pCAM precursor produced from electroextraction technology and its application in synthesis of NMC 811 cathode material

The synthesis and characterization of LiNi 0.8 Co 0.1 Mn 0.1 O 2 (LNMC811) cathodes produced from recycled hydroxide precursors obtained from spent lithium-ion batteries is evaluated. Two precursor batches (Sample 1 and Sample 2) are prepared using modified recycling processes to examine how residual impurities and processing conditions influence the properties of the regenerated materials. Structural and compositional characterization by X-ray diffraction, ICP and SEM shows that the recycled precursors exhibit layered hydroxide structures containing both α Ni(OH) 2 and β Ni(OH) 2 phases. Trace impurities including sodium, boron, and aluminum are detected and partially mitigated during processing, with boron found to play a beneficial role in electrochemical behavior. Following lithiation with lithium carbonate and lithium hydroxide at 800 °C under an oxygen rich atmosphere, the resulting LNMC811 materials show electrochemical performance comparable to conventionally synthesized cathodes. Sample 2, which contains higher boron levels and improved cation ordering, delivers an initial discharge capacity of 174 mAh g -1 and retains more than 93 percent of its capacity after 50 cycles. The stable cycling behavior and structural integrity of these materials demonstrate that recycled precursors can be converted into high performance layered cathodes and support recycling as a practical and sustainable route for lithium-ion battery manufacturing.

25 ENERGY STORAGE↗

Understanding of three different polyvinylpyrrolidone (PVP) based battery binders blends on graphene surfaces from first principles via DFT simulations

Binders play a crucial role in binding electrodes, current collectors, and conductive agents during battery manufacturing. The selection of the binders and their blends considerably affect various properties such as mechanical durability, adhesion performance, ionic/electronic conductivities, and solid electrolyte interface stability for lithium-ion batteries. In this work, polyvinylidene di-fluoride (PVDF), polyacrylic acid (PAA), polyvinylpyrrolidone (PVP), and lithiated polyacrylic acid (Li-PAA) were selected as the model binders, and their blends were studied on graphene surfaces. Further, among them, PVDF is hardly soluble in water unlike the other binders, so in practice, the blend of PVP:PVDF is not thought to be a proper combination. However, the PVP:PVDF binder has also been included because the purpose of this work is to calculate several electronic properties such as binding energies, intermolecular interaction energies, bond critical points, electron density, and the Laplacian of electron density at critical bonding regions of all these blends at the molecular level via density functional theory (DFT) simulations in order to evaluate and compare how is the interaction strength and bonding type of three different lithium-ion batteries (LIBs) binder blends on graphene surfaces. Most stable binder pairs and their binding mechanisms on graphene surfaces were studied. The delocalization of lithium in Li-PAA was studied with the presence of water.

25 ENERGY STORAGE↗

Electrolyte design for Li metal-free Li batteries

Li metal, with the lowest thermodynamically achievable negative electrochemical potential and the highest specific capacity (3860 mAh g -1 ), is the ultimate anode choice for Li batteries. However, the highest reported Li plating/stripping Coulombic efficiency (CE) of 99.5% after extensive efforts is still too low for the Li metal-free (all the Li metal in cycling comes from cathode, without anode pre-lithiation) Li metal batteries. The low CE is attributed to both non-uniform Li plating/stripping on the lithiophobic Cu current collector and Li dendrite growth through lithiophilic organic–inorganic solid electrolyte interphase (SEI) formed in carbonate electrolytes. Here, we use a lithiophilic Bismuth graphite blend (Bi–Gr) substrate to replace lithiophobic Cu current collector to seed a uniform Li nucleation, and form a lithiophobic LiF-rich SEI rather than lithiophilic organic-rich SEI to suppress Li dendrite growth. Molecular dynamics simulations reveal the preferential reduction of anions in 2.0 M LiPF 6 in tetrahydrofuran/2-methyl tetrahydrofuran (2.0 M LiPF 6 –mixTHF) electrolyte to generate LiF-rich SEI on plated Li. Bi–Gr substrate and 2.0 M LiPF 6 –mixTHF electrolyte enable the Li anodes to achieve a record high CE of 99.83% at a high capacity of 1.0 mAh cm -2 and current of 0.5 mA cm -2 . The Bi particles serve as dispersed nucleation centers that promote uniform Li deposition with strong adhesion to the substrate to avoid dead Li, while the lithiophobic LiF-rich SEI promotes lateral Li growth and suppresses the vertical Li dendrite growth even at a high current density of 3.0 mA cm -2 and high areal capacities of 3.0 mAh cm -2 . The regulation of Li nucleation and growth enables the Li metal-free LiFePO 4 full cells to achieve 100 cycles at a practical areal capacity of >2.0 mAh cm -2 . This article highlights the benefits of simultaneous substrate design to improve Li nucleation and electrolyte design to promote lithiophobic SEI growth, enabling a promising and practical route Li metal-free Li metal batteries.

36 MATERIALS SCIENCE↗

The effects of vanadium substitution on one-dimensional tunnel structures of cryptomelane: Combined TEM and DFT study

Rational design of energy storage materials requires mechanistic understanding which relies on atomic scale characterization of structure and defects. In this paper we utilize vanadium (V)-substituted one-dimensional cryptomelane as a model material to study structural features critical to electrochemical reversibility of the cathode in lithium-ion batteries. We found the substitution of manganese (Mn) atoms in the tunnel wall with V enhances structural uniformity in the parent KMn 8 O 16 material by inhibiting formation of irregular (2 × 3 and 2 × 1) manganese oxide tunnel structures. Upon lithiation, both transmission electron microscopy (TEM) and density functional theory (DFT) reveal significant structural evolution, eventually resulting in phase separation and formation of highly reduced manganese oxide. During this process, Mn 4+ accepts electrons donated by intercalated Li, while the V 4+ substituent is not electrochemically reduced but acts to stabilize the tunnel framework structure. As a result, the V substituted material shows higher operating voltage and improved electrochemical reversibility. Our results highlight the benefits of V-substitution in cryptomelane, and the significance of integrating characterization with simulation for understanding and developing design principles for lithium ion battery materials.

25 ENERGY STORAGE↗

In-situ synthesis of porous metal fluoride@carbon composite via simultaneous etching/fluorination enabled superior Li storage performance

Transition metal fluorides as Li-free conversion-type cathode materials have high theoretical specific capacities, however, their preparation strategy, sluggish electrochemical kinetic and poor cyclability have impeded their wide adoption in lithium-ion batteries. Herein, a facile in-situ synthesis of porous metal-fluoride-carbon composites is accomplished via simultaneous polytetrafluorethylene-based hard template etching and metal fluorination. This not only facilitates fast electron transfer and lithium-ion diffusion kinetics, but also buffers severe volume fluctuation during lithiation/delithation and enables the formation of a uniform and thin Li 2 CO 3 /LiF-rich cathode-electrolyte interphase. Here, as a proof of concept, the as-prepared porous FeF 3 @C (p-FeF 3 @C) indeed exhibits a high specific capacity of 230 mAh g -1 at 0.1 C together with an excellent capacity retention of 92.5% at 1 C for 200-cycles. Moreover, the practicality of the strategy is demonstrated by the superb electrochemical performance of the full-cells coupled with pre-lithiated graphite anodes. Therefore, the proposed novel synthetic strategy will enlighten the future design of high-performance metal-fluoride-carbon composites with porous structure for energy storage applications.

25 ENERGY STORAGE↗

Structure design enables stable anionic and cationic redox chemistry in a T2-type Li-excess layered oxide cathode

Coupled with anionic and cationic redox chemistry, Li-rich/excess cathode materials are prospective high-energy-density candidates for the next-generation Li-ion batteries. However, irreversible lattice oxygen loss would exacerbate irreversible transition metal migration, resulting in a drastic voltage decay and capacity degeneration. Herein, a metastable layered Li-excess cathode material, T2-type Li 0.72 [Li 0.12 Ni 0.36 Mn 0.52 ]O 2 , was developed, in which both oxygen stacking arrangement and Li coordination environment fundamentally differ from that in conventional O3-type layered structures. By means of the reversible Li migration processes and structural evolutions, not only can voltage decay be effectively restrained, but also excellent capacity retention can be achieved upon long-term cycling. Moreover, irreversible/reversible anionic/cationic redox activities have been well assigned and quantified by various in/ex-situ spectroscopic techniques, further clarifying the charge compensation mechanism associated with (de)lithiation. These findings of the novel T2 structure with the enhanced anionic redox stability will provide a new scope for the development of high-energy-density Li-rich cathode materials.

25 ENERGY STORAGE↗

First-principles study of the structures and redox mechanisms of Ni-rich lithium nickel manganese cobalt oxides

To reduce the cobalt (Co) content in lithium-ion batteries, Ni-rich (high-Ni) lithium nickel manganese cobalt oxides (NMC) are pursued as one of the next-generation cathode materials. However, there is still debate on the crystal and electronic structures of the baseline, LiNiO 2 . Density Functional Theory (DFT) calculations were performed to provide a theoretical understanding of Ni-rich NMC. First, it was found that the commonly used $R\bar{3}m$ structure for LiNiO 2 is metallic, contrary to the experimentally reported mix-conducting behavior. Among the four different space groups, $R\bar{3}m$, C2/m, P2 1 /c, and P2/c, P2/c with charge disproportionation of Ni 2+ and Ni 4+ is the most energetically stable and semiconducting structure of LiNiO 2 . Therefore, the atomic structures of representative Ni-rich NMC were built by partially replacing Ni with Co or Mn in the P2/c LiNiO 2 to form Li x Ni y Mn z Co 1-y-z O 2 . In the fully lithiated (x=1.0) high Ni content NMC (y>0.5), the oxidation state of all Mn ions becomes 4+, while Co ions still maintain 3+, and part of the Ni ions become 3+ to compensate for the charge. Upon delithiation, the local environment shows more variation of the charge states on the transition metal (TM) ions. The average oxidation on each TM follows a sequence of losing electrons that starts from Ni 2+ to Ni 3+ , then oxidizing Ni 3+ and Co 3+ , while Mn 4+ remains electrochemically inactive till x=0. Finally, a general relationship for the oxidation state change in each TM as a function of x is derived and shows agreement with both modeling and experimental data.

25 ENERGY STORAGE↗

Kinetic Pathways Templated by Low-Temperature Intermediates during Solid-State Synthesis of Layered Oxides

Layered oxides have been the dominant cathodes in lithium-ion batteries, and among them, high-nickel (Ni) systems are attractive because of their high capacity. For practical use, synthetic control of stoichiometry and structural ordering is crucial but has been nontrivial due to the complexity inherent to synthesis reactions, which often proceed via nonequilibrium pathways. In this paper, we report here a combined in situ synchrotron X-ray diffraction and ab initio study of solid-state synthesis of layered oxides starting from acetate precursors for LiCoO 2 and LiNiO 2 and their solid solution LiNi 0.8 Co 0.2 O 2 . While all three systems ultimately evolve into the same thermodynamically stable layered phase ($R\overline{3}m$), each chemistry involves distinct metastable intermediates. We explain the phase progressions using a structural template model, demonstrating that during the synthesis of LiCoO 2 , the formed metastable spinel polymorph (Li 2 Co 2 O 4 ; $Fd\overline{3}m$) is a kinetically facile lithiation product of spinel Co 3 O 4 —the low-temperature (LT) intermediate from the decomposed Co-acetate. Similarly, in the Ni-based systems, the acetate decomposition products, rocksalts (Ni,Co)O, topotactically template the kinetic pathways of forming disordered rocksalts (Li x (Ni,Co) 2–x O 2 ; $Fm\overline{3}m$), consequently leading to off-stoichiometric Li x (Ni,Co)O 2 with undesired high Li/Ni mixing. These findings highlight new opportunities for engineering precursors to form LT intermediates that template the synthesis of target phases and structural properties.

36 MATERIALS SCIENCE↗

Anionic Oxygen Redox in the High-Lithium Material Li 8 SnO 6

Lithiated transition metal oxide cathode materials that combine oxygen-anion redox [O 2 – /(O 2 ) n– ] with cation redox offer substantial capacities and higher voltage than cathodes without oxygen redox, but oxygen-anion redox is usually accompanied by the formation of peroxo or superoxo species that may cause oxygen release. To clarify the relationship between the oxygen release and peroxide and superoxide dimers without the complication of transition-metal redox, we performed density functional theory calculations to study the layered Li 8 SnO 6 cathode because it has only oxygen-anion redox during delithiation. Features with O–O distances of ~1.5 Å (corresponding to the formation of a peroxide) were observed at 75% lithium concentration, and further delithiation to 62.5% lithium concentration shortened the O–O bond distance to ~1.3 Å (corresponding to the formation of superoxide). The solely anionic oxygen redox stabilizes the delithiated structure of Li 8–x SnO 6 , and it does not cause structural disorder or release oxygen gas. Ab initio molecular dynamics calculations in the supercell at 300 K indicate that oxygen dimerization may occur at 75% lithium concentration. On the (0001) surface with a high lithium concentration (98%), oxygen dimerization is unfavorable. The calculations by HSE06 show that oxygen redox in Li 8 SnO 6 offers an initial voltage (vs Li/Li + ) greater than 4.2 V. The GGA+U calculations indicate that the Li + -polaron in Li 95 Sn 12 O 72 migrates with a migration barrier of only 0.43 eV. Here, this work also quantifies a solely anionic oxygen redox mechanism in Li 8 SnO 6 , and it provides a deeper understanding of anionic oxygen redox in Li-excess oxide cathode materials.

25 ENERGY STORAGE↗

Structural Evolution of Layered Manganese Oxysulfides during Reversible Electrochemical Lithium Insertion and Copper Extrusion

The electrochemical lithiation and delithiation of the layered oxysulfide Sr 2 MnO 2 Cu 4-δ S 3 has been investigated by using a combination of in situ powder X-ray diffraction and ex situ neutron powder diffraction, X-ray absorption and 7 Li NMR spectroscopy, together with a range of electrochemical experiments. Sr 2 MnO 2 Cu 4-δ S 3 consists of [Sr 2 MnO 2 ] perovskite-type cationic layers alternating with highly defective antifluorite-type [Cu 4-δ S 3 ] (δ ≈ 0.5) anionic layers. It undergoes a combined displacement/intercalation (CDI) mechanism on reaction with Li, where the inserted Li replaces Cu, forming Li 4 S 3 slabs and Cu + is reduced and extruded as metallic particles. For the initial 2-3% of the first discharge process, the vacant sites in the sulfide layer are filled by Li; Cu extrusion then accompanies further insertion of Li. Mn 2.5+ is reduced to Mn 2+ during the first half of the discharge. The overall charging process involves the removal of Li and re-insertion of Cu into the sulfide layers with re-oxidation of Mn 2+ to Mn 2.5+ . However, due to the different diffusivities of Li and Cu, the processes operating on charge are quite different from those operating during the first discharge: charging to 2.75 V results in the removal of most of the Li, little reinsertion of Cu, and good capacity retention. A charge to 3.75 V is required to fully reinsert Cu, which results in significant changes to the sulfide sublattice during the following discharge and poor capacity retention. This detailed structure-property investigation will promote the design of new functional electrodes with improved device performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Access to Ru(IV)–Ru(V) and Ru(V)–Ru(VI) Redox in Layered Li 7 RuO 6 via Intercalation Reactions

The push to increase the capacity of oxides to store charge as Li-ion battery cathodes has challenged our knowledge of the boundaries of redox chemistry and its relationship to the atomic structure. Layered phases with Ru are now classical models in the quest for refined theories. Current understanding dictates that the highest formal state that can be reached in them is Ru(V), after which activity centered at the oxide anions is triggered. Yet, this picture is challenged by this investigation of the intercalation chemistry of Li 7 RuO 6 . Coupling structural and spectroscopic analysis with computational simulations, we show that Li 7 RuO 6 is capable of highly reversible lithiation to Li 8 RuO 6 through the Ru(V)/Ru(IV) redox couple. Further, Li 7 RuO 6 can also undergo anodic Li deintercalation, showing clear evidence of the reversible formation of Ru(VI) with octahedral coordination, an unusual state that is not accessible in other layered oxides. The results highlight the versatility of the Ru-O bond to undergo distinct redox transitions depending on the specific layered arrangements. They enrich our understanding of redox chemistry in solids while underscoring the need for descriptions of charge compensation that reflect the nuance of covalent interactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Exploring the Origin of Anionic Redox Activity in Super Li-Rich Iron Oxide-Based High-Energy-Density Cathode Materials

Super alkali-rich materials (alkali:transition metal ratio of ≥2:1), such as Li 5 FeO 4 , exhibit the potential to realize anionic redox upon deep delithiation. Li 5 FeO 4 was shown to undergo reversible cycling between Li 4 FeO 3.5 and Li 3 FeO 3.5 with combined cation/anion redox, a remarkable capacity of 189 mAh/g, and no O 2 release. However, the impact of phase transformations on the reaction thermodynamics and the correlation between the structural changes and reaction reversibility remain unclear. In this study, we use first-principles calculations to examine the delithiation and (re)lithiation reactions of Li 5 FeO 4 . We show that the experimentally observed charge and discharge processes go through non-equilibrium pathways. Upon delithiation, the compound undergoes a phase transformation from Li 5 FeO 4 , with tetrahedrally coordinated (T d ) Fe ions, to a delithiated disordered rocksalt structure, with octahedral (O h ) Fe ions. Fe-ion migration has an asymmetric kinetic barrier that makes T d → O h migration facile, whereas the reverse process has a much larger barrier, explaining the difficulties in reaction reversibility. We further elucidate the transition metal and O redox sequences during the charge cycle and identify the complex electrochemistry associated with the dual participation of cationic redox (Fe 3+ /Fe 4+ ) and anionic redox (O 2– /O – /O o ). Armed with this knowledge, we conduct high-throughput screening of known alkali-rich transition metal oxides by evaluating their potential to enable reversible anionic redox, with multiple candidates proposed for further experimental trials. Furthermore, our work provides a useful guide for the further development of super alkali-rich anionic-redox-active electrodes for high-energy-density batteries.

25 ENERGY STORAGE↗

Sequential Fe Reduction, Involving Two Different Fe + Intermediates, in the Conversion Reaction of Prussian Blue in Lithium-Ion Batteries

In this work, ex situ X-ray absorption spectroscopy and in operando 57 Fe-Mössbauer spectroscopy measurements are conducted to examine in detail the ongoing reaction mechanism of potassium Prussian blue (K-PB) within the narrow [1.6–0.005 V] voltage range, and so to determine whether this material truly undergoes a conversion reaction, as we proposed elsewhere. The generation of Fe 0 is confirmed by both techniques, finding that 40 to 58% of iron gets reduced to metallic iron at 5 mV. The elucidation of the mechanism by in situ 57 Fe-Mössbauer spectroscopy further reveals a sequential process for the reduction (lithiation) of the two different iron species initially present in Prussian blue. Both high-spin Fe 2+ –N first and low-spin Fe II –C next go through the unusual Fe 1+/I formal oxidation state during the reduction process, before forming surface Fe 0 nanoparticles (NPs) below 0.48 V. Upon charge, Fe 0 NPs preferentially oxidizes into Fe + –N. Interestingly, these surprising Fe + species play an important role in decreasing the overpotential during the charge (delithiation) process with respect to other conversion systems.

25 ENERGY STORAGE↗

Understanding the Fluorination of Disordered Rocksalt Cathodes through Rational Exploration of Synthesis Pathways

Here, we have designed and tested several synthesis routes targeting a highly fluorinated disordered rocksalt (DRX) cathode, Li 1.2 Mn 0.4 Ti 0.4 O 1.6 F 0.4 , with each route rationalized by thermochemical analysis. Precursor combinations were screened to raise the F chemical potential and avoid the formation of LiF, which inhibits fluorination of the targeted DRX phase. MnF 2 was used as a reactive source of F, and Li 6 MnO 4 , LiMnO 2 , and Li 2 Mn 0.33 Ti 0.66 O 3 were tested as alternative Li sources. Each synthesis procedure was monitored using a multi-modal suite of characterization techniques including X-ray diffraction, nuclear magnetic resonance, thermogravimetric analysis, and differential scanning calorimetry. From the resulting data, we advance the understanding of oxyfluoride synthesis by outlining the key factors limiting F solubility. At low temperatures, MnF 2 consistently reacts with the Li source to form LiF as an intermediate phase, thereby trapping F in strong Li-F bonds. LiF can react with Li 2 TiO 3 to form a highly lithiated and fluorinated DRX (Li 3 TiO 3 F); however, MnO is not easily incorporated into this DRX phase. Although higher temperatures typically increase solubility, the volatility of LiF above its melting point (848 °C) inhibits fluorination of the DRX phase. Based on these findings, metastable synthesis techniques are suggested for future work on DRX fluorination.

36 MATERIALS SCIENCE↗

Reversible Electrochemical Lithium Cycling in a Vanadium(IV)- and Niobium(V)-Based Wadsley–Roth Phase

Fast charging remains one of the greatest safety challenges in Li-ion batteries due to Li-dendrite growth occurring on graphite anodes if they are lithiated too quickly. The search for high-rate anodes has highlighted materials in the Wadsley–Roth (WR) shear phase family. The relative abundance of V compared with traditional WR compositions of Nb and W makes V-based phases attractive. However, the high voltage and poor reversibility typically associated with V redox have made V-rich WR phases less studied than Nb- and W-rich phases. Here, we show that a new V-rich Wadsley–Roth phase, V 7 Nb 6 O 29 , achieves excellent rate capability and 80% capacity retention after 228 cycles with a relatively low average voltage of 1.76 V vs Li/Li + compared with other V-rich WR phases. Single-crystal X-ray diffraction reveals a P4/m space group with repeating 2 × 2 × ∞ and 3 × 3 × ∞ blocks of V 4+ and Nb 5+ octahedra. Finally, combined neutron pair distribution function analysis, X-ray absorption spectroscopy, and density functional theory calculations show that V redox is the primary source of capacity and that cycling stability is provided by the stable octahedral coordination adopted by V 4+ in the material.

25 ENERGY STORAGE↗

Electrochemical Control of Magnetism on the Breathing Kagome Network of Li x ScMo 3 O 8

Controlling properties within a given functional inorganic material structure type is often accomplished through tuning the electronic occupation, which is in turn dictated by the elemental composition determined at the time of material preparation. We employ electrochemical control of the lithium content, with associated electronic occupancy control, to vary the magnetic properties of a material where a kagome-derived network of Mo 3 triangles carry the spin. In this case, Li is electrochemically inserted into LiScMo 3 O 8 , a layered compound containing a breathing Mo kagome network. Up to two additional Li can be inserted into LiScMo 3 O 8 , transforming it into Li 3 ScMo 3 O 8 . Li 2 ScMo 3 O 8 prepared by electrochemical lithiation is compared to the quantum spin liquid candidate compound Li 2 ScMo 3 O 8 prepared through high-temperature solid-state methods, which has a slightly different structural stacking sequence but a similar kagome-derived network. Magnetic measurements are supported by first-principles calculations, showing that electrons remain localized on the Mo clusters throughout the doping series. As x is varied in Li x ScMo 3 O 8 , the measurements and calculations reveal the evolution from a diamagnetic band insulator at x = 1 to a geometrically frustrated magnet at x = 2, back to a diamagnetic insulator at x = 3. These results indicate a likelihood of strong coupling between the degree of Li disorder and charge/magnetic ordering over the Mo 3 clusters.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Annealing on Direct Recycled NMC Cathodes

A substantial number of electric vehicle batteries are poised to reach end-of-life conditions in the next decade. Direct recycling has advantages over typical recycling processes because it preserves the chemical structure of the material. One key step of direct recycling materials like nickel manganese cobalt oxide (NMC) cathodes is relithiation, which includes replacing the depleted lithium inventory in the cathode and annealing the material to fix crystallographic degradation. This work uses multiple characterization techniques (synchrotron X-ray diffraction, Ni X-ray absorption near edge structure, scanning transmission electron microscopy) to understand the lithiation mechanism of degraded and chemically relithiated NMC 622. Despite the necessary reconstruction after relithiation being limited to the surface of the degraded NMC 622, a high annealing temperature of 720 °C is still necessary to restore the NMC 622 structure back to pristine condition after relithiation. This work also finds that treating degraded NMC 622 with an annealing step is sufficient to restore key electrochemical and structural properties, other essential features of pristine NMC 622 material such as particle porosity and morphology are largely unaffected. Understanding the effect of this annealing step has important implications on defining the degree of success of any given direct recycling strategy.

36 MATERIALS SCIENCE↗

Perturbation of 1 J C,F Coupling in Carbon–Fluorine Bonds on Coordination to Lewis Acids: A Structural, Spectroscopic, and Computational Study

A lithiated m-terphenyl ligand bearing fluorine atoms at the ortho positions of the flanking aryl rings was synthesized and characterized using single crystal X-ray diffraction, variable-temperature multinuclear NMR spectroscopy, and computational methods. Here, changes in 1 J C,F on coordination to lithium as a spectroscopic observable parametrizing the strength of the C–F···Li interaction are described, and a general, qualitative relationship between C–F bond lengths, Δ 1 J C,F values, and the extent of C–F bond activation as a result of Lewis acid coordination is proposed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗