Designing In-Situ-Formed Interphases Enables Highly Reversible Cobalt-Free LiNiO2 Cathode for Li-ion and Li-metal Batteries
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
This work presents a non-destructive in-situ method for probing degradation mechanisms in large format, operating, commercial lithium-ion batteries by neutron diffraction. A fresh battery (15 Ah capacity) was shown to have a uniform (homogeneous) local state of charge (SOC) at 4.0 V (9 Ah SOC) and 4.2 V (15 Ah SOC), with 1.33 C and 2.67 C charging rates, respectively. This battery was then aggressively cycled until it retained only a 9 Ah capacity, 60% of its original value. Inhomogeneous deterioration in the battery was observed: near the edges, both the graphite anode and the spinel-based cathode showed a significant loss of capacity, while near the central area, both electrodes functioned properly. An SOC mapping measurement of the degraded battery in the fully charged state (4.2 V) indicated that the loss of local capacity of the anode and cathode is coupled.
Here, 1.5 Ah pouch cells based on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 cathodes and graphite anodes, both containing poly (vinylidene fluoride) (PVDF) binders, were systematically overcharged to 100, 120, 140, 160, 180, and 250% state of charge (SOC), at which point they vented. The cells were subsequently discharged to 0% SOC and disassembled under an inert atmosphere for characterization. A combination of X-ray photoelectron spectroscopy (XPS), scanning-electron microscopy (SEM), energy-dispersive spectroscopy (EDS), 6 Li SSNMR, and X-ray diffraction (XRD) analysis of the NMC532 cathodes indicates the formation of a thin C- and O-rich cathode electrolyte interphase layer, progressive Li loss above 140% SOC, and retention of the bulk crystal structure at all states of charge.
In this work, a unique artificial interface combing characteristics of both high ionic and electronic conductivities has been successfully constructed at the surface of Ni-rich LiNi 0·8 Co 0·1 Mn 0·1 O 2 (NCM811). The ionic conductor layer is fabricated through reacting H 3 PO 4 with the lithium residuals on the surface of NCM811 to form Li 3 PO 4 . The interface with high electronic conductivity is constructed by attaching graphene fragments to the NCM811 spherical particles. Due to the synergistic effect of the Li3PO4 coating layer and the graphene network, the modified sample (GN-LPO-NCM811) exhibits high capacity retention of 94.3% after 150 cycles at 0.5C between 3.0 and 4.3 V, while the pristine material shows a much lower retention of only 88.1%. In addition, the GN-LPO-NCM811 also presents improved cycling stability at elevated temperature of 55 °C. Even at an extremely high rate of 10C, the GN-LPO-NCM811 still remains 70% of its original capacity, while the pristine NCM811 only delivers 50% of the capacity. The stable cycling performance of GN-LPO-NCM811 is demonstrated in a full cell with graphite anode at ambient temperatures. Importantly, the thermal stability of the modified samples is also greatly enhanced. This study provides an effective method to improve the electrochemical performance of LiNi 0·8 Co 0·1 Mn 0·1 O 2 .
A quantitative measurement of wettability between the porous electrode and the electrolyte in lithium-ion batteries can greatly improve our understanding of wetting behavior. Although the wetting balance method is widely used to measure the electrolyte transport rate in the porous electrodes, it suffers from several drawbacks and has limited accuracy. We here presented a combined experimental and theoretical investigation of the dynamics of electrolyte imbibition through electrodes. We suggested a novel method to accurately measure the electrolyte imbibition rate. Excellent agreement between the experimental data and the developed analytical model is obtained. The coefficient of penetrance (COP) and the solid permeability coefficient (SPC) are identified as important parameters, i.e., the electrolyte with higher COP value wets faster into an electrode, whereas for an electrolyte, the electrode with higher SPC value is more amenable to be impregnated. The effect of electrolyte salt concentration and electrolyte solvent has been studied in detail. The result implies that increasing salt concentration adversely influences electrolyte wetting rate, whereas switching from EC-DEC system to EC-EMC system improves electrolyte wetting rate. Moreover, for the electrolytes tested in this study, the imbibition into the uncalendered graphite anode is much faster than that into the uncalendered NMC532 cathode.
The rapidly growing technological demand for lithium-ion batteries has prompted the development of novel cathode materials with high energy density, low cost, and improved safety. High voltage spinel, LiNi 0.5 Mn 1.5 O 4 (LNMO), is one of the most promising candidates yet to be commercialized. The two primary obstacles for this material are the inferior electronic conductivity and fast capacity degradation in full cells due to the high operating voltage. By systematically addressing these limitations, we successfully develop a thick LNMO electrode with areal capacity loadings up to 3 mAh·cm –2 . The optimized thick electrode is paired with a commercial graphite anode at both the coin cell and pouch cell level, achieving a full cell capacity retention as high as 72% and 78%, respectively, after 300 cycles. We attribute this superior cycling stability to careful optimizations of cell components and testing conditions, with a specific focus improving electronic conductivity and high voltage compatibility. These results suggest precise control of materials quality, electrode architecture and electrolyte optimization can soon support the development of a cobalt-free battery system based on a thick LNMO cathode (>4 mAh·cm 2 ), which will eventually meet the needs of next-generation Li-ion batteries with reduced cost, improved safety, and assured sustainability.
Fast charging of lithium-ion (Li-ion) batteries makes it susceptible to lithium plating. Here, we report the correlation between capacity loss and cell impedance changes in the battery due to lithium electrodeposition. Li-ion pouch cells with nickel-manganese-cobalt cathode and graphite anode were charged at rates varying from 0.5C to 6C. The cell voltage evolution immediately after charging was monitored to identify the C-rates that result in lithium plating. Electrochemical impedance spectroscopy (EIS) was used to monitor the cell impedance evolution. The impedance of battery cells at C-rates lower than 1C and no lithium plating showed minimal changes from their baseline values in the period immediately after charging. However, the impedance of battery cells undergoing lithium plating and C-rates higher than 3C showed a substantial reduction immediately after charging, with recovery back to baseline values after 30 min of relaxation. These observations suggest that lithium plating causes damage to the solid electrolyte interface (SEI) layer on the anode particles during the charging period, followed by the reformation of the SEI during the relaxation period. The measured capacity loss has a linear correlation with observed impedance change. The linear relationship suggests that impedance monitoring may be used for prognostication of the state-of-health of Li-ion batteries.
The practical application of graphite anodes in lithium-ion batteries (LIBs) is constrained by low specific capacity (372 mAh g -1 ) and sluggish kinetics. Here, to address these limitations, our present study focuses on high-entropy oxides (HEOs), which offer high theoretical capacity and structural stability. We synthesized spinel-structured (AlMnCoNiZn) 3 O 4 nanoparticles via a solution combustion method and fabricated an (AlMnCoNiZn) 3 O 4 @polypyrrole (PPy) nanocomposite through in-situ polymerization. Our electrochemical tests demonstrate that the PPy modification significantly enhances performance. While the pristine (AlMnCoNiZn) 3 O 4 delivered 445 mAh g −1 after 100 cycles at 100 mA g −1 and 350 mAh g −1 after 1000 cycles at 1000 mA g −1 , the (AlMnCoNiZn) 3 O 4 @PPy composite achieved 695 mAh g −1 after 100 cycles and maintained 675 mAh g −1 after 1000 cycles. Furthermore, the composite improved rate capacity at 1000 mA g −1 from 211 mAh g −1 to 403 mAh g −1 . This work highlights how conductive and flexible polymer modifications can dramatically improve the electrochemical properties of HEOs. The developed (AlMnCoNiZn) 3 O 4 @PPy composite provides a promising direction for designing advanced anodes to meet next-generation energy storage demands.
As fast-charging technology expands across the electric vehicle and emerging energy-storage applications, understanding its impact on battery performance and longevity is critical. In this study, 1.8 Ah LiNi 0.6 Mn 0.2 Co 0.2 O 2 /graphite pouch cells were charged at various charging rates (0.5C, 2C, 4C, and 6C) to investigate the degradation mechanisms. Our results showed that well-designed NMC/Gr pouch cells could reach over 1000 cycles with a 2C charging rate, while only reaching around 500 cycles with 4C and 6C charging rates. Fast-charging effects on NMC and graphite electrodes were obtained through a series of post-mortem characterizations, including electrochemical impedance spectroscopy (EIS), Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS). Although higher charging rates cause pulverization of NMC secondary particles, the dominant degradation mechanism driving the fading of fast-charging-related performance lies in the graphite anode, where lithium plating and LiF-rich solid electrolyte interphase (SEI) formation result in Li inventory loss and impedance growth. The postmortem results suggest that the formation of a LiF-rich SEI, which exacerbates anode impedance and some irreversible Li + ion loss, is likely driven by the substantial decomposition of PF 6 − during fast charging, an effect often overlooked in smaller laboratory-scale studies.
Graphical abstract: Zn/Si core-shell arrays prepared by combined hydrothermal plus sputtering method show good performance with high specific capacity and excellent cycling stability. - Highlights: • Construct Zn/Si core-shell arrays via sputtering. • The Zn/Si core-shell arrays show high capacity and good cycles. • Core-shell arrays is favorable for fast ion/electron transfer. - Abstract: Silicon is considered as the most promising substitute for the commercial graphite anode of lithium ion batteries (LIBs) due to its high capacity and low working voltage. In this work, we realize the rational combination between Zn nanorods and Si forming self-supported Zn/Si core-shell arrays with the aid of hydrothermal and sputtering methods. Amorphous Si layer is well coated on the backbone of Zn nanorods with diameters of 70–80 nm. As a preliminary test, the Zn/Si core-shell arrays are used as the anode of LIBs and demonstrated with a high initial reversible capacity of 2795 mAh g{sup −1} at 0.1C, good high-rate capability with 1985 mAh g{sup −1} at 1C and stable cycling life. The good performance is due to the highly conductive Zn nanorod network and porous core-shell structure providing good mechanical support and fast transport of ions/electrons.
Nickel-rich layered lithium transition metal oxides, LiNi x Co y Mn 1-x-y O 2 , are key cathode materials for high-energy lithium-ion batteries owing to their high specific capacity. However, the commercial deployment of nickel-rich oxides has been hampered by their poor thermostability and insufficient cycle life. In this work full batteries with uncoated and TiO 2 -coated LiNi 0.5 Co 0.2 Mn 0.3 O 2 cathodes and graphite anodes are compared in terms of electrochemical performance and safety behavior. The battery using a TiO 2 -coated LiNi 0.5 Co 0.2 Mn 0.3 O 2 cathode exhibited better cyclic performance at high cutoff voltage. Electrochemical impedance spectroscopy analysis indicated that the TiO 2 -coated LiNi 0.5 Co 0.2 Mn 0.3 O 2 cathode gave the battery a more stable charge transfer resistance. Transmission electron microscopy demonstrated that TiO 2 coating reduced accumulation of the cathode electrolyte interface layer on the particle surface. Time-of-flight secondary ion mass spectrometry demonstrated that TiO 2 coating markedly enhanced the interface stability of the cathode particle and protected the particle from serious etching by the electrolyte. Accelerating rate calorimetry revealed that the trigger temperature of thermal runaway for the battery using TiO 2 -coated LiNi 0.5 Co 0.2 Mn 0.3 O 2 as cathode material was 257 °C, which was higher than that of the battery with the uncoated LiNi 0.5 Co 0.2 Mn 0.3 O 2 cathode (251 °C). In situ X-ray diffraction during heating demonstrated that this enhanced safety can be attributed to the suppressed phase evolution of the coated cathode material.
Transition metal fluorides as Li-free conversion-type cathode materials have high theoretical specific capacities, however, their preparation strategy, sluggish electrochemical kinetic and poor cyclability have impeded their wide adoption in lithium-ion batteries. Herein, a facile in-situ synthesis of porous metal-fluoride-carbon composites is accomplished via simultaneous polytetrafluorethylene-based hard template etching and metal fluorination. This not only facilitates fast electron transfer and lithium-ion diffusion kinetics, but also buffers severe volume fluctuation during lithiation/delithation and enables the formation of a uniform and thin Li 2 CO 3 /LiF-rich cathode-electrolyte interphase. Here, as a proof of concept, the as-prepared porous FeF 3 @C (p-FeF 3 @C) indeed exhibits a high specific capacity of 230 mAh g -1 at 0.1 C together with an excellent capacity retention of 92.5% at 1 C for 200-cycles. Moreover, the practicality of the strategy is demonstrated by the superb electrochemical performance of the full-cells coupled with pre-lithiated graphite anodes. Therefore, the proposed novel synthetic strategy will enlighten the future design of high-performance metal-fluoride-carbon composites with porous structure for energy storage applications.
It is imperative to recover lead (Pb) contained in end-of-life solar modules. In this paper, a two-step leaching and electrowinning process using acetic acid is investigated for Pb recovery. Acetic acid with hydrogen peroxide can dissolve Pb quickly and, under some conditions, in a matter of minutes. Pb electrowinning has been successfully demonstrated from aqueous solutions of 0.009 M lead(II) acetate with 0–10% v/v acetic acid. Pb-containing deposits are found on both the copper cathode and graphite anode. X-ray diffraction, energy-dispersive X-ray spectroscopy, and Fourier transform infrared spectroscopy confirm the presence of metallic Pb and Pb(II) oxide (PbO) co-deposits on the cathode. Further, there is also the formation of lead subacetate on the cathode under certain conditions. On the anode, the deposit consists of lead(IV) oxide and superoxide (PbO 2 and Pb 1–x O 2 ). A Pb recovery rate of 99% is achieved in 0.009 M lead(II) acetate solutions with 10% v/v acetic acid by applying a reduction potential of either –0.8 V or –1.0 V versus the silver/silver chloride reference electrode for 24h. Pb leaching with acetic acid is also demonstrated from milled silicon solar modules.
The need/desire to lower the consumption of fossil fuels and its environmental consequences has reached unprecedented levels in recent years. A global effort has been undertaken to develop advanced renewable energy generation and especially energy storage technologies, as they would enable a dramatic increase in the effective and efficient use of renewable (and often intermittent) energy sources. The development of electrical energy storage (EES) technologies with high energy and power densities, long life, low cost, and safe use represents a challenge from both the fundamental science and technological application points of view. While the advent and broad deployment of lithium-ion batteries (LIBs) has dramatically changed the EES landscape, their performance metrics need to be greatly enhanced to keep pace with the ever-increasing demands imposed by modern consumer electronics and especially the emerging automotive markets. Current battery technologies are mostly based on the use of a transition metal oxide cathode (e.g., LiCoO 2 , LiFePO 4 , or LiNiMnCoO 2 ) and a graphite anode, both of which depend on intercalation/insertion of lithium ions for operation. While the cathode material currently limits the battery capacity and overall energy density, there is a great deal of interest in the development of high-capacity cathode materials as well as anode materials. Conversion reaction materials have been identified/proposed as potentially high-energy-density alternatives to intercalation-based materials. Yet, conversion reaction materials react during lithiation to form entirely new products, often with dramatically changed structure and chemistry, by reaction mechanisms that are still not completely understood. This makes it difficult to clearly distinguish the limitations imposed by the mechanism and practical losses from initial particle morphology, synthetic approaches, and electrode preparations. Transition metal compounds such as transition metal oxides, sulfides, fluorides, phosphides, and nitrides can undergo conversion reactions yielding materials with high theoretical capacity (generally from 500 to 1500 mA h g –1 ). Specifically, a number of transition metal oxides and sulfides have shown excellent electrochemical properties as high-capacity anode materials. In addition, some transition metal fluorides have shown great potential as cathode materials for Li rechargeable batteries. In this Account we present mechanistic studies, with emphasis on the use of operando methods, of selected examples of conversion-type materials as both potentially high-energy-density anodes and cathodes in EES applications. We also include examples of the conceptually similar conversion-type reactions involving chalcogens and halogens, with emphasis on the Li–S system. In this case we focus on the problems arising from the low electrical conductivities of elemental sulfur and Li 2 S and the “redox shuttle” phenomena of polysulfides. In addition to mechanistic insights from the use of operando methods, we further cover several key strategies in electrode materials design such as controlling the size, morphology, composition, and architecture.
High-nickel layered oxides continue to prevail in the energy storage market as the frontmost cathode candidates for next-generation lithium-ion batteries. Demand and development of LiNi 1–x–y Mn x Co y O 2 (NMC) and LiNi 1–x–y Co x Al y O 2 (NCA) cathodes are rampantly increasing, particularly for the electric vehicle (EV) industry. However, the continued presence of cobalt in NMC and NCA cathodes raises global concerns due to geopolitical and ethical issues attributed to Co sourcing. We herein introduce a novel cobalt-free, high-nickel cathode LiNi 0.7 Mn 0.25 Al 0.05 O 2 (NMA70) and benchmark it against Co-containing LiNi 0.7 Mn 0.15 Co 0.15 O 2 (NMC70) as well as Co- and Al-free LiNi 0.7 Mn 0.3 O 2 (NM70) cathodes with equivalent 70% Ni contents that are all synthesized in-house. NMA70 displays a high initial C/10 capacity of 210 mA h g –1 , matching that of NMC70 in half cells with a cutoff voltage of 4.5 V. NMA70 also exhibits an impressive high-voltage full cell cycling performance with a cutoff voltage of 4.4 V with a nearly identical capacity retention of 83% compared to that of 82% for NMC70 after 300 cycles. Postmortem X-ray photoelectron spectroscopy (XPS), high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM), and electron energy loss spectroscopy (EELS) analyses indicate a thinner cathode–electrolyte interface (CEI) developed in NMA70 compared to that in NM70 and unveil a more robust solid-electrolyte interface (SEI) passivation on the graphite anode among all samples. The benefits of Al doping are additionally highlighted with enhanced high-voltage CEI and thermal stabilities in NMA70. Furthermore, this work assesses the roles of Mn, Al, and Co to demonstrate both the practicality and feasibility of synthesizing cobalt-free, high-nickel cathodes that are promising alternatives to current NMC- and NCA-based cathodes.
High-nickel layered oxide cathodes are key to meet the demands of the electric vehicle industry because of their high specific capacity. However, commercialization of these materials is hindered by critical challenges, such as phase transitions, particle cracking, aggressive surface reactivity, and thermal instability. Cation doping along with surface coating has proven to be an effective way to circumvent some of these issues to a large extent. Herein, fluorine coating is employed on a high-nickel Li[Ni 0.95 Mn 0.015 Co 0.02 Al 0.01 Mg 0.005 ]O 2 (NMCAM) cathode via a solution route. Detailed structural and electrochemical analyses indicate fluorine largely decorates the surface at low enough calcination temperatures. The cathode with 1 mol % fluorine coating exhibits a capacity retention of 71% after 500 cycles as compared to 59% for the control sample when cycled to a high cutoff voltage of 4.3 V in a full cell configuration with graphite anode. Post-mortem analysis of cycled electrodes reveals that surface reactivity is a major contributor to capacity fade as compared to particle cracking. Fluorine coating reduces surface reactivity and the depth to which rock-salt phase is formed on the surface during cycling. The thermal stability is also enhanced after fluorine coating as the material shows less heat release at high states of charge. Furthermore, this work demonstrates an effective, economical, and scalable way to stabilize the surface with fluorine and enhance the electrochemical performance of high-nickel cathodes.
Fast charging remains one of the greatest safety challenges in Li-ion batteries due to Li-dendrite growth occurring on graphite anodes if they are lithiated too quickly. The search for high-rate anodes has highlighted materials in the Wadsley–Roth (WR) shear phase family. The relative abundance of V compared with traditional WR compositions of Nb and W makes V-based phases attractive. However, the high voltage and poor reversibility typically associated with V redox have made V-rich WR phases less studied than Nb- and W-rich phases. Here, we show that a new V-rich Wadsley–Roth phase, V 7 Nb 6 O 29 , achieves excellent rate capability and 80% capacity retention after 228 cycles with a relatively low average voltage of 1.76 V vs Li/Li + compared with other V-rich WR phases. Single-crystal X-ray diffraction reveals a P4/m space group with repeating 2 × 2 × ∞ and 3 × 3 × ∞ blocks of V 4+ and Nb 5+ octahedra. Finally, combined neutron pair distribution function analysis, X-ray absorption spectroscopy, and density functional theory calculations show that V redox is the primary source of capacity and that cycling stability is provided by the stable octahedral coordination adopted by V 4+ in the material.
The density functional theory and ab initio molecular dynamics simulations are applied to investigate the migration of Mn(II) ions to above-surface sites on spinel Li x Mn 2 O 4 (001) surfaces, the subsequent Mn dissolution into the organic liquid electrolyte, and the detrimental effects on graphite anode solid electrolyte interphase (SEI) passivating films after Mn(II) ions diffuse through the separator. The dissolution mechanism proves complex; the much-quoted Hunter disproportionation of Mn(III) to form Mn(II) is far from sufficient. Key steps that facilitate Mn(II) loss include concerted liquid/solid-state motions; proton-induced weakening of Mn–O bonds forming mobile OH – surface groups; and chemical reactions of adsorbed decomposed organic fragments. Mn(II) lodged between the inorganic Li 2 CO 3 and organic lithium ethylene dicarbonate (LEDC) anode SEI components facilitate electrochemical reduction and decomposition of LEDC. Our findings help inform future design of protective coatings, electrolytes, additives, and interfaces.