A Phase-Field Model for In-Space Manufacturing of Binary Alloys

The integrity of the final printed components is mostly dictated by the adhesion between the particles and phases that form upon solidification, which is a major problem in printing metallic parts using available In-Space Manufacturing (ISM) technologies based on the Fused Deposition Modeling (FDM) methodology. Understanding the melting/solidification process helps increase particle adherence and allows to produce components with greater mechanical integrity. We developed a phase-field model of solidification for binary alloys. The phase-field approach is unique in capturing the microstructure with computationally tractable costs. The developed phase-field model of solidification of binary alloys satisfies the stability conditions at all temperatures. The suggested model is tuned for Ni-Cu alloy feedstocks. We derived the Ginzburg-Landau equations governing the phase transformation kinetics and solved them analytically for the dilute solution. We calculated the concentration profile as a function of interface velocity for a one-dimensional steady-state diffuse interface neglecting elasticity and obtained the partition coefficient, k, as a function of interface velocity. Numerical simulations for the diluted solution are used to study the interface velocity as a function of undercooling for the classic sharp interface model, partitionless solidification, and thin interface.

36 MATERIALS SCIENCE↗

Harnessing metastability for grain size control in multiprincipal element alloys during additive manufacturing

Abstract Controlling microstructure in fusion-based metal additive manufacturing (AM) remains a significant challenge due to the many parameters that directly impact solidification condition. Multiprincipal element alloys (MPEAs), also known as high entropy alloys, offer a vast compositional space to design for microstructural engineering due to their chemical complexity and exceptional properties. Here, we use the FeMnCoCr system as a model platform for exploring alloy design in MPEAs for AM. By exploiting the decreasing stability of the face-centered cubic phase with increasing Mn content, we achieve notable grain refinement and breakdown of epitaxial columnar grain growth. We employ a multifaceted approach encompassing thermodynamic modeling, operando synchrotron X-ray diffraction, multiscale microstructural characterization, and mechanical testing to gain insight into the solidification physics and its ramifications on the resulting microstructure of FeMnCoCr MPEAs. This work aims toward tailoring desirable grain sizes and morphology through targeted manipulation of phase stability, thereby advancing microstructure control in AM applications.

Wakai, Akane↗

An algorithm for physics informed scan path optimization in additive manufacturing

Site specific microstructure control is a critical research area within the field of additive manufacturing due to its potential to revolutionize part performance. One way to achieve site specific microstructure control is through control of the solidification conditions via the construction of intricate scan paths; however, the search space for such a problem is large. Previous attempts only considered the solidification conditions at the top surface while also requiring either lots of manual-fine tuning or large amounts of computational resources. This paper introduces a general method for scan path optimization which considers the solidification conditions in the bulk of the material without an increase in computational expense. This method consists of three core components:1. A heat transfer model for simulating the temperature field at a given time.2. A surrogate model which takes scan pattern information and temperature data and predicts the solidification conditions of the bulk as well as the meltpool depths for a spot melt.3. A decision algorithm to decide which spot melt should be printed next based on the outputs of the surrogate model.Each of these components can be changed without changing the overall method. Within this work, this method is applied in the creation of an algorithm containing a semi-analytic heat transfer model to simulate the temperature field, a fully convolutional neural network (FCNN) as the surrogate model, and a greedy decision algorithm. The resulting algorithm produced complex scan patterns which gave strong results for simulated microstructure control.

36 MATERIALS SCIENCE↗

Microstructure and In Situ Observations of Undercooling for Nucleation of [beta]-Sn Relevant to Lead-Free Solder Alloys

Difficult nucleation of {beta}-Sn during solidification of tin and tin-based lead-free solder alloys can result in high degrees of undercooling of the liquid prior to solidification. The undercooling can produce solder joints with large grains, anisotropic behavior, and undesirable mechanical properties. This paper describes our examination of the amount of undercooling of tin on both graphite (non-wetting) and copper (wetting) surfaces using in situ x-ray diffraction. The microstructure was further characterized by optical microscopy, scanning electron microscopy, and electron backscattering diffraction imaging microscopy. Undercoolings as high as 61 C were observed for Sn solidified on graphite, while lower undercoolings, up to 30 C, were observed for Sn solidified on copper. The microstructure of the high purity Sn sample solidified on graphite showed very few grains in the cross-section, while the commercially pure Sn sample solidified with only one grain and was twinned. Tin solidified on copper contained significant amounts of copper in the tin, intermetallic phase formation at the interface, and a eutectic microstructure.

36 MATERIALS SCIENCE↗

Influence of Mn addition on the microstructure and mechanical properties of a directionally solidified γ-TiAl alloy

Highlights: • Mn addition can significantly improve the yield strength of TiAl alloy. • Introduction of Mn facilitates the operation of twinning-controlled deformation. • Twin-dislocation interactions cause a continuous increase in work hardening rate. - Abstract: TiAl alloys with nominal compositions of Ti-47Al-2Nb-2Cr-(0, 1, 3, 5)Mn were prepared via electromagnetic cold crucible directional solidification (ECCDS), and the influence of Mn addition on the microstructure and mechanical properties of the alloys was investigated. The experimental results showed that the Mn atoms were dissolved within the TiAl alloy, and no Mn compounds were formed. Based on the X-ray diffraction (XRD) analysis results, the peak angle of the Mn-containing sample shifted to a higher value, indicating lattice shrinkage. The Mn addition also increased the volume fraction of the B2 phase. The yield strength of the TiAl alloy monotonically increased as the content of the substitutional-solute Mn atoms increased. The ultimate strengths of the TiAl alloys containing 1 at.%, 3 at.%, and 5 at.% Mn consequently decreased because micro-cracks were preferentially formed in the B2 phase during room-temperature deformation. The introduction of substitutional-solute Mn atoms could result in a reduction of the stacking-fault energy of the γ phase, and facilitate the operation of twinning-controlled plastic-deformation during the intermediate stage of the plastic deformation process. The interaction between the deformation twins and movable dislocations led to a continuous increase in the work-hardening rate.

36 MATERIALS SCIENCE↗

The microstructure of a selective laser melting (SLM)-fabricated NiTi shape memory alloy with superior tensile property and shape memory recoverability

A selective laser melting (SLM)-fabricated NiTi with superior tensile property and shape memory recoverability was obtained by using a unique stripe rotation scanning strategy. Here, the alloy characteristics, formation mechanisms and evolution in terms of twins, dislocations and precipitations of the alloy were systematically studied. Compared to the conventional smelting-followed-by-machining, the SLM fabrication process involves rapid solidification and repeated heating, which confer distinctive characteristics to the microstructures of SLM-fabricated NiTi alloys. Rapid solidification promotes the formation of a supersaturation solid solution matrix containing a high concentration vacancies, which in turn aggregate to generate a high density of dislocations. During subsequent repeated heating stages, these dislocations occur thermal motion along three directions of <001 > , <111> and <110 >, leading to the formation of thermal kinks, helical dislocations and wave morphology. Simultaneously, precipitated particles Ti 3 Ni 4 repeatedly nucleate and heterogeneous grow with the movement of dislocation. Such precipitation behavior, termed repeated precipitation, has not been previously reported in the conventional NiTi alloys, suggesting that it could be a unique characteristic of such alloy. After martensitic transformation, only two twins, {1 1¯ 1} type I twin and compound twin, are detected. The twinning lamellae of these two twins, where precipitation and dislocation pile-ups exist, often have uneven thickness and chaotic arrangement. Besides, the unique self-accommodated microstructures, such as secondary {1 1¯ 1} type I twin and compound twin with “herring-bone’’ lamellae, which often appear in the deformed or nanocrystalline NiTi, can also be observed. These unique microstructures may confer the distinctive properties to the SLM-fabricated NiTi.

36 MATERIALS SCIENCE↗

Influence of phase composition on microstructure and properties of Mg-5Al-0.4Mn-xRE (x = 0, 3 and 5 wt.%) alloys

The microstructure and mechanical properties investigations of two AME503 and AME505 experimental alloys in as-cast conditions were presented. The investigated materials were fabricated on the basis of the AM50 commercial magnesium alloy with 3 and 5 wt.% cerium rich mischmetal. In the as-cast condition, both experimental alloys were mainly composed of α-Mg, Al{sub 11}RE{sub 3} and Al{sub 10}RE{sub 2}Mn{sub 7} intermetallic phases. Additionally, due to non-equilibrium solidification conditions, a small amount of α + γ divorced eutectic and Al{sub 2}RE intermetallic phase were revealed. The obtained results also show a significant influence of rare earth elements on Brinell hardness, tensile and compression properties at ambient temperature and especially on creep properties at 473 K. Improved alloy properties with a rise in rare earth elements mass fraction results from an increase in Al{sub 11}RE{sub 3} phase volume fraction and suppression of α + γ eutectic volume fraction in the alloy microstructure. Additionally, the influence of rare earth elements on the dendrite arm space value was discussed. The presented results also proved the thermal stability of the intermetallic phases during creep testing. - Highlights: • Two different Mg-5Al-0.4Mn alloys containing 3 and 5 wt.% of rare earth elements were fabricated. • Addition of rare earth elements leads to a reduction of dendrite arm spaces. • Mechanical properties depend on the phase composition of the alloys. • The increase of the rare earth elements content causes rise of the creep resistance.

36 MATERIALS SCIENCE↗

Characterization of the Fe-Co-1.5V soft ferromagnetic alloy processed by Laser Engineered Net Shaping (LENS)

Processing of the low workability Fe-Co-1.5V (Hiperco® equivalent) alloy is demonstrated using the Laser Engineered Net Shaping (LENS) metals additive manufacturing technique. As an innovative and highly localized solidification process, LENS is shown to overcome workability issues that arise during conventional thermomechanical processing, enabling the production of bulk, near net-shape forms of the Fe-Co alloy. Bulk LENS structures appeared to be ductile with no significant macroscopic defects. Atomic ordering was evaluated and significantly reduced in as-built LENS specimens relative to an annealed condition, tailorable through selection of processing parameters. Fine equiaxed grain structures were observed in as-built specimens following solidification, which then evolved toward a highly heterogeneous bimodal grain structure after annealing. The microstructure evolution in Fe-Co is discussed in the context of classical solidification theory and selective grain boundary pinning processes. In conclusion, magnetic properties were also assessed and shown to fall within the extremes of conventionally processed Hiperco® alloys.

36 MATERIALS SCIENCE↗

Microstructural evolution and growth behavior of intermetallic compounds at the liquid Al/solid Fe interface by synchrotron X-ray radiography

Highlights: • A layered and tongue-like η phase was in-situ observed by synchrotron radiation X-ray radiography. • The coalescence of η phase bottom resulted in dissolution, further increasing the growth rate. • The θ phase growth behavior with different morphologies during cooling was analyzed. - Abstract: The growth of Inter-Metallic Compounds (IMCs) with dissolution was investigated on the liquid Al/solid Fe interconnection by using synchrotron radiation real-time imaging technology. At the initial stage of holding at 850 °C, a layer of the η-Fe{sub 2}Al{sub 5} phase formed at the interface, and tongue-like η grew into α-Fe. The tongue-like η phase had a stronger (001) texture than the layered phase. The coalescence of tongue-like η started at the bottom, followed by the dissolution of IMCs, which leads to a further increase in its growth rate. During solidification stage, the dotted, needle-like and flake θ-FeAl{sub 3} phases were sequentially formed.

36 MATERIALS SCIENCE↗

Solidification dynamics in metal additive manufacturing: analysis of model assumptions

Solidification characteristics in the meltpool drive the process-microstructure relationship which helps dictate the material properties of as-built parts in additive manufacturing; therefore, being able to accurately and quickly simulate the size, shape, and solidification characteristics in the melt pool is of great interest to the field. In this study, we investigate various important physical phenomena (dynamic material properties, fluid-flow, radiation and vaporization) which can either be included or neglected in a continuum finite volume model (FVM) and their effect on the solidification conditions. Additionally, since the simplest form of such a model (conduction only) has an analytic solution which is much faster, its viability is also considered. Since the inclusion of some of these physical phenomena will inherently change the net energy input as well as the amount of energy needed to achieve melting of a control volume, each set of included phenomena had an effective absorption efficiency which was calibrated to closely match the dimensions of the melt pool to that of the ground truth data. The ground truth data for this study was defined to be the output of the FVM which included all the physical phenomena (OF). This study then goes on to compare the effects on solidification conditions each of these calibrated models has. It was found that most of the change in solidification conditions comes from the inclusion of latent heat. A posterior correlation factor (PCF) is then introduced to enable an analytic model to predict similar solidification conditions to OF model.

36 MATERIALS SCIENCE↗

Numerical Research on Magnetic Field, Temperature Field and Flow Field During Melting and Directionally Solidifying TiAl Alloys by Electromagnetic Cold Crucible

The electromagnetic cold crucible (EMCC) technique is an effective method to melt and directionally solidify reactive and high-temperature materials without contamination. The temperature field and fluid flow induced by the electromagnetic field are very important for melting and controlling the microstructure. In this article, a 3D EMCC model for calculating the magnetic field in the charges (TiAl alloys) using the T-Ω finite element method was established and verified. Magnetic fields in the charge under different electrical parameters, positions and dimensions of the charge were calculated and analyzed. The calculated results show that the magnetic field concentrates in the skin layer, and the magnetic flux density (B) increases with increasing of the frequency, charge diameter and current. The maximum B in the charge is affected by the position of the charge in EMCC (h{sub 1}) and the charge height (h{sub 2}), which emerges at the middle of coils (h{sub c}) when the relationship of h{sub c} < h{sub 1} + h{sub 2} < h{sub c} + δ is satisfied. Lower frequency and smaller charge diameter can improve the uniformity of the magnetic field in the charge. Consequently, the induced uniform electromagnetic stirring weakens the turbulence and improves temperature uniformity in the vicinity of the solid/liquid (S/L) interface, which is beneficial to forming a planar S/L interface during directional solidification. Based on the above conclusions, the TiAlNb alloy was successfully melted with lower power consumption and directionally solidified by the square EMCC.

36 MATERIALS SCIENCE↗

Characterization of the Interface of an Alloy 625 Overlay on Steels Using Nanoindentation

Industry standards require postweld heat treatment (PWHT) to reduce the heat-affected zone hardness of steels such as F22 (2.25Cr-1Mo) and AISI 8630 overlaid (clad) with Alloy 625 weld metal. PWHT results in carbon diffusion and accumulation at the interface between the steel and overlay. The accumulation of carbon in a planar solidification growth zone adjacent to the fusion boundary results in high hardness and the potential for hydrogen-assisted cracking. The planar growth zone (PGZ) is so narrow that normal Vickers hardness testing cannot fully reveal the hardness distribution in this zone. This study focused on the application of nanoindentation to characterize the hardness in the narrow microstructural regions adjacent to the fusion boundary. The development of nanohardness maps revealed that the PGZ is not necessarily the region that exhibits peak hardness after PWHT. The highest hardness values were associated with clusters of M{sub 7}C{sub 3} carbides in specific subregions in the PGZ and also in the partially-mixed zone adjacent to the fusion boundary or in steel “swirl” structures. It was also confirmed in this study that nanohardness has a linear correlation with Vickers hardness values. The results presented here provide new insight into the role of carbon diffusion during PWHT and its effect on interface embrittlement associated with Alloy 625 overlays on steel.

36 MATERIALS SCIENCE↗

Influence of Powder Characteristics and Processing Methods on Creep Performance of Powder Metallurgy Hot Isostatic Pressed SS316

The U.S. nuclear energy expansion goals are driving the demand for manufacturing routes that can rapidly produce large, complex, near net shape components. Powder metallurgy hot isostatic pressing (PM HIP) is an advanced manufacturing technique that can be economically scaled-up, while alleviating the supply chain challenges that forging and casting face in terms of cost and lead time constraints. This makes PM-HIP a viable technology to aid and accelerate large-scale part manufacturing for nuclear applications. However, large-scale qualification and deployment of this technology require a thorough understanding of the influence of powder feedstock quality, powder handling history, hot isostatic pressing (HIP) parameters, and subsequent heat treatment on microstructural evolution and elevated temperature mechanical performance. The present work focusses on 316 austenitic stainless steel (SS316) which is most commonly used in high temperature environments for nuclear applications Results from this study show that PM HIPed SS316 meets ASME tensile requirements at room temperature and at elevated temperature. However, creep performance of PM-HIPed SS316 remains inferior to its wrought counterpart, demonstrating that tensile performance alone is not a reliable metric for long duration high temperature integrity. Further, this report delineates powder derived microstructural features that govern creep damage, with key evidences pointing to “microstructural inheritance” from gas atomized powder feedstocks. Commercial SS316 powders of varying chemical compositions and recycling histories were studies, and the results showed large differences in elemental segregation, oxide surface layers and secondary phase distributions. Multi-scale characterization revealed segregation of chromium, molybdenum, manganese and silicon at the boundaries and the precipitation of manganese-, silicon-, and molybdenum-oxides. During HIP consolidation, these surface oxides transform into decorated prior particle boundaries (PPBs) and grain boundary inclusions that persist through conventional post-HIP solution annealing treatment. The retained oxides in post-HIP microstructures were found to influence grain growth, precipitation behavior, and ultimately creep cavitation and fracture. Such post-HIP heat treatments are therefore limited by a complex trade-off between grain growth, and oxide coarsening which aggravate creep damage by acting as nucleation sites for cavities. The objective of this work is to establish an integrated processing–structure–property framework for PM-HIP 316 stainless steel by investigating the influence of powder feedstock characteristics in pre- and post-HIP processing as well as to understand the significance of post-HIP heat treatment on microstructural evolution and creep properties. The results from this report emphasize the significance of powder feedstock integrity in improving creep performance of PM-HIPed SS316, by highlight the effect of rapid solidification, elemental segregation, oxide formation and powder recycling on microstructural defect inheritance following HIP consolidation. Rather than considering HIP processing, solution annealing, and mechanical performance independently, this report treats powder production, HIP consolidation, post-HIP thermal processing, and creep deformation as interconnected stages within a continuous metallurgical process. The resulting framework will provide a scientific basis for developing feedstock engineering strategies capable of improving long-term reliability of PM-HIP stainless steels and accelerating their qualification for advanced nuclear applications.

Ajjarapu, Pavan [Oak Ridge National Laboratory (OR↗

Microstructural development and mechanical properties of a near-eutectic directionally solidified Sn–Bi solder alloy

Sn–Bi solders may be applied for electronic applications where low-temperature soldering is required, i.e., sensitive components, step soldering and soldering LEDs. In spite of their potential to cover such applications, the mechanical response of soldered joints of Sn–Bi alloys in some cases does not meet the strength requirements due to inappropriate resulting microstructures. Hence, careful examination and control of as-soldered microstructures become necessary with a view to pre-programming reliable final properties. The present study aims to investigate the effects of solidification thermal parameters (growth rate — V{sub L} and cooling rate — T-dot{sub L}) on the microstructure of the Sn–52 wt.%Bi solder solidified under unsteady-state conditions. Samples were obtained by upward directional solidification (DS), followed by characterization through metallography and scanning electron microscopy (SEM). The microstructures are shown to be formed by Sn-rich dendrites decorated with Bi precipitates surrounded by a complex regular eutectic mixture, with alternated Bi-rich and Sn-rich phases. Experimental correlations of primary (λ{sub 1}), secondary (λ{sub 2}), tertiary (λ{sub 3}) dendritic and eutectic spacings (λ{sub coarse} and λ{sub fine}) with cooling rate and growth rate are established. Two ranges of lamellar eutectic sizes were determined, described by two experimental equations λ = 1.1 V{sub L}{sup −1/2} and λ = 0.67 V{sub L}{sup −1/2}. The onset of tertiary branches within the dendritic array along the Sn–52 wt.%Bi alloy DS casting is shown to occur for cooling rates lower than 1.5 °C/s. - Highlights: • The Sn–52 wt.%Bi solder was shown to have two eutectic sizes. • The fishbone eutectic is preferably located adjacent to the Bi-rich lamellar phases. • The onset of tertiary dendritic branches in Sn–Bi is associated with T-dot{sub L} < 1.5 °C/s. • Higher eutectic fraction and λ{sub 3} provoked a reverse increase in σ{sub u} and σ{sub y}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Multiscale Modeling of Microstructural Evolution in Fused-Coating Additive Manufacturing

A quantitative phase field model with adaptive-computational-domain-expansion (ACDE) method was developed to simulate the microstructural evolution in fused-coating additive manufacturing process. A heat transfer and fluid flow model was established to investigate the solidification behavior of the molten pool in a single deposited layer. The solidification parameters such as temperature gradient and solidification rate were calculated from the macroscopic model and then fed into the phase field model to get the microstructure at different positions within a single deposited layer. Columnar dendrites were formed at the bottom of the deposited layer, and equiaxed dendrites appeared in the upper part of the layer. The ACDE method is used to improve the simulation efficiency. The metallographic experiments and energy-dispersive spectrometer analysis for composition were conducted on the fused-coating specimen, and the results were in good accordance with the simulations.

36 MATERIALS SCIENCE↗

Fracture toughness and corrosion resistance of semisolid AlSi5 alloy

The aim of this work was to investigate fracture toughness and corrosion resistance of semisolid AlSi5 castings, compared to samples obtained from conventional casting operations. In order to have a semisolid microstructure, the melt alloy was treated by means of ultrasound during solidification and then poured into permanent moulds. Mechanical properties of semisolid and conventional castings were compared by means of ultimate tensile strength (R{sub m}), yield stress (Rp{sub 02}) and hardness (HV) measurements. Fracture mechanics tests were carried out on Single Edge Notched Bend (SENB) specimens, machined from castings, and pre-cracked by fatigue. These tests were performed to determine the effect of the microstructure on the J-Integral resistance (J-R) behavior and to deeply understand the ductile fracture behaviour of semisolid parts. The J-Integral versus spaced crack extension (J-{Delta}a) curves showed an improved resistance of the semisolid microstructure, due to the higher ductility. Finally, the corrosion behaviour of semisolid samples was compared to that of castings coming from solidification of fully liquid alloy by means of electrochemical potentiodynamic polarization tests. It was observed that the globular microstructure offers better quality, in terms of higher mechanical properties, as a consequence of a more uniform distribution of the solute.

36 MATERIALS SCIENCE↗

Effect of process parameters on hardness, temperature profile and solidification of different layers processed by direct metal laser sintering (DMLS)

In DMLS process objects are fabricated layer by layer from powdered material by melting induced by a controlled laser beam. Metallic powder melts and solidifies to form a single layer. Solidification map during layer formation is an important route to characterize micro-structure and grain morphology of sintered layer. Generally, solidification leads to columnar, equiaxed or mixture of these two types grain morphology depending on solidification rate and thermal gradient. Eutectic or dendritic structure can be formed in fully equiaxed zone. This dendritic growth has a large effect on material properties. Smaller dendrites generally increase ductility of the layer. Thus, materials can be designed by creating desired grain morphology in certain regions using DMLS process. To accomplish this, hardness, temperature distribution, thermal gradient and solidification cooling rate in processed layers will be studied under change of process variables by using finite element analysis, with specific application to Ti-6Al-4V.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Phase-field investigation on the non-equilibrium interface dynamics of rapid alloy solidification

The research program reported here is focused on critical issues that represent conspicuous gaps in current understanding of rapid solidification, limiting our ability to predict and control microstructural evolution (i.e. morphological dynamics and microsegregation) at high undercooling, where conditions depart significantly from local equilibrium. More specifically, through careful application of phase-field modeling, using appropriate thin-interface and anti-trapping corrections and addressing important details such as transient effects and a velocity-dependent (i.e. adaptive) numerics, the current analysis provides a reasonable simulation-based picture of non-equilibrium solute partitioning and the corresponding oscillatory dynamics associated with single-phase rapid solidification and show that this method is a suitable means for a self-consistent simulation of transient behavior and operating point selection under rapid growth conditions. Moving beyond the limitations of conventional theoretical/analytical treatments of non-equilibrium solute partitioning, these results serve to substantiate recent experimental findings and analytical treatments for single-phase rapid solidification. The departure from the equilibrium solid concentration at the solid-liquid interface was often observed during rapid solidification, and the energetic associated non-equilibrium solute partitioning has been treated in detail, providing possible ranges of interface concentrations for a given growth condition. Use of these treatments for analytical description of specific single-phase dendritic and cellular operating point selection, however, requires a model for solute partitioning under a given set of growth conditions. Therefore, analytical solute trapping models which describe the chemical partitioning as a function of steady state interface velocities have been developed and widely utilized in most of the theoretical investigations of rapid solidification. However, these solute trapping models are not rigorously verified due to the difficulty in experimentally measuring under rapid growth conditions. Moreover, since these solute trapping models include kinetic parameters which are difficult to directly measure from experiments, application of the solute trapping models or the associated analytic rapid solidification model is limited. These theoretical models for steady state rapid solidification which incorporate the solute trapping models do not describe the interdependency of solute diffusion, interface kinetics, and alloy thermodynamics. The phase-field approach allows calculating, spontaneously, the non-equilibrium growth effects of alloys and the associated time-dependent growth dynamics, without making the assumptions that solute partitioning is an explicit function of velocity, as is the current convention. In the research described here, by utilizing the phase-field model in the thin-interface limit, incorporating the anti-trapping current term, more quantitatively valid interface kinetics and solute diffusion across the interface are calculated. In order to sufficiently resolve the physical length scales (i.e. interface thickness and diffusion boundary length), grid spacings are continually adjusted in calculations. The full trajectories of transient planar growth dynamics under rapid directional solidification conditions with different pulling velocities are described. As a validation of a model, the predicted steady state conditions are consistent with the analytic approach for rapid growth. It was confirmed that rapid interface dynamics exhibits the abrupt acceleration of the planar front when the effect of the non-equilibrium solute partitioning at the interface becomes signi ficant. This is consistent with the previous linear stability analysis for the non-equilibrium interface dynamics. With an appropriate growth condition, the continuous oscillation dynamics was able to be simulated using continually adjusting grid spacings. This oscillatory dynamics including instantaneous jump of interface velocities are consistent with a previous phenomenological model by and a numerical investigation, which may cause the formation of banded structures. Additionally, the selection of the steady state growth dynamics in the highly undercooled melt is demonstrated. The transition of the growth morphology, interface velocity selection, and solute trapping phenomenon with increasing melt supersaturations was described by the phase-field simulation. The tip selection for the dendritic growth was consistent with Ivantsov's function, and the non-equilibrium chemical partitioning behavior shows good qualitative agreement with the Aziz's solute trapping model even though the model parameter(V D ) remains as an arbitrary constant. This work is able to show the possibility of comprehensive description of rapid alloy growth over the entire time-dependent non-equilibrium phenomenon.

36 MATERIALS SCIENCE↗