Search NASA⌕ Search

SEARCH · Search NASA

Results for “stabilized electrode interface”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 253 records · Page 14

High‐Energy LiNiO 2 Li Metal Batteries Enabled by Hybrid Electrolyte Consisting of Ionic Liquid and Weakly Solvating Fluorinated Ether

Abstract In pursuit of the highest possible energy density, researchers shift their focus to the ultimate anode material, lithium metal (Li 0 ), and high‐capacity cathode materials with high nickel content (Ni > 80%). The combination of these aggressive electrodes presents unprecedented challenges to the electrolyte. Here, we report a hybrid electrolyte consisting of a highly fluorinated ionic liquid and a weakly solvating fluorinated ether, whose hybridization structure enables the reversible operation of a battery chemistry based on Li 0 and LiNiO 2 (Ni = 100%), delivering nearly theoretical capacity of the latter (up to 249 mAh g −1 ) for >300 cycles with retention of 78.6% and in absence of unwanted morphological changes in both electrodes. Extensive characterization assisted by molecular dynamic simulation and density functional theory calculations reveals the function of the fluorinated ether to be far more profound than simple dilution and viscosity reduction. Instead, it induces drastic changes in Li + ‐solvation environment, the consequence of which engenders simultaneous stabilization of electrode/electrolyte and interfacing via formation of respective interfacial chemistries. This study further unlocks fundamental knowledge underneath the prevailing “diluent strategy” that is extensively applied by the electrolyte researchers and opens more design space for the next‐generation electrolytes and interphases for these coveted battery chemistries.

25 ENERGY STORAGE↗

Stabilizing and understanding the interface between nickel-rich cathode and PEO-based electrolyte by lithium niobium oxide coating for high-performance all-solid-state batteries

The pursuit of high energy density and safe lithium ion batteries (LIBs) is the urgent goal for the development of next-generation electric vehicles (EVs). All-solid-state batteries (ASSBs) with the combination of poly(ethylene oxide) (PEO)-based solid polymer electrolyte (SPE) and Ni-rich lithium nickel manganese cobalt oxide LiNi0.8Mn0.1Co0.1O2 (NMC811) cathode are promising candidates for EVs due to their improved energy density and safety. However, the low electrochemical oxidation window of PEO-based SPE and the instability of NMC811 at the charge/discharge process seriously restrict the battery performance. Herein, a high voltage stable solid-state electrolyte layer lithium niobium oxide (LNO) is coated on the NMC811 electrode surface by atomic layer deposition for stabilizing NMC811-PEO solid polymer batteries. Electrochemical tests show that LNO coating can stabilize the NMC811 active materials and mitigate the decomposition of SPE upon the cycling process, rendering a good performance of NMC811-PEO solid polymer battery. Mechanism studies by SEM, STEM, XAS, and XPS disclose that the uncoated NMC811 suffers from chemomechanical degradations along with oxygen release triggering the decomposition of SPE, which results in unstable cathodic electrolyte interphase. With LNO coating, chemomechanical degradations and oxygen release are inhibited and the decomposition of SPE is mitigated. This paper renders a stable and high-performance high-energy-density SSB for high voltage application, which paves the way toward next-generation solid-state LIBs.

25 ENERGY STORAGE↗

PGM-Free Oxygen-Reduction Catalyst Development for Proton-Exchange Membrane Fuel Cells: Challenges, Solutions, and Promises

Proton-exchange membrane fuel cells (PEMFCs) are efficient and clean hydrogen energy technologies for transportation and stationary applications. Highly active and durable low-cost cathode catalysts for the oxygen-reduction reaction (ORR) under challenging acidic environments are desperately needed to address the cost and durability issues of PEMFCs. The most promising platinum group metal (PGM)-free catalysts for the ORR in acidic media are atomically dispersed and nitrogen-coordinated metal site catalysts denoted as M–N–C, M = Fe, Co, or Mn. Due to significant efforts in the past few decades, these catalysts have demonstrated much-improved ORR activity and promising initial fuel cell performance approaching traditional Pt/C catalysts. However, the insufficient long-term stability (up to 5000 h) under PEMFC operation represents a primary technical barrier to making current PGM-free catalysts less viable yet in PEMFCs. In this Account, we highlight recent advances in synthesizing efficient PGM-free catalysts for the ORR in PEMFCs, emphasizing effective strategies to improve mass and intrinsic activity and the possible degradation mechanisms. In particular, a chemical doping method based on the zeolitic imidazolate framework (ZIF)-8 represents the key to developing efficient M–N–C catalysts containing atomically dispersed and nitrogen-coordinated single metal active sites (i.e., MN 4 ). The newly acquired understanding of the formation mechanism of MN 4 active sites during the thermal activation and its correlation to catalytic properties guide the rational catalyst design rather than relying on current trial-and-error approaches. Considerable efforts have further been invested in increasing the active site density and enhancing intrinsic activity by regulating carbon-phase structures and the local coordination environment. Furthermore, these highly active catalysts usually suffer from significant activity loss during the ORR. Therefore, breaking the activity–stability trade-off is the key to simultaneously achieving activity and stability in one catalyst, which is discussed on the basis of our recent successes in regulating local carbon structures surrounding active single metal sites. Significant research efforts toward understanding the degradation mechanisms and improving the lifetime of PGM-free catalysts are still crucial for viable applications in the future. Novel electrode designing strategies are needed to translate the PGM-free catalysts’ ORR activity to solid-state electrolyte-based membrane electrode assemblies (MEAs) with robust three-phase (i.e., gas–liquid–solid) interfaces for efficient charge and mass transports for performance improvement. On the basis of our effort at the University at Buffalo supported by ElectroCat Consortium associated with U.S. DOE’s Hydrogen and Fuel Cell Technologies Office, we provide a perspective on PGM-free cathode catalysts concerning remaining bottlenecks and future opportunities, aiming to inspire the community in both mechanistic understanding and technological development.

08 HYDROGEN↗

Review on Interface and Interphase Issues in Sulfide Solid-State Electrolytes for All-Solid-State Li-Metal Batteries

All-solid-state batteries have emerged as promising alternatives to conventional Li-ion batteries owing to their higher energy density and safety, which stem from their use of inorganic solid-state electrolytes instead of flammable organic liquid electrolytes. Among various candidates, sulfide solid-state electrolytes are particularly promising for the development of high-energy all-solid-state Li metal batteries because of their high ionic conductivity and deformability. However, a significant challenge remains as their inherent instability in contact with electrodes forms unstable interfaces and interphases, leading to degradation of the battery performance. In this review article, we provide an overview of the key issues for the interfaces and interphases of sulfide solid-state electrolyte systems as well as recent progress in understanding such interface and interphase formation and potential solutions to stabilize them. In addition, we provide perspectives on future research directions in this field.

25 ENERGY STORAGE↗

Durability of Metallic Interconnects and Protective Coatings

To build up a useful voltage, a number of solid oxide fuel cells (SOFCs) are electrically connected into series in a stack via interconnects, which are placed between adjacent cells. In addition to functioning as a bi-polar electrical connector, the interconnect also acts as a separator plate that separates the fuel at the anode side of one cell from the air at the cathode side on an adjacent cell. During SOFC operation at the high temperatures, the interconnects are thus simultaneously exposed to the oxidizing air at one side and a reducing fuel that can be either hydrogen or hydrocarbon at the other. Besides, they are in contact with adjacent components, such as electrodes or electrical contacts, seals, etc. With steady reduction in SOFC operating temperatures into the low or intermediate range 600-850oC, oxidation resistant alloys are often used to construct interconnects. However, the metallic interconnects may degrade via interactions at their interfaces with surrounding environments or adjacent components, potentially affecting the stability and performance of interconnects and the SOFC stacks. Thus protection layers are applied to metallic interconnects that also intend to mitigate or prevent chromium migration into cells and the cell poisoning. This chapter provides a comprehensive review of materials for metallic interconnects, their degradation and coating protection.

solid oxide fuel cell, interconnect, oxidation, co↗

Activity and Stability of (Pr 1-x Nd x ) 2 NiO 4 as Cathodes for Solid Oxide Fuel Cells: Part V. In Situ Studies of Phase Evolution

This study is to complement an early report (the manuscript is attached for review purpose) on the role of interlayer on activity and performance stability in praseodymium nickelates. The aforementioned report showed a remarkable 48% increase in power density while switching from common GDC interlayer to a new interlayer chemistry (PGCO). Furthermore, a stable long-term performance was linked with suppressed reaction between the cathode and PGCO interlayer. In this article, we report in situ studies of the phase evolution. The high energy XRD studies at a synchrotron source showed fully suppressed phase transition in praseodymium nickelates with PGCO interlayer, while the electrodes on the GDC interlayer undergo substantial phase transformation. Furthermore, in operando and post-test XRD analyses shown fully suppressed structural changes in electrodes operated in full cells at 750°C and 0.80 V for 500 hours. SEM-EDS analysis showed that the formation of PrO x at the cathode-interlayer interface may play a role in a decrease of mechanical integrity of the interfaces, due to thermal expansion mismatch, leading to a local stress between the two phases. Furthermore, phase evolution at a narrow interface may propagate toward the electrode bulk, leading to structural changes Q1 and performance degradation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The dynamic behavior of thin-film ionic transition metal complex-based light-emitting electrochemical cells

Light-emitting electrochemical cells (LECs) have received increasing attention during recent years due to their simple architecture, based on solely air-stabile materials, and ease of manufacture in ambient atmosphere, using solution-based technologies. The LEC's active layer offers semiconducting, luminescent as well as ionic functionality resulting in device physical processes fundamentally different as compared with organic light-emitting diodes. During operation, electrical double layers (EDLs) form at the electrode interfaces as a consequence of ion accumulation and electrochemical doping sets in leading to the in situ development of a light-emitting p-i-n junction. In this paper, we comment on the use of impedance spectroscopy in combination with complex nonlinear squares fitting to derive key information about the latter events in thin-film ionic transition metal complex-based light-emitting electrochemical cells based on the model compound bis-2-phenylpyridine 6-phenyl-2,2´-bipyridine iridium(III) hexafluoridophosphate ([Ir(ppy)₂(pbpy)][PF₆]). At operating voltages below the bandgap potential of the ionic complex used, we obtain the dielectric constant of the active layer, the conductivity of mobile ions, the transference numbers of electrons and ions, and the thickness of the EDLs, whereas the transient thickness of the p-i-n junction is determined at voltages above the bandgap potential. Most importantly, we find that charge transport is dominated by the ions when carrier injection from the electrodes is prohibited, that ion movement is limited by the presence of transverse internal interfaces and that the width of the intrinsic region constitutes almost 60% of the total active layer thickness in steady state at a low operating voltage.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Bifacial all-perovskite tandem solar cells

The efficiency of all-perovskite tandem devices falls far below theoretical efficiency limits, mainly because a widening bandgap fails to increase open-circuit voltage. We report on a bifacial all-perovskite tandem structures with an equivalent efficiency of 29.3% under back-to-front irradiance ratio of 30. This increases energy yield and reduces the required bandgap of a wide-bandgap cell. Open-circuit voltage deficit is therefore minimized, although its performance under only front irradiance is not ideal. The bifacial device needs a sputtered rear transparent electrode, which could reduce photon path length and deteriorate stability of Pb-Sn perovskites. Embedding a light-scattering micrometer-sized particle layer into perovskite to trap light, effectively increases absorptance by 5 to 15% in the infrared region. Using a nonacidic hole transport layer markedly stabilizes the hole-extraction interface by avoiding proton-accelerated formation of iodine. These two strategies together increase efficiency of semitransparent Pb-Sn cells from 15.6 to 19.4%, enabling fabrication of efficient bifacial all-perovskite tandem devices.

14 SOLAR ENERGY↗

Thermal decomposition pathways of bulk electrolytes on vanadium oxide nanocrystals

The thermal stability of electrolytes at an elevated temperature induced by battery charge-discharge cycling is critical for the long cycling performance of a rechargeable battery. For many multivalent systems, such as rechargeable magnesium batteries, which offer great potential for high energy density and utilize earth-abundant resources, electrolyte instability and electrode surface passivation, arising from electrolyte decomposition, remain as major roadblocks. Understanding the electrolyte decomposition pathways at the electrode-electrolyte interface is essential to provide guidance in overcoming this challenge. In this work, in situ 13 C magic angle spinning nuclear magnetic resonance (MAS NMR) and first-principles calculations were used to investigate the thermal decomposition of the electrolyte in a system consisting of MgV 2 O 4 , a novel cathode for magnesium batteries, mixed with a bulk electrolyte consisting of magnesium bis(trifluoromethanesulfonyl)imide (Mg(TFSI) 2 ) in diglyme (G2). We show that significant electrolyte decomposition is observed in bulk 1.0 M Mg(TFSI) 2 in G2 mixed with nanometer sized MgV 2 O 4 powder at elevated temperatures. This observation is to mimic the possible thermal decomposition that might happen during battery cycling. We demonstrate that the MgV 2 O 4 surface is covered by a layer of decomposed G2 products. We conclude that the dominant reaction pathway for electrolyte decomposition is the thermal decomposition of the pure electrolytes at elevated temperatures, followed by adsorption of G2 decomposition products to the MgV 2 O 4 surface. The activation energy for the major decomposition pathway is obtained. In conclusion, this work highlights the importance of studying thermal decomposition of electrolytes for overall system stability and explores electrolyte stability at significantly elevated temperatures.

25 ENERGY STORAGE↗

Polyethylene Glycol Surface Modification and Polythiophene Side-Chain Chemistry: A Combined Strategy toward High-Capacity Lithium-Ion Battery Anodes

In the development of high-capacity lithium-ion batteries (LIBs), the combined optimization of active material interfaces and polymer binder chemistry plays a critical role in improving electrode performance and longevity. This work explores a dual design strategy incorporating polyethylene glycol (PEG) surface modification and carboxylated polythiophene side-chain tailoring to enhance the electrochemical behavior of magnetite (Fe 3 O 4 )-based anodes. PEG is employed to improve interfacial stability, while carboxylated polythiophene binders with varying alkyl side-chain lengths─poly[3-(potassium-4-butanoate)thiophene-2,5-diyl] (P3KBT), poly[3-(potassium-5-pentanoate)thiophene-2,5-diyl] (P3KPT), and poly[3-(potassium-6-hexanoate)thiophene-2,5-diyl] (P3KHT)─are used to modulate molecular interactions and ion transport. Among these three analogs, the PEG–Fe 3 O 4 –P3KHT electrode exhibits superior ion-transfer kinetics, the highest capacity retention, and the lowest charge-transfer resistance after extended cycling. Compared to their non-PEG analogs, PEG-coated electrodes demonstrate enhanced structural integrity and electrochemical behavior, emphasizing the synergistic effects of surface modification and side-chain chemistry. These findings highlight the importance of interfacial interactions and molecular design in achieving robust and high-performance composite anodes for next-generation LIBs.

Fe3O4↗

Enable High-Energy LiNi0.5Co0.2Mn0.3O2 by Ultra-Thin Coating through Wet Impregnation

A high cut-off voltage is required for nickel-rich layered oxide LiNixCoyMnzO2 (NCM) to meet the high energy density requirement of lithium-ion batteries in electric vehicles. However, such a high voltage application leads to an unstable interface between NCM and liquid electrolytes. To stabilize the interface, the facile wet impregnation method has been developed to apply an ultra-thin Al2O3 coating layer on the NCM particles. This coating layer was found to have a strong interaction with the NCM and resulted in Al-doped NCM at the surface structure of NCM. The change of surface structure can not only reduce the surface resistance of lithium diffusion of LiNi0.5Co0.2Mn0.3O2 (NCM523), but also stabilize the solid electrolyte interface between NCM523 and the electrolyte with the cut-off voltage of 4.5 V vs. Li/Li+. Compared to other coating methods, wet impregnation coating can provide an ultra-thin and uniform coating with surface doping on NCM particles. Furthermore, this scalable coating method can be applied to various electrode materials without adding much additional cost.

25 ENERGY STORAGE↗

Charge-mediated cation deposition on metallic surfaces

This work reveals the general mechanisms of Li + cation partial reduction and further deposition under specific electrolyte conditions, and in the proximity of an electrified metal surface. The factors affecting the ion complexation and transport and resultant adsorbed structures are identified for various external electric fields and for several applied voltages. Using ab initio methods, we investigate the relation between solvent–salt structures and dynamics, cation reductive stability, and the existing electric field between electrodes, or under the applied potential if the system is designed as an electrochemical cell. In absence of an applied field, it is found that not only cation but also non-solvated salt deposition on a metallic surface is an endothermic process. However, localized surface polarization orbitals created by an external electric field affect both the thermodynamics and kinetics of the adsorption, leading to a drastic change on the energetic profile; ab initio molecular dynamics simulations describe in detail the underlying mechanisms. Externally applied bias to an electrochemical cell also changes the deposition dynamics: by examining various solvent/salt combinations, we unravel the cation deposition mechanisms at both low and moderately high voltages, determining the relative time scale of each separate process. In this work, different polyhedra formed by the metal cation and its surrounding oxygen atoms appear to be the key indicator driving deposition dynamics at different voltages. Our findings disclose the importance of selecting appropriate voltage windows for stable and uniform growth of metal anode layers, showing the mechanisms leading to impurity formation and non-uniform cation deposition, as well as the role of charged interfacial phenomena in designing stable electrode–electrolyte interfaces.

25 ENERGY STORAGE↗

Water reduction by a p-GaInP2 photoelectrode stabilized by an amorphous TiO2 coating and a molecular cobalt catalyst

Producing hydrogen through solar water splitting requires the coverage of large land areas. Abundant metal-based molecular catalysts offer scalability, but only if they match noble metal activities. We report on a highly active p-GaInP2 photocathode protected through a 35-nm TiO2 layer functionalized by a cobaloxime molecular catalyst (GaInP2-TiO2-cobaloxime). This photoelectrode mediates H2 production with a current density of ~9"0mA"0cm-2 at a potential of 0"0V versus RHE under 1-sun illumination at pH"013. The calculated turnover number for the catalyst during a 20-h period is 139,000, with an average turnover frequency of 1.9"0s-1. Bare GaInP2 shows a rapid current decay, whereas the GaInP2-TiO2-cobaloxime electrode shows </=5% loss over 20"0min, comparable to a GaInP2-TiO2-Pt catalyst particle-modified interface. The activity and corrosion resistance of the GaInP2-TiO2-cobaloxime photocathode in basic solution is made possible by an atomic layer-deposited TiO2 and an attached cobaloxime catalyst.

14 SOLAR ENERGY↗

Improving the performance for direct electrolysis of CO 2 in solid oxide electrolysis cells with a Sr 1.9 Fe 1.5 Mo 0.5 O 6– δ electrode via infiltration of Pr 6 O 11 nanoparticles

Direct CO 2 electrolysis using solid oxide electrolysis cells (CO 2 -SOECs) holds promise to efficiently convert carbon dioxide to carbon monoxide and oxygen. Cathodes with desirable catalytic activity and chemical stability play a critical role in the development of direct CO 2 -SOECs. Although Sr 2 Fe 1.5 Mo 0.5 O 6–δ (SFM) has exhibited promise for direct CO 2 -SOECs due to its redox stability, it suffers from insufficient activity for the CO 2 reduction reaction (CO 2 RR). Here we report interface engineering of nanosized Pr 6 O 11 on the SFM cathode obtained through infiltration to promote the CO 2 RR performance for direct CO 2 -SOECs. The effect of Pr 6 O 11 loading on the performance of the CO 2 RR is systematically investigated. At 800 °C, the current density of the Pr 6 O 11 infiltrated SFM cathode with an optimum Pr 6 O 11 loading of 14.8 wt% reaches 1.61 A cm –2 at 1.5 V, more than double that of the SFM cathode (0.76 A cm –2 ) under the same operating conditions. X-ray photoelectron spectroscopy (XPS) characterization and in situ diffuse reflectance infrared Fourier transform spectroscopy (DRIFTS) analysis indicate that the adsorption ability of CO 2 on the SFM cathode has been significantly improved by the formation of Pr 6 O 11 . Temperature-programmed desorption (TPD) of CO 2 measurements further manifest that a 14.8 wt% Pr 6 O 11 -SFM cathode has better CO desorption capacity. In addition, polarization resistance of the SFM cathode has significantly decreased with the addition of Pr 6 O 11 . Three-electrode measurement was used to analyze the improved electrode kinetics. Finally, these results demonstrate that the formation of Pr 6 O 11 in the SFM cathode through infiltration is a promising approach for increasing CO 2 RR activity for CO 2 -SOECs.

03 NATURAL GAS↗

Multidimensional visualization of the dynamic evolution of Li metal via in situ/operando methods

The growing demands for high-energy density electrical energy storage devices stimulate the coupling of conversion-type cathodes and lithium (Li) metal anodes. While promising, the use of these “Li-free” cathodes brings new challenges to the Li anode interface, as Li needs to be dissolved first during cell operation. In this study, we have achieved a direct visualization and comprehensive analysis of the dynamic evolution of the Li interface. The critical metrics of the interfacial resistance, Li growth, and solid electrolyte interface (SEI) distribution during the initial dissolution/deposition processes were systematically investigated by employing multidimensional analysis methods. They include three-electrode impedance tests, in situ atomic force microscopy, scanning electrochemical microscopy, and cryogenic scanning transmission electron microscopy. The high-resolution imaging and real-time observations show that a loose, diffuse, and unevenly distributed SEI is formed during the initial dissolution process. This leads to the dramatically fast growth of Li during the subsequent deposition, deviating from Fick’s law, which exacerbates the interfacial impedance. The compactness of the interfacial structure and enrichment of electrolyte species at the surface during the initial deposition play critical roles in the long-term stability of Li anodes, as revealed by operando confocal Raman spectroscopic mapping. In conclusion, our observations relate to ion transfer, morphological and structural evolution, and Li (de)solvation at Li interfaces, revealing the underlying pathways influenced by the initial dissolution process, which promotes a reconsideration of anode investigations and effective protection strategies.

25 ENERGY STORAGE↗