A directionally solidified multivariant eutectic gamma-gamma prime nickel-base superalloy casting having improved high temperature properties was developed. The alloy is comprised of a two phase eutectic structure consisting essentially of on a weight percent base, 6.0 to 9.0 aluminum, 5.0 to 17.0 tantalum, 0-10 cobalt, 0-6 vanadium, 0-6 rhenium, 2.0-6.0 tungsten, and the balance being nickel, subject to the proviso that the sum of the atomic percentages of aluminum plus tantalum is within the range of from 19-22, and the ratio of atomic percentages of tantalum to aluminum plus tantalum is within the range of from 0.12 to 0.23. Embedded within the gamma nickel-base matrix are aligned eutectic gamma prime phase (primarily nickel-aluminum-tantalum) reinforcing fibers.

Jackson, M. R.↗

Study of the effects of gaseous environments on sulfidation attack of superalloys

Studies were conducted to examine the effect of the gaseous corrodents NaCl, HCl, and NaOH on the high temperature oxidation and Na2SO4-induced corrosion behavior of the alumina former NiAl, the chromia former Ni-25 wt.% Cr, elemental Cr, and the superalloy B-1900. Experiments were conducted at 900 and 1050 C in air in the presence and absence of the gaseous corrodents. Effects involving both reaction rates and microstructural changes in oxide morphology were observed due to the presence of these corrodents at levels anticipated to be present in operating industrial and marine gas turbines. The effect of gaseous NaCl, HCl, and possibly NaOH on NiAl in simple oxidation was to remove aluminum from below the protective alumina layer and to simultaneously weaken the adherence of the protective alumina oxide scale to the substrate. The aluminum removed from below the oxide scale was redeposited on its surface as alpha-Al2O3 whiskers. With respect to the chromia formers, gaseous NaCl and HCl promoted breakaway oxidation kinetics and changes in the microstructures of the oxide scales.

Smeggil, J. G.↗

An experimental P/M wrought superalloy for advanced temperature service

A study was undertaken in order to adapt IIB-11 (an experimental wrought superalloy with high temperature strength) to manufacture via powder metallurgy techniques, and to improve its microstructural stability. Three compositional modifications were produced and evaluated. Among the conclusions reached it was found that: (1) IIB-11 having a low C and low Hf alloy content is suitable for advanced temperature turbine disks, and is applicable to fabrication by powder metallurgy techniques, (2) IIB-11, when compared to modifications with higher C and/or higher Hf, is somewhat weaker in tension at intermediate temperatures but superior in tensile ductility, rupture strength and ductility, and stability during long-time heating, (3) increases in the cross-rolling temperature increase the grain size of alloys after solution treatment, and (4) both the lower C modifications develop larger grain sizes than the higher C modification.

Miner, R. V.↗

Strength enhancement of prealloyed powder superalloys

Strengthening and forming process for prealloyed powder superalloys greatly increases material strength in the 900-1,200F temperature range. Process which involves superplastically-deforming compacted powders at controlled rates and temperature is most effective on nickel-base alloys.