Search NASA⌕ Search

SEARCH · Search NASA

Results for “Shear strength”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Factors Affecting the Processing of Epoxy Film Adhesives

The increasing awareness that adhesive performance is controlled not only by the condition of the adherend surface but also the condition or state of the adhesive and the process parameters used during fabrication is expected to result in improved reliability, as well as bond performance. The critical process variables which have been found to control adhesive bond formation and ultimate bond strength in 250F and 350F curing epoxy adhesives are described in terms of fabrication parameters and adhesive characteristics. These include the heat-up rate and cure temperature during processing and the adhesive moisture content and age condition (degree of advancement). The diagnostic methods used to delineate the effects of these process variables on adhesive performance are illustrated. These are dielectric, thermomechanical (TMA) and dynamic mechanical (DMA) analyses. Correlation of test results with measured mechanical tensile lap shear strengths of bonded joints is presented and the results briefly discussed in terms of the additives and hardeners used in the adhesive systems.

Pike, R. A.↗

Investigation of instability, dynamic forces, and effect of dynamic loading on strength of cages for the bearings in the high pressure oxygen turbopumps for the space shuttle main engine

Experiments were performed to determine the effect of cyclic loading on bearing cage strength. A long term working tensile load of approximately 1300 N (300 lbs) was found to be the likely maximum. Higher loads caused a decrease in cage tensile strength after the 125,000 cycle testing period. Poisson's ratio in compression was found to be highly dependent upon the direction of the fiberglass plies. At room temperature the value was 0.15 with the plies and 0.68 across the plies. At -196 C (-321 F), the value with the plies was 0.20. The results of the analyses conducted have again demonstrated the critical need for improved lubrication in the high pressure oxygen turbopump bearings. Lubricant films with low shear strength and low friction coefficients promote cage stability and decrease ball/cage forces during marginal operating conditions. The analysis of the effect of combined bearing loads on ball/cage loads has identified a radial load of 3600 N (800 lbs) as the maximum for the current clearance of the balls and cage pockets. Liquid oxygen impinging on the cage in the direction of rotation was found to enhance cage stability.

Dufrane, K. F.↗

Test methods and design allowables for fibrous composites; Proceedings of the Symposium, Dearborn, MI, October 2, 3, 1979

Papers are presented on special test methods for fibrous composites for quantifying design material properties. Studies are divided into four major areas: (1) new and special test methods, including those for transverse tensile strength, shear modulus, longitudinal compression, and impact resistance; (2) special test methods and analysis, including off-axes and angle-plied tension and compression, fracture and fatigue, and biaxial stress states; (3) design allowables, describing procedures for setting and selecting design allowables in general, and also for composite aircraft structures, graphite/polyimide bolted joints, cost-effective mechanical property characterization, statistical considerations, intraply hybrids, and compression and fatigue; (4) design allowables for special applications, describing procedures for buckling of cylindrical components, proof load of pressure vessels, strength of composite joints, and environmental effects and creep. The papers provide considerable information for test methods and for composite analysis of these methods, as well as tests and procedures for establishing design allowables.

Chamis, C. C.↗

Design and Development of a Laboratory-Scale Ice Adhesion Testing Device

When an aircraft traverses through clouds containing supercooled water droplets, in-flight icing can occur that negatively affects vehicle performance by increasing weight and drag leading to loss of lift. Super-cooled water droplets present in clouds that impact vehicle surfaces can lead to inflight icing any time during the year.1 Most events occur at temperatures ranging from 0 to -20degC. Ice generated on the aircraft can vary between clear/glaze, rime, and mixed (Fig. 1) depending on air temperature (-5 to -20degC), liquid water content (0.3-0.6 g/m3), and droplet size (median volumetric diameter of 15-40 μm). Current strategies to remove ice are based on active technologies such as pneumatic boots, heated surfaces, and deicing agents (i.e., ethylene- and propylene-based glycols). The latter have potential environmental concerns. A passive approach to mitigate accreting ice that is actively being investigated are protective coatings. An ice mitigating coating could potentially be used as a stand-alone material, but more likely in combination with an active approach. In the latter scenario, potential reduction in power consumption by the active approach may be realized. To determine the ice adhesion strength of impact ice that is representative of the aircraft environment is not a trivial matter. Test methods utilizing slowly formed ice (i.e., freezer ice) do not accurately simulate this environment. Likewise, some testing methodologies involve sample relocation from the icing environment to the test chamber that can result in thermal shock to the sample, thus affecting the results. The Adverse Environment Rotor Test Stand (AERTS) located at Pennsylvania State University (PSU) has been demonstrated to simulate impact icing conditions within the icing envelope for the determination of ice adhesion shear strength (IASS) without removal/relocation of the sample.2 Due to the confidence in results obtained from AERTS, this instrument is in high demand and requires a significant amount of lead time and capital investment to obtain IASS results. As a solution for quickly and economically screening coatings in a controlled manner under impact icing conditions, a laboratory-scale ice adhesion test and dead blades were then removed from the rotor/blade assembly to obtain the final mass. The IASS of the live blade was determined from the difference in mass (before and after testing) of the live and dead blades, the ice shed area, and the rpm of the shed event. The same live blade sample was tested in triplicate at all three test temperatures. Surface roughness was determined using a Bruker Dektak XT Stylus Profilometer. Measurements were conducted using a 12.5 μm tip at a vertical range of 65.5 μm with an applied force of 3 mg. Data were collected over a 1.0 mm length at a resolution of 0.056 μm/point. Five single line scans at different locations were collected and processed using a two-point leveling subtraction. The resultant Ra (arithmetic roughness) and Rq (root mean square roughness) average values were calculated.

Smith, Joseph G., Jr.↗

Preliminary evaluation of a novel polyimide adhesive for bonding titanium and reinforced composites

A novel polyimide has been developed which shows promise as an adhesive for bonding titanium-to-titanium, titanium-to-polyimide composite and composite-to-composite with excellent lap shear strengths at room temperature and moderate strengths at 288 C. The adhesive is a high molecular weight polyimide made from commercially available monomers. The use of an ether as the solvent for the polymerization and for application of the polyamic acid enhanced the adhesive properties of the polyimide. At room temperature, P13N/glass composite bonded to titanium or to itself failed primarily in the surface layer of the composite, whereas at 260 C the failure was primarily cohesive. Failure of the P13N/unidirectional HT-S graphite composite-to-titanium bonded composites occurred in the composite regardless of the test temperature. Preliminary shear results with cross-plied P13N/HT-S graphite composite-to-composite specimens showed failure in the bonded surface fibers.

Progar, D. J.↗

Joining, Disassembly, and Reconfiguration of Thermoplastic Composites for Space Applications

Thermoplastic composites are increasingly being investigated for aerospace applications because of their relatively short processing time, good chemical and radiation resistance, and potential for reforming and reuse via melting. The manufacturing, reforming, and reuse of thermoplastic composites can be leveraged to advance joining, disassembly, and reassembly of structures for space exploration activities. Potential applications include, but are not limited to, habitats and on-orbit assembly and reassembly of large-scale truss structures. This work focuses on demonstrating the feasibility of joining, disassembly, and reassembly of a thermoplastic bond using heat and pressure. Polyether ether ketone (PEEK) composite adherends were joined using low-melt polyaryl ether ketone (LM-PAEK) thermoplastic films at the bonding interface. The single lap shear specimens with LM-PAEK film were tested and had a maximum shear strength between 5 and 8 MPa and consistently failed adhesively at the bondline. Reassembly of disassembled specimens was successfully demonstrated using additional thermoplastic interlayers. Thus, the reassembly of thermoplastic composite joints was found to be feasible. However, additional work is required to reduce film flowout and optimize consolidation parameters for an in space environment.

thermoplastic composites↗

Explosive Welding of Aluminum, Titanium and Zirconium to Copper Sheet Metal

The main material properties affecting the explosive weldability of a certain metal combination are the yield strength, the ductility, the density and the sonic velocity of the two metals. Successful welding of the metal combination depends mainly on the correct choice of the explosive welding parameters; i.e., the stand off distance, the weight of the explosive charge relative to the weight of the flyer plate and the detonation velocity of the explosive. Based on the measured and the handbook values of the properties of interest, the explosive welding parameters were calculated and the arrangements for the explosive welding of the Al alloy 6061-T6, titanium and zirconium to OFHC copper were determined. The relatively small sheet metal thickness (1/8") and the fact that the thickness of the explosive layer must exceed a certain minimum value were considered during the determination of the explosive welding conditions. The results of the metallographic investigations and the measurements of the shear strength at the interface demonstrate the usefulness of these calculations to minimize the number of experimental trials.

Hegazy, A. A.↗

AERoBOND Project Summary

Under NASA’s Convergent Aeronautics Solutions (CAS) project, the Adhesive-Free Bonding of Complex Composites (AERoBOND) project investigated off-stoichiometric epoxy polymers for fast, reliable assembly of epoxy matrix composite structures. The project goal was to demonstrate feasibility of the AERoBOND joining method by demonstrating mechanical properties greater than 80% of conventional co-cured materials while reducing structure weight by 1%. The project consisted of three convergent research areas: material and process development, systems analysis, and material and process modeling. Material and process development was the largest component of AERoBOND with approximately 6 FTE and 1WYE of support to formulate and characterize new resins, prepare carbon fiber prepregs, fabricate laminates, measure mechanical properties, analyze failure results, and select material and process improvements. The systems analysis activity estimated the potential reduction in part count and aircraft weight by comparing models of composite wing boxes with no fasteners (co-cured structure), fasteners in major joints (co-cured stringers), and fasteners in all joints. The materials and process modeling activity included a molecular model of the AERoBOND materials system to predict mechanical properties of resins with offset stoichiometry and a process model to predict the effect of resin formulation and processing conditions on the extent of mixing and degree of cure in a finished joint. As the number of airline passenger trips doubles in the next 20 years (IATA/Tourism Economics Air Passenger Forecasts, April 2019), the increased demand for new commercial aircraft is now the single greatest technical challenge to the airframe manufacturing industry. To meet efficiency requirements, new aircraft must be fabricated primarily from high performance structural composites, but manufacturing processes are inherently slow with the largest bottleneck attributed to assembly and installation of fasteners (NASA/TM–2019-220428). Manufactures of commercial transport aircraft are compelled to install more than 100,000 redundant fasteners into bonded joints to prevent failures due to unpredictable weak bonds. In structural adhesive bonds, the interface between adherend and adhesive is nearly two-dimensional making it susceptible to minute quantities of contamination, which can cause weak bonds. Currently, bond strength assessment is only possible through destructive testing (i.e., breaking the joint). For these reasons, regulatory organizations such as the Federal Aviation Administration (FAA) often require redundant load paths in secondary-bonded, primary-structures to alleviate concerns with bond performance. The AERoBOND process enables reflow of matrix resin during assembly to eliminate the material discontinuity at the interface, thereby eliminating the dependence of mechanical performance on interfacial adhesion. The AERoBOND joint is equivalent to the interlaminar region obtained during a co-cure process, so joint performance depends on the cohesive properties of the matrix resin. Conventional co-cured structures, although too costly and complex for large-scale manufacturing, are trusted by manufacturers and regulators, and are certified for flight with few or no redundant fasteners.Systems analysis performed on a composite wing model at the scale of a single-aisle commercial transport aircraft indicated that >20,000 redundant fasteners per wing could be eliminated by implementing the AERoBOND joining method. A total weight reduction of 15% was predicted in a wing box by eliminating fasteners and thinning components that must no longer support localized fastener loads and accommodate fastener dimensions. Interlaminar shear fracture toughness measured by the end-notched flexure test was greater than 1 kJ/m2 (nearly 140% of the co-cured benchmark property), which is greatly in excess of the project goals for mechanical properties. Testing was planned to measure interlaminar tensile fracture toughness as well as interlaminar tensile and shear strengths using the same AERoBOND configuration, but was delayed due to closure of LaRC facilities during the COVID-19 pandemic. The AERoBOND process model is partially validated and available for experimental use. It allows the user to input AERoBOND process parameters such as material composition, laminate configuration, and cure cycle to predict the final cure state of the AERoBOND joint. A preliminary, multi-scale material model was developed to predict AERoBOND joint mechanical properties (stiffness and strength) based on the cure state of the joint provided by the process model. The timing for transition of this technology within NASA is excellent as NASA initiates new enduring projects to address composites manufacturing rate challenges. AERoBOND technology is well suited to AAVP/AATT objectives for rapid manufacturing of a composite wing. A minimal effort (1 FTE/$15k procurement/0 WYE) is proposed in FY21 to continue a minor mechanical testing effort and maintain a SAA with ASX composites to develop commercial quality prepreg material. An RFI with the composites industry is suggested to quantify the technology gap between the current TRL and the TRL needed for transition to industry. A moderate effort [3-4 FTE/$150k/1 WYE (~$115k)] is proposed in FY22 for the “high rate composites manufacturing” project currently in planning. The partnership with ASX Composites will be expanded to produce material for sub-element/element-scale “panel-off” activities. Industry partnerships with airframe manufacturers is an expected component to explore damage tolerance and environmental stability. Further development of multi-scale modeling tools (process model, meso-scale model, and molecular model) is planned to enhance and deliver tools for rapid manufacturing infusion.

Frank Louis Palmieri↗

Improved BN Coatings on SiC Fibers in SiC Matrices

Modifications of BN-based coatings that are used as interfacial layers between the fibers and matrices of SiCfiber/SiC-matrix composite materials have been investigated to improve the thermomechanical properties of these materials. Such interfacial coating layers, which are also known as interphases (not to be confused with interphase in the biological sense), contribute to strength and fracture toughness of a fiber/matrix composite material by providing for limited amounts of fiber/matrix debonding and sliding to absorb some of the energy that would otherwise contribute to the propagation of cracks. Heretofore, the debonding and sliding have been of a type called inside debonding because they have taken place predominantly on the inside surfaces of the BN layers that is, at the interfaces between the SiC fibers and the interphases. The modifications cause the debonding and sliding to include more of a type, called outside debonding, that takes place at the outside surfaces of the BN layers that is, at the interfaces between the interphases and the matrix (see figure). One of the expected advantages of outside debonding is that unlike in inside debonding, the interphases would remain on the crack-bridging fibers. The interphases thus remaining should afford additional protection against oxidation at high temperature and should delay undesired fiber/fiber fusion and embrittlement of the composite material. A secondary benefit of outside debonding is that the interphase/matrix interfaces could be made more compliant than are the fiber/interphase interfaces, which necessarily incorporate the roughness of the SiC fibers. By properly engineering BN interphase layers to favor outside debonding, it should be possible, not only to delay embrittlement at intermediate temperatures, but also to reduce the effective interfacial shear strength and increase the failure strain and toughness of the composite material. Two techniques have been proposed and partially experimentally verified as candidate means to promote outside debonding in state-of-the-art SiC/SiC composites.

Morscher, Gregory N.↗

Microstructure, Mechanical Properties, Hot-Die Forming, and Joining of 47XD Gamma TiAl Rolled Sheets

The microstructure and mechanical properties, along with the hot-die forming and joining of Ti-47Al-2Nb-2Mn-0.8 vol% TiB, sheets (known as 47XD), produced by a low-cost rolling process, were evaluated. A near-gamma microstructure was obtained in the as-rolled condition. The microstructures of heat-treated sheets ranged from a recrystallized equiaxed near-gamma microstructure at 1,200 to 1,310 C, to a duplex microstructure at 1,350 C, to a fully lamellar microstructure at 1,376 C. Tensile behavior was determined for unidirectionally rolled and cross-rolled sheets for room temperature (RT) to 816 C. Yield stress decreased gradually with increasing deformation temperature up to 704 C; above 704 C, it declined rapidly. Ultimate tensile strength exhibited a gradual decrease up to 537 C before peaking at 704 C, followed by a rapid decline at 816 C. The modulus showed a gradual decrease with temperature, reaching approximately 72% of the RT value at 816 C. Strain to failure increased slowly from RT to 537 C; between 537 C and 704 C it exhibited a phenomenal increase, suggesting that the ductile-brittle transition temperature was below 704 C. Fracture mode changed from transgranular fracture at low temperature, to a mixture of transgranular and intergranular fracture at intermediate temperature, to ductile fracture at 816 C, coupled with dynamic recrystallization at large strains. Creep rupture response was evaluated between 649 and 816 C over the stress range of 69 to 276 MPa. Deformation parameters for steady-state creep rate and time-to-rupture were similar: activation energies of approximately 350 kJ/mol and stress exponents of approximately 4.5. Hot-die forming of sheets into corrugations was done at elevated temperatures in vacuum. The process parameters to join sheets by diffusion bonding and brazing with TiCuNi 70 filler alloy were optimized for test coupons and successfully used to fabricate large truss-core and honeycomb structures. Nondestructive evaluation methods, e.g., ultrasonic C-scans and thermography along with metallography, were used to characterize bond quality. Microstructural evaluation during heat treatment, identification of phases at the braze/matrix interface, determination of shear strengths of brazed joints, and deformation mechanisms during tensile and creep processes will be discussed.

Das, G.↗

Materials, and engineering problems

Composite material engineering problems, discussing tensile, compressive and shear strengths, design approaches, unidirectional properties and substance characterizations

Dow, N. F.↗

New primers for adhesive bonding of aluminum alloys

Synthetic polypeptide adhesive primers are effective, with high temperature epoxy resins, at temperatures from 100 deg to 300 deg C. Lap-shear failure loads and lap-shear strength of both primers are discussed.

Burrell, B. W.↗