Search NASA⌕ Search

SEARCH · Search NASA

Results for “Oxidation behavior”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Oxidation kinetics of aluminum diboride

The oxidation characteristics of aluminum diboride (AlB{sub 2}) and a physical mixture of its constituent elements (Al+2B) were studied in dry air and pure oxygen using thermal gravimetric analysis to obtain non-mechanistic kinetic parameters. Heating in air at a constant linear heating rate of 10 °C/min showed a marked difference between Al+2B and AlB{sub 2} in the onset of oxidation and final conversion fraction, with AlB{sub 2} beginning to oxidize at higher temperatures but reaching nearly complete conversion by 1500 °C. Kinetic parameters were obtained in both air and oxygen using a model-free isothermal method at temperatures between 500 and 1000 °C. Activation energies were found to decrease, in general, with increasing conversion for AlB{sub 2} and Al+2B in both air and oxygen. AlB{sub 2} exhibited O{sub 2}-pressure-independent oxidation behavior at low conversions, while the activation energies of Al+2B were higher in O{sub 2} than in air. Differences in the composition and morphology between oxidized Al+2B and AlB{sub 2} suggested that Al{sub 2}O{sub 3}–B{sub 2}O{sub 3} interactions slowed Al+2B oxidation by converting Al{sub 2}O{sub 3} on aluminum particles into a Al{sub 4}B{sub 2}O{sub 9} shell, while the same Al{sub 4}B{sub 2}O{sub 9} developed a needle-like morphology in AlB{sub 2} that reduced oxygen diffusion distances and increased conversion. The model-free kinetic analysis was critical for interpreting the complex, multistep oxidation behavior for which a single mechanism could not be assigned. At low temperatures, moisture increased the oxidation rate of Al+2B and AlB{sub 2}, but both appear to be resistant to oxidation in cool, dry environments. - Graphical abstract: Isothermal kinetic data for AlB{sub 2} in air, showing a constantly decreasing activation energy with increasing conversion. Model-free analysis allowed for the calculation of global kinetic parameters despite many simultaneous mechanisms occurring concurrently. (a) Time–temperature plots, (b) conversion as a function of time, (c) Arrhenius plots used to calculate activation energies, and (d) activation energy as a function of conversion. Display Omitted - Highlights: • First reported kinetic parameters for AlB{sub 2} and Al+2B oxidation in air and O{sub 2}. • Possible mechanism of enhanced boron combustion presented. • Moisture sensitivity shown to be problematic for AlB{sub 2}, less for Al+2B.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Evaluating the efficacy of aluminide coatings to improve oxidation resistance of high performance engine valve alloys

Increasing peak cylinder pressures and operating temperatures of turbo-charged internal combustion engines (ICEs) engines present new challenges for existing materials employed in engine exhaust valves. Oxidation induced degradation of current Ni based alloys for these components will be a life-limiting mechanism while strict cost margins in the automotive transportation industry further limit the choice of suitable candidate materials. Metallic diffusion aluminide coatings can provide a cost-effective way to improve the oxidation resistance of underlying materials. In this study, the high temperature oxidation behavior of diffusion nickel aluminide coatings on two Ni based alloys (commercially available alloy 31V and a developmental alloy) during cyclic oxidation behavior in air+10% H 2 O at 900 °C was investigated. A complete depletion of the beneficial Al-rich β-(NiFe)Al phase was observed in the coating on alloy 31V while a significant fraction of this phase was retained in the coating on the second alloy. A coupled thermodynamic-kinetic model showed that the disappearance of the Al-rich phase in the coating on 31V was mainly due to the combined effect of steeper chemical potential gradients of Al and Ti between the coating and the substrate and their faster diffusivities compared to the coated developmental alloy. Finally, a higher content of Fe was shown to support the retention of β-(NiFe)Al phase in the coating on the developmental alloy while the presence of Ti in the alloy was shown to be detrimental for long-term coating performance.

36 MATERIALS SCIENCE↗

The evaluation of aluminum and iron metal oxide settling behaviors for Hanford insoluble solids waste preprocessing

The Hanford site is currently one of the largest and most expensive cleanup sites for hazardous, radioactive waste. Over 20% of the waste found at the Hanford site is in the form of a high activity sludge. The insoluble solids in the sludge will need to be concentrated prior to vitrification in the high-level waste (HLW) melter. This will minimize the amount of liquid that will be evaporated during the melting process and expedite the melter processing rate. One proposed option for concentrating the insoluble solids is gravity settling in the storage tanks. Metal oxide compounds containing aluminum and iron make up the majority of the insoluble solids in the sludge, therefore understanding the behavior of these compounds in various tank waste matrices can facilitate sludge pretreatment options. A study of non-radioactive slurry solutions containing Al(OH) 3 (gibbsite), AlO(OH) (boehmite), and Fe 2 O 3 (iron (III) oxide) was conducted to determine the time dependent interface behavior and settling rates of these compounds. Variations in solids loading and sodium concentration were evaluated to represent waste processing conditions and the results of these settling studies were compared with prior tank waste settling tests. Information gathered from these studies can be used to inform future decisions on sludge treatment processes of the insoluble solids processed at the Hanford site.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Comparison of Irradiated and Unirradiated Graphite Oxidation Performance

This work examines the oxidation behavior of NBG-25 graphite using irradiated specimens and (not irradiated) companion specimens from the Advanced Graphite Creep (AGC) Experiment. Irradiated and companion specimens were quartered, split into four small samples, to enable four oxidation test runs for each (0.5 inch diameter by 0.25 inch tall) piggyback button obtained from the AGC Experiment inventory. These split samples were oxidized in air in a thermogravimetric analyzer (TGA) and benchmarked against observations with separately sourced same-grade specimens of three geometries oxidized either in the TGA or in a vertical furnace built and operated to satisfy the specifications of ASTM D7542. The study considers both irradiation damage and relief of damage by thermal annealing. A range of isothermal oxidation temperatures were tested for specimens exposed to a similar irradiation environment, nominally 6.5 dpa at 650°C. To assess the dose dependency of observed oxidation behavior, specimens with a range of irradiation exposures (up to 6.8 dpa) were tested at the single oxidation temperature of 650°C. In the conventional analysis (rate determined over the 5-10% mass loss range) any annealing effects appear to be negligible, while irradiation to ~6.5 dpa may double or triple the subsequent oxidation rate. However, examination of rate with extent of reaction (over incremental ranges from initial onset up to 5% mass loss) illustrates that (at least for ~6.5 dpa) irradiation initially inhibits oxidation. Slower rates of oxidation than companion split samples are clearly indicated across all oxidation temperatures tested up to ~0.5% mass loss. Over the range of 0.5-1% mass loss, regardless of normalization strategy, there is no statistically meaningful difference in oxidation rate. However, beyond 0.5% mass loss oxidation of the irradiated sample becomes progressively faster than the companion sample (up to the 10% mass loss level observed).

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural analysis of tristructural isotropic particles in high-temperature steam mixed gas atmospheres

High-temperature gas-cooled reactors (HTGRs) use tristructural isotropic (TRISO) particles embedded in a graphitic matrix material to form the integral fuel element. Potential off-normal reactor conditions for HTGRs include steam ingress with temperatures above 1,000 °C. Fuel element exposure to steam can cause the graphitic matrix material to evolve, forming an atmosphere composed of oxidants and oxidation products and potentially exposing the TRISO particles to these conditions. Investigating the oxidation response of TRISO particles exposed to a mixed gas atmosphere will provide insight into the stability under off-normal conditions. In this study, surrogate TRISO particles were exposed to high temperatures (T = 1,200 °C) in flowing steam (3% < pH 2 O < 21%) and CO (pCO < 1%) to determine the oxidation behavior of the SiC layer when exposed to various mixed gas atmospheres. Scanning electron microscopy, x-ray diffraction, and focused ion beam milling was used to determine the impact of CO and steam on the oxidation behavior of the SiC layer. Therefore, the data presented demonstrates how the SiC layer showed strong oxidation resistance due to limited SiO 2 growth and maintained its structural integrity under these off-normal conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Arc Jet Testing of Hafnium Diboride Based Ultra High Temperature Ceramics

Hafnium Diboride (HFB,) based materials have shown promise for use in a number of high temperature aerospace applications, including rocket nozzles and as leading edges on hypersonic reentry vehicles. The stability of the materials in relevant environments is key to determining their suitability for a particular application. In this program we have been developing HfB2/SiC materials for use as sharp leading edges. The program as a whole included processing and characterization of the HfBJSiC materials. The specific work discussed here will focus on studies of the materials oxidation behavior in simulated reentry environments through arc jet testing. Four flat face models were tested to examine the influence of heat flux and stagnation pressure on the materials oxidation behavior. The results from arc jet testing of two HfB2/SiC cone models will also be discussed. Each cone model was run multiple times with gradually increasing heat fluxes. Total run times on a single cone model exceeded 80 minutes. For both the flat face and cone models surface temperatures well in excess of 2200 C were measured. Post test microstructural examination of the models and correlations with measured temperatures will be discussed.

Ellerby, Don↗

Durability of Environmental Barrier Coatings in a Water Vapor/Oxygen Environment

Silicon carbide (Sic) and silicon nitride (Si3N4) show potential for application in the hot sections of advanced jet engines. The oxidation behavior of these materials has been studied in great detail. In a pure oxygen environment, a silica (SiO2) layer forms on the surface and provides protection from further oxidation. Initial oxidation is rapid, but slows as silica layer grows; this is known as parabolic oxidation. When exposed to model fuel-lean combustion applications (standard in jet engines), wherein the partial pressure of water vapor is approximately 0.5 atm., these materials exhibit different characteristics. In such an environment, the primary oxidant to form silica is water vapor. At the same time, water vapor reacts with the surface oxide to form gaseous silicon hydroxide (Si(OH)4). The simultaneous formation of both silica and Si(OH)4 -the latter which is lost to the atmosphere- the material continues to recede. Recession rates for uncoated Sic and Si3N4 are unacceptably high, for use in jet engines, - on the order of 1mm/4000h. External coatings have been developed that protect Si-based materials from water vapor attack. One such coating consists of a Ba(0.75)Sr(0.25)Al2Si2O8 (BSAS) topcoat, a mullite/BSAS intermediate layer and a Si bond coat. The key function of the topcoat is to protect the Si-base material from water vapor; therefore it must be fairly stable in water vapor (recession rate of about 1mm/40,000h) and remain crack free. Although BSAS is much more resistant to water vapor attack than pure silica, it exhibits a linear weight loss in 50% H2O - 50% O2 at 1500 C. The objective of my research is to determine the oxidation behavior of a number of alternate hot-pressed monolithic top coat candidates. Potential coatings were exposed at 1500 C to a 50% H2O - 50% O2 gas mixture flowing at 4.4 cm/s . These included rare- earth silicates, barium-strontium aluminosilicates. When weight changes were measured with a continuously recording microbalance, linear weight loss was observed. BSAS materials have a fairly high volatility at this temperature, but rare-earth mono-silicate compounds were significantly more stable.

Holchin, John E.↗

Modified fused silicide coatings for tantalum (Ta-10W) reentry heat shields

Results are presented of a program of research to develop a reliable, high performance, fused slurry silicide coating for the Ta-10W alloy. The effort was directed toward developing new and improved formulations for use at 2600 to 2800 F (1700 to 1811 K) in an atmospheric reentry thermal protection system with a 100-mission capability. Based on a thorough characterization of isothermal and cyclic oxidation behavior, bend transition temperatures, room- and elevated-temperature tensile properties, and creep behavior, a 2.5 Mn-33Ti-64.5Si coating (designated MTS) provides excellent protection for the Ta-10W alloy in simulated reentry environments. An extensive analysis of the oxidation behavior and characteristics of the MTS coating in terms of fundamental mechanisms also is presented.

Packer, C. M.↗

Use of Modeling and Experiments to Assess the Effect of Minor Alloying Additions on Alumina Scale Formation during High-Temperature Oxidation

During the last decades, new generations of Ni-based superalloys have emerged with judiciously controlled chemistries. These alloys heavily rely on the addition of refractory elements to enhance their mechanical properties at elevated temperatures; however, a clear interpretation of the influence of these minor-element additions on the alloy's high-temperature oxidation behavior is still not well understood, particularly from the standpoint of predicting the transition from internal to external alumina formation. In this context, the present investigation describes a systematic study that addresses the intrinsic effects that minor element additions of Nb, Ta, and Re have on the oxidation behavior of alumina-scale forming γ-Ni alloys. By combining a novel simulation approach with high-temperature oxidation experiments, the present study evidences the generally positive effect associated with 2 at. % addition of Ta and Re as well as the detrimental consequences of Nb additions on the 1100 °C oxidation of (in at. %) Ni-6Al-(0,4,6,8)Cr alloys.

Rodriguez, Rafael↗

Design Rules for Carboborothermic Reduction Synthesis of High Uranium Density UB 4 –UBC Composites

Uranium borides are promising candidate fuel forms for use in advanced nuclear reactors due to their high thermal conductivity and potential for dual use as both fuel and burnable absorber. In this work, uranium tetraboride () and uranium monoboroncarbide (UBC) composite were synthesized by using industrially scalable carboborothermic reduction method. The final uranium boride phase composition is sensitive to the sample holding crucibles ( and graphite) such that graphite supply excess carbon, promoting the formation of a predominant UBC phase. The high‐temperature in situ synchrotron X‐ray diffraction of pristine –UBC show persistence , UBC, and phases while preoxidized –UBC leads to predominant and formation due to progressive oxidation and boron loss at high temperature. The oxidation behavior was further characterized using thermogravimetric analysis, allowing direct comparison with other potential accident tolerant fuels such as , , UC, and UN. The –UBC shows higher uranium loading than monolithic and demonstrates promising oxidation behavior at high temperature, pointing to its potential as an improved uranium boride‐based fuel form.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Oscillatory redox behavior in oxides: Cyclic surface reconstruction and reactivity modulation via the Mars–van Krevelen mechanism

The breaking of translational symmetry at oxide surfaces gives rise to coordinatively unsaturated cations/anions and surface restructuring—key factors that govern surface reactivity. Using direct in situ environmental transmission electron microscopy (TEM) observations along with atomistic modeling, we report oscillatory redox behavior in CuO under H 2 , where cyclic surface reconstruction and reactivity modulation occur via the Mars–van Krevelen (MvK) mechanism. We observe self-switching between oxygen-rich and oxygen-deficient surface reconstructions, alternately activating and deactivating the surface for H 2 O formation. During periods of chemical inactivity, the oxygen-deficient surface undergoes slow reoxidation via lattice oxygen diffusing from subsurface and bulk reservoirs, restoring the active oxygen-rich surface termination. The inherent disparity in chemical activity among undercoordinated surface ions, along with sluggish subsurface-to-surface oxygen replenishment, drives this oscillatory redox cycle, modulating H2-induced loss of lattice oxygen at the surface and its delayed replenishment from the subsurface. This creates spatiotemporally separated redox steps at the oxide surface. The phenomena and atomistic insights presented here have significant implications for manipulating the surface reactivity of oxides by tuning the separation of these redox steps.

36 MATERIALS SCIENCE↗

Oxidation Characterization of Hafnium-Based Ceramics Fabricated by Hot Pressing and Electric Field-Assisted Sintering

Ceramic borides, such as hafnium diboride (HfB2) and zirconium diboride (ZrB2), are members of a family of materials with extremely high melting temperatures referred to as Ultra High Temperature Ceramics (UHTCs). UHTCs constitute a class of promising materials for use in high temperature applications, such as sharp leading edges on future-generation hypersonic flight vehicles, because of their high melting points. The controlled development of microstructure has become important to the processing of UHTCs, with the prospect of improving their mechanical and thermal properties. The improved oxidation resistance of HfB2 has also become important if this material is to be successfully used at temperatures above 2000 C. Furthermore, the use of UHTCs on the leading edges of vehicles traveling at hypersonic speeds will mean exposure to a mixed oxidation environment comprised of both molecular and atomic oxygen. The current study has investigated the high-temperature oxidation behavior of HfB2-based materials in a pure O2 environment, as well as in environments containing different levels of dissociated oxygen (O/O2). Materials were processed by two techniques: conventional hot pressing (HP) and electric field-assisted sintering (FAS). Their oxidation behavior was evaluated in both a tube furnace at 1250 C for 3 hours and in a simulated re-entry environment in the Advanced Heating Facility (AHF) arcjet at NASA Ames Research Center, during a 10-minute exposure to a cold wall heat flux of 250W/sq cm and stagnation pressure of 0.1-0.2 atm. The microstructure of the different materials was characterized before and after oxidation using scanning electron microscopy (SEM).

Gasch, Matt↗

Oxidation resistance of novel ferritic stainless steels alloyed with titanium for SOFC interconnect applications

Chromia (Cr2O3) forming ferritic stainless steels are being developed for interconnect application in Solid Oxide Fuel Cells (SOFC). A problem with these alloys is that in the SOFC environment chrome in the surface oxide can evaporate and deposit on the electrochemically active sites within the fuel cell. This poisons and degrades the performance of the fuel cell. The development of steels that can form conductive outer protective oxide layers other than Cr2O3 or (CrMn)3O4 such as TiO2 may be attractive for SOFC application. This study was undertaken to assess the oxidation behavior of ferritic stainless steel containing 1 weight percent (wt.%) Ti, in an effort to develop alloys that form protective outer TiO2 scales. The effect of Cr content (6–22 wt.%) and the application of a Ce-based surface treatment on the oxidation behavior (at 800° C in air+3% H2O) of the alloys was investigated. The alloys themselves failed to form an outer TiO2 scale even though the large negative {delta}G of this compound favors its formation over other species. It was found that in conjunction with the Ce-surface treatment, a continuous outer TiO2 oxide layer could be formed on the alloys, and in fact the alloy with 12 wt.% Cr behaved in an identical manner as the alloy with 22 wt.% Cr.

30 DIRECT ENERGY CONVERSION↗

Long-Term Performance of High Temperature Alloys in Oxidizing Environments and Supercritical CO 2

Long-term performance of high temperature alloys is critically linked to the oxidation behavior in power generation applications in wet air and steam. As power generation systems move towards higher efficiency operation, next-generation fossil, nuclear and concentrating solar power plants are considering supercritical CO 2 cycle above 700°C. Wrought solid solution strengthened and precipitations strengthened alloys are leading candidates for both steam and Supercritical CO 2 power cycles.This study evaluates the cyclic oxidation behavior of HAYNES® 230®, 282®, and 625 alloys in wet air, flowing laboratory air, steam and in 1 and 300 bar Supercritical CO 2 at ~750oC for duration of 1000 -10,000h. Test samples were thermally cycled for various times at temperature followed by cooling to room temperature. Alloy performances were assessed by analyzing the weight change behavior and extent of attack. The results clearly demonstrated the effects of alloy composition and environment on the long-term cyclic oxidation resistance. The extents of attack varied from alloy to alloy but none of the alloys underwent catastrophic corrosion and no significant internal carburization was observed in supercritical CO 2 . The performance of these alloys indicates that these materials are compatible not only in oxidizing environments, but also in Supercritical CO 2 environments for extended service operation.

Deodeshmukh, Vinay↗

Oxidation and Metal-Insertion in Molybdenite Surfaces: Evaluation of Charge-Transfer Mechanisms and Dynamics

Molybdenum sulfide (MoS2), an important representative member of the layered transition-metal dichalcogenides, has been of special importance to the research community of geochemistry, materials and environmental chemistry, and industrial science and technology. Understanding the oxidation behavior and charge-transfer mechanisms in MoS2 is important to gain better insight into the degradation of this mineral in the environment. On the other hand understanding the insertion of metals into molybdenite and evaluation of charge-transfer mechanism and dynamics is quite important to utilize these minerals in technological applications. Furthermore, such a detailed investigation of thermal oxidation behavior and intercalation process will provide a basis to further explore and model the mechanism of adsorption of metal ions on to geomedia. Therefore, the present work was performed to understand the oxidation and intercalation processes of molybdenite surfaces. The results obtained, using a wide variety of analytical techniques, are presented and discussed in this paper.

36 MATERIALS SCIENCE↗

Effects of chromium and aluminum on mechanical and oxidation properties of iron-nickel-base superalloys based on CG-27

The effects of chromium and aluminum on the mechanical and oxidation properties of a series of gamma-prime-strengthened alloys based on CG-27 were studied. Gamma-prime dispersion and solid-solution strengthening were the principal modes of alloy strengthening. The oxidation attack parameter K sub a decreased with increasing Cr and Al contents for each alloy group based on Al content. As a group, alloys with 3 wt % Al had the lowest attack parameters. Therefore, 3 wt % is the optimum level of Al for parabolic oxidation behavior. Spalling, due to diffusion-induced grain growth, was controlled by the overall Cr and Al levels. The alloy with 4 wt % Cr and 3 wt % Al had stress-rupture properties superior to those of the base alloy, CG-27, and maintained parabolic oxidation behavior while the Cr content was reduced by two-thirds of its value in cast CG-27.

Schuon, S. R.↗

Computer simulation of cyclic oxidation

A computer program has been developed which simulates the cyclic oxidation behavior of materials. The simulation is based on the assumption that the weight fraction of scale that spalls in any thermal cycle is proportional to the amount of scale present on the surface at the beginning of the cycle. The program provides plots as well as tabular data which describe the cyclic oxidation behavior of a given material. Individual input parameters can be selectively altered and the resulting change in cyclic kinetics determined, allowing the user to quickly survey a wide range of cyclic conditions on the kinetics of a given material.

Probst, H. B.↗

High Temperature and Pressure Steam-H 2 Interaction with Candidate Advanced LWR Fuel Claddings

This report summarizes the work completed to evaluate cladding materials that could serve as improvements to Zircaloy in terms of accident tolerance. This testing involved oxidation resistance to steam or H 2 -50% steam environments at 800-1350°C at 1-20 bar for short times. A selection of conventional alloys, SiC-based ceramics and model alloys were used to explore a wide range of materials options and provide guidance for future materials development work. Typically, the SiC-based ceramic materials, alumina-forming alloys and Fe-Cr alloys with ≥25% Cr showed the best potential for oxidation resistance at ≥1200°C. At 1350°C, FeCrAl alloys and SiC remained oxidation resistant in steam. Conventional austenitic steels do not have sufficient oxidation resistance with only ≈18Cr-10Ni. Higher alloyed type 310 stainless steel is protective but Ni is not a desirable alloy addition for this application and high Cr contents raise concern about α' formation. Higher pressures (up to 20.7 bar) and H 2 additions appeared to have a limited effect on the oxidation behavior of the most oxidation resistant alloys but higher pressures accelerated the maximum metal loss for less oxidation resistant steels and less metal loss was observed in a H 2 -50%H 2 O environment at 10.3 bar. As some of the results regarding low-alloyed FeCrAl and Fe-Cr alloys were unexpected, further work is needed to fundamentally understand the minimum Cr and Al alloy contents needed for protective behavior in these environments in order to assist in alloy selection and guide alloy development.

36 MATERIALS SCIENCE↗