At least 289 records · Page 16

Electrochemical stability and corrosion behavior of Ni-Cr alloy in molten LiCl-KCl salt

This study investigated the electrochemical properties and potential-dependent stability of Cr(II) and Ni(II) in a eutectic LiCl-KCl molten salt at 500 °C under an argon atmosphere using a three-electrode cell configuration with a glassy carbon working electrode, Ag/Ag + reference electrode, and graphite counter electrode. Cyclic voltammetry was employed to characterize the Cr(0)/Cr(II)/Cr(III) and Ni(0)/Ni(II) redox transitions, yielding diffusion coefficients of 0.50 (±0.01) × 10 −5 cm 2 s −1 for Cr(II) and 0.91 (±0.16) × 10 −5 cm 2 s −1 for Ni(II) at 500 °C. The redox stability domains of these species provided insight into the corrosion mechanisms of a Ni-Cr alloy (80–20 wt %) in LiCl-KCl salt. The measured open circuit potential of the alloy corresponded to the range of potentials where the Ni(0) and Cr(II) species are stable, indicating a preferential dissolution of Cr. Immersion testing of the alloy for 336 h confirmed significant Cr depletion (or Ni-enrichment) at the surface layer, corroborating Cr dealloying as the dominant corrosion reaction under open circuit conditions. Additionally, the application of a small anodic overpotential (0.11 V) resulted in selective Cr dissolution while a large anodic overpotential (0.25 V) resulted in co-dissolution of both Cr and Ni. Furthermore, these results demonstrate that the corrosion mechanisms of a Ni-Cr alloy in LiCl-KCl depend upon the applied potential, and thus the redox conditions of the molten salt should be carefully controlled in the design of a redox buffer to mitigate corrosion in molten salt environments.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Corrosion of 316 SS in direct contact with Zircaloy-4 in repository relevant conditions

The effects of interfacial contact between 316 stainless steel (316 SS) waste canister and spent fuel cladding material (Zircaloy-4) in case of water intrusion into a deep geological repository are investigated. Hydrothermal corrosion experiments of 316 SS and Zircaloy-4 in direct contact were performed at elevated temperatures in MilliQ water and simulated Mont Terri groundwater. Hematite, magnetite, chromite, and baddeleyite form as secondary phases. pH of the Mont Terri solution increases with corrosion duration and magnetite forms preferentially instead of hematite. Thermodynamic modeling shows that iron oxidation in 316 SS controls the pH and redox potential of the aqueous environment and is in good agreement with experimental Mont Terri results, showing that experimental Mont Terri results trend to equilibrium. All oxides except hematite are predicted to exist at thermodynamic equilibrium based on calculations, implying that experimentally formed hematite will be reduced or transformed to magnetite at equilibrium. The thermodynamically predicted chromite was observed to form only at the interface where 316 SS was in contact with Zircaloy-4 at 250°C, showing that contact with Zircaloy-4 seems to accelerate the 316 SS corrosion to thermodynamic equilibrium. Finally, Mont Terri groundwater readily trends towards thermodynamic equilibrium, leading to a pH and redox buffered system that is dominated by iron in solution coming from the accelerated corrosion of 316 SS caused by Zircaloy-4 contact.

316 stainless steel↗

Considerations for realistic atmospheric environments: An application to corrosion testing

Measured salt compositions in dust collected over roughly the last decade from surfaces of in-service stainless-steel alloys at four locations around the United States are presented, along with the predicted brine compositions that would result from deliquescence of these salts. The salt compositions vary greatly from ASTM seawater and from laboratory salts (i.e., NaCl or MgCl 2 ) commonly used on corrosion testing. The salts contained relatively high amounts of sulfates and nitrates, evolved to basic pH values, and exhibited deliquescence relative humidity values (RH) higher than seawater. Additionally, inert dust in components were quantified and considerations for laboratory testing are presented. The observed dust compositions are discussed in terms of the potential corrosion behavior and are compared to commonly used accelerated testing protocols. Finally, ambient weather conditions and their influence on diurnal fluctuations in temperature (T) and RH on heated metal surfaces are evaluated and a relevant diurnal cycle for laboratory testing a heated surface has been developed. Suggestions for future accelerated tests are proposed that include exploration of the effects of inert dust particles on atmospheric corrosion, chemistry considerations, and realistic diurnal fluctuations in T and RH. Understanding mechanisms in both realistic and accelerated environments will allow development of a corrosion factor (i.e., scaling factor) for the extrapolation of laboratory-scale test results to real world applications.

54 ENVIRONMENTAL SCIENCES↗

FY24 Progress Report: SRNL Analysis of ICCWR LCM and WAMS data for Corrosion and Cracking

Algorithms for Machine Learning (ML) and data analysis for the 3013 Surveillance Program have been developed in an ongoing collaborative effort by the Savannah River National Laboratory (SRNL) and the University of South Carolina (USC). The objective of the algorithms is to automate the identification of corrosion and crack formation in the Inner Container Closure Weld Region (ICCWR) of the canister system used to store Pu-bearing material. Data for corrosion and cracking is collected from large binary files generated by a Laser Confocal Microscope (LCM), the Wide Area 3D Measurement System (WAMS), or,in a recent proposal, by a Scanning Electron Microscope (SEM). The ML software uses the physical attributes in the data files (e.g., one or more of: height, color, and 16-bit grayscale values as functions of position in a plane projection) to detect signs of surface corrosion and cracking after being trained on similar data, with the features to be detected. Although the initial scope included screening for broader indicators of corrosion, e.g., pitting, identification of potential cracks was prioritized for the past several years at the request of program leadership. Labeled training data is essential to developing the ML algorithm, and enhancements to data labeling capability have been developed to address this essential precursor to application of ML routines. Efficient labeling is particularly important in view of the large volume of data required to train ML algorithms and the relative rarity of cracks in the ICCWR data set. The updated program will read binary data from either LCM, WAMS or SEM files, interrogate data attributes, facilitate user labeling of data for training ML algorithms, execute ML algorithms, output parameters from trained ML algorithms, report ML model accuracy with respect to labeled data, and generate graphical representations for various analyses. In FY24, hourglass neural networks (HNNs) that were initiated in FY22 were further developed and tested using available LCM data, and their performance was tested against that of the alternative U-Net Neural Network algorithm structure. HNNs along with previously developed Convolutional Neural Networks (CNNs) and Deep Neural Networks (DNNs) comprise a suite of ML tools for identification of cracks in the ICCWR

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

FY25 Progress Report: SRNL Analysis of ICCWR LCM and WAMS data for Corrosion and Cracking

Algorithms for Machine Learning (ML) and image analysis for the 3013 Surveillance Program have been developed in an ongoing collaborative effort by the Savannah River National Laboratory (SRNL) and the University of South Carolina (USC). The objective of the algorithms is to automate the identification of corrosion and cracks in the Inner Container Closure Weld Region (ICCWR) of the canister system used to store Pu-bearing material. Data for corrosion and cracking is collected from large binary files generated by a Laser Confocal Microscope (LCM), the Wide Area 3D Measurement System (WAMS), or, in a recent proposal, by a Scanning Electron Microscope (SEM). The ML software uses the physical attributes in the data files (e.g., one or more of: height, color, and 16-bit grayscale values as functions of position in a plane projection) to detect signs of surface corrosion and cracking after being trained on similar data with the features to be detected. Although the initial scope included screening for broader indicators of corrosion, e.g., pitting, the identification of potential cracks was prioritized for the past several years at the request of program leadership.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Elevated-Temperature Tribo-Corrosion Response of Eutectic High-Entropy Alloy

The combination of elevated temperature and tribo-corrosion leads to the accelerated degradation of structural components used in many extreme environments. Recently developed high-entropy alloys (HEAs) with multiple principal elements have the potential for superior degradation resistance compared with presently used structural alloys. Here, we demonstrate the microstructural stability, pitting resistance, and superior tribo-corrosion degradation resistance of the AlCoCrFeNi 2.1 eutectic HEA in comparison with duplex stainless steel 2205 in deionized water (controlled low-ionic-strength electrolyte) at 25 °C, 50 °C and 100 °C. The AlCoCrFeNi 2.1 HEA showed excellent microstructural stability and tribo-corrosion resistance at all three temperatures, an order-of-magnitude lower wear rate, and a lower coefficient of friction compared with duplex 2205 steel. The lowest wear volume loss and wear rate for both AlCoCrFeNi 2.1 and duplex steel were recorded at 50 °C, which was attributed to temperature-assisted passivation and formation of a comparatively stable tribological surface condition. These results suggest superior performance of eutectic HEAs in tribo-corrosion applications compared with currently used dual-phase steels and motivate future evaluation in ion-containing industrial water chemistries.

36 MATERIALS SCIENCE↗

Effects of uranium metal carbon content on hydriding kinetics and corrosion blister number/area at sub-ambient pressures

Carbon is a common impurity in uranium metal, resulting in a number of uranium–carbon inclusion phases that contribute to an increase in metal defect density as carbon content increases. It is widely held that uranium hydride corrosion preferentially nucleates at these defect sites, and that an increase in carbon content will therefore represents an increase in uranium hydride corrosion sites on the metal surface. We hydrided six uranium sources with differing carbon contents to explore whether this assumption holds in a sub-ambient (~ 0.1 atm hydrogen), sealed environment, and report the resulting reaction kinetics and uranium hydride blister benchmarking data. We find that carbon content is not strongly correlated with reaction kinetics terms or the resulting hydride blister number and area, but that there is a tight relationship between corrosion blister number/area and kinetics as is expected. Further, we find that there is a strong trend of decreasing variance in the blister number, blister area, and induction time as carbon content increases (higher carbon content results in more reproducible blister populations). Additionally, we find a narrow band of uranium metal consumption at the end of the parabolic phase of reaction progress (beginning of linear growth phase) of 0.098 ± 0.011 w/w%, a fact that may be useful in assaying hydrogen corrosion of uranium metal within sealed environments generally.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Early age hydration and application of blended magnesium potassium phosphate cements for reduced corrosion of reactive metals

Highlights: • Magnesium potassium phosphate cements were studied for nuclear waste encapsulation. • The optimised formulation in this study was determined to be 0.24 w/s ratio. • Different reaction kinetics were discovered for the FA/MKPC and BFS/MKPC binders. • Struvite-K was the only crystalline reaction product observed via in-situ SXPD. • Uranium trials revealed MKPC corrosion was reduced compared to a UK nuclear grout. Magnesium potassium phosphate cements (MKPC) were investigated to determine their efficacy towards retardation of reactive uranium metal corrosion. Optimised low-water content, fly ash (FA) and blast furnace slag (BFS) blended MKPC formulations were developed and their fluidity, hydration behaviour, strength and phase assemblage investigated. In-situ time resolved synchrotron powder X-ray diffraction was used to detail the early age (~60 h) phase assemblage development and hydration kinetics, where the inclusion of BFS was observed to delay the formation of struvite-K by ~14 h compared to FA addition (~2 h). All samples set within this period, suggesting the possible formation of a poorly crystalline binding phase prior to struvite-K crystallisation. Long-term corrosion trials using metallic uranium indicated that MKPC systems are capable of limiting uranium corrosion rates (reduced by half), when compared to a UK nuclear industry grout, which highlights their potential application radioactive waste immobilisation.

36 MATERIALS SCIENCE↗

A time-dependent chloride diffusion model for predicting initial corrosion time of reinforced concrete with slag addition

The effect of granulated blast furnace slag (GBFS) addition on the threshold chloride concentration (TCC) for rebar corrosion was investigated. A modified diffusion model, coupled with a time-dependent effective diffusion coefficient and surface chloride concentration, was proposed to predict the chloride profile. The corrosion initiation time was estimated based on the model predictions and the measured TCC. The results indicate that adding GBFS decreases the TCC by lowering the pH value of the pore solution. The evolution of corrosion potential and current density is found to obey a 3-parameter Weibull distribution. MIP tests show that adding GBFS contributes to refinement of pore structure by decreasing the fraction of large capillary pores. The time-dependent model exhibits good predictive strength and helps understand how GBFS addition delays the corrosion initiation by retarding the chloride diffusion, though a lower TCC is obtained.

36 MATERIALS SCIENCE↗

Influence of SiC microstructure on its corrosion behavior in molten FLiNaK salt

The influence of the microstructure on the corrosion rate of three monolithic SiC samples in FLiNaK salt at 900 °C for 250 h was studied. The SiC samples, labeled as SiC-1, SiC-2, and SiC-3, had corrosion rates of 0.137, 0.020, and 0.043 mg/cm 2 h, respectively. Compared with grain size and the presence of special grain boundaries (i.e., Σ3), the content of high-angle grain boundaries (HAGBs) appeared to have the strongest influence on the corrosion rate of SiC in FLiNaK salt, since the corrosion rate increased six times as the concentration of high-angle grain boundaries increased from 19 to 32% for SiC-2 and SiC-1, respectively. The results here stress the importance of controlling the content of HAGBs during the production process of SiC.

36 MATERIALS SCIENCE↗

A study of corrosion on electrodeposited superhydrophobic copper surfaces

This study considers the corrosion characteristics of superhydrophobic copper surfaces with multiscale asperities formed inherently on a copper substrate, using a facile, low energy, electrodepostion method. A systematic study is presented for the first time on the effect of surface functionalization time on long-term immersion in a wide range of corrosive environments from the extremely acidic to the extremely alkaline. The corrosion resistance is also reported for the first time as a function of temperature in the range 23–85°C. The superhydrophobic surfaces are shown to enhance corrosion resistance by up to four orders of magnitude compared to bare copper.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Uranium hydride corrosion. II Modeling spatially random growth using reaction and nucleation kinetics

A uranium hydride (UH 3 ) corrosion kinetics model has been developed, based on dimensionally restricted nucleation kinetics, which combines heretofore separate reaction and nucleation kinetics models into a single predictive construct. This theoretical framework accounts for the superficial and random pitting behaviour of UH 3 corrosion. The model can be used to generate the net corrosion surface area and volume fractions for a uranium specimen, generally accounting for its geometric form factor through the surface-to-volume ratio. Furthermore, the combined corrosion kinetics model enables the generation of quantities which may be directly compared to those obtained by non-destructive, non-contact evaluation methods.

36 MATERIALS SCIENCE↗

Effect of oxide impurities on the corrosion behavior of structural materials in molten LiF-NaF-KF

The corrosion of materials in molten fluoride salts is largely influenced by the presence of impurities in the salt. Very few studies have been done on the effect of oxide impurities on the corrosion of structural alloys in molten fluoride salts. In this study, corrosion behavior of selected alloys was studied in molten FLiNaK with the addition of different oxides such as Li 2 O, NiO, and Cr 2 O 3 . The results show that addition of oxides can lead to significant effects on this corrosion, depending on the type and amount of oxide added and the alloy being used.

14 SOLAR ENERGY↗

Corrosion of 316 L stainless steel under the natural circulation of molten NaCl-MgCl 2 salt

The corrosion behavior of 316 L stainless steel (SS) was studied via the natural circulation of molten eutectic NaCl-MgCl 2 salt through a microloop. The post-corrosion tested 316 L SS microloop sections were characterized with microscopy techniques to determine the microstructural and microchemical changes that occurred at the alloy/salt interface. It was found that 316 L SS showed heterogeneous dissolution at the hot-leg, whereas deposition of corrosion products occurred at the cold-leg. For the first time, experimentally obtained molten salt flow-induced corrosion of 316 L SS results were combined with computational thermodynamic-kinetic models to validate the dissolution and deposition in terms of elemental compositional changes at the alloy/salt interface. The thermodynamic-kinetic modeling predicted that the heterogeneous dissolution of Cr and Fe from the hot-leg section of 316 L SS persisted throughout the salt circulation. The model also estimated that, despite Cr deposition starting earlier than Fe, the total redeposition of Fe is expected to be significantly greater than that of Cr over the circulation of salt. Furthermore, the modeling accurately predicted the subsurface enrichment of Mo which is attributed to the reduced Cr activity and the relatively higher diffusion rate of Mo within the alloy matrix. Here, the agreement between modeling and experimental results confirms that Fe chlorides dissolve at the hot-leg and subsequently deposit at the cold-leg due to activity changes driven by the thermal gradient. By contrast, Cr was not detected in the cold-leg deposits, which is attributed to its weaker temperature dependence on activity, limiting its redeposition under these conditions.

36 - MATERIALS SCIENCE↗

Validating corrosion models: A comparison of governing equations

Experimental validation of Finite Element Method (FEM) models varying electrochemical governing equations, inclusion of chemical reactions, and time on the resultant damage profile for two galvanic couples is explored. Two anode materials (Magnesium AZ31 and Carbon Steel) in contact with a cathode (Stainless Steel 304 L) were modeled in/exposed to NaCl (1 and 0.1 M respectively for the anode materials) for up to one week. The physics approach, inclusion of chemical reactions, and the boundary conditions required to accurately represent the damage profile in FEM models depended on the galvanic couple materials and, ultimately, the corrosion rate. For high rates of corrosion (i.e., magnesium anode), the Nernst-Planck equation with Electroneutrality was sufficient to describe the damage, while, for low rates of corrosion (i.e., carbon steel anode), the Laplace equation was sufficient. In all cases, the most complete governing equation (Nernst-Planck-Poisson Equation) was not necessary to accurately describe the damage. Precipitation reactions in solution also played a critical role in the predicted damage profile, especially for high corrosion rate systems. Finally, for short time periods (< 6 h), the choice of governing equations does not significantly influence damage profile results. Overall, the choice of physics to reduce error in simulations relies on the boundary conditions, geometry, conductivity of the solution, electrochemical potential differences, and time of exposure. The above results are discussed with regard to accuracy and computational savings.

Carbon steel↗

Corrosion resistance of functionally graded TiN/Ti coatings for proton exchange membrane fuel cells

Bipolar Plates (BPP) are important components of proton exchange membrane fuel cell (PEMFC) stacks. In the development of innovative fuel cell designs, it is advantageous to use aluminum for these applications, however, this material lacks the necessary corrosion resistance. Since the performance of PEMFC stacks depends on BPP properties, in particular, corrosion resistance, depositing titanium nitride (TiN) thin films onto aluminum substrates may improve their efficiency and durability. Present work focuses on improving corrosion resistance and hydrophobicity of TiN/Ti by using N graded films deposited onto aluminum substrates (AA-1100) by grid-assisted magnetron sputtering (GAMS). Electrochemical impedance spectroscopy (EIS) with potentiodynamic and potentiostatic polarization are used to investigate the performance of the substrate/film system at room temperature and 70 oC, thus simulating a prototypic PEMFC electrolyte environment. Electrochemical test results showed that graded TiN films improved corrosion resistance when compared with both the homogeneous films and the AA1100 uncoated substrate. Furthermore, contact angle results reveal improved hydrophobicity for both homogeneous and graded TiN coatings when compared with the AA1100 substrate.

25 ENERGY STORAGE↗

In-situ visualization of corrosion behavior of Al CoCrFeNi high-entropy alloys during electrochemical polarization

In this study, the corrosion behavior of the Al x CoCrFeNi (x = 0.3, 0.5, 0.7) high-entropy alloys (HEAs) is investigated by an in-situ visualization system. Surface morphology changes on both micro-spatial and temporal scales are monitored in the 3.5 wt% NaCl solution during the potentiodynamic polarization. The microstructures of the Al x CoCrFeNi HEAs are characterized by SEM, EBSD, and EDS. The results show that the microstructure evolves from singe face-centered cubic (FCC) phase to multi-phases by increasing the Al content. The in-situ observations directly reveal the different localized corrosion processes in the AlxCoCrFeNi HEAs. In the single FCC phase Al 0.3 CoCrFeNi HEA, localized corrosion shows in the form of pitting. In the Al 0.5 CoCrFeNi and Al 0.7 CoCrFeNi alloys, which possess FCC and body-centered cubic (BCC) phases, the localized corrosion initiates and propagates in the Cr-depleted BCC phase. In addition, the in-situ visualization uncovers the evolution of current serration, which represents the propagation and repassivation of metastable pit during the polarization. The frequent occurrence of metastable pits indicates distinct repassivation ability of the Al 0.3 CoCrFeNi HEA.

36 MATERIALS SCIENCE↗

Effect of cold forging on the microstructure and corrosion behavior of type 316L stainless steel in molten FLiNaK salt

Here, the effect of cold forging on the microstructure and corrosion behavior of 316L stainless steel (SS) in molten salt was investigated. Static corrosion experiments were performed in FLiNaK (LiF-NaF-KF: 46.5–11.5–42 mol.%) at 600 °C for 50 h in a glove box. The results show that cold forging gives rise to enhanced corrosion of 316L SS in molten fluoride salt due to the increase of crystallographic defects. Based on the potentiodynamic polarization results, the corrosion current density of 50 % cold-forged 316L SS is about 2.1 times larger than that of the as-received 316L SS in molten FLiNaK salt at 600 °C.

316L stainless steel↗