At least 253 records · Page 14

Free dendritic growth

Free dendritic growth refers to the unconstrained development of crystals within a supercooled melt, which is the classical 'dendrite problem'. Great strides have been taken in recent years in both the theoretical understanding of dendritic growth and its experimental status. The development of this field will be sketched, showing that transport theory and interfacial thermodynamics (capillarity theory) were sufficient ingredients to develop a truly predictive model of dendrite formation. The convenient, but incorrect, notion of 'maximum velocity' was used for many years to estimate the behavior of dendritic transformations until supplanted by modern dynamic stability theory. The proper combinations of transport theory and morphological stability seem to able to predict the salient aspects of dendritic growth, especially in the neighborhood of the tip. The overall development of cast microstructures, such as equiaxed zone formation, rapidly solidified microstructures, etc., also seems to contain additional non-deterministic features which lie outside the current theories discussed here.

Glicksman, M. E.↗

Structure and properties during aging of an ultra-high strength Al-Cu-Li-Ag-Mg alloy

The structure and properties of the strengthening phases formed during aging in an Al-Cu-Li-Ag-Mg alloy (Weldalite 049) were elulcidated, by following the development of the microstructure by means of TEM. The results of observations showed that the Weldalite 049 alloy has a series of unusual and technologically useful combinations of mechanical properties in different aging conditions, such as natural aging without prior cold work to produce high strengths, a reversion temper of lower yield strength and unusually high ductility, a room temperature reaging of the reversion temper eventually leading to the original T4 hardness, and ultrahigh-strength T6 properties.

Gayle, Frank W.↗

Influence of molybdenum on the creep properties of nickel-base superalloy single crystals

The Mo content of an alloy series based on Ni-6 wt pct Al-6 wt pct Ta was systematically varied from 9.8 to 14.6 wt pct, in order to ascertain the influence of Mo on the creep properties of single crystals. The optimum initial gamma-gamma prime microstructure for raft development and creep strength was established in each alloy before testing. It was found that, as the Mo content increased from 9.8 to 14.0 percent, the magnitude of the lattice mismatch increased; upon reaching 14.6 percent, a degradation of mechanical properties occurred due to the precipitation of a third phase. These results suggest that small refractory metal content and initial gamma-prime variations can profoundly affect mechanical properties.

Mackay, R. A.↗

Structure and properties during aging of an Al-Cu-Li-Ag-Mg alloy, Weldalite (tm) 049

An Al-Cu-Li-Ag-Mg alloy, Weldalite (trademark) 049, was recently introduced as an ultra-high strength alloy (7000 MPa yield strength in artificially aged tempers) with good weldability. In addition, the alloy exhibits an extraordinary natural aging response (440 MPa yield strength (YS) in the unstretch condition) and a high ductility reversion condition which may be useful as a cold-forming temper. In contrast to other Al-Li alloys, these properties can essentially be obtained with or without a stretch or other coldworking operation prior to aging. Preliminary studies have revealed that the T4 temper (no stretch, natural age) is strengthened by a combination of GP zones and delta prime (Al3Li). The T6 temper (no stretch, aged at 180 C to peak strength) was reported to be strengthened primarily by T(sub 1) phase (Al2CuLi) with a minor presence of a theta prime like (Al2Cu) phase. On the other hand, a similar but lower solute containing alloy was reported to contain omega, (stoichiometry unknown), theta prime, and S prime in the peak strength condition. The purpose of this study is to further elucidate the strengthening phases in Weldalite (trademark) 049 in the unstretched tempers, and to follow the development of the microstructure from the T4 temper through reversion (180 C for 5 to 45 minutes) to the T6 temper.

Gayle, Frank W.↗

Sol-Gel Synthesis Of Aluminoborosilicate Powders

Application of sol-gel process to synthesis of aluminoborosilicate powders shows potential for control of microstructures of materials. Development of materials having enhanced processing characteristics prove advantageous in extending high-temperature endurance of fibrous refractory composite insulation made from ceramic fibers.

Bull, Jeffrey↗

A creep cavity growth model for creep-fatigue life prediction of a unidirectional W/Cu composite

A microstructural model was developed to predict creep-fatigue life in a (0)(sub 4), 9 volume percent tungsten fiber-reinforced copper matrix composite at the temperature of 833 K. The mechanism of failure of the composite is assumed to be governed by the growth of quasi-equilibrium cavities in the copper matrix of the composite, based on the microscopically observed failure mechanisms. The methodology uses a cavity growth model developed for prediction of creep fracture. Instantaneous values of strain rate and stress in the copper matrix during fatigue cycles were calculated and incorporated in the model to predict cyclic life. The stress in the copper matrix was determined by use of a simple two-bar model for the fiber and matrix during cyclic loading. The model successfully predicted the composite creep-fatigue life under tension-tension cyclic loading through the use of this instantaneous matrix stress level. Inclusion of additional mechanisms such as cavity nucleation, grain boundary sliding, and the effect of fibers on matrix-stress level would result in more generalized predictions of creep-fatigue life.

Kim, Young-Suk↗

Fracture Mechanisms For SiC Fibers And SiC/SiC Composites Under Stress-Rupture Conditions at High Temperatures

The successful application of SiC/SiC ceramic matrix composites as high-temperature structural materials depends strongly on maximizing the fracture or rupture life of the load-bearing fiber and matrix constituents. Using high-temperature data measured under stress-rupture test conditions, this study examines in a mechanistic manner the effects of various intrinsic and extrinsic factors on the creep and fracture behavior of a variety of SiC fiber types. It is shown that although some fiber types fracture during a large primary creep stage, the fiber creep rate just prior to fracture plays a key role in determining fiber rupture time (Monkman-Grant theory). If it is assumed that SiC matrices rupture in a similar manner as fibers with the same microstructures, one can develop simple mechanistic models to analyze and optimize the stress-rupture behavior of SiC/SiC composites for applied stresses that are initially below matrix cracking.

DiCarlo, James A.↗

Aerospace Structural Materials Handbook Supplement GRCop-84

GRCop-84 is a high strength-high conductivity copper-based alloy developed at NASA Glenn Research Center for combustion chamber liners of regeneratively cooled rocket engines. It also has promise for other high heat flux applications operating at temperatures up to 700 C (1292 F) and potentially higher. The alloy must be made by powder metallurgy techniques such as gas atomization. Slower cooling rates such as those experienced during casting do not develop a proper microstructure. Once made into powder, the alloy exhibits excellent processability using conventional consolidation and forming techniques, e.g., extrusion and rolling. GRCop-84 is strengthened by a combination of dispersion and precipitation strengthening by fine (50-500 nanometer (2-20 microinch)) Cr2Nb particles and Hall-Petch strengthening from a fine copper grain size. The presence of a high volume fraction of particles prevents grain boundary sliding at high temperatures and contributes to the alloy's overall good high temperature mechanical properties. Maximum thermal conductivity is obtained by using two alloying elements (Cr, Nb) with limited solubility in solid Cu that form a high temperature intermetallic compound with an even lower solid solubility. The resulting matrix of the alloy is nearly pure copper. The limited solubility also minimizes Cr2Nb particle coarsening at elevated temperatures and enhances microstructural and mechanical property stability. Further enhancement of the microstructural stability is obtained by using a high volume fraction (approx. 14 vol.%) of Cr2Nb particles that effectively pin grain growth.

Ellis, David L.↗

Solar Ion Sputter Deposition in the Lunar Regolith: Experimental Simulation Using Focused-Ion Beam Techniques

As regions of the lunar regolith undergo space weathering, their component grains develop compositionally and microstructurally complex outer coatings or "rims" ranging in thickness from a few 10 s to a few 100's of nm. Rims on grains in the finest size fractions (e.g., <20 m) of mature lunar regoliths contain optically-active concentrations of nm size metallic Fe spherules, or "nanophase Fe(sup o)" that redden and attenuate optical reflectance spectral features important in lunar remote sensing. Understanding the mechanisms for rim formation is therefore a key part of connecting the drivers of mineralogical and chemical changes in the lunar regolith with how lunar terrains are observed to become space weathered from a remotely-sensed point of view. As interpreted based on analytical transmission electron microscope (TEM) studies, rims are produced from varying relative contributions from: 1) direct solar ion irradiation effects that amorphize or otherwise modify the outer surface of the original host grain, and 2) nanoscale, layer-like, deposition of extrinsic material processed from the surrounding soil. This extrinsic/deposited material is the dominant physical host for nanophase Fe(sup o) in the rims. An important lingering uncertainty is whether this deposited material condensed from regolith components locally vaporized in micrometeorite or larger impacts, or whether it formed as solar wind ions sputtered exposed soil and re-deposited the sputtered ions on less exposed areas. Deciding which of these mechanisms is dominant, or possibility exclusive, has been hampered because there is an insufficient library of chemical and microstructural "fingerprints" to distinguish deposits produced by the two processes. Experimental sputter deposition / characterization studies relevant to rim formation have particularly lagged since the early post-Apollo experiments of Hapke and others, especially with regard to application of TEM-based characterization techniques. Here we report on a novel design for simulating solar ion sputter deposition in the lunar regolith, with characterization of the resulting sputter deposits by an array of advanced analytical TEM techniques.

Christoffersen, R.↗

High Temperature Joining and Characterization of Joint Properties in Silicon Carbide-Based Composite Materials

Advanced silicon carbide-based ceramics and composites are being developed for a wide variety of high temperature extreme environment applications. Robust high temperature joining and integration technologies are enabling for the fabrication and manufacturing of large and complex shaped components. The development of a new joining approach called SET (Single-step Elevated Temperature) joining will be described along with the overview of previously developed joining approaches including high temperature brazing, ARCJoinT (Affordable, Robust Ceramic Joining Technology), diffusion bonding, and REABOND (Refractory Eutectic Assisted Bonding). Unlike other approaches, SET joining does not have any lower temperature phases and will therefore have a use temperature above 1315C. Optimization of the composition for full conversion to silicon carbide will be discussed. The goal is to find a composition with no remaining carbon or free silicon. Green tape interlayers were developed for joining. Microstructural analysis and preliminary mechanical tests of the joints will be presented.

Joining↗

Evolution of Local Microstructures: Spatial Instabilities of Coarsening Clusters

This work examines the diffusional growth of discrete phase particles dispersed within a matrix. Engineering materials are microstructurally heterogeneous, and the details of the microstructure determine how well that material performs in a given application. Critical to the development of designing multiphase microstructures with long-term stability is the process of Ostwald ripening. Ripening, or phase coarsening, is a diffusion-limited process which arises in polydisperse multiphase materials. Growth and dissolution occur because fluxes of solute, driven by chemical potential gradients at the interfaces of the dispersed phase material, depend on particle size. The kinetics of these processes are "competitive," dictating that larger particles grow at the expense of smaller ones, overall leading to an increase of the average particle size. The classical treatment of phase coarsening was done by Todes, Lifshitz, and Slyozov, (TLS) in the limit of zero volume fraction, V(sub v), of the dispersed phase. Since the publication of TLS theory there have been numerous investigations, many of which sought to describe the kinetic scaling behavior over a 0 range of volume fractions. Some studies in the literature report that the relative increase in coarsening rate at low (but not zero) volume fractions compared to that predicted by TLS is proportional to v(sub v)(exp 1/2), whereas others suggcest V(sub v)(exp 1/3). This issue has been resolved recently by simulation studies at low volume fractions in three dimensions by members of the Rensselaer/MSFC team. Our studies of ripening behavior using large-scale numerical simulations suggest that although there are different circumstances which can lead to either scaling law, the most important length scale at low volume fractions is the diffusional analog of the Debye screening length. The numerical simulations we employed exploit the use of a recently developed "snapshot" technique, and identifies the nature of the coarsening dynamics at various volume fractions. Preliminary results of numerical and experimental investigations, focused on the growth of finite particle clusters, provide important insight into the nature of the transition between the two scaling regimes. The companion microgravity experiment centers on the growth within finite particle clusters, and follows the temporal dynamics driving microstructural evolution, using holography.

Frazier, Donald O.↗

The effect of microstructure on microbiologically influenced corrosion

Results of several investigations involving stainless steels, aluminum alloys, and low-alloy steels are reviewed, and the effect of welding on microbiologically influenced corrosion (MIC) susceptibility in these materials is discussed. Emphasis is placed on research performed at California Polytechnic State University on the relationship between MIC and metallurgical microstructure. Topics addressed include initial stages of film development in materials with different microstructure and surface conditions, effects of inclusion on the MIC response of materials, aluminum 2219, effects of welding, and constitutional liquation.

Walsh, Dan↗

Coupled cluster and dislocation dynamics modeling of microstructure evolution in irradiated materials

We develop here a coupled cluster and dislocation dynamics framework to study the microstructure evolution of irradiated materials. The framework not only accounts for the three dimensional diffusion of radiation-generated clusters, but also their interaction with dislocation networks and the resultant climb motion of discrete dislocations within finite crystals. The framework is solved with a superposition solution scheme, and is applied to investigate the evolution of the irradiation-induced dislocation loops in zirconium (Zr), considering the effects of various bias factors including the diffusion anisotropy difference (DAD) of interstitials and interstitial clusters, the dislocation bias of defects to discrete dislocation segments, and the production bias of defects from the radiation cascade. We find that the DAD is the most critical factor influencing the kinetics of the loop evolution in Zr, while the recombination/interaction of mobile defects can induce a strong spatial dependence of the loop evolution together with the DAD. Here, the method is also adopted to study the evolution of interstitial $\langle$a$\rangle$ and vacancy $\langle$c$\rangle$ dislocation loop ensembles consistent with the microstructure observed during irradiation-induced growth of Zr. Our findings not only reveal the spatial dependence of the size and ellipticity of the dislocation loops, but also suggest a limit on the anisotropy factor of interstitials to reproduce the co-growth of $\langle$a$\rangle$ and $\langle$c$\rangle$ loops in zirconium, in good agreement with experimental observations and other simulation results.

Bias factors↗

Evolution of Local Microstructures (ELMS): Spatial Instabilities of Coarsening

This work examines the diffusional growth of discrete phase particles dispersed within a matrix. Engineering materials are microstructurally heterogeneous, and the details of the microstructure determine how well that material performs in a given application. Critical to the development of designing multiphase microstructures with long-term stability is the process of Ostwald ripening. Ripening, or phase coarsening, is a diffusion-limited process which arises in polydisperse multiphase materials. Growth and dissolution occur because fluxes of solute, driven by chemical potential gradients at the interfaces of the dispersed phase material, depend on particle size. The kinetics of these processes are "competitive," dictating that larger particles grow at the expense of smaller ones, overall leading to an increase of the average particle size. The classical treatment of phase coarsening was done by Todes, Lifshitz, and Slyozov, (TLS) in the limit of zero volume fraction, V(sub v), of the dispersed phase. Since the publication of TLS theory there have been numerous investigations, many of which sought to describe the kinetic scaling behavior over a range of volume fractions. Some studies in the literature report that the relative increase in coarsening rate at low (but not zero) volume fractions compared to that / 2 1/ 3 predicted by TLS is proportional to V(sub v)(exp 1/2), whereas others suggest V(sub v)(exp 1/3). This issue has been resolved recently by simulation studies at low volume fractions in three dimensions by members of the Rensselaer/MSFC team.

Glicksman, Martin E.↗

Evolution of Local Microstructures: Spatial Instabilities of Coarsening Clusters

This work examines the diffusional growth of discrete phase particles dispersed within a matrix. Engineering materials are often microstructurally heterogeneous, and the details of the microstructure determine how well that material performs in a given application. Critical to the development of designing multiphase microstructures with long-term stability is the process of Ostwald ripening. Ripening, or phase coarsening, is diffusion-limited and arises in polydisperse multiphase materials. Growth and dissolution occur because fluxes of solute, driven by chemical potential gradients at the interfaces of the dispersed phase material, depend on particle size. Competitive kinetics of these processes dictates that larger particles grow at the expense of smaller ones, overall leading to an increase of the average particle size. The classical treatment of phase coarsening was done by Todes, Lifshitz, and Slyozov, (TLS) in the limit of zero volume fraction, V(sub V)=0 of the dispersed phase. Since the publication of TLS theory, there have been numerous investigations, many of which sought to describe the kinetic scaling behavior over a range of volume fractions. Some studies in the literature report that the relative increase in coarsening rate at low (but not zero) volume fractions compared to that predicted by TLS is proportional to V(exp 1/2)(sub v) whereas others suggest V(exp 1/3)(sub v).This issue has been addressed recently by simulation studies at low volume fractions in three dimensions by members of the Rensselaer/MSFC team.

Glicksman, Martin E.↗

Degradation of a Cr-Mo steel by carbide precipitation over long-term service

Microstructure of the 40-year service-exposed 1Cr-0.5Mo steel extracted from pressure vessels through the boat sampling technique was characterized using x-ray diffraction, field-emission scanning electron microscopy, energy dispersive spectrometry, electron backscatter diffraction, focused ion beam, and transmission electron microscopy. The microstructure degradation during long-term service was identified. Statistical crystal plastic ity models were developed to correlate the microstructure and mechanical properties quantitatively. The steel is found significantly strengthened but slightly embrittled. Nanoscale Mo 2 C carbides have nucleated within the ferrite matrix over the long-term service, resulting in significant strengthening of the matrix. The coarser grain boundary Cr 23 C 6 carbides, on the other hand, act as the damage accumulation sites and lead to the degradation.

36 MATERIALS SCIENCE↗

Quantifying the effect of hydride microstructure on zirconium alloys embrittlement using image analysis

Since hydride microstructure can significantly influence Zr alloy nuclear fuel cladding’s ductility, a new metric has been developed to quantify hydride microstructure in 2D micrographs and relate it to crack propagation. As cladding failure usually results from a hoop stress, this new metric, called the Radial Hydride Continuous Path (RHCP), is based on quantifying the continuity of brittle hydride particles along the radial direction of the cladding tube. Compared to previous metrics, this approach more closely relates to the propensity of a crack to propagate radially through the cladding tube thickness. The RHCP takes into account hydride length, orientation, and connectivity to choose the optimal path for crack propagation through the cladding thickness. The RHCP can therefore be more closely linked to hydride embrittlement of the Zr alloy material, thus creating a relationship between material structure, properties, and performance. The new definition, along with previously proposed metrics such as the Radial Hydride Fraction (RHF), the Hydride Continuity Coefficient (HCC), and the Radial Hydride Continuity Factor (RHCF), have been implemented and automated in MATLAB. These codes are made available with this publication as supplementary materials. These metrics were verified by comparing their predictions of hydride morphology against expected values in simple cases, and the implementation of the new metric was validated by comparing its predictions with manual measurements of hydride microstructure performed on ImageJ. The RHCP was also validated against experimental measurements of fracture behavior and it was shown to correlate with cladding failure better than previous metrics. The information provided by these metrics will help accurately assess cladding integrity during operation, transportation, and storage.

36 MATERIALS SCIENCE↗