Search NASA⌕ Search

SEARCH · Search NASA

Results for “fracture toughness”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Hydrogen-assisted fracture resistance of pipeline welds in gaseous hydrogen

Fracture resistance of pipeline welds from a range of strength grades and welding techniques was measured in air and 21 MPa hydrogen gas, including electric resistance weld of X52, friction stir weld of X100 and gas metal arc welds (GMAW) of X52, X65 and X100. Welds exhibited a decrease in fracture resistance in hydrogen compared to complementary tests in air. A general trend was observed that fracture resistance in 21 MPa hydrogen gas decreased with increasing yield strength. To accommodate material constraints, two different fracture coupon geometries were used in this study, which were shown to yield similar fracture resistance values in air and 21 MPa hydrogen gas; values using different coupons resulted in less than 15% difference. In addition, fracture coupons were removed from controlled locations in select welds to examine the potential influence of orientation and residual stress. The two orientations examined in the X100 GMAW exhibited negligible differences in fracture resistance in air and, similarly, negligible differences in hydrogen. Residual stress exhibited a modest influence on fracture resistance; however, a consistent trend was not observed between tests in air and hydrogen, suggesting further studies are necessary to better understand the influence of residual stress. A comparison of welds and base metals tested in hydrogen gas showed similar susceptibility to hydrogen-assisted fracture. The overall dominant factor in determining the susceptibility to fracture resistance in hydrogen is the yield strength.

08 HYDROGEN↗

Accelerated Self-Healing and Property Recovery in Brush Particle Solids Featuring Brush Dispersity

Brush particles, hybrid materials consisting of polymer chains tethered to particle surfaces, offer tunable properties that make them promising candidates for advanced functional materials. This study investigated the role of chain dispersity in the viscoelastic self-healing of poly (methyl acrylate) (PMA)-based brush particle solids. Increasing the molecular weight dispersity of grafted chains significantly enhanced both strain-to-fracture and toughness of brush particle solids, while the elastic modulus and glass transition temperature were independent of chain dispersity. Cut-and-adhere testing revealed a significant acceleration of the rate of toughness recovery in high-dispersity systems as compared to low-dispersity analogs for which toughness recovery markedly lagged the recovery of Young’s modulus. The results suggest that structure and property recovery in brush particle solids are sensitive to the dynamical heterogeneity of brush canopies and highlight the role of molecular weight dispersity as a design parameter to enable hybrid materials with advanced self-healing ability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Irradiation and PIE of alloys X-750 and XM-19 (EPRI Phase III)

The Nuclear Science User Facilities (NSUF) based at Idaho National Laboratory (INL), along with the Electric Power Research Institute (EPRI), formed an agreement to test representative alloys used as reactor structural materials as a pilot program to establish guidelines for future NSUF research programs. This report contains results from the portion of this program established as Phase III (of three phases), entailing irradiation and post-irradiation examination of select alloys typical of boiling water reactor (BWR) internal structural materials. Phases I and II are the subject of separate reports and represent baseline material test results and irradiation experiment design, respectively. The intent of this Phase III research program is to determine properties for the materials of interest after being irradiated at the Advanced Test Reactor (ATR) to three different target fast (E>1MeV) fluences: 5.0 x 10¹⁹ n/cm², 2.0 x 10²⁰ n/cm², and 1.0 x 10²¹ n/cm². These correspond to irradiation damage levels (displacements per atom [dpa]) of approximately 0.08, 0.30, and 1.4 dpa, which represent comparable levels to (a) a previous study which looked at X-750 irradiated to ~1 x 10¹⁹ n/cm², comparable to the lowest fluence; (b) approximately a medium level of fluence for BWR components; and (c) extended life (60 – 80 years) for BWR components. The materials chosen for this research are the nickel-based alloy X-750 and austenitic stainless steel XM-19. A spare core shroud upper support bracket of alloy X-750 was purchased by EPRI from Southern Co., and a section of XM-19 plate was purchased by EPRI from GE-Hitachi. These materials were sectioned at GE Global Research Center (GE-GRC), and parts were provided to INL for use in this pilot project.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Irradiation and PIE of alloys X-750 and XM-19 (EPRI Phase III)

The Nuclear Science User Facilities (NSUF) based at Idaho National Laboratory (INL), along with the Electric Power Research Institute (EPRI), formed an agreement to test representative alloys used as reactor structural materials as a pilot program to establish guidelines for future NSUF research programs. This report contains results from the portion of this program established as Phase III (of three phases), entailing irradiation and post-irradiation examination of select alloys typical of boiling water reactor (BWR) internal structural materials. Phases I and II are the subject of separate reports and represent baseline material test results and irradiation experiment design, respectively. The intent of this Phase III research program is to determine properties for the materials of interest after being irradiated at the Advanced Test Reactor (ATR) to three different target fast (E>1MeV) fluences: 5.0 x 10¹⁹ n/cm², 2.0 x 10²⁰ n/cm², and 1.0 x 10²¹ n/cm². These correspond to irradiation damage levels (displacements per atom [dpa]) of approximately 0.08, 0.30, and 1.4 dpa, which represent comparable levels to (a) a previous study which looked at X-750 irradiated to ~1 x 10¹⁹ n/cm², comparable to the lowest fluence; (b) approximately a medium level of fluence for BWR components; and (c) extended life (60 – 80 years) for BWR components. The materials chosen for this research are the nickel-based alloy X-750 and austenitic stainless steel XM-19. A spare core shroud upper support bracket of alloy X-750 was purchased by EPRI from Southern Co., and a section of XM-19 plate was purchased by EPRI from GE-Hitachi. These materials were sectioned at GE Global Research Center (GE-GRC), and parts were provided to INL for use in this pilot project.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Evolution of the role of molybdenum in duplex stainless steels during thermal aging: From enhancing spinodal decomposition to forming heterogeneous precipitates

Thermal aging of ferrite in duplex stainless steels leads to a complex microstructural evolution that can give way to large deleterious changes in mechanical properties. The microstructural evolution mechanisms that happen concurrently are strongly linked to minor changes in composition. By characterizing duplex stainless steels with various compositions over a range of aging conditions, it was revealed that adding a modest amount of Mo to cast austenitic stainless steel (such as changing from grade CF3 to grade CF3M) not only increases the kinetics of spinodal decomposition and Ni-Si-Mn-rich G-phase precipitation, but it also forms a separate Mo-rich phase. At shorter equivalent aging times, Mo segregates from Fe and towards Cr accelerating spinodal decomposition. At longer aging times, Mo enriches in the Ni-Si-Mn clusters before phase separating into an adjoined Mo-rich cluster. We found that these phase changes and precipitation events result in a rather steep drop in fracture and impact toughness. These results will inform the design of similar alloys for use at high temperatures.

36 MATERIALS SCIENCE↗

A Dual Approach in Direct Ink Writing of Thermally Cured Shape Memory Rubber Toughened Epoxy

Bisphenol A-based epoxies are much used in a wide range of composite and coating applications due to their excellent thermomechanical properties. However, their 3D printability remains a challenge with most reported materials suffering from high brittleness and low toughness. In this work, we have described especially modified epoxy resins that enable 3D printing with both fast and slow curing rates. These materials exhibit greatly enhanced toughness, tunable thermomechanical properties, and excellent shape memory behavior. Two different printing systems, including a two-part static mixing printhead and a single extrusion printhead, were developed for fast- and slow-curing epoxies, respectively. The rheology of inks in both systems has been modified into printable thixotropic fluids with the aid of silica nanoparticles and other additives. Epoxide-functionalized telechelic polybutadiene was added into the resins, which are then introduced inside the epoxy network after cross-linking. The addition of polybutadiene rubber significantly improves the toughness (over 135%), fracture strain (over 200%), and shape memory behavior. By adding different amounts of the rubber telechelic, thermomechanical properties, including modulus, elongation, and Tg of epoxy, can be well controlled in a wide range to satisfy different applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dynamic Bottlebrush Polymer Networks: Self-Healing in Super-Soft Materials

Here, we introduce a design strategy to expand the range of accessible mechanical properties in covalent adaptable networks (CANs) using bottlebrush polymer building blocks. Well-defined bottlebrush polymers with rubbery poly(4-methylcaprolactone) side-chains were crosslinked in formulations that include a bislactone and strong Lewis acid (tin ethylhexanoate). The resulting materials exhibit tunable stress relaxation rates at elevated temperatures (160–180 °C) due to dynamic ester crosslinks that undergo transesterification with residual hydroxy groups. Varying the crosslinker loading or bottlebrush backbone degree of polymerization yields predictable low-frequency shear moduli ca. 10–100 kPa, well below values typical of linear polymer CANs (1 MPa). These extensible networks can be stretched to strains as large as 350% before failure and undergo efficient self-healing to recover >85% of their original toughness upon repeated fracture and melt processing. In summary, molecular architecture creates new opportunities to tailor the mechanical properties of CANs in ways that are otherwise difficult to achieve.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Toughening of interface networks through the introduction of weak links

The resistance of polycrystalline materials to intergranular fracture depends on the toughness of the interfaces between neighboring grains. Using finite element simulations on model, two-dimensional microstructures, we demonstrate that the steady-state crack growth resistance of a polycrystal that contains exclusively high toughness interfaces is suboptimal: its crack growth resistance may be increased by introducing a minority fraction of weak interfaces at random locations within the interface network. Furthermore, the weaker are these interfaces, the greater is their toughening effect. These weak interfaces toughen the material through crack deflection and branching, nucleation of secondary cracks, and inelastic dissipation within intact interfaces. Furthermore, our findings suggest that fracture resistance-oriented material development should not aim to eliminate all weak interfaces, but rather judiciously incorporate a low fraction of them.

36 MATERIALS SCIENCE↗

Finite domain solution of a hydraulic fracture in a permeable rock

In this work, we present a domain-based algorithm to simulate the propagation of a plane-strain hydraulic fracture in a zero-toughness permeable elastic medium. The algorithm utilizes a domain-based method to solve the elasticity equation and integrates a multi-scale tip asymptote, which is particular to hydraulic fractures, into this framework. This integration is key to accurately model the energy dissipation and the fluid leak-off in the fracture tip region. The algorithm combines a 2D finite volume method (FVM) for solving the elasticity equation with a 1D FVM for solving the nonlinear lubrication equation. Incorporating the far-field asymptotics and using a moving-mesh scheme reduces the computational burden while improving the accuracy of the scheme. The paper concludes with an analysis of the numerical results. This study demonstrates the potential of this domain-based approach for modeling hydraulic fractures in poroelastic media.

Domain-based method↗

Microstructure and crystallographic texture of high frequency electric resistance welded X65 pipeline steel

Here, microstructure and crystallographic texture and their correlation with impact toughness of high-frequency electric resistance welded (HF-ERW) X65 Grade pipeline steel have been investigated. X65 base metal after HF-ERW has formed a typical hourglass-shaped weld joint with four different regions, including the thermomechanical-affected zone (TMAZ), fine-grained heat affected zone (FGHAZ), coarse-grained heat affected zone (CGHAZ), and bondline (Weld Zone). X65 base metal shows prominent (113) [110] and (112) [110] texture components due to thermomechanical-controlled processing. TMAZ depicted random texture with a minor intensity of Cube component (001)[110] due to the partial recrystallization during welding. In the FGHAZ and CGHAZ, near the bondline, the base metal texture has been converted to rotated Goss (110) [110], Goss (110) [001], and rotated cube (001) [110] due to the recrystallization of the austenite and the shear deformation in the austenite temperature range. A high density of {100} and {110} cleavage planes is observed in the CGHAZ, which is often found to be the fracture location for the impact toughness testing.

36 MATERIALS SCIENCE↗

Dual Recycling of Depolymerization Catalyst and Biodegradable Polyester that Markedly Outperforms Polyolefins

Abstract Chemically recyclable, circular polymers continue to attract increasing attention, but rendering both catalysts for depolymerization and high‐performance polymers recyclable is a more sustainable yet challenging goal. Here we introduce a dual catalyst/polymer recycling system in that recyclable inorganic phosphomolybdic acid catalyzes selective depolymerization of high‐ceiling‐temperature biodegradable poly(δ‐valerolactone) in bulk phase, which, upon reaching suitable molecular weight, exhibits outstanding mechanical performance with a high tensile strength of ≈66.6 MPa, fracture strain of ≈904 %, and toughness of ≈308 MJ m −3 , and thus markedly outperforms commodity polyolefins, recovering its monomer in pure state and quantitative yield at only 100 °C. In sharp contrast, the uncatalyzed depolymerization not only requires a high temperature of >310 °C but is also low yielding and non‐selective. Importantly, the recovered monomer can be repolymerized as is to reproduce the same polymer, thereby closing the circular loop, and the recycled catalyst can be reused repeatedly for depolymerization runs without loss of its catalytic activity and efficiency.

Li, Xin‐Lei↗

Toughening Brittle Bio‐P3HB with Synthetic P3HB of Engineered Stereomicrostructures

Abstract Poly(3‐hydroxybutyrate) (P3HB), a biologically produced, biodegradable natural polyester, exhibits excellent thermal and barrier properties but suffers from mechanical brittleness, largely limiting its applications. Here we report a mono‐material product design strategy to toughen stereoperfect, brittle bio or synthetic P3HB by blending it with stereomicrostructurally engineered P3HB. Through tacticity ([ mm ] from 0 to 100 %) and molecular weight ( M n to 788 kDa) tuning, high‐performance synthetic P3HB materials with tensile strength to ≈30 MPa, fracture strain to ≈800 %, and toughness to 126 MJ m −3 (>110× tougher than bio‐P3HB) have been produced. Physical blending of the brittle P3HB with such P3HB in 10 to 90 wt % dramatically enhances its ductility from ≈5 % to 95–450 % and optical clarity from 19 % to 85 % visible light transmittance while maintaining desirably high elastic modulus (>1 GPa), tensile strength (>35 MPa), and melting temperature (160–170 °C). This P3HB‐toughening‐P3HB methodology departs from the traditional approach of incorporating chemically distinct components to toughen P3HB, which hinders chemical or mechanical recycling, highlighting the potential of the mono‐material product design solely based on biodegradable P3HB to deliver P3HB materials with diverse performance properties.

Zhang, Zhen↗

Dual Recycling of Depolymerization Catalyst and Biodegradable Polyester that Markedly Outperforms Polyolefins

Chemically recyclable, circular polymers continue to attract increasing attention, but rendering both catalysts for depolymerization and high-performance polymers recyclable is a more sustainable yet challenging goal. Here we introduce a dual catalyst/polymer recycling system in that recyclable inorganic phosphomolybdic acid catalyzes selective depolymerization of high-ceiling-temperature biodegradable poly(δ-valerolactone) in bulk phase, which, upon reaching suitable molecular weight, exhibits outstanding mechanical performance with a high tensile strength of ≈66.6 MPa, fracture strain of ≈904 %, and toughness of ≈308 MJ m –3 , and thus markedly outperforms commodity polyolefins, recovering its monomer in pure state and quantitative yield at only 100 °C. In sharp contrast, the uncatalyzed depolymerization not only requires a high temperature of >310 °C but is also low yielding and non-selective. Importantly, the recovered monomer can be repolymerized as is to reproduce the same polymer, thereby closing the circular loop, and the recycled catalyst can be reused repeatedly for depolymerization runs without loss of its catalytic activity and efficiency.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗