Reaction–drift–diffusion models from master equations: application to material defects

We present a general method to produce well-conditioned continuum reaction–drift–diffusion equations directly from master equations on a discrete, periodic state space. We assume the underlying data to be kinetic Monte Carlo models (i.e. continuous-time Markov chains) produced from atomic sampling of point defects in locally periodic environments, such as perfect lattices, ordered surface structures or dislocation cores, possibly under the influence of a slowly varying external field. Our approach also applies to any discrete, periodic Markov chain. Here, the analysis identifies a previously omitted non-equilibrium drift term, present even in the absence of external forces, which can compete in magnitude with the reaction rates, thus being essential to correctly capture the kinetics. To remove fast modes which hinder time integration, we use a generalized Bloch relation to efficiently calculate the eigenspectrum of the master equation. A well conditioned continuum equation then emerges by searching for spectral gaps in the long wavelength limit, using an established kinetic clustering algorithm to define a proper reduced, Markovian state space.

36 MATERIALS SCIENCE↗

30 cm Drop Modeling

This report documents modeling and analysis of the 30 cm cask drop scenario for spent nuclear fuel (SNF) casks. The 30 cm drop is an important hypothetical dynamic loading scenario for SNF because 10 CFR 71.71 defines testing requirements for normal conditions of transport (NCT) of SNF packages, and free drop (of 30 cm for the heaviest packages) tests are required. Other NCT conditions specified in 10 CFR 71.71 include vibration normally incident to transport, and DOE’s multimodal transportation test (MMTT) and related analysis concluded that mechanical shock and vibration incident to transportation is negligible for SNF structural integrity because the loads are so small. The SNF cask 30 cm drop has a lot more potential to cause damage to SNF because the kinetic energy and momentum of the system is stopped abruptly during the cask impact event. Test data and model predictions both agree that the SNF assemblies are subjected to significantly higher loads in a cask drop event than normal transportation shock and vibration, but currently there is no reason to expect gross structural damage of the fuel assembly or widespread SNF cladding failure as a result of a 30 cm cask drop. The ultimate goal of this work is to close the knowledge gap of stress profiles on SNF rods and fuel assembly components during NCT, and this report describes the progress toward reaching that goal as well as a plan for finishing this work over the next year or two. Key remaining tasks include refining the fuel assembly model, calculating a selection of specific fuel assembly cases to populate the damage model, and finally running the damage model to predict the full general response range of 30 cm drop loads on SNF.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Entrapment Behavior of Solid Surrogate Fission Products at Engineered UN Nano‐Hetero‐Interfaces Within Metallic Nuclear Fuels

Nanometric hetero-interfaces provide a wealth of scientific and engineering opportunities due to their complex and often misunderstood properties that can differ from their respective bulk constituents. In this work, the ability for engineered nanostructures within a bulk U─Mo alloy to arrest simulant fission products is investigated experimentally and computationally. Nanostructured 90 wt% U/ 10 wt% Mo (U-10Mo) with 7.1 at% Nd is consolidated using spark-plasma- sintering (SPS) techniques and is heat-treated at 500 °C under vacuum for 24, 100, 500, and 1000 h. Analysis on the sintered and heat-treated U-10Mo reveals rapid kinetics in Nd diffusion to nanocluster sites, with evidence of Nd diffusion occurring during sintering and during the following heat-treatment. The segregation behavior of Nd at two different U─Mo/UN interfaces is computationally verified using density functional theory (DFT) to reinforce experimental data.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Simulation and flow physics of a shocked and reshocked high-energy-density mixing layer

This work describes a computational investigation of multimode instability growth and multimaterial mixing induced by multiple shock waves in a high-energy-density (HED) environment, where pressures exceed 1 Mbar. The simulations are based on a series of experiments performed at the National Ignition Facility (NIF) and designed as an HED analogue of non-HED shock-tube studies of the Richtmyer–Meshkov instability and turbulent mixing. A three-dimensional computational modelling framework is presented. It treats many complications absent from canonical non-HED shock-tube flows, including distinct ion and free-electron internal energies, non-ideal equations of state, radiation transport and plasma-state mass diffusivities, viscosities and thermal conductivities. The simulations are tuned to the available NIF data, and traditional statistical quantities of turbulence are analysed. Integrated measures of turbulent kinetic energy and enstrophy both increase by over an order of magnitude due to reshock. Large contributions to enstrophy production during reshock are seen from both the baroclinic source and enstrophy–dilatation terms, highlighting the significance of fluid compressibility in the HED regime. Dimensional analysis reveals that Reynolds numbers and diffusive Péclet numbers in the HED flow are similar to those in a canonical non-HED analogue, but conductive Péclet numbers are much smaller in the HED flow due to efficient thermal conduction by free electrons. It is shown that the mechanism of electron thermal conduction significantly softens local spanwise gradients of both temperature and density, which causes a minor but non-negligible decrease in enstrophy production and small-scale mixing relative to a flow without this mechanism.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Determining the Reaction Kinetics and Thermodynamics of a Diels–Alder Network Using Dynamic Gel Criteria

We undertook a detailed rheological investigation to evaluate the kinetic parameters of the forward and reverse Diels–Alder (DA) reactions of a model network cross-linked using a furan prepolymer and a common aromatic bismaleimide. At high temperature where the Winter–Chambon’s criterion of frequency-independence was more applicable, a multiwave technique permitted van’t Hoff analysis and calculation of the reaction thermodynamic parameters, specifically the enthalpy and entropy of the reaction: ΔH° = –38.3 ± 5.2 kJ mol –1 and ΔS° = –94.3 ± 13.4 J mol –1 . At mild temperatures where the G'–G" crossover point is experimentally convenient to measure gelation, isothermal tests were used to obtain reasonable fDA kinetic parameters from Eyring analysis such as the apparent activation enthalpy and entropy of ΔH$^{‡}_{fDA}$ = 76.8 ± 6.9 kJ mol –1 and ΔS$^{‡}_{fDA}$= –82.8 ± 22.2 J mol –1 K –1 . Comparable rheokinetic methods include cross-linking density measurements and stress relaxation tests to calculate effective kinetics, whereas the critical gel conversion was consistently applied here. As a result, rate data are fitted with the Arrhenius equation for comparison purposes and the Eyring equation to demonstrate its broader utility.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Chemistry and P-V-T equation of state of FeO 2 H x at the base of Earth’s lower mantle and their geophysical implications

The hydrogen-absorbing ability of a mantle mineral in its structure determines the capacity of the water reservoirs hosted by the mineral. Water reservoirs at the base of Earth’s mantle directly influence the fate of water brought down by slab subduction and the seismic heterogeneity such as ultralow-velocity zones (ULVZs) at the core-mantle boundary. Pyrite-FeO 2 H x (0 ≤ x ≤ 1) presents a possibility of such reservoirs in the deep mantle. Ever since the discovery of this mineral phase, however, its chemistry at the lower mantle conditions has been debated. We conducted kinetics experiments of pyrite-FeO 2 H x dehydrogenation at 110 GPa/2100 K, 110 GPa/2300 K, and 120 GPa/2300 K and P-V-T equation of state analysis using in situ synchrotron X-ray diffraction. We found that x approaches 0.80, 0.75, and 0.79, respectively, at the above conditions. The collective P-V-T data yield K 0 = 241(13) GPa, K' = 4.2(4), dK/dT = –0.028(1) GPa/K, α 0 = 4.32(13) × 10 –5 K –1 , and α 1 = 0.31(10) × 10 –8 K –2 for the composition of x = 0.75 ± 0.04. Our first-principles calculations indicate that FeO 2 H 0.75 with a slightly distorted pyrite structure is stable at 100 GPa. These results indicate that this mineral is likely present in the deep mantle with rather a partially dehydrogenated composition than FeO 2 or FeOOH. Furthermore, the results also clarify the difference between the ULVZs originated from pyrite-FeO 2 H x and those from partial melting in terms of shear and compressional wave seismic velocity reduction ratio δlnV S /δlnV P .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Autoignition Delay Times of Hydrogen/Ammonia/Air Mixtures at Gas Turbine Relevant Conditions

This study reports the autoignition delay times of hydrogen/ammonia mixtures at conditions similar to turbine engine operating conditions (23 bar, 1100-1250 K). H2 was mixed with NH3 and shock-heated using synthetic air as the oxidizer. The data is compared against the current state-of-the-art NH3 chemical kinetic mechanisms found in the literature for undiluted fuel validation and refinement. Experiments were performed in a high-pressure shock tube and have shown detonation pressures reaching 200 bar. Lower temperature points have also exhibited non-ideal behavior, which calls for extensive chemical analysis to accurately report the IDTs. This work will aid in the design of air-breathing turbine engines using hydrogen and ammonia as fuel and develop a well-built NH3-based chemical kinetic mechanism.

Pierro, Michael↗

Proton Transfer Dynamics in the Aprotic Proton Accepting Solvent 1-Methylimidazole

The dynamics of proton transfer to the aprotic solvent 1-methylimidazole (MeIm, proton acceptor) from the photoacid 8-hydroxypyrene-1,3,6-trisulfonic acid trisodium salt (HPTS) were investigated using fast fluorescence measurements. The closely related molecule, 8- methoxypyrene-1,3,6-trisulfonic acid trisodium salt (MPTS), which is not a photoacid, was also studied for comparison. Following optical excitation, the wavelength-dependent population dynamics of HPTS in MeIm resulting from the deprotonation process were collected over the entire fluorescence emission window. Analysis of the time-dependent fluorescence spectra revealed four distinct fluorescence bands that appear and decay on different time scales. We label these four states as: protonated (P), associated I (A I ), associated II (A II ), and deprotonated (D). We find that the simple kinetic scheme of P → A I → A II → D is not consistent with the data. Instead, the kinetic scheme that describes the data has P decaying into A I , which mainly goes on to deprotonation (D), but AI can also feed into A II . A II can return to A I or decay to the ground state, but does not deprotonate within experimental error. Finally, quantum chemistry and excitedstate QM/MM Born-Oppenheimer molecular dynamics simulations indicate that A I and A II are two H-bonding conformations of MeIm to the HPTS hydroxyl, axial and equatorial, respectively.

14 SOLAR ENERGY↗

Intercalative Redox Tuning for Cu/Li x Mn 2 O 4 -Catalyzed Oxidative Alkyne Coupling

Modulation of heterogeneous catalyst structure is ubiquitous within efforts to improve catalytic activity and selectivity at the molecular level. Herein, manganese oxide (MnO 2 ) is employed as a continuously tunable catalyst support through increasing extent of lithium intercalation and reduced surface potential. Oxidative grafting of an organocopper complex onto various lithium manganese oxides (Li x Mn 2 O 4 , x = 0-2.1) produced divalent and monovalent copper species on the partially reduced (0 ≤ x ≤ 1.2) and fully reduced (x = 2.1) surfaces, respectively, as determined by X-ray absorption fine structure (XAFS) analysis. In this study, the resultant materials are catalytically active for the oxidative coupling of terminal alkynes, with steady-state reaction rate data of oxidative propyne dimerization (200 °C, 0.6-2.4 kPa propyne, 2.4-9.9 kPa O 2 ) indicating that complete support lithiation (Li 2.1 Mn 2 O 4 ) provides increased catalytic performance and renders reoxidation steps less kinetically demanding compared to the unreduced parent material. Enacting a dual site (Cu and MnO x ) kinetic model can account for dimerization rates measured over Cu/Li 2.1 Mn 2 O 4 under various reactant concentrations, copper loadings, and surface coverages, providing supporting evidence for the synergistic role of the metal and support in facilitating the coupling reaction. Overall, results presented here provide an extension for general strategies of systematically controlling catalytic structure and function through lithium reduction of bulk oxides and subsequent electronic modulation of the metals supported thereon.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Final-stage densification kinetics of direct current–sinteredZrB2

Final-stage sintering was analyzed for nominally phase pure zirconium diboride synthesized by borothermal reduction of high-purity ZrO2. Analysis was conducted on ZrB2 ceramics with relative densities greater than 90% using the Nabarro–Herring stress–directed vacancy diffusion model. Temperatures of 1900°C or above and an applied uniaxial pressure of 50 MPa were required to fully densify ZrB2 ceramics by direct current sintering. Ram travel data were collected and used to determine the relative density of the specimens during sintering. Specimens sintered between 1900 and 2100°C achieved relative densities greater than 97%, whereas specimens sintered below 1900°C failed to reach the final stage of sintering. The average grain size ranged from 1.0 to 14.7 μm. The activation energy was calculated from the slope of an Arrhenius plot that used the Kalish equation. The activation energy was 162 ± 34 kJ/mol, which is consistent with the activation energy for dislocation movement in ZrB2. The diffusion coefficients for dislocation motion that controls densification were 5.1 × 10−6 cm2/s at 1900°C and 5.1 × 10−5 cm2/s at 2100°C, as calculated from activation energy and average grain sizes. This study provides evidence that the dominant mechanism for final-stage sintering of ZrB2 ceramics is dislocation motion.

36 MATERIALS SCIENCE↗

High-throughput calculations of charged point defect properties with semi-local density functional theory—performance benchmarks for materials screening applications

Abstract Calculations of point defect energetics with Density Functional Theory (DFT) can provide valuable insight into several optoelectronic, thermodynamic, and kinetic properties. These calculations commonly use methods ranging from semi-local functionals with a-posteriori corrections to more computationally intensive hybrid functional approaches. For applications of DFT-based high-throughput computation for data-driven materials discovery, point defect properties are of interest, yet are currently excluded from available materials databases. This work presents a benchmark analysis of automated, semi-local point defect calculations with a-posteriori corrections, compared to 245 “gold standard” hybrid calculations previously published. We consider three different a-posteriori correction sets implemented in an automated workflow, and evaluate the qualitative and quantitative differences among four different categories of defect information: thermodynamic transition levels, formation energies, Fermi levels, and dopability limits. We highlight qualitative information that can be extracted from high-throughput calculations based on semi-local DFT methods, while also demonstrating the limits of quantitative accuracy.

36 MATERIALS SCIENCE↗

Graphite Oxidation Rate Study on ET-10 and ETU-10 Grades - Task 4: QA Support and Testing for Structural Graphite Oxidation

INL performed targeted oxidation tests to measure oxidation rates for samples of ET-10 and ETU-10 graphite under CRADA No. 21CRA22 Mod. 3, Annex A, “Tritium Testing to Support Kairos Power Advanced Reactor Demonstration” (04/02/2024). All testing was conducted within INL’s Carbon Characterization Laboratory (CCL) using test standard ASTM D7542-21 "Standard Test Method for Air Oxidation of Carbon and Graphite in the Kinetic Regime" [ASTM International, 2021]. Kairos Power provided all test specimens through its graphite vendor Ibiden, Inc. to INL and ASTM specimen specified dimensions. Information within this report only provides the Arrhenius oxidation rate plots as a function of temperature for each graphite grade tested. The raw mass loss per time data will be provided on the Nuclear Data Management and Analysis System (NDMAS) portal located on the INL information system.

36 MATERIALS SCIENCE↗

Insights into the Oxidative Degradation Mechanism of Solid Amine Sorbents for CO 2 Capture from Air: Roles of Atmospheric Water

Abstract Direct air capture (DAC) processes for extraction of CO 2 from ambient air are unique among chemical processes in that they operate outdoors with minimal feed pretreatments. Here, the impact of humidity on the oxidative degradation of a prototypical solid supported amine sorbent, poly(ethylenimine) (PEI) supported on Al 2 O 3 , is explored in detail. By combining CO 2 adsorption measurements, oxidative degradation rates, elemental analyses, solid‐state NMR and in situ IR spectroscopic analysis in conjunction with 18 O labeling of water, a comprehensive picture of sorbent oxidation is achieved under accelerated conditions. We demonstrated that the presence of water vapor can play an important role in accelerating the degradation reactions. From the study we inferred the identity and kinetics of formation of the major oxidative products, and the role(s) of humidity. Our data are consistent with a radical mediated autooxidative degradation mechanism.

Carneiro, Juliana S. A.↗

Tracking structural solvent reorganization and recombination dynamics following e – photoabstraction from aqueous I – with femtosecond x-ray spectroscopy and scattering

Here we present a sub-picosecond resolved investigation of the structural solvent reorganization and geminate recombination dynamics following 400 nm two-photon excitation and photodetachment of a valence p electron from the aqueous atomic solute, I–(aq). The measurements utilized time-resolved X-ray Absorption Near Edge Structure (TR-XANES) spectroscopy and X-ray Solution Scattering (TR-XSS) at the Linac Coherent Light Source x-ray free electron laser in a laser pump/x-ray probe experiment. The XANES measurements around the L 1 -edge of the generated nascent iodine atoms (I 0 ) yield an average electron ejection distance from the iodine parent of 7.4 ± 1.5 Å with an excitation yield of about 1/3 of the 0.1M NaI aqueous solution. The kinetic traces of the XANES measurement are in agreement with a purely diffusion-driven geminate iodine–electron recombination model without the need for a long-lived (I 0 :e–) contact pair. Nonequilibrium classical molecular dynamics simulations indicate a delayed response of the caging H 2 O solvent shell and this is supported by the structural analysis of the XSS data: We identify a two-step process exhibiting a 0.1 ps delayed solvent shell reorganization time within the tight H-bond network and a 0.3 ps time constant for the mean iodine–oxygen distance changes. The results indicate that most of the reorganization can be explained classically by a transition from a hydrophilic cavity with a well-ordered first solvation shell (hydrogens pointing toward I–) to an expanded cavity around I 0 with a more random orientation of the H 2 O molecules in a broadened first solvation shell.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Chloride Salt Purification by Reaction With Thionyl Chloride Vapors to Remove Oxygen, Oxygenated Compounds, and Hydroxides

Molten chloride salts (including MgCl 2 , KCl, NaCl, and ZnCl 2 ) are being considered for heat transfer media for renewable (solar) and nuclear power generators, as fuel carrier for nuclear reactors, and as thermal energy storage media. Impurities such as oxygen, hydroxides, moisture, and sulfur are known to negatively influence the corrosion of materials in contact with the salt (e.g., structural metals). Commercially available chloride salts come with a range of impurities. Before using the chloride salts at high temperature, it is desirable to remove the impurities to increase the performance of the salt and reduce corrosion. In this study, we tested the use of thionyl chloride vaporized into a stream of argon to react with oxygenated impurities in a mixture of MgCl 2 -KCl-NaCl, removing them as HCl and SO 2 . The reagent was bubbled through the salt when both above and below the melting point. The reaction was followed using thermocouple data from the salt and by Fourier transform infrared (FTIR) spectroscopy on the exhaust of the reactor. The reaction kinetics were followed by comparing the peaks from SO 2 product to SOCl 2 reagent in the FTIR spectra. The purity of the salt was assessed at the end of the purification process by x-ray diffraction and inductively coupled plasma analysis. Although the process was effective in removing the oxygen content of the mixture, ternary compounds were formed in the process, including KNiCl 3 and KMgCl 3 . The nickel in KNiCl 3 came from the reaction between the salt and the nickel vessel. Thus, these experiments suggest that improvements to the process must be made before using SOCl 2 vapors for the purification of chloride salts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Predicting Pulsed-Laser Deposition SrTiO 3 Homoepitaxy Growth Dynamics Using High-Speed Reflection High-Energy Electron Diffraction

Pulsed-laser deposition (PLD) is a powerful technique for growing complex oxides with controlled stoichiometry. To understand growth dynamics therein, it is common to leverage in situ spectroscopies, such as reflection high-energy electron diffraction (RHEED), to monitor surface crystallinity. Most commercial systems rely on video-rate cameras operating at 60-120 Hz that lack sufficient temporal resolution to capture growth dynamics at practical deposition frequencies. Here, a high-speed platform to record in situ dynamics via RHEED at >500 Hz is implemented. An open-source analysis package is designed to fit diffraction spots to 2D Gaussians, allowing single-pulse surface reconstruction kinetics extraction. Using homoepitaxially deposited (001)-oriented SrTiO 3 as a model system, we demonstrate how high-speed RHEED can provide real-time insight into growth processes obscured by slower acquisition systems. By fitting the single-pulse intensity to a set of exponential functions, we observe changes in the characteristic decay time and mechanism correlated to the substrate step width and surface termination. We observe distinct surface effects, with diffraction intensity decaying on lower-energy TiO 2 -terminated surfaces and stabilizing on SrO- or mixed-terminated surfaces. Similarly, using an exponential model, the extracted characteristic time of adatom deposition decreases with increased density of bonding sites associated with mixed termination and narrower step widths. Ultimately, this work shows how increasing RHEED temporal resolution can uncover new insights into growth processes, with practical implications for the design and control of PLD processes. This experimental platform provides new capabilities to enable data-driven machine learning analysis and autonomous control systems to enhance the complexity and fecundity of PLD.

(SrO)↗

The OCEAN ICE mooring compilation: a standardised, pan-Antarctic database of ocean hydrography and current time series

Continuous moored time series of temperature, salinity, pressure and current speed and direction are of great importance for understanding the continental shelf and under-ice-shelf dynamics and thermodynamics that govern water mass transformations and ice melting in and around Antarctic marginal seas. In these regions, icebergs and sea ice make ship-based mooring deployment and recovery challenging. Nevertheless, over decades, expeditions around the fringe of Antarctica sporadically deployed and recovered hundreds of moored instruments, including those facilitated through ice shelves boreholes. These datasets tend to be archived in a wide range of data centres, with, to our knowledge, no clear format standardisation. As a result, systematic analysis of historical mooring time series in the marginal seas is often challenging. Here we present the first version of a standardised pan-Antarctic moored hydrography and current time series compilation, with broad international contributions from data centres, research institutes and individual data owners. The mooring records in this compilation span over five decades, from the 1970s to the 2020s, providing an opportunity for a systematic study of the pan-Antarctic water mass transport and shelf connectivity. As a demonstration of the utility of this compilation, we present spectral analysis of the compiled current velocity time series, which unsurprisingly shows the dominating presence of tidal variability within most records. This component of the variability is fitted using multi-linear regression to tidal frequencies, and the tidal fit is removed from the original time series to leave de-tided variability. Given the limited record durations to months to years, de-tided variability is dominated by synoptic (3–10 d period), intraseasonal (10–80 d) and seasonal (∼6 months–1 year) signals. The spatial distribution of the kinetic energy integrated within frequency bands is presented and discussed within respective regional contexts, and future avenues of research are proposed. This data compilation is assembled under the endorsement of Ocean-Cryosphere Exchanges in ANtarctica: Impacts on Climate and the Earth System (OCEAN ICE) project (https://ocean-ice.eu/, last access: 23 October 2025) funded by the European Commission and UK Research and Innovation. It is available and regularly updated in NetCDF format with the SEANOE database at https://doi.org/10.17882/99922 (Zhou et al., 2024a).

54 ENVIRONMENTAL SCIENCES↗

Insights into the Oxidative Degradation Mechanism of Solid Amine Sorbents for CO 2 Capture from Air: Roles of Atmospheric Water

Direct air capture (DAC) processes for extraction of CO 2 from ambient air are unique among chemical processes in that they operate outdoors with minimal feed pretreatments. Here, the impact of humidity on the oxidative degradation of a prototypical solid supported amine sorbent, poly(ethylenimine) (PEI) supported on Al 2 O 3 , is explored in detail. By combining CO 2 adsorption measurements, oxidative degradation rates, elemental analyses, solid-state NMR and in situ IR spectroscopic analysis in conjunction with 18 O labeling of water, a comprehensive picture of sorbent oxidation is achieved under accelerated conditions. Here we demonstrated that the presence of water vapor can play an important role in accelerating the degradation reactions. From the study we inferred the identity and kinetics of formation of the major oxidative products, and the role(s) of humidity. Our data are consistent with a radical mediated autooxidative degradation mechanism.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗