Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructural evolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Strengthening mechanisms, hardening/softening behavior, and microstructure evolution in an LPSO magnesium alloy at elevated temperatures

Here, rapid degradation of the mechanical properties of conventional Mg alloys with temperature precludes their wide application in industry. The LPSO (long period stacking ordered) Mg alloys, on the other hand, show considerable potential to achieve excellent high-temperature mechanical performance. In this study, a Mg-5.1Y-2.4Zn (wt.%) extrusion alloy with the microstructure comprising of α-Mg matrix and LPSO phase was prepared. It is shown that the yield strength of the alloy at 200 °C retained ~83% of the yield strength of 198 MPa at room temperature (RT). Importantly, the ductility also improved, owing to the increased non-basal slip activities at elevated temperatures. In contrast to RT and 200 °C, the alloy exhibited softening tensile behavior with an apparent loss of yield strength at 300 °C. In-situ lattice strain analysis revealed that load transfer from α-Mg to LPSO remains effective at temperatures up to 200 °C, governing the high yield strength of the alloy. The post-mortem analysis by means of electron microscopy confirmed that the LPSO phase is structurally stable at 200 °C. In particular, the high strain hardenability is rationalized by the sandwiched LPSO structures together with stacking faults serving as effective obstacles to the motion of non-basal dislocations. The load transfer effect disappears at the temperature of 300 °C, resulting in the fast deterioration of strength of the alloy. The cracking of the LPSO phase along with the recrystallizing of α-Mg grains were found to be the main causes for the softening behavior of the alloy at 300 °C.

36 MATERIALS SCIENCE↗

Friction stir welded AM50 and AZ31 Mg alloys: Microstructural evolution and improved corrosion resistance

One of the major drawbacks of Mg alloys is poor weldability, caused by porosity formation during conventional fusion welding processes. Friction Stir Welding (FSW) is promising technique in this context since it is a solid state technique. Contradicting results were published in the literature regarding the FSWed Mg alloys joint's properties. Current research was performed in order to investigate the microstructure and corrosion properties of FSWed Mg alloys, studying representatives of two commercial families: wrought AZ31-H24 and die cast AM50. It was found that in both alloys recrystallization occurred during the FSW. In AM50 the mechanism of the recrystallization was continuous, manifested by dislocation rearrangement into sub grain boundaries. In AZ31 discontinuous recrystallization had occurred through grain boundaries migration - twins rotated with respect to the matrix, turning into low angle grain boundaries. Corrosion resistance has improved during the FSW in both alloys to different extents. In the AM50 alloy, the nugget exhibited significantly higher surface potential than the base metal mainly due to the higher Al concentration in the matrix of the nugget, resulting from the dissolution of Al-enrichment and β-Mg{sub 17}Al{sub 12} phase. In the AZ31 alloy, no change in Al concentration had occurred, and the surface potential measured in the nugget was only slightly higher than in the base metal. These results underline the appropriateness of the FSW for Mg alloys since during the conventional welding deterioration of the corrosion resistance occurs. - Highlights: • Following FSW, AZ31-H24 experienced discontinuous recrystallization. • In AZ31 grain boundaries migration occurred, thus twins rotated. • In die cast AM50 continuous recrystallization occurred during the FSW. • In AM50 - dislocations rearranged into sub grain boundaries. • Corrosion resistance has improved during the FSW in both alloys to different extent.

36 MATERIALS SCIENCE↗

Microstructure Evolution During Controlled Solidification of “Fe{sub 2}O{sub 3}”-CaO-SiO{sub 2} Liquids in Air

The principal chemical components in iron ore sintering are Fe{sub 2}O{sub 3}, CaO, and SiO{sub 2}. This sintering process consists of three key steps: heating, holding at peak temperature, and cooling. During the cooling stage, a liquid oxide solidifies to form the final sinter microstructures. To investigate the fundamental processes taking place during the cooling of sinters, a new experimental technique has been developed that allows the stages of solidification to be determined in isolation, rather than inferred from the final microstructures. Fe{sub 2}O{sub 3}-CaO-SiO{sub 2} oxide samples of a bulk composition having a CaO/SiO{sub 2} mass ratio of 3.46 and 73.2 wt pct Fe{sub 2}O{sub 3} were cooled in air from 1623 K (1350 °C) at 2 K/s, quenched at 5 K temperature intervals from 1533 K to 1453 K (1260 °C to 1180 °C), and analyzed using Electron Probe Micro X-Ray Analysis (EPMA). During cooling, four distinct stages were observed, consisting of the phase assemblages Liquid + Hematite (I), Liquid + Hematite + C{sub 2}S(II), Liquid + C{sub 2}S + CF{sub 2}(III), and C{sub 2}S + CF{sub 2} + CF (IV). This solidification sequence differs from that predicted under equilibrium and Scheil–Gulliver Cooling. Importantly, no Silico-Ferrite of Calcium (SFC) phase was observed to form on solidification of the liquid. Based on the microstructures formed and liquid compositions, measured by EPMA, it was demonstrated that kinetic factors play a major role in determining the phases and microstructures formed under the conditions investigated.

36 MATERIALS SCIENCE↗

Microstructure Evolution and Mechanical Properties of Large-Scale AZ80 Magnesium Alloy Billets Produced by Multitemperature Multidirectional Forging

Grain refinement is an effective method to improve the mechanical properties of magnesium (Mg) alloys. In the present research, the combination of multidirectional forging (MDF) and forward extrusion for sizing with decreasing temperature pass by pass was employed to deform as-cast AZ80 magnesium alloy billet with large size to obtain fine grains and homogeneous microstructure. It was found that with the increasing number of MDF passes, the average grain size decreases; the homogeneity of microstructures and the percentages of dynamic recrystallised grains increase simultaneously. After six-pass MDF, fine and homogeneous microstructure with an average grain size of 15 μm was achieved; however, grain refinement became very difficult with a further increase in the MDF pass number. After eight-pass MDF plus forward extrusion for sizing, excellent mechanical properties of large-scale AZ80 magnesium alloy billet were obtained. The tensile strength, the yield strength and the elongation of billet are 410 MPa, 292 MPa and 14%, respectively. Furthermore, during multitemperature MDF, the inverse of the square root of grain size and tensile yield strength fit well with the Hall–Petch relationship.

36 MATERIALS SCIENCE↗

Microstructure evolution of a dissimilar junction interface between an Al sheet and a Ni-coated Cu sheet joined by magnetic pulse welding

An Al sheet and a Ni-coated Cu sheet were lap joined by using magnetic pulse welding (MPW). Tensile tests were performed on the joined sheets, and a good lap joint was achieved at a discharge energy of > 0.9 kJ. The weld interface exhibited a wavy morphology and an intermediate layer along the weld interface. Microstructure observations of the intermediate layer revealed that the Ni coating region consisted of a Ni–Al binary amorphous alloy and that the Al sheet region contained very fine Al nanograins. Ni fragments indicative of unmelted residual Ni from the coating were also observed in parts of the intermediate layer. Formation of these features can be attributed to localize melting and a subsequent high rate cooling of molten Al and Ni confined to the interface during the MPW process. In the absence of an oxide film, atomic-scale bonding was also achieved between the intermediate layer and the sheet surfaces after the collision. MPW utilises impact energy, which affects the sheet surfaces. From the obtained results, good lap joint is attributed to an increased contact area, the anchor effect, work hardening, the absence of an oxide film, and suppressed formation of intermetallic compounds at the interface. - Highlights: •Good lap joint of an Al sheet and a Ni-coated Cu sheet was achieved by using magnetic pulse welding. •A Ni–Al binary amorphous alloy was formed as an intermediate layer at weld interface. •Atomic-scale bonding was achieved between the intermediate layer and the sheet surfaces.

36 MATERIALS SCIENCE↗

Modeling and Simulation of Microstructure Evolution and Deformation in an Irradiated Environment

The ability to predict the behavior of structural components in a nuclear power plant is critical to the nuclear industry. Structural metals in the primary loop of nuclear power plants must endure challenges such as irradiation and mechanical and thermal loading, and these structural metal components must continue to function in potential transient and accident conditions throughout the operational lifetime of the power plant. This extreme operational environment changes the metal microstructure by creating additional defects. The physical interactions of dislocations with these defects govern how the metal will respond to future conditions. Therefore predicting the mechanical response of these metals requires a set of physically based and reliable models of dislocation and defect interactions. These microstructure elements include glide mobile and immobile dislocations, geometrically necessary dislocations, twinning dislocations, irradiation defects, and thermal aging defects. We present here a continuum dislocation dynamics crystal plasticity framework to capture the interaction mechanisms of these dislocations and defects, verified with a combination of benchmark problems and comparisons with experimental data for two different types of structural metals: alpha iron and nickel-based alloys. In our simulations of $\alpha$ iron we highlight the advantages of applying a Monte Carlo stochastic model of cross slip dislocation motion and show the importance of capturing the 3D nature of glide dislocation and self-interstitial atom loop radiation defect interactions. We demonstrate coupling of glide dislocations with geometrically necessary dislocations to capture the influence of lattice bending, including the sensitivity of the geometrically necessary dislocations to changes in the grain boundary angle. We further examine the interaction of glide dislocations with the twin dislocations and thermally aged defects which have been observed in a nickel-based alloy with additional models. Finally we assess the reliability of this crystal plasticity framework by comparing two dislocation glide velocity models across the range of normal operation temperatures. In successfully applying our crystal plasticity framework to multiple metals, we provide further evidence of the reliability of our approach. The results of this mechanism-based continuum dislocation dynamics crystal plasticity framework can be used to inform engineering scale models throughout the nuclear industry.

36 MATERIALS SCIENCE↗

Microstructural Evolution and Mechanical Properties of LP-DED NASA HR-1 – A Hydrogen Resistant AM Superalloy for Space Propulsion Applications

The National Aeronautics and Space Administration (NASA) has actively pursued metal additive manufacturing (AM) technologies for spaceflight applications since the late 2000s. AM offers transformative advantages in cost, schedule, part consolidation, and design flexibility. Among the various AM techniques, laser powder directed energy deposition (LP-DED) is particularly well suited for fabricating complex geometries with fine feature resolution. In propulsion systems that utilize high-pressure gaseous hydrogen—such as liquid hydrogen rocket engines—hydrogen environment embrittlement (HEE) presents a serious threat to material performance 1,2 . Mechanical property degradation under these conditions can compromise component reliability, especially under cyclic loading. To address this challenge, NASA developed NASA HR-1 (Hydrogen Resistant-1) as a solution for liquid rocket engine components operating in hydrogen-rich environments, using the LP-DED technique 3-9 . A key component in a liquid rocket engine is the exhaust nozzle, which is typically regeneratively cooled (regen) due to the high heat flux. NASA HR-1 was specifically developed for regen nozzle applications using hydrogen as a propellant, providing resistance to HEE, a critical issue for many materials. The AM version of NASA HR-1 was also formulated to achieve high ultimate tensile strength, along with high yield strength and ductility in this environment 5,6 . Low-cycle fatigue (LCF) is another important consideration in nozzle design, as components are expected to endure multiple starts and missions. Additionally, the LP-DED version of the alloy exhibits improved thermal conductivity compared to its wrought counterpart, which benefits nozzle cooling. Overall, NASA HR-1 offers an excellent balance of high strength, HEE resistance, LCF performance, thermal conductivity, and ductility to meet the demanding requirements of channel-cooled nozzles and other components used with hydrogen and other propellants. The LP-DED–processed NASA HR-1 requires several post-processing heat treatment steps to achieve the material properties desirable for its intended application 6 . These steps include stress relief, homogenization, solution annealing, and aging for precipitation hardening. The stress relief treatment mitigates residual stresses accumulated during the LP-DED process and minimizes the potential for distortion. Homogenization, a common step for AM materials, reduces elemental segregation and promotes recrystallization to develop a more equiaxed grain structure. The subsequent solution annealing treatment heats the part to a solid solution temperature to dissolve the undesirable η-phase that forms during cooling from homogenization, followed by rapid cooling to retain an η-phase–free microstructure. Finally, aging promotes precipitation of the strengthening γ′ phase in the alloy. The integration of compositional design and optimized thermal processing enables high-quality LP-DED NASA HR-1 components with excellent microstructural and mechanical stability. Improved chemical and microstructure homogeneity enhances ductility and fatigue resistance—both critical for safe and reliable operation in high-pressure hydrogen environments. NASA has successfully fabricated and hot-fire tested multiple subscale and full-scale channel wall nozzles using LP-DED NASA HR-1 5,6, 9-14 . These efforts included process refinements to support thin-wall construction and various channel geometries. Throughout development, several key observations emerged. After homogenization, the as-built columnar grain structure transforms into a fully equiaxed microstructure. However, subsequent treatments—such as solution annealing and aging—result in changes that are more difficult to track. The grain structure remains largely unchanged, and the γ′ precipitates, typically 5–10 nm in diameter, are beyond the resolution of scanning electron microscopy (SEM). While transmission electron microscopy (TEM) can resolve these fine precipitates, TEM sample preparation is time-consuming and difficult for LP-DED material. As an alternative, differential scanning calorimetry (DSC) offers a useful, qualitative approach to monitor precipitate evolution throughout different stages of heat treatment. The overall goal is to improve the understanding of how heat treatment affects the microstructure and mechanical performance of LP-DED NASA HR-1. This paper presents heat treatment design considerations, microstructural characterization, mechanical testing – including tensile and LCF testing in both air and hydrogen environments.

Superalloy↗

Microstructural evolution on crystallizing the glassy phase in a 6 weight percent Y2O3-Si3N4 ceramic

X-ray diffraction and analytical electron microscopy have been used to study the crystallization of the grain-boundary glass in a 6 wt pct Y2O3-Si3N4 ceramic. Upon crystallization, high densities of dislocations formed in the Si3N4 grains and remained after 5 h at temperature. However, prolonged holds at the crystallization temperature effectively annealed out the dislocations. Other features present in the microstructure are characterized.

Lee, W. E.↗

Microstructural Evolution of NiCrBSi Coatings Fabricated by Stationary Local Induction Cladding

The development of induction cladding has been restricted by the complicated geometric characteristics of workpieces and the large heat-affected zone in the cladded workpieces. In this paper, three-dimensional continual local induction cladding (3D-CLIC) was proposed as a potential process to clad coating over a substrate with curved surface, and a stationary local induction cladding (SLIC) experiment was conducted as an exploratory study of 3D-CLIC. The microstructures and microhardness in the coatings were measured by SEM, EDS, XRD and microsclerometer, respectively. The results indicate that the coating is metallurgically bonded with the substrate without any defects. A compositional gradient exists in the diffusion transfer belt (DTB), and it decreases with the increase in induction heating time. The coating is mainly composed of (Fe, Ni), CrB, M{sub 7}C{sub 3}, Ni{sub 3}B, Ni{sub 3}Si and M{sub 23}C{sub 6} (M = Cr, Ni, Fe). Among the carbides, M{sub 7}C{sub 3} presents several morphologies and M{sub 23}C{sub 6} is always attached to the DTB. A special phenomenon of texture was found in the SLIC coatings. The preferred orientation in (200) crystal plane or the restrained orientation in (111) (200) crystal plane becomes more obvious as the scanning speed increases. The maximum average microhardness is 721 HV when the coating is heated for 5 s. The wear loss of different samples increases with increasing induction heating time. The longer heating time would result in higher dilution in the SLIC coatings due to the complete mixing with the substrate, thus leading to the decrease in microhardness and wear loss.

36 MATERIALS SCIENCE↗

Microstructure evolution, enhanced aging kinetics, and mechanical properties of AA7075 alloy after friction extrusion

In the present study we utilized Friction Extrusion (FE) a solid phase processing technique to produce fully consolidated dense 5 mm rods of AA7075 alloy. The combination of large shear stresses and temperatures at the tool-billet interface during the FE process resulted in the formation of dynamically recrystallized ~2.0 μm equiaxed grains and fine uniformly distributed stable η (MgZn 2 ) precipitates ~25–100 nm in size. Formation of such a microstructure resulted in lower solutionizing temperature and times (flash annealing) as compared to the conventionally extruded counterparts. Here we demonstrate for the first time that the solutionizing times for the T6 heat treatment of AA7075 can be reduced by three times using this FE process. In addition to being an energy efficient process, FE also serves to improve the performance of AA7075 alloys by retaining their strength while enhancing the ductility of the material. The tensile data for samples that were flash annealed and artificially aged after FE processing showed exceptional increase in ultimate tensile strength by over 19% and yield strength by over 59%, compared with an as-FE-processed sample.

36 MATERIALS SCIENCE↗

Passivation‐Induced Species Dynamics and Microstructural Evolution in Solid‐State Lithium–Sulfur Cathodes

Solid-state lithium–sulfur (SSLS) batteries offer high theoretical energy density, yet their practical viability is hindered by poor sulfur utilization and limited rechargeability. At the core of this challenge lies the passivating nature of Li 2 S, which restricts ionic and electronic transport, suppresses interfacial activity, and severely impedes the reversibility of electrochemical reactions. In this study, we elucidate the mechanistic origins of these limitations by resolving how charge and discharge species form, grow, and spatially evolve within the cathode microstructure under varied current densities and electrode compositions. By resolving the species distribution at the particle scale and coupling it with Raman spectroscopy and X-ray diffraction, we demonstrate how Li 2 S formation induces localized surface passivation that progressively limits electrochemical accessibility within the cathode microstructure. Sulfur utilization is found to be strongly governed by the interplay between sulfur loading, residual porosity, and interfacial architecture. High sulfur contents result in buried, electrochemically isolated domains due to poor solid electrolyte (SE) percolation, while low sulfur contents trigger SE degradation via parasitic reactions. The resulting sulfur-porosity maps delineate the mechanistic boundaries between reversible and transport-limited regimes, offering actionable design guidance for SSLS cathodes with enhanced sulfur utilization.

electrode microstructure↗

Phase equilibria and microstructure evolution in the Ni-rich region of binary Ni-Ce and ternary Ni-Ce-X (X=Al, Nb, Cr, Ti) systems at 900 °C

The equilibrium compositions of all phases in the Ni-rich region of binary Ni-Ce and ternary Ni-Ce-X (X=Al, Nb, Cr, Ti) systems at 900 °C were determined experimentally through isothermal annealing for up to 500 h and compared with currently available computational thermodynamic descriptions. Additionally, the study examined how adding a third element to the binary system affects the microstructure by analyzing changes in the volume fraction of the intermetallic phase in the eutectic region. It was observed that Nb and Ti addition lowered the intermetallic fraction in the eutectic region while Al and Cr addition did the opposite. The fraction of intermetallic phase in the eutectic region is very important because it contributes to extreme brittleness of these alloys. Also, Al, Nb and Ti addition promoted different precipitates upon annealing when added in sufficient amounts. The collected data on composition and phase equilibria provides crucial information for improving the thermodynamic assessments of the binary and ternary alloy systems.

energy dispersive spectrometry↗

Elucidating microstructural evolution and hardness variation across friction self-piercing riveted Al-7055 using synchrotron X-ray scattering and advanced microscopy techniques

Friction self-piercing riveting (FSPR) is a unique hybrid joining technique that combines the advantages of mechanical interlocking, frictional heat, and solid-state joining (if metallurgically compatible) to produce crack free joints in high strength and/or low-ductility alloys at room temperature. Here, in the current study, Al-7055 sheets were joined using FSPR for lightweight automotive applications and significant microhardness variations were observed across the joint cross-section. A detailed microstructural characterization at multiple length scales was carried out using advanced electron microscopy and X-ray scattering techniques to provide a fundamental understanding of the process-structure-property relationships. The relative contributions of microstructural characteristics at various length scales (i.e., grain size, dislocation density, solute concentration, precipitate nature) to strengthening were estimated using existent formulations (i.e., Hall-Petch, Taylor, precipitate bypass/shear equations) and correlated to the observed microhardness values across different regions. Small-angle X-ray scattering and scanning transmission electron microscopy revealed significant changes in the size and volume fraction of precipitate species, i.e., GP-I Zones, η′, and Mg/Zn solute co-clusters, depending on the process region. It was observed that the dissolution of the small η′/GP-I zones (T ∼ 150–200 °C) in the heat-affected zone were the key reason for the hardness drop. Further, it was shown that solid-solution, dislocation, grain size and solute co-cluster strengthening played a key role in the thermo-mechanically affected zone and grain-refined zone (GRZ). Finally, these observations were leveraged along with the Zener-Holloman relationship and grain size in the GRZ to estimate the peak joining temperature of the GRZ (∼ 350 °C) near the steel rivet.

aluminum 7xxx alloy↗

Interfacial microstructure evolution and weld formation during ultrasonic welding of Al alloy to Cu

Highlights: • Surface oxide layer was fractured and dispersed around the weld interface during ultrasonic welding of Al alloy to Cu. • Mechanical mixing around the weld interface was caused by compressive deformation with ultrasonic vibration. • Once micro-bonds were generated between Al and Cu, shear deformation occurred around the weld interface. • Enhanced Cu diffusion into Al in the severely deformed region significantly contributed to the weld formation. - Abstract: Dissimilar welds of Al alloy 1050 to Cu were prepared via ultrasonic spot welding in order to understand the formation of welds and interfacial microstructures. To observe oxide layer behavior at the weld interface, the anodized Al alloy 1050 was also welded to Cu. Mechanical mixing and material flow during ultrasonic welding broke and dispersed the oxide layers into the Al matrix. This material flow is attributed to compressive deformation that occurred due to ultrasonic vibrations. Direct bonding in the Al/Cu region increased with welding time. Once micro-bonds were generated between Al and Cu, the Al matrix in the vicinity of the weld interface was severely deformed in the direction of the ultrasonic vibrations. Consequently, a recrystallized microstructure with shear texture was formed in the Al matrix. Deformation heating and severe shear deformation formed Al{sub 2}Cu intermetallic compound layers at the weld interface. The growth rate of the Al{sub 2}Cu layer was much faster than had previously been estimated based upon the peak temperature and ultrasonic welding heating time. This is likely due to the increased rate of Cu diffusion into Al in the severely deformed region.

36 MATERIALS SCIENCE↗

Microstructure evolution during near-net-shape fabrication of Ni x Al y -TiC cermets through binder jet additive manufacturing and pressureless melt infiltration

Titanium carbide-nickel aluminide (TiC-Ni x Al y ) intermetallic matrix composite materials were fabricated with additive manufacturing and pressureless melt infiltration for applications intended for high-wear and corrosive environments while maintaining low density. In this work, two compositions of nickel aluminide are infiltrated into porous, printed TiC preforms. Net shaping of a nickel-rich infiltrant is less compared to the net shaping of the aluminum-rich infiltrant due to dissolution of TiC in the molten infiltrant. The microstructures and porosity of the two infiltrants with TiC are examined after processing. The explanation of shape retention from infiltration is explained, and the excellent shape retention in an Al-rich infiltrant system is thought to be from peritectic behavior and a metered infiltration of different phases during cooling and solidification without significant dissolution. The metered infiltration contributed to some porosity, microcracking, and segregated Ni x Al y phases. We show that TiC can be shaped and infiltrated with intermetallics to provide a method of making composites with limited shrinkage and controlled geometry.

36 MATERIALS SCIENCE↗

Microstructure evolution in ion-irradiated of UO{sub 2}

Uranium dioxide (UO{sub 2}) is today's most widely used nuclear fuel in commercial light water reactors. The cumulative radiation damage during the fission process causes severe degradation in the thermophysical properties of UO{sub 2} fuels, which limits their lifetime and increases their operational cost. There are four main sources for decreasing the thermal conductivity during reactor-irradiation: i) irradiation induced defects, ii) solid fission products, iii) fission gas and volatile fission products, and iv) fission gas precipitation and porosity evolution. Therefore, investigating the defect production and evolution, and fission product transport under irradiation, and revealing their physical mechanisms is of great importance in understanding the degradation of thermophysical properties of UO{sub 2} fuels. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Deformation Behavior and Microstructure Evolution of Powder Metallurgy Ti6Al4V Alloy During Hot Compression

In order to determine appropriate workability parameters for cross-wedge rolling products of powder metallurgy (PM) Ti6Al4V alloys, thermal compression experiments were carried out within the temperature range of 850-1050 °C, the strain rate range of 0.1-10 s{sup −1}, and with a height decrease of 60%. The compression deformation behavior was investigated. A strain-compensated constitutive model was established based on the flow stress curves corrected by the friction, which can predict the flow behaviors under the entirety of the experimental deformation conditions. Moreover, the processing map was developed, and stable and unstable deformation regimes were established. The microstructure analysis illustrated that globularization and dynamic recrystallization were the main deformation mechanisms. The porosity of the compressed samples was greatly reduced and influenced by the temperature and strain rate. Considering the material flow stress, hot processing map, microstructure and porosity, the appropriate hot deformation parameters for PM Ti6Al4V alloy preforms are suggested.

36 MATERIALS SCIENCE↗

Microstructural evolution and intermetallic formation in Zn-3Mg (wt%) powder mixture processed by high-pressure torsion

Severe plastic deformation (SPD) techniques have been used extensively over the past 40 years for producing strong metals and alloys. High-pressure torsion (HPT) is one of the most promising SPD techniques for achieving high strength through nanoscale grain refinement and phase transformation. In this research, a mixture of pure zinc (Zn) and magnesium (Mg) powders, Zn-3Mg (wt%), was HPT-processed under a pressure of 6 GPa for 1, 5, 10, 20, and 30 turns at room temperature to achieve a high strength biodegradable material. In order to understand the effects of pre-consolidation on the resulting microstructure and hardness, HPT processing was performed on loose powders placed in the die and also on a pre-compacted powder mixture and the resulting HPT disks were characterized by X-ray diffraction, scanning electron microscopy, atom probe tomography, and Vickers microhardness. In both cases, the HPT disk microstructures contained nanoscale grains, and stable and metastable strain-induced intermetallics, but an unusual softening appeared at large shear strains. Grain size, grain morphology, and the formation of different intermetallics were analyzed to explain the unusual hardness distribution, and it was found that an inverse Hall-Petch relationship between hardness and grain size exists. It is suggested that thermally-activated phenomena such as grain boundary sliding contributed to the strain-induced softening of this nano-structured biomaterial due to its low melting point. Finally, the current results are compared with those for HPT-processed cast alloys and hybrids of the same composition.

36 MATERIALS SCIENCE↗