Microstructural and textural evolution of AZ61 magnesium alloy sheet during bidirectional cyclic bending

In this work, the microstructural and textural evolution in the sheets of AZ61 magnesium alloy was studied by means of bidirectional cyclic bending for 8 passes at 623 K. The bended samples were examined by optical microscopy and electron backscatter diffraction analysis. The results showed that a gradient structure with fine grains about 3 μm in the regions near two surfaces and, in contrast, coarse grains in the middle of the sheet were formed. The evident grain refinement was attributed to twin-assisted dynamic recrystallization and continuous dynamic recrystallization induced by kink bands. The texture intensity was clearly reduced, resulting in a negative gradient distribution, with the texture intensity decreases from the center of the sheet to two surfaces. The weakened texture greatly facilitated the reduction of the yield strength. A higher fracture elongation and a slightly improved ultimate tensile strength were achieved concurrently. - Highlights: • The AZ61 Mg alloy is deformed at 623 K by bidirectional cyclic bending. • A symmetric gradient distribution of fine grains along the thickness is formed. • The basal texture in the regions near two surfaces is weakened significantly.

36 MATERIALS SCIENCE↗

Fabrication and Mechanical Properties of In Situ Synthesized Ti{sub 2}AlN/TiAl Composite

TiAl matrix composites reinforced with Ti{sub 2}AlN were fabricated by in situ reactive method of powder metallurgy. Microstructures, bending properties at room temperature and compressive properties at elevated temperatures were investigated in contrast with those of TiAl alloy. The results reveal that the microstructure of TiAl matrix is significantly refined due to the synthesis of Ti{sub 2}AlN. 15 vol.%Ti{sub 2}AlN/TiAl exhibits excellent bending properties at room temperature, with bending strength of 753 MPa and fracture strain of 0.74%, which are 24.3 and 19.7% higher than those of TiAl alloy. The compressive strength of Ti{sub 2}AlN/TiAl is markedly improved in comparison to that of TiAl alloy at elevated temperatures. Noticeably, the compressive strength of 15 and 35 vol.%Ti{sub 2}AlN/TiAl increases by 67.4 and 58.7% at 1000 °C, respectively. The remarkable enhancement of mechanical performance is mainly due to the noteworthy refinement of TiAl matrix and the efficient obstruction of Ti{sub 2}AlN particles to crack propagation, as well as the effective load-carrying role of Ti{sub 2}AlN with high elastic modulus.

36 MATERIALS SCIENCE↗

Conductivity enhancement in mechanosynthesized Bi{sub 2}O{sub 3}

Nanostructured Bi{sub 2}O{sub 3} was prepared through mechanical alloying method. Detailed microstructural information was obtained after Rietveld refinement of the prepared samples. The Transmission Electron Microscope images confirmed the crystallinity of the sample. The average crystallite size decreases whereas microstrain increases due to milling. The ionic conductivity of the milled sample was found to have increased few orders than the unmilled sample. The change in structural and electrical properties due to milling were discussed and correlated.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and magnetic properties of Sm{sub 2−x}Mn{sub x}O{sub 3} nanoparticles

Graphical abstract: - Highlights: • C-type Sm{sub 2−x}Mn{sub x}O{sub 3} (0.0 ≤ x ≤0.20) is prepared by sol–gel method. • A maximum solubility of x = 0.15 is confirmed by X-ray diffraction, Raman and infrared techniques. • Samples with x > 0.05 exhibit weak ferromagnetic properties; for x ≤ 0.05 antiferromagnetic behaviors is obtained. • Correlation between magnetic behaviors and structural and microstructural parameters is discussed. - Abstract: Mixed oxide Sm{sub 2−x}Mn{sub x}O{sub 3} (SMO), x = 0.0, 0.05, 0.10, 0.15 and 0.20 were synthesized by a sol–gel process. A single phase solid solution is formed up to x = 0.15 which confirmed by using X-ray diffraction, Raman spectroscopy and infrared techniques. Crystal structure and microstructure analyses were performed by Rietveld refinement. Preferential cationic distribution, over the two crystallographic sites 8b and 24d of space group Ia3{sup ¯}, is found for doped samples but with different extent. The r.m.s. microstrain 〈ε{sub L}{sup 2}〉{sup 1/2} depends on composition x in a systematic way emphasizing the preferential distribution. Magnetization measurements show that samples with x ≤ 0.05 have antiferromagnetic behavior, while samples with x > 0.05 exhibit a weak ferromagnetic behavior with magnetic phase transformation at 15 and 16 K for x = 0.1 and x = 0.15, respectively.

36 MATERIALS SCIENCE↗

Effect of particle size distribution on the structure, hyperfine, and magnetic properties of Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} nanopowders

Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} nano powders were synthesized by an auto combustion method and then heat treated at different temperatures in air for a fixed time. As a consequence, a distribution in particle size and strain was incorporated within the specimens, as estimated from the Rietveld refinement analysis of the powder x-ray diffraction data. The changes in the microstructure and crystal structure parameters were carefully extracted through the refinement analysis. Thermal annealing causes increment in the dispersion and mean of the size distribution. Reallocation of cations in the lattice sites occur as a consequence of the heat treatment which was manifested in their altered unit cell length (a), r.m.s. strain (〈ε{sup 2}〉{sup 1/2}), oxygen positional parameter (u), metal-oxygen bond lengths (R{sub OA} and R{sub OB}), and the band positions (ν{sub 1}and ν{sub 2}) in the vibrational spectroscopy. We also investigate the hyperfine and magnetic properties of the samples using different instrumental techniques (with different operating time scales) like Mössbauer spectroscopy, electron paramagnetic resonance spectroscopy, and superconducting quantum interference device magnetometry. Results show that the effect of particle size distribution was manifested in their hyperfine field distribution profile, paramagnetic resonance spectra, and magnetic anisotropy energy distribution profile. Co-existence of superparamagnetic and ferrimagnetic phase was recorded at room temperature in the samples when annealed at lower temperature. However, with increase in annealing temperature, the nature of the size distribution changes and ferrimagnetic ordering predominates for the larger size nanoparticles. Thus, the effect of particle size distribution on the structural, hyperfine, and magnetic properties of various Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} nanoparticles was investigated herein which hitherto has not been discussed in the literature.

36 MATERIALS SCIENCE↗

Control of Carbide Precipitation During Electroslag Remelting-Continuous Rapid Solidification of GCr15 Steel

The effect of the electroslag remelting-continuous rapid solidification (ESR-CRS) process on element segregation and carbide precipitation in GCr15 bearing steel was investigated. The results showed that a microstructure with fewer primary carbides and less segregation can be achieved via the ESR-CRS process. In the specimen subjected to ESR, the morphology of primary carbide changed from angular to lumplike. After the ESR-CRS process, the dimension of primary carbide and the mass fraction of Cr in primary carbide decreased. With the increase of cooling intensity during the ESR-CRS process, the microstructure of ESR ingot became more refined and uniform and the size of large primary carbides in ESR ingot gradually decreased. Suppressing the formation of grain boundary cementite and primary carbide during ESR of GCr15 steel is beneficial to inhibiting the presence of large secondary carbide formation after annealing. With the increase of cooling intensity, the mass fraction of carbides in ESR ingot decreased and the mass fraction of Cr in carbides increased, whereas the types of carbides did not change; all the M{sub 3}C, M{sub 3}C{sub 2}, and M{sub 7}C{sub 3} exist before and after ESR-CRS. Al{sub 2}O{sub 3} inclusions promoted the formation of Ti(N,C) by serving as preferred heterogeneous nucleation sites, whereas the formation of Ti(N,C) was suppressed through the refinement of Al{sub 2}O{sub 3} inclusions by increasing the cooling intensity.

36 MATERIALS SCIENCE↗

Robustness of magnetocrystalline anisotropy and coercivity in Fe–Co–B

As a potential candidate for critical chemical element free permanent magnet, (Fe 0.7 Co 0.3 ) 2 B, shows promising intrinsic magnetic properties, including large magnetization, high Curie temperature and moderate magnetocrystalline anisotropy (MCA). Still, the coercivity that has been achieved is relatively low. To understand and improve coercivity, here we study the robustness of MCA related to the fluctuation of chemical composition and the structural distortion and its effect on coercivity in (Fe 0.7 Co 0.3 ) 2 B from first principles DFT (density functional theory) calculation and micromagnetic simulation. A fluctuation of cobalt content of 10%, or 1% isotropic lattice strain, or 2% tetragonal distortion reduces MCA energy up to 30%. By considering randomly distributed local MCA energy reduction up to 30%, the calculated coercivity of anisotropic bulk magnets reduced from 3.6 kOe to 2.2 kOe. Rational microstructure design, such as grain size refinement and development of strong crystal texture of MCA easy-axis (i.e., degree of alignment for (Fe 0.7 Co 0.3 ) 2 B grains), can enhance coercivity and mitigate the effect of local MCA reduction. In addition to acceptable intrinsic magnetic properties, the promising hard magnetic phase needs good MCA robustness to facilitate the development of practical magnets.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Cyclic deformation and lattice strain distribution of high Nb containing TiAl alloy

Low cycle fatigue of lamellar TiAl with 8.5 at.-%Nb was studied with a total strain amplitude of 0.28% at three temperatures: room temperature, 750°C and 900°C. At room temperature, the material exhibited cyclic hardening and the fracture mode was mainly interlamellar. At 750°C and 900°C, the material showed cyclic softening and the fracture mode was translamellar. The lattice strain in γ phase was almost tensile and larger tensile lattice strain in γ phase seems detrimental. Besides, the opposite direction of {201} γ and {100} α2 lead to crack propagation along α 2 /γ interfaces. B2/β o phase always suffered compressive lattice strain in the tests. Finally, the destruction of lamellar microstructure was the reason for colony refinement at 750°C and 900°C.

phase transformation↗

Advanced Synthesis of Na 4 Si 24

The recently discovered orthorhombic allotrope of silicon, Si 24 , is an exciting prospective material for the future of solar energy due to a quasi-direct bandgap near 1.3 eV, coupled with the abundance and environmental stability of silicon. Synthesized via precursor Na 4 Si 24 at high temperature and pressure (~850 °C, 9 GPa), typical synthesis results have yielded polycrystalline samples with crystallites on the order of 20 μm. Several approaches to increase the crystal size have yielded success, including in-situ thermal spikes and refined selection of the starting materials. Microstructural analysis suggests that coherency exists between diamond silicon (d-Si) and Na 4 Si 24 . This hypothesis has led to the successful attempts at single crystal synthesis by selecting large crystals of d-Si along with metallic Na as the precursors rather than powdered and mixed precursor material. The new synthesis approach has yielded single crystals of Na 4 Si 24 greater than 100 μm. These results represent a breakthrough in synthesis that enables further characterization and utility. The promise of Si 24 for the future of solar energy generation and efficient electronics is strengthened through these advances in synthesis.

catalysis (heterogeneous)↗

Residual Stress Distribution and Microstructure of a Multiple Laser-Peened Near-Alpha Titanium Alloy

Laser peening without coating (LPwC) was performed on a Ti-2.5 Cu alloy with multiple passes (1, 3 and 5), using a Nd:YAG laser (1064 nm) at a constant overlap rate of 70% and power density of 6.7 GW cm{sup −2}. Hardness and residual stress profiles indicated thermal softening near the surface (< 100 μm) and bulk softening due to adiabatic heating. Maximum hardness (235 HV at 500 μm) and maximum residual stress (− 890 MPa at 100 μm) were observed for LPwC with 1 pass. Surface roughness and surface 3-D topography imaging showed that the surface roughness increased with the increase in the number of passes. XRD results indicated no significant β phases. However, peak shifts, broadening and asymmetry were observed and interpreted based on dislocation activity. Microstructures indicated no melting or resolidification or refinement of grains at the surface. Twin density was found to increase with the increase in the number of passes.

36 MATERIALS SCIENCE↗

Effect of Accumulative Roll Bonding on Plastic Flow Properties of Commercially Pure Zirconium

Accumulative roll bonding (ARB) has been considered as one of the promising techniques for fabrication of ultra-fine grained (UFG) metallic materials. The ARB process consists of several cycles of cutting, stacking, and rolling of metal sheets, so very high strains can be induced in the material resulting in significant grain refinement and in the formation of UFG microstructures. The ARB technique has been applied to a wide range of metallic materials such as Al and Al alloys, Mg, Fe and steels, Zr, Cu, as well as composite materials. UFG metallic materials processed via ARB show increased strength. Despite a significant body of experimental research into the deformation behaviour of the ARB-processed materials, the fundamentals of their plastic deformation are not fully understood yet. This work focuses on the effect of grain refinement via ARB-processing on the mechanical behavior and on the strain-rate sensitivity of commercially pure Zr (99.8% purity). The mechanical properties of the as-received coarse-grained (CG) and UFG (as-ARB processed) samples were studied at room temperature at two different strain rates. Mechanical strain rate jump tests were performed during tensile deformation to estimate the instantaneous strain-rate sensitivity. The evolution of surface relief during plastic deformation of pure Zr in both CG and UFG conditions was studied. The features of plastic deformation of pure Zr in both CG and UFG conditions are discussed.

36 MATERIALS SCIENCE↗

Microstructural Analysis of Severe Plastic Deformed Twin Roll Cast AZ31 for the Optimization of Superplastic Properties

In recent years magnesium alloys have attracted significant attention as potential candidates to replace many of the heavier metals used in some automotive applications. However, the limited formability of magnesium and its alloys at room temperature has driven interest in the superplastic forming magnesium as an alternative shaping method. Severe plastic deformation techniques have become a well studied method of refining the grain size and modifying the microstructural characteristics of many magnesium alloys to achieve greater superplastic properties. In this study twin roll cast (TRC) AZ31 magnesium alloy was subjected to equal channel angular pressing (ECAP) and friction stir welding (FSW). The influence of these severe plastic deformation processes on the grain size, texture and grain boundary character distribution was investigated to identify the optimum severe plastic deformation process for the superplastic forming of AZ31.

Young, John P.↗

Direct numerical simulation of mechanical response in synthetic additively manufactured microstructures

Additive manufacturing (AM) processes for metals can yield as-built microstructures that vary significantly from their cast or wrought counterparts. These microstructural variations can in turn, have profound effects on the properties of a component. Here, a modeling methodology is presented to investigate microstructurally-influenced mechanical response in additively manufactured structures via direct numeral simulation. Three-dimensional, synthetic voxelized microstructures are generated by kinetic Monte Carlo (kMC) additive manufacturing process simulations performed at four scan speeds to create a thin-wall cylindrical geometry notionally constructed using a concentric-pathed directed energy deposition AM process. The kMC simulations utilize a steady-state molten pool geometry that is held constant throughout the study. Resultant microstructures are mapped onto a highly-refined conformal finite-element mesh of a part geometry. A grain-scale anisotropic crystal elasticity model is then used to represent the constitutive response of each grain. Here, the response of the structure subjected to relatively simple load conditions is studied in order to provide understanding of both the influence of AM processing on microstructure as well as the microstructure's influence on the macroscale mechanical response.

42 ENGINEERING↗

Facile synthesis of B-type carbonated nanoapatite with tailored microstructure

Nanolime and a phosphate-based chelating agent were used to synthesize B-type carbonated apatite. Developed Rietveld refinement strategies allowed one to determine process yield, product crystallinity as well as structural (unit cell) and microstructural (size, strain) parameters. The effect of synthesis temperature (20–60 °C) as well as Ca/P ratio (1.5–2.5) and solid content (10–30 wt%) of the starting batch on these properties were investigated. FTIR, TEM and gas adsorption data provided supporting evidence. The process yield was 42–60 wt% and found to be governed by the Ca/P ratio. The purified products had high specific surface area (107–186 m{sup 2}/g) and crystallinity (76–97%). The unit cell parameters, correlated to the degree of structural carbonate, were sensitive to the Ca/P ratio. Instead, temperature governed the microstructural parameters. Less strained and larger crystals were obtained at higher temperatures. Long-term aging up to 6 months at 20 °C compensated for higher crystal growth kinetics at higher temperature. - Graphical abstract: Controlled synthesis of carbonated apatite at moderate temperatures using nanolime and sodiumhexametaphosphate as starting reagent. - Highlights: • Chemical synthesis of nano-sized apatite with tailored microstructure was performed. • Colloidal Ca(OH){sub 2} and a phosphorus-based chelating agents were used as reagents. • The method is simple and reproducible which facilitate industrial process scale-up. • Rietveld refinement strategies for product characterization were developed. • Rietveld analyses provided yield, microstructural and structure information.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Refinement performance and mechanism of an Al-50Si alloy

The microstructure and melt structure of primary silicon particles in an Al-50%Si (wt.%) alloy have been investigated by optical microscopy, scanning electron microscopy, electron probe micro-analysis and a high temperature X-ray diffractometer. The results show that the Al-50Si alloy can be effectively refined by a newly developed Si-20P master alloy, and the melting temperature is crucial to the refinement process. The minimal overheating degree {delta}T{sub min} ({delta}T{sub min} is the difference between the minimal overheating temperature T{sub min} and the liquidus temperature T{sub L}) for good refinement is about 260 deg. C. Primary silicon particles can be refined after adding 0.2 wt.% phosphorus amount at sufficient temperature, and their average size transforms from 2-4 mm to about 30 {mu}m. The X-ray diffraction data of the Al-50Si melt demonstrate that structural change occurs when the melting temperature varies from 1100 deg. C to 1300 deg. C. Additionally, the relationship between the refinement mechanism and the melt structure is discussed.

36 MATERIALS SCIENCE↗

Effect of Deformation Parameters on Microstructure and Properties During DIFT of X70HD Pipeline Steel

Grain refinement is a critical approach to improve the strength of materials without damaging the toughness. The grains of deformation-induced ferrite are considerably smaller than those of proeutectoid ferrite. Grain refinement is crucial to the application of deformation-induced ferrite. The composition of ferrite and bainite or martensite is important in controlling the performance of X70HD pipeline steel, and cooling significantly influences the control of their ratio and grain size. By analyzing the static and dynamic phase-transition points using Gleeble-3800 thermal simulator, thermal simulations were performed through two-stage deformations in the austenite zone. Ferrite transformation rules were studied with thermal simulation tests under different deformation and cooling parameters based on the actual production of cumulative deformation. The influence of deformation parameters on the microstructure transformation was analyzed. Numerous fine-grain deformation-induced ferrites were obtained by regulating various parameters, including deformation temperature, strain rate, cooling rate, final cooling temperature and other parameters. Results of metallographic observation and microtensile testing revealed that the selection of appropriate parameters can refine the grains and improve the performance of the X70HD pipeline steel.

36 MATERIALS SCIENCE↗

Enhanced strength and toughness in ultra-fine grained 99.9% copper obtained by cryo-hydrostatic extrusion

Highlights: • Cryo-HE can increase the yield strength of Cu by more than threefold. • In cryo-HE of Cu, the grain refinement is stronger by 30% than in room-HE. • Cryo-HE with post-annealing effectively creates a bimodal microstructure in Cu. • Short-term post-annealing applied to cryo-HE-treated Cu can double its ductility. • Grain refinement with recrystallization results in a slight increase of Cu toughness. - Abstract: Ultrafine grained 99.9% Cu with enhanced strength and toughness was produced by hydrostatic extrusion conducted at the temperature of liquid nitrogen. The cryo-extruded Cu has a tensile yield strength of 490 MPa, hardness of 145 HV0.2, and tensile fracture toughness of 39.5 MPa m{sup 1/2}, which means that their values increased by 380%, 185% and ~10%, respectively, compared to those of the starting material. The significant strengthening is due to the strong grain refinement to 320 nm and the high energy of defects stored during the processing at liquid nitrogen temperature. The short term post deformation annealing doubles the ductility of material even by above 10% of the elongation to fracture at a slight expense of the yield strength (485 MPa). The observed behavior of Cu can be explained in terms of its low stacking fault energy, the susceptibility to dynamic recrystallization within the working zone of the extrusion die, and the triaxial strain components with the very large strain gradients, combined with the significant adiabatic heating effect active during the hydrostatic extrusion. The better homogeneity of the grain refinement and the higher efficiency of the distribution of defects and of the energy storage accompanied by the decreased dislocation mobility during the cryo hydrostatic extrusion contributed to the higher strength.

36 MATERIALS SCIENCE↗

Mesh Computing Remote Automatic Workflow

The software suite uses a microservice architecture using Docker and `docker-compose`. The microservices are as follows: 1. User interface. This interface is written in JavaScript using the Svelte framework. It exposes form elements and a 3D visualizer to prompt the user through the definition of microstructure parameters, and setting parameters for mesh generation and refinement. 2. Mesh generator. This is a container running the Python package for DREAM3D to generate a voxelized mesh that represents a microstructure defined by the user in the interface. 3. Cubit runner. This is a secure shell protocol tool that makes the submitting the DREAM mesh to an HPC instance and starts to run Cubit shell commands to smooth the grain boundaries with its `sculpt` library, applies user-defined boundary node sets, and bundles and returns the simulation-ready meshes and input files as a zipped directory.

Harris, BrennanKay↗