At least 271 records · Page 15

Insights into Boron-Based Polyanion-Tuned High-Nickel Cathodes for High-Energy-Density Lithium-Ion Batteries

Ultrahigh-Ni layered oxide cathodes (Ni content > 90%) are at the forefront for potentially enabling higher-energy density lithium-ion batteries. Unfortunately, they suffer from rapid capacity fade, poor thermal stability, and increased air sensitivity. Introduction of boron-based polyanion into layered cathodes has been found to be effective in stabilizing high-Ni cathodes, but the mechanism behind it is not yet fully understood. To develop a better understanding, we present here an extensive characterization of the ultrahigh-Ni cathode LiNi 0.94 Co 0.06 O 2 (NC) and B 2 O 3 -LiNi 0.94 Co 0.06 O 2 (B-NC). The B-NC delivers a capacity of 223 mA h g -1 with 80% capacity retention after 400 cycles in full cells with graphite anodes, superior to 61% retention for NC. In-depth interphase investigations reveal that the improved cyclability is attributed to the development of a well-passivated boron/phosphorus-rich cathode-electrolyte interphase in B-NC. Moreover, B-NC demonstrates a considerably enhanced air-exposure and thermal stability. A 30-day air-stored B-NC delivers a discharge capacity of 125 mA h g -1 at 10C rate, in sharp contrast to 65 mA h g -1 for the stored NC. Finally, this work advances the understanding of the effect boron-based polyanion insertion into layered oxides has on battery performance and offers a viable strategy for developing practically viable ultra-high-Ni cathodes with high-energy density.

25 ENERGY STORAGE↗

Compositions and Formation Mechanisms of Solid-Electrolyte Interphase on Microporous Carbon/Sulfur Cathodes

We report the formation mechanism and compositions of a solid-electrolyte interphase (SEI) on a microporous carbon/sulfur (MC/S) cathode in Li–S batteries using a carbonate-based electrolyte (1 M LiPF 6 in ethylene carbonate (EC)/dimethyl carbonate, v:v = 1:1). Through characterizations using 1D and 2D solution-phase nuclear magnetic resonance spectroscopy, coupled with model chemical reactions and DFT calculations, we have identified two critical roles of Li + in steering the SEI formation. First, the preferential solvation of Li + by EC in the mixed carbonate electrolyte renders EC as the dominant participant in the SEI formation, and second, Li + coordination to the EC carbonyl alters activation barriers and changes the reaction pathways relative to Na + . The main organic components in the SEI are identified as lithium ethylene monocarbonate and lithium methyl carbonate, which are virtually identical to those formed on Li and graphite anodes of lithium-ion batteries but via a different pathway.

25 ENERGY STORAGE↗

An Atomistic Study of Reactivity in Solid-State Electrolyte Interphase Formation for Li/Li7P3S11

Lithium metal batteries offer superior volumetric and gravimetric specific capacities compared to those based on traditional graphite anodes. Although advancements in solid-state electrolytes address safety concerns, challenges remain, particularly regarding interphase formation in lithium metal anodes. This work presents a computational framework based on high-throughput first-principles density functional theory and machine-learning interatomic potentials (MLIPs) including automated iterative, active learning to enable robust computational exploration of interphase formation between lithium metal anodes and an inorganic solid-state electrolyte. As a demonstration, we apply the framework to a Li/Li7P3S11 interface and find that it accurately identifies the experimentally observed, thermodynamically stable interphase products as well as their overall spatial arrangement within a heterogeneous, amorphous layered structure, with Li2S domains of nanocrystallinity. Our simulations show two stages, a fast and slow diffusion reaction regime, that corroborate the relative phase formation rate of Li x P, Li2S, and Li3P. Using the Onsager transport theory, we capture time-dependent ionic diffusion within the reacting interface, including cross-correlation effects. We found that cross-correlation effects between Li-P and P-S ionic motion significantly influence P-ion diffusion, making it highly sensitive to the local environment and potentially leading to "kinetic trapping" of Li-P phases. The passivation of the interface is shown as the ionic fluxes all approach zero, effectively halting interphase growth.

Diffusion↗

Superionic Surface Li-Ion Transport in Carbonaceous Materials

Unlike Li-ion transport in the bulk of carbonaceous materials, little is known about Li-ion diffusion on their surface. Here, in this study, we have discovered an ultrafast Li-ion transport phenomenon on the surface of carbonaceous materials with limited reversible Li insertion capacity and high surface area. An ionic conductivity of 18.1 mS cm –1 at room temperature is observed in lithiated Ketjen black (KB), far exceeding those of most solid-state ion conductors. Theoretical calculations reveal low diffusion barriers for the surface Li species. As a result, lithiated KB functions effectively as an interlayer between Li and solid-state electrolytes (SSEs) to mitigate dendrite growth. Further, lithiated KB acts as a high-performance mixed ionic–electronic conductor and replaces solid electrolytes to enhance graphite anode performance, demonstrating full utilization with ∼85% capacity retention over 300 cycles. The discovery of this surface-mediated ultrafast Li-ion transport mechanism provides new directions for the design of solid-state ion conductors and solid-state batteries.

Li metal batteries↗

Long-Term Cycling of a Mn-Rich High-Voltage Spinel Cathode by Stabilizing the Surface with a Small Dose of Iron

The high-voltage, cobalt-free spinel cathode LiNi 0.5 Mn 1.5 O 4 (LNMO) is receiving extensive attention for lithium-ion batteries due to its low cost, high operating voltage and energy density, superior power density, and good thermal stability. However, its high operating voltage hampers its stability with commercial electrolytes and makes its practical viability challenging. We present here a Mn-rich LNMO cathode to encourage the disordering of Mn and Ni in the lattice and the incorporation of a small dose of Fe into Mn-rich LNMO (Fe-LNMO) to improve the cycling stability. The introduction of Fe further increases the cation disorder between Mn and Ni, thus enabling a better rate capability. Electron energy loss spectroscopy analysis indicates that Fe is concentrated on the surface, and X-ray photoelectron spectroscopy analysis shows that Fe-LNMO alleviates the aggressive reaction between the cathode surface and the electrolyte, thus stabilizing the interface and cycle life. Furthermore, a full cell assembled with a graphite anode with an areal capacity of 3 mA h cm –2 displays a capacity retention of 90% over 300 cycles. Furthermore, the present work demonstrates an effective way to promote cation disordering and lower the surface reactivity of LNMO with the electrolyte, thereby enhancing the conductivity, stabilizing the cathode–electrolyte interphase, and making LNMO promising for practical applications.

25 ENERGY STORAGE↗

Mechanistic Analysis of Microstructural Attributes to Lithium Plating in Fast Charging

Metallic lithium deposition on graphite anodes is a critical degradation mode in lithium-ion batteries, which limits safety and fast charge capability. A conclusive strategy to mitigate lithium deposition under fast charging yet remains elusive. Herein, we examine the role of electrode microstructure in mitigating lithium plating behavior under various operating conditions, including fast charging. The multilength scale characteristics of the electrode microstructure lead to a complex interaction of transport and kinetic limitations that significantly governs the cell performance and the occurrence of Li plating. We demonstrate, based on a comprehensive mesoscale analysis, that the performance and degradation can be significantly modulated via systematic design improvements at the hierarchy of length scales. It is found that the improvement in kinetic and transport characteristics achievable at disparate scales can dramatically affect Li plating propensity.

25 ENERGY STORAGE↗

Zinc-Doped High-Nickel, Low-Cobalt Layered Oxide Cathodes for High-Energy-Density Lithium-Ion Batteries

High-Ni layered oxides with Ni contents greater than 90% are promising cathode candidates for high-energy-density Li-ion batteries. However, drastic electrode-electrolyte reactions and mechanical degradation issues limit their cycle life and practical viability. We demonstrate here that LiNi 0.94 Co 0.04 Zn 0.02 O 1.99 (NCZ), obtained by incorporating 2 mol% Zn 2+ into an ultrahigh-Ni baseline cathode material LiNi 0.94 Co 0.06 O 2 (NC), delivers superior cell performance. NCZ retains 74% of the initial capacity after 500 cycles in full cell assembled with graphite anode, outperforming NC (62% retention). NCZ also possesses a higher average discharge voltage relative to NC with an outstanding average voltage retention of over 99% after 130 cycles in half cells. Bulk structural investigations unveil that Zn doping promotes a smoother phase transition, suppresses anisotropic lattice distortion, and maintains the mechanical integrity of cathode particles. Furthermore, NCZ shows an enhanced interphase stability after long-term cycling, in contrast to the seriously degraded surface chemistry in NC. Finally, this work provides a practically viable approach for designing higher-energy-density high-Ni layered oxide cathodes for lithium-ion batteries.

25 ENERGY STORAGE↗

Influence of Calendering on the Electrochemical Performance of LiNi 0.9 Mn 0.05 Al 0.05 O 2 Cathodes in Lithium-Ion Cells

Electrode calendering is a necessary process used in industry to improve the volumetric capacity of lithium-ion batteries. However, calendering high-nickel cathodes leads to electrode particle pulverization, raising concerns of a reduced cycle life due to parasitic side reactions. We present here an investigation of the impact of calendering on the morphology and electrochemical performance of the cobalt-free layered oxide cathode LiNi 0.9 Mn 0.05 Al 0.05 O 2 (NMA-90). We find that secondary particle pulverization and fusion simultaneously occur at sufficiently high pressures. The initial surface area of the cathode is shown to increase with the degree of calendering, despite the higher likelihood of secondary particle fusion. Long-term cycling of full coin cells assembled with the NMA-90 cathode and the graphite anode indicates that cells with higher degrees of cathode calendering exhibit lower capacity fade compared to uncalendered cathodes. Hybrid pulse-power tests demonstrate that the usable capacity range of cells with calendered cathodes far exceeds those with uncalendered cells after long-term cycling. The improved capacity retention and pulse-power performance are attributed to the enhanced mechanical properties of the electrode after calendering that prevents loss of the primary particle contact during long-term cycling. As a result, we find that calendering high-nickel NMA-90 to industrially relevant densities does not have a detrimental effect on capacity fade, marking an important step toward commercial adoption.

25 ENERGY STORAGE↗

High-Performance Layered Ni-Rich Cathode Materials Enabled by Stress-Resistant Nanosheets

Here, layered O3-type transition metal oxides are promising cathode candidates for high-energy-density Li-ion batteries. However, the structural instability at the highly delithiated state and low kinetics at the fully lithiated state are arduous challenges to overcome. Here, a facile approach is developed to make secondary particles of Ni-rich materials with nanosheet primary grains. Because the alignment of the primary grains reduces internal stress buildup within the particle during charge-discharge and provides straightforward paths for Li transport, the as-synthesized Ni-rich materials do not undergo cracking upon cycling with higher overall Li + ion diffusion rates. Specifically, a LiNi 0.75 Co 0.14 Mn 0.11 O 2 cathode with nanosheet grains delivers a high reversible capacity of 206 mAh g -1 and shows ultrahigh cycling stability, e.g., 98% capacity retention over 500 cycles in a full cell with a graphite anode.

25 ENERGY STORAGE↗

Critical Contribution of Imbalanced Charge Loss to Performance Deterioration of Si-Based Lithium-Ion Cells during Calendar Aging

Increasing the energy density of lithium-ion batteries, and thereby reducing costs, is a major target for industry and academic research. One of the best opportunities is to replace the traditional graphite anode with a high-capacity anode material, such as silicon. However, Si-based lithium-ion batteries have been widely reported to suffer from a limited calendar life for automobile applications. Heretofore, there lacks a fundamental understanding of calendar aging for rationally developing mitigation strategies. Both open-circuit voltage and voltage-hold aging protocols were utilized to characterize the aging behavior of Si-based cells. Particularly, a high-precision leakage current measurement was applied to quantitatively measure the rate of parasitic reactions at the electrode/electrolyte interface. The rate of parasitic reactions at the Si anode was found 5 times and 15 times faster than those of LiNi 0.8 Mn 0.1 Co 0.1 O 2 and LiFePO 4 cathodes, respectively. Here, the imbalanced charge loss from parasitic reactions plays a critical role in exacerbating performance deterioration. In addition, a linear relationship between capacity loss and charge consumption from parasitic reactions provides fundamental support to assess calendar life through voltage-hold tests. These new findings imply that longer calendar life can be achieved by suppressing parasitic reactions at the Si anode to balance charge consumption during calendar aging.

25 ENERGY STORAGE↗

Integrative Additive Design for Robust SEI Formation in NMC811||Silicon Batteries

Silicon (Si) is considered a promising replacement for graphite anodes in lithium-ion batteries (LIBs) due to its high abundance and exceptional specific capacity, but its widespread commercialization has been hindered by poor electrochemical performance. Among various strategies, the use of functional additives has emerged as one of the most effective and cost-efficient methods to enhance the electrochemical properties of LIBs. In this study, several additives—vinylene carbonate (VC), vinyl ethylene carbonate (VEC), lithium difluorophosphate (LiDFP), lithium difluoro(oxalato)borate (LiDFOB), lithium tetrafluorooxalatophosphate (LiTFOP), and lithium difluorobis(oxalato)phosphate (LiDFBOP)—were systematically investigated in LiNi₀.₈Mn₀.₁Co₀.₁O₂ (NMC811)||Si full cells. Notably, LiDFBOP, a lithium salt containing two oxalate groups, outperformed all other additives, delivering the best capacity retention after 300 cycles. Comprehensive characterizations, including FTIR, SEM, and XPS, revealed that LiDFBOP's superior performance stems from its ability to form a more stable solid electrolyte interphase (SEI) on the Si anode, owing to its favorable molecular structure that integrates the beneficial features of the other additives.

25 ENERGY STORAGE↗

Capacity Fading Mechanism of the Commercial 18650 LiFePO 4 -Based Lithium-Ion Batteries: An in Situ Time-Resolved High-Energy Synchrotron XRD Study

In this paper, in situ high-energy synchrotron XRD studies were carried out on commercial 18650 LiFePO 4 cells at different cycles to track and investigate the dynamic, chemical, and structural changes in the course of long-term cycling to elucidate the capacity fading mechanism. The results indicate that the crystalline structural deterioration of the LiFePO 4 cathode and the graphite anode is unlikely to happen before capacity fades below 80% of the initial capacity. Rather, the loss of the active lithium source is the primary cause for the capacity fade, which leads to the appearance of inactive FePO 4 that is proportional to the absence of the lithium source. Our in situ HESXRD studies further show that the lithium-ion insertion and deinsertion behavior of LiFePO 4 continuously changed with cycling. For a fresh cell, the LiFePO 4 experienced a dual-phase solid-solution behavior, whereas with increasing cycle numbers, the dynamic change, which is characteristic of the continuous decay of solid solution behavior, is obvious. Finally, the unpredicted dynamic change may result from the morphology evolution of LiFePO 4 particles and the loss of the lithium source, which may be the cause of the decreased rate capability of LiFePO 4 cells after long-term cycling.

18650 cell↗

Electrolyte Regulating toward Stabilization of Cobalt-Free Ultrahigh-Nickel Layered Oxide Cathode in Lithium-Ion Batteries

Cobalt (Co)-free ultrahigh-nickel (Ni) layered oxides exhibit a double-edged competitive advantages in reducing the cathode cost and boosting the energy density, promising the sustainable development of batteries for electric vehicles. However, the increased Ni content, resultantly more highly oxidative Ni 4+ , potentially induces severe capacity fading due to the aggravated side reactions, limiting the practical applications. Here, we evaluate the compatibility of two localized high-concentration electrolytes (LHCEs) with LiNi 0.96 Mg 0.02 Ti 0.02 O 2 (NMT) cathode under a high charging voltage of 4.4 V in lithium ion batteries. The LHCE with EC additive enables the formation of stable interfacial layers on both NMT cathode and graphite anode, thus realizing a capacity retention of 97.2% over 200 cycles at 25 °C and high reversible capacities of ~180.2 and ~185.8 mAh g -1 , respectively, at 5C charge rate and 5C discharge rate. This study offers a promising approach to enable Co-free ultrahigh-Ni layered oxides for practical applications.

25 ENERGY STORAGE↗

Sustainable and Energy-Efficient Production of Rare-Earth Metals via Chloride-Based Molten Salt Electrolysis

Neodymium metal is a critical component of rare earth magnets, essential for electric vehicles and the green energy transition, but its production has severe environmental impacts across its mining, separation, purification, and metal electrowinning steps. Specifically, conventional neodymium electrowinning in oxyfluoride molten salts using a consumable graphite anode generates greenhouse gases, e.g., carbon dioxide and perfluorocarbon (PFC). We propose an alternative chloride-based molten salt electrolysis process utilizing a novel dimensionally stable anode (DSA). Our process lowers the specific electrical energy consumption compared to the state of the art, while producing reusable chlorine gas and eliminating direct CO 2 and PFC emissions. Chloride-based molten salt electrolysis of NdCl 3 (1.65 M) added to a LiCl–KCl eutectic (45:55 wt %), while using a RuO 2 -coated DSA enables high Coulombic efficiency (>80%), low specific energy consumption (2.3 kWh/kg-Nd), and excellent electrowon Nd product purity (>97 wt %). Life cycle analysis, excluding the common input feedstock (Nd 2 O 3 ), shows that the global warming potential for the proposed chloride-based electrolysis approach is 5 kg CO 2 equivalent, compared to 9–16 kg CO 2 equivalent for the conventional process, representing a 44–69% reduction in CO 2 emissions.

36 MATERIALS SCIENCE↗

Hollow-core optical fibre sensors for operando Raman spectroscopy investigation of Li-ion battery liquid electrolytes

Improved analytical tools are urgently required to identify degradation and failure mechanisms in Li-ion batteries. However, understanding and ultimately avoiding these detrimental mechanisms requires continuous tracking of complex electrochemical processes in different battery components. Here, we report an operando spectroscopy method that enables monitoring the chemistry of a carbonate-based liquid electrolyte during electrochemical cycling in Li-ion batteries with a graphite anode and a LiNi 0.8 Mn 0.1 Co 0.1 O 2 cathode. By embedding a hollow-core optical fibre probe inside a lab-scale pouch cell, we demonstrate the effective evolution of the liquid electrolyte species by background-free Raman spectroscopy. The analysis of the spectroscopy measurements reveals changes in the ratio of carbonate solvents and electrolyte additives as a function of the cell voltage and show the potential to track the lithium-ion solvation dynamics. The proposed operando methodology contributes to understanding better the current Li-ion battery limitations and paves the way for studies of the degradation mechanisms in different electrochemical energy storage systems.

47 OTHER INSTRUMENTATION↗

Nonintrusive thermal-wave sensor for operando quantification of degradation in commercial batteries

Abstract Monitoring real-world battery degradation is crucial for the widespread application of batteries in different scenarios. However, acquiring quantitative degradation information in operating commercial cells is challenging due to the complex, embedded, and/or qualitative nature of most existing sensing techniques. This process is essentially limited by the type of signals used for detection. Here, we report the use of effective battery thermal conductivity ( k eff ) as a quantitative indicator of battery degradation by leveraging the strong dependence of k eff on battery-structure changes. A measurement scheme based on attachable thermal-wave sensors is developed for non-embedded detection and quantitative assessment. A proof-of-concept study of battery degradation during fast charging demonstrates that the amount of lithium plating and electrolyte consumption associated with the side reactions on the graphite anode and deposited lithium can be quantitatively distinguished using our method. Therefore, this work opens the door to the quantitative evaluation of battery degradation using simple non-embedded thermal-wave sensors.

25 ENERGY STORAGE↗

Topology-enhanced mechanical stability of swelling nanoporous electrodes

Abstract Materials like silicon and germanium offer a 10-fold improvement in charge capacity over conventional graphite anodes in lithium-ion batteries but experience a roughly threefold volume increase during lithiation, which challenges ensuring battery integrity. Nanoporous silicon, created by liquid-metal-dealloying, is a potentially attractive anode design to mitigate this challenge, exhibiting both higher capacity and extended cycle lifetimes. However, how nanoporous structures accommodate the large volume change is unknown. Here, we address this question by using phase-field modeling to produce nanoporous particles and to investigate their elastoplastic swelling behavior and fracture. Our simulations show that enhanced mechanical stability results from the network topology consisting of ligaments connected by bulbous, sphere-like nodes. The ligaments forcefully resist elongation while the nodes, behaving like isolated spherical particles, experience large stresses driving fracture. However, being smaller compared to a sphere of the same volume as the entire nanoporous particle, the nodes are more protected against fracture.

36 MATERIALS SCIENCE↗

Challenges and opportunities towards fast-charging battery materials

Extreme fast charging, with a goal of 15 minutes recharge time, is poised to accelerate mass market adoption of electric vehicles, curb greenhouse gas emissions and, in turn, provide nations with greater energy security. However, the realization of such a goal requires research and development across multiple levels, with battery technology being a key technical barrier. The present-day high-energy lithium-ion batteries with graphite anodes and transition metal oxide cathodes in liquid electrolytes are unable to achieve the fast-charging goal without negatively affecting electrochemical performance and safety. Here we discuss the challenges and future research directions towards fast charging at the level of battery materials from mass transport, charge transfer and thermal management perspectives. Additionally, we highlight advanced characterization techniques to fundamentally understand the failure mechanisms of batteries during fast charging, which in turn would inform more rational battery designs.