Search NASA⌕ Search

SEARCH · Search NASA

Results for “ADHESION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Thermo-Oxidation Analysis of Structural Adhesives: An Experimental Study

Abstract Cross-linked polymers play an important role in structural applications as adhesives. In this article, we performed an experimental study to understand the effects of high temperature i.e. thermo-oxidative aging on the mechanical behavior of polymers. Subsequently, the constitutive behavior, i.e. stress-strain relation of these adhesives before and after the accelerated aging tests were studied on samples aged at different temperature and different time durations at zero humidity. The aging conditions and periods selected for the tests have been specifically designed to simulate the effects of aging under the working conditions that the materials will be subjected to in their standard applications. The focus of this study is on the investigation of the effects of aging on the polymeric adhesives used in automotive applications. Consequently, four different polymeric adhesives (one silicone-based, two polyurethane-based, and one acrylic type), which are being used extensively in these applications, have been chosen. The quasi-static tensile loading was used on these four adhesives and the changes in the constitutive behavior were measured. The failure tensile tests as well as the cyclic tensile tests were performed in our lab using a Test-Resources tensile testing machine. The temperatures that were used in this work are 60, 80 and 95°C for varying aging periods of 24hrs, 240hrs, and 720hrs. Then, all the data was collected and consequently analyzed, and the resulting behavior was compared to that of the unaged material, showing varying results depending on the material, temperature, and aging period. Different behaviors have been observed after aging. The polymers’ behavior was expanding from no effect to significant damage caused by aging conditions. This work provides the core understanding required for modeling the material behavior during aging and lays down the groundwork for further data-infused model-free approaches.

Alazhary, Sharif↗

Design of tough adhesive from commodity thermoplastics through dynamic crosslinking

Tough adhesives provide resistance against high debonding forces, and these adhesives are difficult to design because of the simultaneous requirement of strength and ductility. Here, we report a design of tough reversible/recyclable adhesive materials enabled by incorporating dynamic covalent bonds of boronic ester into commodity triblock thermoplastic elastomers that reversibly bind with various fillers and substrates. The spectroscopic measurements and density functional theory calculations unveil versatile dynamic covalent binding of boronic ester with various hydroxy-terminated surfaces such as silica nanoparticles, aluminum, steel, and glass. The designed multiphase material exhibits exceptionally high adhesion strength and work of debonding with a rebonding capability, as well as outstanding mechanical, thermal, and chemical resistance properties. Bonding and debonding at the interfaces dictate hybrid material properties, and this revelation of tailored dynamic interactions with multiple interfaces will open up a new design of adhesives and hybrid materials.

36 MATERIALS SCIENCE↗

Adhesion-force micro-scale study of desiccating granular material

Experiments on five-, four-, three- and two-wet-hydrophilic-grain clusters were performed to investigate evolution of adhesion of granular media during drying on the micro-scale. The experiments show that the adhesion-force of a cluster initially grows at most to three times the original value before decreasing to zero by the end of evaporation. The adhesion-force is composed of capillary pressure force acting over the liquid/solid contact surface area, and surface tension forces acting over the three-phase contact perimeter length. This is in contrast with most macro-scale phenomenological models, in which the only desaturation process variables affecting strength are suction and saturation. Both the contact surface area and contact perimeter length are reduced to zero upon complete liquid evaporation. The morphology of an evaporating water body evolves through slow flow controlled by evaporation rate, interrupted by various modes of fast air entry, which are non-equilibrium jumps of liquid/gas interfaces (Haines jumps). The instabilities involve large adhesion force discontinuities and substantial water mass reconfiguration with water flow in an extremely short time, which makes the process transient. The reconfigurations can reduce the original multi-grain water clusters to four-, three- and two-grain clusters by way of three different instability modes: of thin-sheet instability, or meniscus snap-through instability, depending on the sign of the Gauss curvature of the liquid surface, or finally, for two-grain bridges only, a liquid wire pinch-off. For larger meso-scale assemblies, however, the global adhesion-force evolution is little affected by the jumps. The air entries are potential sites for drying cracks. The (approximately) calculated capillary pressure for two- and three-grain clusters, in no cases is seen to reach high values, predicted from water retention curves.

Engineering↗

Adhesion measurement of highly-ordered TiO 2 nanotubes on Ti-6Al-4V alloy

Self-assembled nanotubular arrays on Ti alloys could be used for more effective implantable devices in various medical approaches. In the present work, the adhesion of TiO 2 nanotubes (TiO 2 NTs) on Ti-6Al-4V (Ti64) was investigated by laser spallation and scratch test techniques. At first, electrochemical anodization was performed in an ammonium fluoride solution dissolved in a 90:10 ethane-1,2-diol (ethylene glycol) and water solvent mixture. This process was performed at room temperature (23 °C) at a steady potential of 60 V for 1 h. Next, the TiO 2 nanotubes layer was heat-treated to improve the adhesion of the coating. The formation of self-organized TiO 2 nanotubes as well as the microstructural evolution, are strongly dependent on the processing parameters and subsequent annealing. From microscopic analysis, highly oriented arrays of TiO 2 nanotubes were grown by thermal treatment for 90 min at 500 °C. Further heat treatment above 500 °C led to the detachment of the nanotubes and the complete destruction of the nanotubes occurred at temperature above 700 °C. Scratch test analysis over a constant scratch length (1000 μm) indicated that the failure point was shifted from 247.4 to 557.9 μm while the adhesion strength was increased from ~862 to ~1814 mN after annealing at 500 °C. Finally, the adhesion measurement determined by laser spallation technique provided an intrinsic adhesion strength of 51.4 MPa for the TiO 2 nanotubes on the Ti64 substrate.

36 MATERIALS SCIENCE↗

Adhesives and the ATS satellite

Adhesives in the ATS satellite allow the designers to save weight, simplify design and fabrication and provide thermal and electrical conductivity or resistivity as required. The selections of adhesives are restricted to those few which can pass rigorous outgassing tests in order to avoid contaminating lenses and thermal control surfaces in space. An epoxy adhesive is used to construct the honeycomb panels which constitute most of the satellite's structure. General purpose epoxy adhesives hold doublers and standoffs in place and bond the truss to its fittings. Specialized adhesives include a high temperature resistant polyamide, a flexible polyurethane and filled epoxies which conduct heat or electricity.

Hancock, F. E.↗

Adhesion and friction behavior of group 4 elements germanium, silicon, tin, and lead

Adhesion and friction studies were conducted with thin films of the group IV elements silicon, germanium, tin, and lead ion plated on the nickel (011) substrate. The mating surface was gold (111). Contacts were made for the elements in the clean state and with oxygen present. Adhesion and friction experiments were conducted at very light loads of 1 to 10 g. Sliding was at a speed of 0.7 mm/min. Friction results indicate that the more covalently bonded elements silicon and germanium exhibit lower adhesion and friction than the more metallic bonded tin and lead. The adhesion of gold to germanium was observed, and recrystallization of the transferred gold occurred. Plastic flow of germanium was seen with sliding. Oxygen reduced, but did not eliminate, the adhesion observed with germanium and silicon.

Buckley, D. H.↗

The effect of bending on the stresses in adhesive joints

The problem of stress distribution in adhesive joints where two orthotropic plates are bonded through a flexible adhesive layer is analyzed. It is shown that the effect of bending of the adherends on the stresses in the adhesive layer is very significant. The transverse shear deformations of the adherends appear to have little influence on the adhesive layer stresses. The maximum transverse normal stress in the adhesive is shown to be larger than the maximum longitudinal shear stress. The method of solution is applied to several examples of specific joint geometries and material combinations, and is proven to be applicable to other related problems.

Yuceoglu, U.↗

The effect of adhesive layer on crack propagation in laminates

The effect of the adhesive layer on crack propagation in composite materials is investigated. The composite medium consists of parallel load carrying laminates and buffer strips arranged periodically and bonded with thin adhesive layers. The strips, assumed to be isotropic and linearly elastic, contain symmetric cracks of arbitrary lengths located normal to the interfaces. Two problems are considered: (1) thin adhesive layers are approximated by uncoupled tension and shear springs distributed along the interfaces of the strips for which only the case of internal cracks can be treated rigorously; (2) broken laminates and the true singular behavior in the presence of the adhesive layer are studied. The adhesive is then treated as an isotropic, linearly elastic continuum. General expressions for field quantities are obtained in terms of infinite Fourier integrals. These expressions give a system of singular integral equations in terms of the crack surface displacement derivatives. By using appropriate quadrature formulas, the integral equations reduce to a system of linear algebraic equations which are solved numerically.

Gecit, M. R.↗

The effect of adhesive layers on the fracture of laminated structures

The effect of the thickness and the elastic properties of the adhesive layers in laminated structures is considered. The structure is assumed to consist of two sets of periodically arranged dissimilar layers which may contain cracks perpendicular to the interfaces. The crack problem is solved under the assumption of plane strain or generalized plane stress and by using two different models for the adhesive layers. In the first model the adhesive layer is approximated by a combination of tensile and shear springs. In the second the adhesive layer is considered to be an elastic continuum, hence involving no approximating assumptions. The results regarding the stress intensity and stress concentration factors obtained from these two models and that found by ignoring the adhesive layers are presented and some comparisons are made.

Gecit, M. R.↗

Viscoelastic analysis of adhesively bonded joints

An adhesively bonded lap joint is analyzed by assuming that the adherends are elastic and the adhesive is linearly viscoelastic. After formulating the general problem a specific example for two identical adherends bonded through a three parameter viscoelastic solid adhesive is considered. The standard Laplace transform technique is used to solve the problem. The stress distribution in the adhesive layer is calculated for three different external loads, namely, membrane loading, bending, and transverse shear loading. The results indicate that the peak value of the normal stress in the adhesive is not only consistently higher than the corresponding shear stress but also decays slower.

Delale, F.↗

LARC-13 adhesive development

A LARC-13 type adhesive system was developed and property data obtained that demonstrated improved thermomechanical properties superior to base LARC-13 adhesive. An improved adhesive for 589 K (600 F) use was developed by physical or chemical modification of LARC-13. The adhesive was optimized for titanium and composite bonding, and a compatible surface preparation for titanium and composite substrates was identified. The data obtained with the improved adhesive system indicated it would meet the 589 K (600 F) properties desired for application on space shuttle components. Average titanium lap shear data were: (1) 21.1 MPa (3355 psi) at RT, (2) 13.0 MPa (1881 psi) at 600 F, and (3) 16.4 MPa (2335) after aging 125 hours at 600 F and tested at 600 F.

Hill, S. G.↗

Stresses in adhesively bonded joints: A closed form solution

The plane strain of adhesively bonded structures which consist of two different orthotropic adherents is considered. Assuming that the thicknesses of the adherends are constant and are small in relation to the lateral dimensions of the bonded region, the adherends are treated as plates. The transverse shear effects in the adherends and the in-plane normal strain in the adhesive are taken into account. The problem is reduced to a system of differential equations for the adhesive stresses which is solved in closed form. A single lap joint and a stiffened plate under various loading conditions are considered as examples. To verify the basic trend of the solutions obtained from the plate theory a sample problem is solved by using the finite element method and by treating the adherends and the adhesive as elastic continua. The plate theory not only predicts the correct trend for the adhesive stresses but also gives rather surprisingly accurate results.

Delale, F.↗

Experimental determination of the effects of moisture on composite-to-composite adhesive joints

The primary mode of moisture ingress into bonded composite joints is determined using a nuclear probe for deuterium (NPD) to measure the localized D2O content along the length of the adhesive (FM-300 and EA-9601) and through the thickness of bonded composite speciments. Calculated diffusivities and NPD measured equilibrium moisture contents are used to predict the moisture profiles along the length of the adhesives as a function of exposure time, temperature, and relative humidity. These results are compared with the observed moisture profiles to evaluate the extent of enhanced edge diffusion. The FM-300 adhesive exhibits good agreement between measured and predicted profiles at 49 C, 70% and 90% RH, and 77 C, 70% RH. At 77 C, 90% RH, the measured moisture content near the adhesive edge is substantially larger than the predicted level. The EA-9601 adhesive also shows good agreement at 49 C, 70% and 90% RH, but at 77 C, the concentration of D20 near the edges is enhanced at each humidity level. The effect of moisture content on the bond shear strength at room temperature and at elevated temperature is evaluated.

Deiasi, R. J.↗

A review of high-temperature adhesives

The development of high temperature adhesives and polyphenylquinoxalines (PPQ) is reported. Thermoplastic polyimides and linear PPQ adhesive are shown to have potential for bonding both metals and composite structures. A nadic terminated addition polyimide adhesive, LARC-13, and an acetylene terminated phenylquinoxaline (ATPQ) were developed. Both of the addition type adhesives are shown to be more readily processable than linear materials but less thermooxidatively stable and more brittle. It is found that the addition type adhesives are able to perform, at elevated temperatures up to 595 C where linear systems fail thermoplastically.

St.clair, A. K.↗

Viscoelastic analysis of adhesively bonded joints

In this paper an adhesively bonded lap joint is analyzed by assuming that the adherends are elastic and the adhesive is linearly viscoelastic. After formulating the general problem a specific example for two identical adherends bonded through a three parameter viscoelastic solid adhesive is considered. The standard Laplace transform technique is used to solve the problem. The stress distribution in the adhesive layer is calculated for three different external loads namely, membrane loading, bending, and transverse shear loading. The results indicate that the peak value of the normal stress in the adhesive is not only consistently higher than the corresponding shear stress but also decays slower.

Delale, F.↗

Material characterization of structural adhesives in the lap shear mode

A general method for characterizing structual adhesives in the bonded lap shear mode is proposed. Two approaches in the form of semiempirical and theoretical approaches are used. The semiempirical approach includes Ludwik's and Zhurkov's equations to describe respectively, the failure stresses in the constant strain rate and constant stress loading modes with the inclusion of the temperature effects. The theoretical approach is used to describe adhesive shear stress-strain behavior with the use of viscoelastic or nonlinear elastic constitutive equations. Two different model adhesives are used in the single lap shear mode with titanium adherends. These adhesives (one of which was developed at NASA Langley Research Center) are currently considered by NASA for possible aerospace applications. Use of different model adhesives helps in assessment of the generality of the method.

Sancaktar, E.↗

Fatigue behavior of adhesively bonded joints

The fatigue damage mechanism of composite to composite adhesively bonded joints was characterized. The mechanics of the possible modes of fatigue damage propagation in these joints when subjected to constant amplitude cyclic mechanical loading were investigated. The possible failure modes in composite bonded joints may be cyclic debonding (i.e., progressive separation of the adhesive), interlaminar damage (delamination), adherend fatigue or a combination of these. Two composite systems - graphite/epoxy adhesively bonded to graphite/epoxy and Kevlar 49/epoxy adhesively bonded to Kevlar 49/epoxy were investigated. Both composite systems consisted of quasi-isotropic lay-ups, i.e., 0 deg/-45 deg/+45 deg/90 degs. The two adhesives, employed in the study were (1) EC 3445 with cure temperature of 250 F for secondary bonding and (2) FM 300 with cure temperature of 350 F for co-cure bonding.

Mall, S.↗

A fracture mechanics approach for designing adhesively bonded joints

An analytical and experimental investigation was undertaken to determine if the adhesive debond initiation stress could be predicted for arbitrary joint geometries. The analysis was based upon a threshold total strain-energy-release rate (Gth) concept. Two bonded systems were tested: T300/5208 graphite/epoxy adherends bonded with either EC-3445 or FM-300 adhesive. The Gth for each adhesive was determined from cracked-lap-shear (CLS) specimens by initiation tests. Finite-element analyses of various tapered CLS specimen geometries predicted the specimen stress at which the total strain-energy-release rate (GT) equaled Gth at the joint tip. Experiments verified the predictions. The approach described herein predicts the maximum stress at which an adhesive joint can be cycled yet not debond. Furthermore, total strain-energy-release rate appeared to be the driving parameter for cyclic debonding and debond initiation in structural adhesives. In addition, debond initiation and growth were found to occur with virtually no peel stress present.

Johnson, W. S.↗