At least 271 records · Page 15

Evaluation of a thermoplastic polyimide (422) for bonding GR/PI composite

A hot-melt processable copolyimide previously studied and characterized as an adhesive for bonding Ti-6Al-4V was used to bond Celion 6000/LARC-160 composite. Comparisons are made for the two adherend systems. A bonding cycle was determined for the composite bonding and lap shear specimens were prepared which were thermally exposed in a forced-air oven for up to 5000 h at 204 C. The lap shear strengths (LSSs) were determined at RT, 177, and 204 C. After thermal exposure at RT, 177, and 204 C the LSS decreased significantly; however, a slight increase was noted for the 204 C tests. Initially the LSS values are higher for the bonded Ti-6Al-4V than for the bonded composite, however, the LSS decreases dramatically between 5000 and 10,000 h of 204 C thermal exposure. Longer periods of thermal exposure up to 20,000 h results in further decreases in the LSSs. Although the bonded composite retained useful strengths for exposures up to 5000 h, based on the poor results of the bonded Ti-6Al-4V beyond 5000 h, the 422 adhesive bonded composites would most likely also produce poor strengths beyond 5000 h exposure. Adhesive bonded composite lap shear specimens exposed to boiling water for 72 h exhibited greatly reduced strengths at all test temperatures. The percent retained after water boil for each test temperature was essentially the same for both systems.

Progar, Donald J.↗

A study of thermal transitions in a new semicrystalline thermoplastic polyimide

A polyimide derive from 4,4'-isophthaloyl diphthalic anhydride (IDPA) and 1,3-bis (4-aminophenoxy 4'-benzoyl) benzene (1,3-BABB) having semicrystalline behavior was prepared and characterized by differential scanning calorimetry (DSC) and wide angle X-ray scattering (WAXS). Thus a poly(amic acid) film cured in air for one hour each at 100 and 200 C displayed an endotherm at 286 C, followed by a crystallization exotherm at 317 C, and a second melting transition at 350 C. The 286 C melting point appeared to result from earlier solvent-induced crystallization. Films cast from DMAc, air dried, and soaked in methylene chloride could not be induced into semicrystallinity. The fully cured polyimide has a Tg of 216 C. Films heated to temperatures as high as 100 C for one hour in air were transparent and light yellow in color. Those films heated to or above 125 C were translucent. Polarized light microscopy revealed the presence of spherulites 608 micrometers in diameter in a sample cured to 275 C in air. Two film samples, one cured to 275 and the other to 325 C, were evaluated for tensile and ultimate strength, modulus, and percent elongation at 25 and 200 C. These values remained essentially constant at each test temperature.

Pratt, J. Richard↗

Evaluation of a thermoplastic polyimide (422) for bonding GR/PI composite

A hot-melt processable copolyimide previously studied and characterized as an adhesive for bonding Ti-6Al-4V was used to bond Celion 6000/LARC-160 composite. Comparisons are made for the two adherend systems. A bonding cycle was determined for the composite bonding and lap shear specimens were prepared which were thermally exposed in a forced-air oven for up to 5000 h at 204 C. The lap shear strengths (LSSs) were determined at RT, 177, and 204 C. After thermal exposure at RT, 177, and 204 C the LSS decreased significantly; however, a slight increase was noted for the 204 C tests. Initially the LSS values are higher for the bonded Ti-6Al-4V than for the bonded composite, however, the LSS decreases dramatically between 5000 and 10,000 h of 204 C thermal exposure. Longer periods of thermal exposure up to 20,000 h results in further decreases in the LSSs. Although the bonded composite retained useful strengths for exposures up to 5000 h, based on the por results of the bonded Ti-6Al-4V beyond 5000 h, the 422 adhesive bonded composites would most likely also produce poor strengths beyond 5000 h exposure. Adhesive bonded composite lap shear specimens exposed to boiling water for 72 h exhibited greatly reduced strengths at all test temperatures. The percent retained after water boil for each test temperature was essentially the same for both systems.

Progar, Donald J.↗

The effect of processing on autohesive strength development in thermoplastic resins and composites

In the present investigation of processing effects on the autohesive bond strength of neat polysulfone resin and graphite-reinforced polysulfone-matrix composites measured resin bond strength development in precracked compact tension specimens 'healed' by heating over a contact period at a given temperature. The critical strain energy release rate of refractured composite specimens did not exhibit the strong time or temperature dependence of the neat resin tests; only 80-90 percent of the undamaged fracture energy is recoverable.

Howes, Jeremy C.↗

Damage induced constitutive response of a thermoplastic related to composites and adhesive bonding

The volume-averaged constitutive behavior of a polymer sustaining void growth under dilational deformation is addressed. Polyvinylacetate is deformed between two aluminum beams in a double cantilever geometry and the deformations, recorded with the aid of optical interferometry, are used to deduce the stress-strain behavior of the material as it passes from small strain behavior, through the voiding process, to near-failure under exclusion of rate-sensitivity considerations.

Parvin, M.↗

Interface effects in interlaminar fracture of thermoplastic composites

Mode I interlaminar fracture toughness was determined on a series of unidirectional poly(phenylene oxide)/carbon fiber composites using the double cantilever beam test. Initial toughness for growth of a delamination from an insert depends on fiber type, and ranges from 190 to 440 J/sq m, with intermediate modulus fibers tending to give lower values than high-strain fibers. Low toughness values are attributed to poor fiber-matrix adhesion. As a delamination progress down the beam, fiber bridging increases the apparent toughness by up to a factor of 7, depending on the fiber.

Hinkley, J. A.↗

Additives to reduce susceptibility of thermosets and thermoplastics to erosion from atomic oxygen

Polymeric materials have many attractive features such as light weight, high strength, and broad applicability in the form of films, fibers, and molded objects. In low earth orbit (LEO), these materials, when exposed on the exterior of the spacecraft, have the serious disadvantage of being susceptible to erosion by atomic oxygen (AO). AO is the most common chemical species at LEO altitudes. AO can be an extremely efficient oxidizing agent as was apparent from the extensive erosion of organic films exposed in STS missions. The mechanism for erosion involves the reaction of oxygen atoms at the surface of the substrate to form small molecular species. The susceptibility of polymeric materials varies with their chemical composition. Films with silicon atoms incorporated in the molecular structures have large coefficients of thermal expansion. This limits their utility. In an alternative approach additives were sought that mix physically and form a protective oxide layer when the film is exposed to AO. A large number of organic compounds containing silicon, germanium, or tin atoms were screened. Most were found to have very limited solubility in the polyetherimide (Ultem) films that were being protected from AO. However, one, bis(triphenyl tin) oxide, (BTO), is miscible in Ultem up to about 25 percent. Films of Ultem polyimide containing up to 25 wt percent BTO were prepared by evaporation of solvent from a solution of Ultem and BTO. The effects of AO on these films were simulated in the oxygen atmosphere of a radio frequency glow-discharge chamber. In the second part of this study, atoms were incorporated in epoxy resins. Experiments are in progress to measure the resistance of films of the cured epoxy to AO in the discharge chamber.

Orwoll, Robert A.↗

Thermoplastic coating of carbon fibers

Using a continuous powder coating process, more than 1500 meters of T 300/LaRC-TPI prepreg were produced. Two different types of heating sections in the coating line, namely electrical resistance and convection heating, were utilized. These prepregs were used to fabricate unidirectional composites. During composite fabrication the cure time of the consolidation was varied, and composites samples were produced with and without vacuum. Under these specimens, the effects of the different heating sections and of the variation of the consolidation parameters on mechanical properties and void content were investigated. The void fractions of the various composites were determined from density measurements, and the mechanical properties were measured by tensile testing, short beam shear testing and dynamic mechanical analysis.

Edie, D. D.↗

Advanced thermoplastic resins, phase 2

High temperature structural resins are required for use on advanced aerospace vehicles as adhesives and composite matrices. NASA-Langley developed polyimide resins were evaluated as high temperature structural adhesives for metal to metal bonding and as composite matrices. Adhesive tapes were prepared on glass scrim fabric from solutions of polyamide acids of the semicrystalline polyimide LARC-CPI, developed at the NASA-Langley Research Center. Using 6Al-4V titanium adherends, high lap shear bond strengths were obtained at ambient temperature (45.2 MPa, 6550 psi) and acceptable strengths were obtained at elevated temperature (14.0 MPa, 2030 psi) using the Pasa-Jell 107 conversion coating on the titanium and a bonding pressure of 1.38 MPa (200 psi). Average zero degree composite tensile and compressive strengths of 1290 MPa (187 ksi) and 883 MPa (128 ksi) respectively were obtained at ambient temperature with unsized AS-4 carbon fiber reinforcement.

Brown, A. M.↗

The development of an alternative thermoplastic powder prepregging technique

Discussed is a novel powder prepregging technique that is based on the deposition of the powder onto fibers that have been moistened using an ultrasonic humidifier. The moisture acts as an initial binding agent for the powder until the powder can be melted onto the fiber in a subsequent heating step. LaRC-TPI powder, produced by Mitsui Toastsu, and Hercules AS-4 fiber served as the process development material system. The influence of powder particle size on this process, and the quality of the resulting composite are discussed.

Ogden, A. L.↗

Effects of fiber and interfacial layer architectures on the thermoplastic response of metal matrix composites

Examined here is the effect of fiber and interfacial layer morphologies on thermal fields in metal matrix composites (MMCs). A micromechanics model based on an arbitrarily layered concentric cylinder configuration is used to calculate thermal stress fields in MMCs subjected to spatially uniform temperature changes. The fiber is modelled as a layered material with isotropic or orthotropic elastic layers, whereas the surrounding matrix, including interfacial layers, is treated as a strain-hardening, elastoplastic, von Mises solid with temperature-dependent parameters. The solution to the boundary-value problem of an arbitrarily layered concentric cylinder under the prescribed thermal loading is obtained using the local/global stiffness matrix formulation originally developed for stress analysis of multilayered elastic media. Examples are provided that illustrate how the morphology of the SCS6 silicon carbide fiber and the use of multiple compliant layers at the fiber/matrix interface affect the evolution of residual stresses in SiC/Ti composites during fabrication cool-down.

Pindera, Marek-Jerzy↗

The synthesis of monomers with pendent ethynyl group for modified high performance thermoplastics

The objectives of this project were to develop synthetic schemes for the following classes of modified monomers: (1) difunctional triarylethanes with pendent acetylenic groups; and (2) tertiary aspartimides with terminal acetylene groups at the two ends. Our efforts have resulted in the successful development of high yield schemes for the syntheses of several diamino and bisphenolic analogs of difunctional triarylethanes with pendent ethynyl group. A scheme for one new tertiary aspartimide was also established. Multi-gram samples of all prepared new monomers were provided to our technical contact at NASA-LaRC and preliminary polymerization studies were encouraging. Details of the accomplished work within the last four years are described.

Nwokogu, Godson C.↗

Environmental effects on the compressive properties - Thermosetting vs. thermoplastic composites

The influence of moisture and temperature on the compressive properties of graphite/epoxy and APC-2 materials systems was investigated to assess the viability of using APC-2 instead of graphite/epoxy. Data obtained indicate that the moisture absorption rate of T-300/epoxy is higher than that of APC-2. Thick plate with smaller surface area absorbs less moisture than thin plate with larger surface area. The compressive strength and modulus of APC-2 are higher than those of T-300/epoxy composite, and APC-2 sustains higher compressive strength in the presence of moisture. The compressive strength and modulus decrease with the increase of temperature in the range of 23-100 C. The compression failure was in the form of delamination, interlaminar shear, and end brooming.

Haque, A.↗

Continuous fiber thermoplastic prepreg

A pultrusion machine employing a corrugated impregnator vessel to immerse multiple, continuous strand, fiber tow in an impregnating material, and an adjustable metered exit orifice for the impregnator vessel to control the quantity of impregnating material retained by the impregnated fibers, is provided. An adjustable height insert retains transverse rod elements within each depression of the corrugated vessel to maintain the individual fiber tows spread and in contact with the vessel bottom. A series of elongated heating dies, transversely disposed on the pultrusion machine and having flat heating surfaces with radiused edges, ensure adequate temperature exposed dwell time and exert adequate pressure on the impregnated fiber tows, to provide the desired thickness and fiber/resin ratio in the prepreg formed. The prepreg passing through the pulling mechanism is wound on a suitable take-up spool for subsequent use. A formula is derived for determining the cross sectional area opening of the metering device. A modification in the heating die system employs a heated nip roller in lieu of one of the pressure applying flat dies.

Wilson, Maywood L.↗

An analytical/numerical correlation study of the multiple concentric cylinder model for the thermoplastic response of metal matrix composites

The utility of a recently developed analytical micromechanics model for the response of metal matrix composites under thermal loading is illustrated by comparison with the results generated using the finite-element approach. The model is based on the concentric cylinder assemblage consisting of an arbitrary number of elastic or elastoplastic sublayers with isotropic or orthotropic, temperature-dependent properties. The elastoplastic boundary-value problem of an arbitrarily layered concentric cylinder is solved using the local/global stiffness matrix formulation (originally developed for elastic layered media) and Mendelson's iterative technique of successive elastic solutions. These features of the model facilitate efficient investigation of the effects of various microstructural details, such as functionally graded architectures of interfacial layers, on the evolution of residual stresses during cool down. The available closed-form expressions for the field variables can readily be incorporated into an optimization algorithm in order to efficiently identify optimal configurations of graded interfaces for given applications. Comparison of residual stress distributions after cool down generated using finite-element analysis and the present micromechanics model for four composite systems with substantially different temperature-dependent elastic, plastic, and thermal properties illustrates the efficacy of the developed analytical scheme.

Pindera, Marek-Jerzy↗

The synthesis of monomers with pendent ethynyl groups for modified high performance thermoplastics

Synthetic schemes were developed and optimized for twelve new monomers possessing unique structural features and one aspartimide. Two synthetic pathways were compared for preparation of the triarylethane monomers with pendent ethynyl groups. The results show that one of these pathways can be generally applied. The alternative pathway was applicable to the preparation of only one of the twelve compounds, the problem being secondary reactions of the initially formed desired product.

Nwokogu, Godson C.↗

On the thermally-induced residual stresses in thick fiber-thermoplastic matrix (PEEK) cross-ply laminated plates

An analytical method for calculating thermally-induced residual stresses in laminated plates is applied to cross-ply PEEK laminates. We considered three cooling procedures: slow cooling (uniform temperature distribution); convective and radiative cooling; and rapid cooling by quenching (constant surface temperature). Some of the calculated stresses are of sufficient magnitude to effect failure properties such as matrix microcracking.

Hu, Shoufeng↗

Mechanical characterization of two thermoplastic composites fabricated by automated tow placement

AS4/PEEK towpreg and IM7/Radel 8320 slit tape were used to make flat panels by automated tow placement. The panels were tested in notched and un-notched tension, notched and un-notched compression and compression after impact (CAI) at room temperature and under hot/wet conditions (notched and un-notched compression and CAI only). The properties were compared with AS4/PEEK tape laminate properties found in the literature. The tow placed AS4/PEEK material was stronger in tension but weaker in compression than the AS4/PEEK tape laminates. The tow placed AS4/PEEK was stronger but less stiff than the tow placed IM7/Radel 8320 in all compression tests. The IM7/Radel performed better in all other mechanical tests. The IM7/Radel outperformed the AS4/PEEK in all CAI tests.

Dickinson, Larry C.↗