Low Viscosity Imides Based on Asymmetric Oxydiphthalic Anhydride

A series of low-melt viscosity imide resins were prepared from asymmetric oxydiphthalic dianhydride (a-ODPA) and 4-phenylethynylphthalic anhydride as the endcap, along with 3,4' - oxydianiline (3,4' -ODA), 3,4' -methylenedianiline (3,4' -MDA), 3,3' -methylenedianiline (3,3' - MDA) and 3,3'-diaminobenzophenone (3,3'-DABP), using a solvent-free melt process. These imide oligomers displays low-melt viscosities (2-15 poise) at 260-280 C, which made them amenable to low-cost resin transfer molding (RTM) process. The a-ODPA based RTM resins exhibits glass transition temperatures (Tg's) in the range of 265-330 C after postcure at 343 C. The mechanical properties of these polyimide/carbon fiber composites fabricated by RTM will be discussed.

Chuang, Kathy C.↗

Checking Contamination during Storage of Carbonaceous Chondrites for Micro FTIR Measurements

We examined organic contamination by Fourier transform infrared micro spectroscopic (micro FTIR) measurements of carbonaceous chondrite samples. Carbonaceous chondrites, Tagish Lake (C2), Murchison (CM2) and Moss (CO3), and some mineral powder samples pressed on aluminum plates were measured by micro FTIR before and after storage in several containers with silicone rubber mat. During storage, samples did not touch directly anything except the holding aluminum plates. The carbonaceous chondrites containing hydrous minerals (Tagish Lake and Murchison) pressed on aluminum plates and measured by transmission-reflection micro FTIR measurements were found to be contaminated during storage after only one day, as revealed by an increase of approximately 2965 /cm and approximately 1260 /cm peaks. The Moss meteorite which contains no hydrous minerals, did not show an increase of these peaks, indicating no organic contamination. This difference is probably related to the differing mineralogy and physical properties (including porosity and permeability) of these chondrites. Hydrous minerals such as antigorite, muscovite, montmorillonite and silica gel showed organic contamination by the same infrared measurements, while anhydrous materials such as SiO2 and KBr showed no contamination. These results indicate importance of surface OH groups for the organic contamination. Organic contamination was found on silica gel samples pressed on aluminum plates when they were stored within containers including silicone rubber, silicone grease or adhesive tape. Long path gas cell FTIR measurements for silicone rubber indicated methylsiloxane oligomers were released from the silicone rubber. In-situ heating infrared measurements on the contaminated antigorite and Tagish Lake showed decrease of the 1262 /cm (Si-CH3) and 2963 /cm (CH3) peaks from room temperature to 200-300 C indicating desorption of volatile contaminants. These results indicate that careful preparation and storage are essential for FTIR measurements on precious astromaterial samples such as meteorites, IDPs and samples returned from comets, asteroids and Mars. Every possible contamination source should be evaluated before anything is done to these samples.

Zolensky, Michael E.↗

Processing Robustness for A Phenylethynyl Terminated Polyimide Composite

The processability of a phenylethynyl terminated imide resin matrix (designated as PETI-5) composite is investigated. Unidirectional prepregs are made by coating an N-methylpyrrolidone solution of the amide acid oligomer (designated as PETAA-5/NMP) onto unsized IM7 fibers. Two batches of prepregs are used: one is made by NASA in-house, and the other is from an industrial source. The composite processing robustness is investigated with respect to the prepreg shelf life, the effect of B-staging conditions, and the optimal processing window. Prepreg rheology and open hole compression (OHC) strengths are found not to be affected by prolonged (i.e., up to 60 days) ambient storage. Rheological measurements indicate that the PETAA-5/NMP processability is only slightly affected over a wide range of B-stage temperatures from 250 deg C to 300 deg C. The OHC strength values are statistically indistinguishable among laminates consolidated using various B-staging conditions. An optimal processing window is established by means of the response surface methodology. IM7/PETAA-5/NMP prepreg is more sensitive to consolidation temperature than to pressure. A good consolidation is achievable at 371 deg C (700 deg F)/100 Psi, which yields an RT OHC strength of 62 Ksi. However, processability declines dramatically at temperatures below 350 deg C (662 deg F), as evidenced by the OHC strength values. The processability of the IM7/LARC(TM) PETI-5 prepreg was found to be robust.

Hou, Tan-Hung↗

Synthesis and Compatibility of Ionic Liquid Containing Rod-Coil Polyimide Gel Electrolytes with Lithium Metal Electrodes

A highly cross-linked polyimide-polyethylene oxide copolymer has been synthesized that is capable of holding large volumes of liquid component, simultaneously maintaining good dimensional stability. An amine end capped oligomer was made that was imidized in solution, followed by reaction with a triisocyanate in the presence of desired additives at ambient temperature. Polymer films are able to hold over 4 times their weight in room temperature ionic liquid RTIL or carbonate solvent. Electrolytes were studied that contained varying amounts of RTIL, lithium trifluoromethanesulfonimide LiTFSi, and alumina nanoparticles. Electrochemical stability of these electrolytes with lithium metal electrodes was studied by galvanic cycling and impedance spectroscopy. Improved cycling stability and decreased interfacial resistance were observed when increasing amounts of RTIL and LiTFSi were added. The addition of small amounts of alumina further decreased interfacial resistance by nearly an order of magnitude. During the course of the study, cycling stability increased from less than 3 to greater than 1000 h at 60 C and 0.25 mA/cm2 current density.

Tigelaar, Dean M.↗

Photochemically Synthesized Polyimides

An alternative to the conventional approach to synthesis of polyimides involves the use of single monomers that are amenable to photopolymerization. Heretofore, the synthesis of polyimides has involved multiple-monomer formulations and heating to temperatures that often exceed 250 C. The present alternative approach enables synthesis under relatively mild conditions that can include room temperature. The main disadvantages of the conventional approach are the following: Elevated production temperatures can lead to high production costs and can impart thermal stresses to the final products. If the proportions of the multiple monomeric ingredients in a given batch are not exactly correct, the molecular weight and other physical properties of the final material could be reduced from their optimum or desired values. To be useful in the alternative approach, a monomer must have a molecular structure tailored to exploit Diels-Alder trapping of a photochemically generated ortho-quinodimethane. (In a Diels-Alder reaction, a diene combines with a dienophile to form molecules that contain six-membered rings.) In particular, a suitable monomer (see figure) contains ortho-methylbenzophenone connected to a dienophile (in this case, a maleimide) through a generic spacer group. Irradiation with ultraviolet light gives rise to a photochemical intermediate the aforementioned ortho-quinodimethane from the ortho-methylbenzophenone. This group may react with the dienophile on another such monomer molecule to produce an oligomer that, in turn may react in a stepgrowth manner to produce a polyimide. This approach offers several advantages in addition to those mentioned above: The monomer can be stored for a long time because it remains unreactive until exposed to light. Because the monomer is the only active starting ingredient, there is no need for mixing, no concern for ensuring correct proportions of monomers, and the purity of the final product material is inherently high. The use of solvents is optional: The synthesis can be performed using the neat monomer or the monomer mixed with one or more solvent(s) in dilute or concentrated solution. The solubility of the monomer and the physical and chemical properties of the final polymer can be tailored through selection of the spacer group.

Meador, Michael A.↗

High internal free volume compositions for low-k dielectric and other applications

The present invention provides materials, devices, and methods involving new heterocyclic, shape-persistent monomeric units with internal free volume. In some cases, materials the present invention may comprise monomers, oligomers, or polymers that incorporate a heterocyclic, shape-persistent iptycene. The present invention may provide materials having low dielectric constants and improved stability at high operating temperatures due to the electron-poor character of materials. In addition, compositions of the invention may be easily synthesized and readily modified to suit a particular application.

Swager, Timothy M.↗

Phenylethynyl Terminated Imide (PETI) Composites Made by High Temperature Vartm

The use of composites as primary structures on aerospace vehicles has increased dramatically over the past decade. As these advanced structures increase in size and complexity, their production costs have grown significantly. A major contributor to these manufacturing costs is the requirement of elevated pressures, during high temperature processing, to create fully consolidated composite parts. Recently, NASA Langley has licensed a series of low viscosity Phenyl Ethynyl Terminated Imide, PETI, oligomers that possess a wide processing window to allow for Resin Transfer Molding, RTM, processing. These resins, PETI-8 and PETI-330, demonstrate void fractions of approx.1% under elevated pressure consolidation. However, when used with a standardized thermal curing cycle in a High Temperature Vacuum Assisted RTM (HT-VARTM) process, they display undesirable void contents in excess of 7%. It was determined previously that under the thermal cycles used for laminate fabrication, the phenylethynyl endcap underwent degradation leading to volatile evolution. Modifications to the processing cycle used in the laminate fabrication have reduced the void content significantly (typically less than 3%) for carbon fiber biaxially woven fabric. For carbon fiber uniaxial fabric, void contents of less than 2% have been obtained using both PETI-8 and PETI-330. The resins were infused into carbon fiber preforms at 260 C and cured between 316 C and 371 C. Photomicrographs of the panels were taken and void contents were determined by acid digestion. Mechanical properties of the panels were determined at both room and elevated temperatures. These include short beam shear and flexure tests. The results of this work are presented herein.

Ghose, Sayata↗

Modifying Silicates for Better Dispersion in Nanocomposites

An improved chemical modification has been developed to enhance the dispersion of layered silicate particles in the formulation of a polymer/silicate nanocomposite material. The modification involves, among other things, the co-exchange of an alkyl ammonium ion and a monoprotonated diamine with interlayer cations of the silicate. The net overall effects of the improved chemical modification are to improve processability of the nanocomposite and maximize the benefits of dispersing the silicate particles into the polymer. Some background discussion is necessary to give meaning to a description of this development. Polymer/silicate nanocomposites are also denoted polymer/clay composites because the silicate particles in them are typically derived from clay particles. Particles of clay comprise layers of silicate platelets separated by gaps called "galleries." The platelet thickness is 1 nm. The length varies from 30 nm to 1 m, depending on the silicate. In order to fully realize the benefits of polymer/silicate nanocomposites, it is necessary to ensure that the platelets become dispersed in the polymer matrices. Proper dispersion can impart physical and chemical properties that make nanocomposites attractive for a variety of applications. In order to achieve nanometer-level dispersion of a layered silicate into a polymer matrix, it is typically necessary to modify the interlayer silicate surfaces by attaching organic functional groups. This modification can be achieved easily by ion exchange between the interlayer metal cations found naturally in the silicate and protonated organic cations - typically protonated amines. Long-chain alkyl ammonium ions are commonly chosen as the ion-exchange materials because they effectively lower the surface energies of the silicates and ease the incorporation of organic monomers or polymers into the silicate galleries. This completes the background discussion. In the present improved modification of the interlayer silicate surfaces, the co-ion exchange strengthens the polymer/silicate interface and ensures irreversible separation of the silicate layers. One way in which it does this is to essentially tether one amine of each diamine molecule to a silicate surface, leaving the second amine free for reaction with monomers during the synthesis of a polymer. In addition, the incorporation of alkyl ammonium ions into the galleries at low concentration helps to keep low the melt viscosity of the oligomer formed during synthesis of the polymer and associated processing - a consideration that is particularly important in the case of a highly cross-linked, thermosetting polymer. Because of the chemical bonding between the surface-modifying amines and the monomers, even when the alkyl ammonium ions become degraded at high processing temperature, the silicate layers do not aggregate and, hence, nanometer-level dispersion is maintained.

Campbell, Sandi↗

Safer Electrolytes for Lithium-Ion Cells

A number of nonvolatile, low-flammability liquid oligomers and polymers based on aliphatic organic carbonate molecular structures have been found to be suitable to be blended with ethylene carbonate to make electrolytes for lithium-ion electrochemical cells. Heretofore, such electrolytes have often been made by blending ethylene carbonate with volatile, flammable organic carbonates. The present nonvolatile electrolytes have been found to have adequate conductivity (about 2 mS/cm) for lithium ions and to remain liquid at temperatures down to -5 C. At normal charge and discharge rates, lithiumion cells containing these nonvolatile electrolytes but otherwise of standard design have been found to operate at current and energy densities comparable to those of cells now in common use. They do not perform well at high charge and discharge rates -- an effect probably attributable to electrolyte viscosity. Cells containing the nonvolatile electrolytes have also been found to be, variously, nonflammable or at least self-extinguishing. Hence, there appears to be a basis for the development of safer high-performance lithium-ion cells.

Kejha, Joe↗

Exploring the Fate of Nitrogen Heterocycles in Complex Prebiotic Mixtures

A long standing question in the field of prebiotic chemistry is the origin of the genetic macromolecules DNA and RNA. DNA and RNA have very complex structures with repeating subunits of nucleotides, which are composed of nucleobases (nitrogen heterocycles) connected to sugar-phosphate. Due to the instability of some nucleobases (e.g. cytosine), difficulty of synthesis and instability of D-ribose, and the likely scarcity of polyphosphates necessary for the modern nucleotides, alternative nucleotides have been proposed for constructing the first genetic material. Thus, we have begun to investigate the chemistry of nitrogen heterocycles in plausible, complex prebiotic mixtures in an effort to identify robust reactions and potential alternative nucleotides. We have taken a complex prebiotic mixture produced by a spark discharge acting on a gas mixture of N2, CO2, CH4, and H2, and reacted it with four nitrogen heterocycles: uracil, 5-hydroxymethyluracil, guanine, and isoxanthopterin (2-amino-4,7-dihydroxypteridine). The products of the reaction between the spark mixture and each nitrogen heterocycle were characterized by liquid chromatography coupled to UV spectroscopy and Orbitrap mass spectrometry. We found that the reaction between the spark mixtUl'e and isoxanthopterin formed one major product, which was a cyanide adduct. 5-hydroxymethyluracil also reacted with the spark mixture to form a cyanide adduct, uracil-5-acetonitrile, which has been synthesized previously by reacting HCN with S-hydroxymethyluracil. Unlike isoxanthopterin, the chromatogram of the 5-hydroxymethyluracil reaction was much more complex with multiple products including spark-modified dimers. Additionally, we observed that HMU readily self-polymerizes in solution to a variety of oligomers consistent with those suggested by Cleaves. Guanine and uracil, the biological nucleobases, did not react with the spark mixture, even at high temperature (100 C). This suggests that there are alternative nucleobases which are more reactive under prebiotic conditions and may have been involved in producing precursor nucleotides.

Smith, Karen E.↗

Application of Glow Discharge Plasma to Alter Surface Properties of Materials

Some polymer materials that are considered important for spaceport operations are rendered noncompliant when subjected to the Kennedy Space Center (KSC) Standard electrostatic testing. These materials operate in stringent environmental conditions, such as high humidity. Treating materials that fail electrostatic testing and altering their surface properties so that they become compliant would result in considerable cost savings. Significant improvement in electrostatic dissipation of Saf-T-Vu PVC after treatment with air Atmospheric Plasma Glow Discharge (APGD) was observed and the material now passed the KSC electrostatic test. The O:C ratio on the surface, as monitored by X-ray Photoelectron Spectroscopy, increased from 0.165 tO 0.275 indicating enhanced oxidation, and surface contact angle measurements decreased from 107.5 to 72.6 showing increased hydrophilicity that accounted for the increased conductivity. Monitoring of the aging showed that the materials hydrophobic recovery resulted in it failing the electrostatic test 30 hours after treatment. This was probably due to the out-diffusion of the added Zn, Ba, and Cd salt stabilizers detected on the surface and/or diffusion of low molecular weight oligomers. On going work includes improving the long term hydrophilicity by optimizing the APGD process with different gas mixtures. Treatment of other spaceport materials is also presented.

Trigwell, Steve↗

Synthesis, Characterization, Topographical Modification, and Surface Properties of Copoly(Imide Siloxane)s

Novel copoly(imide siloxane)s were synthesized from commercially available aminopropyl terminated siloxane oligomers, aromatic dianhydrides, and diamines. This synthetic approach produced copolymers with well-defined siloxane blocks linked with imide units in a random fashion. The copoly(amide acid)s were characterized by solution viscosity and subsequently used to cast thin films followed by thermal imidization in an inert atmosphere. Thin films were characterized using contact angle goniometry, attenuated total reflection Fourier transform infrared spectroscopy, confocal and optical microscopy, and tensile testing. Adhesion of micronsized particles was determined quantitatively using a sonication device. The polydimethylsiloxane (PDMS) moieties lowered the copolymer surface energy due to migration of siloxane moieties to the film s surface, resulting in a notable reduction in particle adhesion. A further reduction in particle adhesion was achieved by introducing topographical features on a scale of several to tens of microns by a laser ablation technique.

Wohl, Christopher J.↗

Electrostatic Properties of PE and PTFE Subjected to Atmospheric Pressure Plasma Treatment; Correlation of Experimental Results with Atomistic Modeling

The use of an atmospheric pressure glow discharge (APGD) plasma was used at KSC to increase the hydrophilicity of spaceport materials to enhance their surface charge dissipation and prevent possible ESD in spaceport operations. Significant decreases in charge decay times were observed after tribocharging the materials using the standard KSC tribocharging test. The polarity and amount of charge transferred was dependent upon the effective work function differences between the respective materials. In this study, polyethylene (PE) and polytetrafluoroethylene (PTFE) were exposed to a He+O2 APGD. The pre and post treatment surface chemistry was analyzed by X-ray photoelectron spectroscopy and contact angle measurements. Semi-empirical and ab initio calculations were performed to correlate the experimental results with some plausible molecular and electronic structure features of the oxidation process. For the PE, significant surface oxidation was observed, as indicated by XPS showing C-O, C=O, and O-C=O bonding, and a decrease in the surface contact angle from 98.9 deg to 61.2 deg. For the PTFE, no C-O bonding appeared and the surface contact angle increased indicating the APGD only succeeded in cleaning the PTFE surface without affecting the surface structure. The calculations using the PM3 and DFT methods were performed on single and multiple oligomers to simulate a wide variety of oxidation scenarios. Calculated work function results suggest that regardless of oxidation mechanism, e.g. -OH, =0 or a combination thereof, the experimentally observed levels of surface oxidation are unlikely to lead to a significant change in the electronic structure of PE and that its increased hydrophilic properties are the primary reason for the observed changes in its electrostatic behavior. The calculations for PTFE argue strongly against significant oxidation of that material, as confirmed by the XPS results.

Trigwell, Steve↗

Electrostatic Properties of Polymers Subjected to Atmospheric Pressure Plasma Treatment; Correlation of Experimental Results with Atomistic Modeling

this study, PE, PTFE, PS and PMMA were exposed to a He+O2, APGD and pre and post treatment surface chemistries were analyzed by X-ray photoelectron spectroscopy and contact angle measurements. Semi-empirical and ab-initio calculations were performed to correlate the experimental results with sonic plausible molecular and electronic structure features of the oxidation process. For the PE and PS, significant surface oxidation showing C-O, C=O, and O-C=O bonding, and a decrease in the surface contact angles was observed. For the PTFE and PM MA, little change in the surface composition was observed. The molecular modeling calculations were performed on single and multiple oligomers and showed regardless of oxidation mechanism, e.g. -OH, =O or a combination thereof, experimentally observed levels of surface oxidation were unlikely to lead to a significant change in the electronic structure of PE and PS, and that the increased hydrophilic properties are the primary reason for the observed changes in its electrostatic behavior. Calculations for PTFE and PMMA argue strongly against significant oxidation of those materials, as confirmed by the XPS results.

Trigwell, S.↗

Novel Epoxy Particulate Composites for Mitigation of Insect Residue Adhesion on Future Aircraft Surfaces

Drag is reduced significantly for airflow over surfaces when laminar flow can be maintained over greater chord lengths, the distance from the leading edge of an airfoil.1 However, surface imperfections, such as chipped paint, scratches, and events that change topography on a microscopic scale can introduce airflow instabilities resulting in premature transition to turbulent flow.1 Although many of these surface imperfections can be avoided with proper maintenance, advanced materials, and advanced manufacturing practices, topographical surface anomalies arising during flight from insect impacts cannot be controlled and can influence laminar flow stability. Practical solutions to this operational challenge need to be developed for future aircraft to have full advantage of laminar flow designs that improve fuel efficiency.2 Researchers have investigated various methods to mitigate insect residue adhesion for decades.3 Although several techniques have demonstrated efficacy including mechanical scrapers, active liquid discharge systems, and sacrificial paper coatings, they have not been commercially implemented due to increased manufacturing and operational complexity, environmental impact, and weight penalties. Coatings offer a simple route for passive insect residue adhesion prevention without many of the challenges associated with maintenance of laminar flow.4 In our previous work, we determined that most commercially available materials were not effective at insect residue adhesion.5 We also identified improvements when both surface energy could be controlled by surface modifying agents and the topography could be altered through the use of micron-sized and nanometer-sized filler materials.6 In this work, these general principles were applied to an epoxy system to evaluate the behavior of the surface modifying agent, a fluorinated alkyl ether oligomer, on surface energy and insect residue adhesion properties.

Wohl, Christopher J.↗

Flexible Polyimide Aerogel Cross-linked by Poly(maleic Anhydride-alt-alkylene)

Aerogels are potential materials for aerospace applications due to their lower thermal conductivity, lighter weight, and low dielectric constant. However, silica aerogels are restricted due to their inherent fragility, hygroscopic nature, and poor mechanical properties, especially in extreme aerospace environments. In order to fit the needs of aerospace applications, developing new thermal insulation materials that are flexible, and moisture resistant is needed. To this end, we fabricated a series of polyimide aerogels crosslinked with different poly(maleic anhydride-alt-alkylene)s as seen in Scheme 1. The polyimide oligomers were made with 3,3,4,4-biphenyltetracarboxylic dianhydride (BPDA), and different diamines or diamine combinations. The resulting aerogels have low density (0.06 gcm3 to 0.16 gcm3) and high surface area (240-440 m2g). The effect of the different backbone structures on density, shrinkage, porosity, surface area, mechanical properties, moisture resistance and thermal properties will be discussed. These novel polyalkylene-imide aerogels may be potential candidates for applications such as space suit insulation for planetary surface missions, insulation for inflatable structures for habitats, inflatable aerodynamic decelerators for entry, descent and landing (EDL) operations, and cryotank insulation for advance space propulsion systems. Scheme 1. Network of polyimide aerogels crosslinked with deifferent poly(maleic anhydride).

cross-link↗

Evaluation of RTM370 Polyimide Composites by Resin Film Infusion (RFI)

RTM370 imide oligomer based on 2,3,3',4'-biphenyl dianhydride (a-BPDA), 3,4'-oxydianiline (3,4'-ODA) and terminated with the 4-phenylethynylphthalic (PEPA) endcap has been shown to exhibit a low melt viscosity (10-30 poise) at 280 C with a pot-life of 1-2 h and a high cured glass-transition temperature (Tg) of 370 C. RTM370 resin has been successfully infused into fiberglass-stitched T650-35 carbon-fabric preforms (ranged from 3- to 6-mm thick) by resin film infusion (RFI). The resulting composite panels were inspected by ultrasonic C-scan and by photomicrographs before and after post-curing as a quality control. Mechanical tests such as unnotched compression (UNC), open-hole compression (OHC), and short-beam shear strength (SBS) at ambient and elevated temperatures were performed before and after isothermal aging at 288 C for 1000 h to assess high-temperature performance. Thermal cycling of RTM370 stitched composites was also conducted from -54 C to 288 C for up to 1600 cycles to evaluate the microcrack resistance of RTM370 polyimide composites fabricated by RFI.

Polyimide↗

Synthesis and Properties of Cross-Linked Polyamide Aerogels

We report our ongoing research on polyamide aerogels made by step growth polymerization using a combination of terephthaloyl chloride, isophthaloyl chloride and m-phenylenediamine. Crosslinking of the amine capped polymer chains with 1,3,5-benzenetricarbonyl trichloride causes gelation in as little as two to five minutes. Removing the reaction solvent is accomplished through solvent exchange, followed by drying using supercritical CO2 extraction to give colorless aerogels with densities ranging from 0.07 to 0.33 grams per cubic centimeter and surface areas as high as 440 square meters per gram. Statistical experimental design methodology has been utilized to investigate dependence of properties of these aerogels, such as density, compressive modulus, and surface area, on changes in fabrication parameters including formulated number of amide oligomer repeat units (n-value), acid chloride (meta, para or combination), and solids concentration of solution used for gelation. For example, the density of these materials was found to be dependent on the acid chloride type and the solids concentration, but n was not a significant variable. However, surface area was significantly influenced by all three parameters. The polyamide aerogels represent a potential cost savings over previously reported polyimide aerogels, since monomers are all inexpensive and commercially available. Surface area and density were both highest when 100 terephthaloyl chloride was used but a combination of 5 solid concentration, 100 terephthaloyl chloride and n of 20 gave the best combination of properties.