Testing of Materials and Coatings at up to 1150°C and 300 bar for use in Oxy-Combustion Turbine
Various materials that may be used in a supercritical carbon dioxide (sCO2) oxy-fuel turbine in the 150-300 MWe size range are being evaluated in various environments of interest. The inlet of the turbine must be capable of 1,150 °C at 300 bar and the exhaust temperature is expected to be within the 725-775 °C range. The design requirements are pushing the known limits of high temperature materials. Little is known about the oxidation of the metallic alloys considered for turbine nozzles and blades or about the resilience of thermal management solutions, such as thermal barrier coatings (TBC), required to accommodate these high temperatures. The combinations of high temperature resistant materials and coatings must be tested in sCO2 to evaluate their reliability in an oxy-fuel turbine environment. A total of 13 alloys were chosen to be tested. They included bare samples, with nano deposited MCrAlY bond coat only, or with the addition of a TBC. A unique test facility was developed to expose those materials in sCO2 at up to 300 bar and 1150 °C for up to 5,000 hours. This was accomplished by placing an induction heater inside an autoclave to achieve those high temperature locally while the pressurized vessel is cooled externally. The specimens are weighed before and after exposure to determine the oxidation rate. The integrity, morphology, and composition of some of the coatings and thermally grown oxide will be investigated by scanning electron microscopy (SEM). This paper presents the up-to-date results of the testing coated and uncoated superalloys in sCO2 at up to 1150 °C and up to 300 bar performed at Southwest Research Institute.