Search NASA⌕ Search

SEARCH · Search NASA

Results for “subscriptions”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 271 records · Page 15

Preparation of carbon supported cobalt by electrostatic adsorption of [Co(NH[subscript 3])[subscript 6]]Cl[subscript 3]

Our previous paper [L. D'Souza, L. Jiao, J.R. Regalbuto, J.T. Miller, A.J. Kropf, J. Catal. 248 (2007) 165] presented the synthesis of cobalt catalysts on carbon (Timrex) and silica supports by strong electrostatic adsorption (SEA), using a cobalt hexaamine chloride ([Co(NH{sub 3}){sub 6}]Cl{sub 3}, CoHA) precursor. The CoHA undergoes reductive deammination in an uncontrolled manner in the presence of NaOH and adsorbs as Co{sub 3}O{sub 4} on carbon with broad size distribution. The present paper extends these studies toward the end of synthesizing well-dispersed Co oxide particles in a narrow size range on carbon supports using NH{sub 4}OH. Cobalt uptake versus pH was determined in NH{sub 4}OH and NaOH basified solutions over a number of carbons with varying point of zero charge (PZC). The resulting materials were characterized by ICP, powder XRD, XAS, TPR and STEM. CoHA in the presence of NH{sub 4}OH adsorbs as well dispersed as CoO, Co{sub 3}O{sub 4} and Co(OH){sub 4}{sup 2-} depending upon the pH of the adsorption solution. These phases were undetectable by powder XRD and STEM Z-contrast imaging, but could be identified by XAS. Additionally, non-adsorbed CoHA complexes underwent transformation to [Co(NH{sub 3}){sub 5}Cl]Cl{sub 2} at pH > 11 in solution. After calcinations of 250 C, particle sizes of Co{sub 3}O{sub 4} range from 20-50 {angstrom} from NH{sub 4}OH and 50-200 {angstrom} from NaOH. Maximum metal uptake was approximately 3.3 and 2.7 {micro}mol/m{sup 2} in presence of NaOH and NH{sub 4}OH, respectively. The SEA method of preparation was compared with incipient wetness impregnation (IWI) of Co(NO{sub 3}){sub 2}{sm_bullet}6H{sub 2}O; this method yields Co{sub 3}O{sub 4} particles after 250 C calcinations which are almost as small or in one case, smaller than the calcined SEA samples. Higher metal loadings can be achieved by the SEA method by successive adsorption steps with a little variation in particle size and distribution. However, the main advantage of SEA is in forming mono- or submonolayer of different Co oxide phases on carbon surface.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Kinetics of Mg[subscript 6]Ni nanocrystallization in amorphous Mg[subscript 83]Ni[subscript 17]

A comprehensive crystallization kinetics study was carried out in order to understand the mechanism of formation of a Mg-rich nanocrystalline Mg{sub 6}Ni phase in a metallic glass with similar overall composition, Mg{sub 83}Ni{sub 17}. Adequate description of the transformation kinetics was obtained by the JMKA equation with an integer Avrami exponent n = 4, associated with nucleation and three-dimensional linear growth crystallization mechanism. To study the nanocrystals growth mechanism separately a controlled heat treatment of the amorphous alloy was applied and thus a three-dimensional growth with a constant rate was obtained (n = 3) for the pre-annealed alloys. For all transformation curves the dependence of n on the degree of transformation {alpha}, n({alpha}), was analyzed and the regions with constant n were defined. The correct separation of the processes of nucleation and crystal growth allowed reliable values for the activation energies of both nucleation and growth processes to be determined.

36 MATERIALS SCIENCE↗

Effects of irradiation temperature on the response of CeO2, ThO2, and UO2 to highly ionizing radiation

Microcrystalline CeO 2 , ThO 2 , and UO 2 were irradiated with 198 MeV 132 Xe ions to the same fluence at temperatures ranging from 25°C to 700°C then characterized by synchrotron X-ray diffraction and X-ray absorption spectroscopy. All samples retain crystallinity and their nominal fluorite-type phase at a fluence of 1.5x10 13 ions/cm 2 . Both CeO 2 and ThO 2 display defect-induced unit cell expansion after irradiation at room temperature (~0.15% and ~0.10%, respectively), yet as irradiation temperature increases, the maximum swelling produced decreases to ~0.02%. Alternatively, UO 2 shows an initial contraction in unit cell parameter (approximately -0.05%), for room temperature irradiation most likely related to irradiation-enhanced annealing or irradiation-induced oxidation. At higher temperatures (above 200°C), UO 2 begins to swell, surpassing its unit cell parameter prior to irradiation (~0.05%), an effect which could be attributed to minor reduction in uranium oxidation state in vacuum. However, while CeO 2 irradiated at room temperature undergoes partial reduction, both UO 2 and ThO 2 exhibit no measurable change in cation oxidation state as evidenced by X-ray absorption spectroscopy. All samples display a decrease in irradiation-induced heterogeneous microstrain as a function of increasing irradiation temperature.

36 MATERIALS SCIENCE↗

Stiffening of nanoscale anatase Ti[subscript 0.9]Zr[subscript 0.1]O[subscript 2] upon multiple compression cycles

The compression behavior of nanoscale Zr-doped anatase was studied by means of a diamond anvil cell experiment with alternating cycles of compression and decompression in the stability field of anatase (up to 13 GPa). We found that multiple cycles of compression lead to stiffening of the material: Precompressed samples of nanoanatase Ti{sub 0.9}Zr{sub 0.1}O{sub 2} have a higher bulk modulus (K{sub 0} = 249(9) and 266(6) GPa) compared with the sample when compressed for the first time (K{sub 0} = 211(7) GPa). Upon compression, the crystallite size remains the same and the crystalline areas are free of defects. After the experiment, the crystallites are surrounded by amorphous rims, confirming the theoretical prediction by Pischedda et al. [Ultrastability and enhanced stiffness of similar to 6 nm TiO{sub 2} nanoanatase and eventual pressure-induced disorder on the nanometer scale, Phys. Rev. Let. 96 (2006) 035509] for nanoscale anatase, but yielding much lower pressures (12 GPa) for the onset of partial amorphization.

36 MATERIALS SCIENCE↗