Search NASA⌕ Search

SEARCH · Search NASA

Results for “GAS WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Hydrogen embrittlement of structural steels.

Carbon-manganese steels are candidates for the structural materials in hydrogen gas pipelines, however it is well known that these steels are susceptible to hydrogen embrittlement. Decades of research and industrial experience have established that hydrogen embrittlement compromises the structural integrity of steel components. This experience has also helped identify the failure modes that can operate in hydrogen containment structures. As a result, there are tangible ideas for managing hydrogen embrittement in steels and quantifying safety margins for steel hydrogen containment structures. For example, fatigue crack growth aided by hydrogen embrittlement is a key failure mode for steel hydrogen containment structures subjected to pressure cycling. Applying appropriate structural integrity models coupled with measurement of relevant material properties allows quantification of safety margins against fatigue crack growth in hydrogen containment structures. Furthermore, application of these structural integrity models is aided by the development of micromechanics models, which provide important insights such as the hydrogen distribution near defects in steel structures. The principal objective of this project is to enable application of structural integrity models to steel hydrogen pipelines. The new American Society of Mechanical Engineers (ASME) B31.12 design code for hydrogen pipelines includes a fracture mechanics-based design option, which requires material property inputs such as the threshold for rapid cracking and fatigue crack growth rate under cyclic loading. Thus, one focus of this project is to measure the rapid-cracking thresholds and fatigue crack growth rates of line pipe steels in high-pressure hydrogen gas. These properties must be measured for the base materials but more importantly for the welds, which are likely to be most vulnerable to hydrogen embrittlement. The measured properties can be evaluated by predicting the performance of the pipeline using a relevant structural integrity model, such as that in ASME B31.12. A second objective of this project is to enable development of micromechanics models of hydrogen embrittlement in pipeline steels. The focus of this effort is to establish physical models of hydrogen embrittlement in line pipe steels using evidence from analytical techniques such as electron microscopy. These physical models then serve as the framework for developing sophisticated finite-element models, which can provide quantitative insight into the micromechanical state near defects. Understanding the micromechanics of defects can ensure that structural integrity models are applied accurately and conservatively.

08 HYDROGEN↗

Oxy-Combustion Boiler Material Development

Under U.S. Department of Energy Cooperative Agreement No. DE-NT0005262 Foster Wheeler North America Corp conducted a laboratory test program to determine the effect of oxy-combustion on boiler tube corrosion. In this program, CFD modeling was used to predict the gas compositions that will exist throughout and along the walls of air-fired and oxy-fired boilers operating with low to high sulfur coals. Test coupons of boiler tube materials were coated with deposits representative of those coals and exposed to the CFD predicted flue gases for up to 1000 hours. The tests were conducted in electric tube furnaces using oxy-combustion and air-fired flue gases synthesized from pressurized cylinders. Following exposure, the test coupons were evaluated to determine the total metal wastage experienced under air and oxy-combustions conditions and materials recommendations were made. Similar to air-fired operation, oxy-combustion corrosion rates were found to vary with the boiler material, test temperature, deposit composition, and gas composition. Despite this, comparison of air-fired and oxy-fired corrosion rates showed that oxy-firing rates were, for the most part, similar to, if not lower than those of air-firing; this finding applied to the seven furnace waterwall materials (wrought and weld overlay) and the ten superheater/reheater materials (wrought and weld overlay) that were tested. The results of the laboratory oxy-combustion tests, which are based on a maximum bulk flue gas SO 2 level of 3200 ppmv (wet) / 4050 ppmv (dry), suggest that, from a corrosion standpoint, the materials used in conventional subcritical and supercritical, air-fired boilers should also be suitable for oxy-combustion retrofits. Although the laboratory test results are encouraging, they are only the first step of a material evaluation process and it is recommended that follow-on corrosion tests be conducted in coal-fired boilers operating under oxy-combustion to provide longer term (one to two year) data. The test program details and data are presented herein.

20 FOSSIL-FUELED POWER PLANTS↗

Oxy-Combustion Boiler Material Development

Under U.S. Department of Energy Cooperative Agreement No. DE-NT0005262 Foster Wheeler North America Corp conducted a laboratory test program to determine the effect of oxy-combustion on boiler tube corrosion. In this program, CFD modeling was used to predict the gas compositions that will exist throughout and along the walls of air-fired and oxy-fired boilers operating with low to high sulfur coals. Test coupons of boiler tube materials were coated with deposits representative of those coals and exposed to the CFD predicted flue gases for up to 1000 hours. The tests were conducted in electric tube furnaces using oxy-combustion and air-fired flue gases synthesized from pressurized cylinders. Following exposure, the test coupons were evaluated to determine the total metal wastage experienced under air and oxy-combustions conditions and materials recommendations were made. Similar to air-fired operation, oxy-combustion corrosion rates were found to vary with the boiler material, test temperature, deposit composition, and gas composition. Despite this, comparison of air-fired and oxy-fired corrosion rates showed that oxy-firing rates were, for the most part, similar to, if not lower than those of air-firing; this finding applied to the seven furnace waterwall materials (wrought and weld overlay) and the ten superheater/reheater materials (wrought and weld overlay) that were tested. The results of the laboratory oxy-combustion tests, which are based on a maximum bulk flue gas SO2 level of 3200 ppmv (wet) / 4050 ppmv (dry), suggest that, from a corrosion standpoint, the materials used in conventional subcritical and supercritical, air-fired boilers should also be suitable for oxy-combustion retrofits. Although the laboratory test results are encouraging, they are only the first step of a material evaluation process and it is recommended that follow-on corrosion tests be conducted in coal-fired boilers operating under oxy-combustion to provide longer term (one to two year) data. The test program details and data are presented herein.

36 MATERIALS SCIENCE↗

Fluid modeling of low-temperature plasmas

Fluid models are essential for understanding and predicting low-temperature plasma (LTP) behavior in various scientific and industrial settings. This paper provides an introductory tutorial on fluid modeling of LTPs, covering model formulation, implementation, and computational simulations. The tutorial focuses on five main components of the formulation of LTP fluid models: fluid flow, energy, chemistry, electromagnetism, and material properties, as well as in essential aspects of model implementations, including multiscale phenomena, multiphysics coupling, and numerical convergence. Designed for students and early-career researchers, this work offers a practical foundation for developing and using fluid models, from in-house computational codes to commercial software, bridging fundamental theory with real-world applications.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Stainless steel corrosion by molten nitrates : analysis and lessons learned.

A secondary containment vessel, made of stainless 316, failed due to severe nitrate salt corrosion. Corrosion was in the form of pitting was observed during high temperature, chemical stability experiments. Optical microscopy, scanning electron microscopy and energy dispersive spectroscopy were all used to diagnose the cause of the failure. Failure was caused by potassium oxide that crept into the gap between the primary vessel (alumina) and the stainless steel vessel. Molten nitrate solar salt (89% KNO{sub 3}, 11% NaNO{sub 3} by weight) was used during chemical stability experiments, with an oxygen cover gas, at a salt temperature of 350-700 C. Nitrate salt was primarily contained in an alumina vessel; however salt crept into the gap between the alumina and 316 stainless steel. Corrosion occurred over a period of approximately 2000 hours, with the end result of full wall penetration through the stainless steel vessel; see Figures 1 and 2 for images of the corrosion damage to the vessel. Wall thickness was 0.0625 inches, which, based on previous data, should have been adequate to avoid corrosion-induced failure while in direct contact with salt temperature at 677 C (0.081-inch/year). Salt temperatures exceeding 650 C lasted for approximately 14 days. However, previous corrosion data was performed with air as the cover gas. High temperature combined with an oxygen cover gas obviously drove corrosion rates to a much higher value. Corrosion resulted in the form of uniform pitting. Based on SEM and EDS data, pits contained primarily potassium oxide and potassium chromate, reinforcing the link between oxides and severe corrosion. In addition to the pitting corrosion, a large blister formed on the side wall, which was mainly composed of potassium, chromium and oxygen. All data indicated that corrosion initiated internally and moved outward. There was no evidence of intergranular corrosion nor were there any indication of fast pathways along grain boundaries. Much of the pitting occurred near welds; however this was the hottest region in the chamber. Pitting was observed up to two inches above the weld, indicating independence from weld effects.

36 MATERIALS SCIENCE↗

LOCALIZED CORROSION OF AUSTENITIC STAINLESS STEELEXPOSED TO MIXTURES OF PLUTONIUM OXIDE AND CHLORIDE SALTS

Laboratory corrosion tests were conducted to investigate the corrosivity of moist plutonium oxide/chloride (PuO{sub 2}/Cl-) salt mixtures on 304L and 316L stainless steel coupons. The tests exposed flat coupons for pitting evaluation and 'teardrop' stressed coupons for stress corrosion cracking (SCC) evaluation at room temperature to various mixtures of PuO{sub 2} and chloride-bearing salts for periods up to 500 days. The two flat coupons were placed so that the solid oxide/salt mixture contacted about one half of the coupon surface. One teardrop coupon was placed in contact with solid mixture; the second teardrop was in contact with the headspace gas only. The mixtures were loaded with nominally 0.5 wt % water under a helium atmosphere. Observations of corrosion ranged from superficial staining to pitting and SCC. The extent of corrosion depended on the total salt concentration and on the composition of the salt. The most significant corrosion was found in coupons that were exposed to 98 wt % PuO{sub 2}, 2 wt % chloride salt mixtures that contained calcium chloride. SCC was observed in two 304L stainless steel teardrop coupons exposed in solid contact to a mixture of 98 wt % PuO{sub 2}, 0.9 wt % NaCl, 0.9 wt % KCl, and 0.2 wt % CaCl{sub 2}. The cracking was associated with the heat-affected zone of an autogenous weld that ran across the center of the coupon. Cracking was not observed in coupons exposed to the headspace gas, nor in coupons exposed to other mixtures with either 0.92 wt% CaCl{sub 2} or no CaCl{sub 2}. The corrosion results point to the significance of the interaction between water loading and the concentration of the hydrating salt CaCl{sub 2} in the susceptibility of austenitic stainless steels to corrosion.

36 MATERIALS SCIENCE↗

Helium pressure increase inside GPHS clads: implications for formation of distended clads

Distension of GPHS clads has generally been attributed to gas buildup inside the clad. The bulging vent frit cover can be caused only by gas pressure, since the vent cover is isolated from the fuel by the vent frit. Gas generation is the only change expected as the oxide fuel ages. However, several data suggest that gas pressure is not the origin of the distension of the clad body. Gas pressure sufficient to distend the iridium body of the clad would be on the order of 1500 psi. This high pressure is very unlikely to be reached inside a GPHS clad, because the vent frit cover weld cannot sustain high pressures. Every distended clad that has been examined has an open vent frit, suggesting that the vent frit cover eventually opens on all distended GPHS clads. No gas pressure has been observed in any distended clad. In addition, the vent frit cover is sufficiently thin, about 2 grains thick, that diffusion of helium through the intact cover is possible and almost certainly occurs. Conversely, no clad has ever been definitively observed to distend after venting. Removal of the vent cover allows free escape of any radiolytically generated helium. However, there is little data on the behavior of vented GPHS. The vent cover is seldom removed at LANL, and vent covers are not removed on clads that will be stored. The vent covers are known to have been removed from the four clads residing in a module which was stored for 8 years. Expansion of the fuel is more likely to provide sufficient force on the iridium clad to distort the iridium metal. Radiographs indicate that the fuel inside a distended GPHS clad is also distended, filling all or most of the interior volume of the GPHS. No radiograph shows the fuel expanded and in contact with the weld shield and the distorted side of the GPHS clad without distension. However, radiography is infrequently done on stored clads unless they exhibit distension, so the dimensions of fuel in normal clads are not generally known.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Cold Spray Deposition of 304L Stainless Steel to Mitigate Chloride-Induced Stress Corrosion Cracking in Canisters for Used Nuclear Fuel Storage

A feasibility study of the cold spray deposition process of 304L stainless steel on 304L stainless steel substrates as a mitigation method for chloride-induced stress corrosion cracking (CISCC) has been investigated under various substrate conditions. The study is aimed at the application of this technology to mitigate CISCC that may potentially occur in or nearthe fusion welded regions of stainless steel canisters in Dry Cask Storage System (DCSS) for used nuclear fuels. Spherical gas-atomized 304L stainless steel powder, in the size range of 25 µm to 44 µm, was used as a feedstock powder for the cold spray process. The powder was deposited on four types of 304L substrates with various surface conditions: as-polished, oxidized, cold-rolled, plates with prototypical CISCC. The effects of cold spray parameters on quality of cold spray coatings were investigated. Thickness, porosity, and phases in the as-deposited materials were evaluated using scanning electron microscopy (SEM) and X-ray diffraction (XRD), and correlated with microhardness and adhesion strength measured via micro-indentation and ASTM C633 pulling test, respectively. XRD analysis of the coatings was also conducted to examine the effects of cold spray condition on residual stress state in the coating. Detailed cross-sectional examination of coating/substrate interfaces was performed with transmission electron microscopy (TEM) equipped with energy dispersive spectroscopy (EDS). Dense and continuous coatings with good adhesion strength and hardness were produced for the various substrate conditions by adjusting cold spray parameters. The results demonstrate that cold spray stainless steel coating is a viable option to provide a physical barrier against CISCC in fusion weld regions of stainless steel in corrosive chloride salt-bearing environments.

Dry Cask Storage Systems, cold spray, 304L stainle↗

An approach for spent nuclear fuel containment integrity verification using gas tagging

Verification of containment integrity is required for spent nuclear fuel (SNF) managed by the commercial nuclear industry and U.S. Department of Energy (DOE), especially after extended storage. Certain SNF storage systems, such as the DOE road-ready dry storage system, hold several packaged containments within a welded over-canister. These packaged containments are called Department of Energy Standard Canisters (DOESCs). DOESC leakage identification is challenging because their containment boundary cannot be accessed for testing and their contents (i.e., SNF and fill gas) are often similar. There are concerns that this could result in costly characterization and repackaging operations of DOE road-ready dry storage systems if compromised DOESCs are suspected. Here, to address these concerns, this paper presents an approach for applying a gas tagging process using xenon to uniquely identify compromised inaccessible containments following extended storage. The containments considered for this application are seven DOESCs, each packaged within a single over-canister. Two different SNF loading configurations from the Advanced Test Reactor and Fort Saint Vrain nuclear power plant are considered. These configurations are used to represent research reactor aluminum-clad spent nuclear fuel (ASNF) and TRi-structural ISOtropic (TRISO) SNF types. Results for this application show that for ASNF and TRISO type fuels for which the selected fuels are representative, the volume of taggant required at loading is determined primarily by the lower detection limit and leak rate of taggant from a compromised DOESC, rather than the amount of fission-generated xenon in the loaded fuel. While the application presented is suited for larger leaks, smaller leaks could be detected by modifying certain design parameters. This gas tagging approach can also be applied to other DOE containments and advanced reactor SNF storage systems.

07 - ISOTOPES AND RADIATION SOURCES↗

Nonequilibrium Phenomena in (Quasi-)thermal Plasma Flows

Thermal plasmas are utilized in diverse applications that require high power densities or throughputs, such as metal cutting, welding, spraying, metallurgy, and materials synthesis. Thermal plasma applications involve interactions between the highly energetic plasma and working gas streams, confining devices, or processing materials. Whereas thermal plasma implies a state of equilibrium (i.e. Local Thermodynamic Equilibrium, LTE), due to the above interactions, thermal plasma flows depict nonequilibrium phenomena of two types: kinetic and dissipative. Kinetic nonequilibrium manifests microscopically and is caused by localized imbalances between particles and fields interactions. Its occurrence is illustrated, for example, as deviations from thermal equilibrium between heavy-species and electrons or from mass-action laws. In contrast, dissipative nonequilibrium reveals macroscopically and is produced by external driving forces that incite distributed responses, such as the growth of instabilities, the occurrence of self-organization, or the establishment of turbulence. While kinetic nonequilibrium has been increasingly incorporated in thermal plasma flow models (e.g. finite-rate chemistry, two-temperature models), it is the great advances in numerical computing that is enabling the exploration of dissipative nonequilibrium (e.g. pattern formation, small-scale turbulent features). Both types of nonequilibrium are reviewed, including their estimation and incidence, within the context of computational models and their relevance to thermal plasma sources and processes.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Synthesis of nanoscale magnesium diboride powder

A procedure has been developed for the preparation of small grained magnesium diboride (MgB 2 ) powder by reacting nanometer size boron powder in a magnesium vapor. Plasma synthesized boron powder that had particle sizes ranging from 20 to 300nm was mixed with millimeter size chunks of Mg by rolling stoichiometric amounts of the powders in a sealed cylindrical container under nitrogen gas. This mixture then was placed in a niobium reaction vessel, evacuated, and sealed by e-beam welding. The vessel was typically heated to approximately 830°C for several hours. The resulting MgB 2 particles have a grain size in the 200 nm to 800 nm range. Agglomerates of loosely bound particles could be broken up by light grinding in a mortar and pestle. At 830°C, many particles are composed of several grains grown together so that the average particle size is about twice the average grain size. Furthermore, experiments were conducted primarily with undoped boron powder, but carbon-doped boron powder showed very similar results.

36 MATERIALS SCIENCE↗

Relative Humidity and the Susceptibility of Austenitic Stainless Steel to Stress Corrosion Cracking in an impure Plutonium Oxide Environment

Laboratory tests to investigate the corrosivity of moist plutonium oxide/chloride salt mixtures on 304L and 316L stainless steel coupons showed that corrosion occurred in selected samples. The tests exposed flat coupons for pitting evaluation and 'teardrop' stressed coupons for stress corrosion cracking (SCC) evaluation at room temperature to various mixtures of PuO{sub 2} and chloride-bearing salts for periods up to 500 days. The exposures were conducted in sealed containers in which the oxide-salt mixtures were loaded with about 0.6 wt % water from a humidified helium atmosphere. Observations of corrosion ranged from superficial staining to pitting and SCC. The extent of corrosion depended on the total salt concentration, the composition of the salt and the moisture present in the test environment. The most significant corrosion was found in coupons that were exposed to 98 wt % PuO{sub 2}, 2 wt % chloride salt mixtures that contained calcium chloride and 0.6 wt% water. SCC was observed in two 304L stainless steel teardrop coupons exposed in solid contact to a mixture of 98 wt % PuO{sub 2}, 0.9 wt % NaCl, 0.9 wt % KCl, and 0.2 wt % CaCl{sub 2}. The cracking was associated with the heat-affected zone of an autogenous weld that ran across the center of the coupon. Cracking was not observed in coupons exposed to the headspace gas above the solid mixture, or in coupons exposed to other mixtures with either no CaCl{sub 2} or 0.92 wt% CaCl{sub 2}. SCC was present where the 0.6 wt % water content exceeded the value needed to fully hydrate the available CaCl{sub 2}, but was absent where the water content was insufficient. These results reveal the significance of the relative humidity in the austenitic stainless steels environment to their susceptibility to corrosion. The relative humidity in the test environment was controlled by the water loading and the concentration of the hydrating salts such as CaCl{sub 2}. For each salt or salt mixture there is a threshold relative humidity below which the necessary liquid electrolyte cannot exist, and therefore below which the SCC risk is very low. This threshold is a thermodynamic quantity known as the deliquescence relative humidity that is dependent on the identity of the salt but is independent of the quantity of salt. Below the deliquescence RH there should be low corrosion risk, and above it the corrosion risk increases rapidly as a liquid phase, which is initially saturated with salt, grows and becomes more widespread in the container.

36 MATERIALS SCIENCE↗

Sampling and Analysis of the Headspace Gas in 3013 Type Plutonium Storage Containers at Los Alamos National Laboratory

Department of Energy (DOE) sites have packaged approximately 5200 3013 containers to date. One of the requirements specified in DOESTD-3013, which specifies requirements for packaging plutonium bearing materials, is that the material be no greater than 0.5 weight percent moisture. The containers are robust, nested, welded vessels. A shelf life surveillance program was established to monitor these cans over their 50 year design life. In the event pressurization is detected by radiography, it will be necessary to obtain a head space gas sample from the pressurized container. This technique is also useful to study the head space gas in cans selected for random destructive evaluation. The atmosphere is sampled and the hydrogen to oxygen ratio is measured to determine the effects of radiolysis on the moisture in the container. A system capable of penetrating all layers of a 3013 container assembly and obtaining a viable sample of the enclosed gas and an estimate of internal pressure was designed.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Multichannel gas-uptake/evolution reactor for monitoring liquid-phase chemical reactions

The design of a headspace pressure-monitoring reactor for measuring the uptake/evolution of gas in gas–liquid chemical transformations is described. The reactor features a parallel setup with ten-reactor cells, each featuring a low working volume of 0.2–2 ml, a pressure capacity from 0 to 150 PSIa, and a high sensitivity pressure transducer. The reactor cells are composed of commercially available disposable thickwalled glassware and compact monolithic weld assemblies. The software interface controls the reactor temperature while monitoring pressure in each of the parallel reactor cells. Reactions are easy to set up and yield high-density gas uptake/evolution data. This instrument is especially well suited to acquire quantitative time-course data for reactions with small quantities of gas consumed or produced.

47 OTHER INSTRUMENTATION↗

Electrically driven rapidly vaporizing foils, wires and strips used for collision welding and sheet metal forming

A method for forming a piece of a sheet metal is performed by positioning a consumable body, made of metal, proximate to the piece of the sheet metal. The consumable body is rapidly vaporized, and the gas pressure generated thereby is directed into the piece of the sheet metal. This results in acceleration of the piece of sheet metal, and it is collided into a stationary body at a velocity, generally in excess of 200 m/s. Depending upon the type of stationary body, the piece of sheet metal is deformed into a predetermined shape or is welded onto the stationary body. The vaporization is accomplished by passing a high current of electricity into the consumable body. The effect of the vaporized metal may be augmented by additional components in the consumable body.

36 MATERIALS SCIENCE↗

Using Additive Manufacturing to Repair Gas Turbine Hot Section Components

Ni-based superalloys are used in the hot sections of gas turbine engines due to their excellent high temperature performance. During service the material degrades due to exposure at high temperature and mechanical loads. Hence, utility provides often inspect, service, and repair components in gas turbine engines to ensure safe operation. A major challenge, however, is that the most heat-resistant alloys are generally considered ‘non-weldable’ rendering them difficult to repair via welding operations. In these cases components are often scrapped and then replaced by parts which must be re-manufactured. This burdens utilities with additional cost and supply chain issues can result in long term outages or reduced operating limtis. In this work EPRI and ORNL investigated a proposed repair strategy for gas turbine hot section components. Hot section superalloy GTD-111 was selected as a candidate repair material system and AM material ABD-900 the repair material. Sandwich structures were fabricated via electron beam melting additive manufacturing (EBM-AM) producing tensile bars with gage sections consisting of dissimilar ABD-900 / GTD-111 / ABD-900 material. Metallography revealed that the interface exhibited no deleterious phases or processing defeats. Creep rupture experiments on heat treated material demonstrates that the emulated repair coupons exhibit creep resistance between GTD-111 and ABD-900. This study demonstrates that the proposed EBM-AM repair strategy presents a viable opportunity towards enabling AM repair of gas turbine engine components.

99 GENERAL AND MISCELLANEOUS↗

Using Additive Manufacturing to Repair Gas Turbine Hot Section Components

Ni-based superalloys are used in the hot sections of gas turbine engines due to their excellent high temperature performance. During service the material degrades due to exposure at high temperature and mechanical loads. Hence, utility provides often inspect, service, and repair components in gas turbine engines to ensure safe operation. A major challenge, however, is that the most heat-resistant alloys are generally considered ‘non-weldable’ rendering them difficult to repair via welding operations. In these cases components are often scrapped and then replaced by parts which must be re-manufactured. This burdens utilities with additional cost and supply chain issues can result in long term outages or reduced operating limits. In this work EPRI and ORNL investigated a proposed repair strategy for gas turbine hot section components. Hot section superalloy GTD-111 was selected as a candidate repair material system and AM material ABD-900 the repair material. Sandwich structures were fabricated via electron beam melting additive manufacturing (EBM-AM) producing tensile bars with gage sections consisting of dissimilar ABD-900 / GTD-111 / ABD-900 material. Metallography revealed that the interface exhibited no deleterious phases or processing defeats. Creep rupture experiments on heat treated material demonstrates that the emulated repair coupons exhibit creep resistance between GTD-111 and ABD-900. This study demonstrates that the proposed EBM-AM repair strategy presents a viable opportunity towards enabling AM repair of gas turbine engine components.

36 MATERIALS SCIENCE↗