Search NASA⌕ Search

SEARCH · Search NASA

Results for “Pit”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Influence of AA6061 surface preparation on the resistance to surface degradation of thermally grown boehmite films

Understanding substrate–coating interactions is crucial for designing durable, corrosion-resistant systems. This study investigates the effects of surface treatments— polishing, acid etching, and alkaline etching—on AA6061 aluminum alloy and its thermally grown boehmite coatings. Surface treatments were found to significantly alter boehmite film properties by modifying the alloy’s surface composition. X-ray photoelectron spectroscopy revealed a 10% alumina drop after acid etching alongside chemisorbed species formation in wet treatments. Structural analysis, including grazing incidence X-ray diffraction and TEM, showed α-Al 2 O 3 formation on polished surfaces, improving wear resistance but inducing cathodic E corr shifts, pointing to higher corrosion susceptibility. In contrast, acid and alkaline etching produced anodic E corr shifts with stable, pit-free films observed via potentiodynamic scans. Electrochemical impedance spectroscopy highlighted reduced oxide resistance with extended boehmite growth. The findings emphasize the role of surface pre-treatments and boehmite optimization in balancing durability and corrosion resistance for AA6061 substrates.

AA6061↗

Probing corrosion using a simple and versatile in situ multimodal corrosion measurement system

In this work, we have developed a unique in situ multimodal corrosion system that is capable of acquiring electrochemical data, sample imaging/visualization and hydrogen collection, simultaneously. Each of these modalities yield valuable information pertaining to the ongoing corrosion process. Combining them can yield holistic information on the role of microstructure, processing history, presence of coatings, etc., on the sequence of steps occurring during the corrosion process, and how they correlate with the acquired electrochemical data. Four materials systems, namely AA6061-T6 aluminum alloy, AZ91 magnesium alloy, galvanized DP590 steel, and pure Zn, were investigated under open circuit potential and under potentiodynamic polarization. The multimodal corrosion system was utilized to observe processes such as surface passivation and dissolution, pit and filiform corrosion initiation and propagation, and was correlated with location and magnitude of hydrogen evolution. This approach is shown to yield a truly multimodal understanding of the ongoing corrosion processes.

36 MATERIALS SCIENCE↗

Differentiating multi-MeV, multi-ion spectra with CR-39 solid-state nuclear track detectors

The development of high intensity petawatt lasers has created new possibilities for ion acceleration and nuclear fusion using solid targets. In such laser-matter interaction, multiple ion species are accelerated with broad spectra up to hundreds of MeV. To measure ion yields and for species identification, CR-39 solid-state nuclear track detectors are frequently used. However, these detectors are limited in their applicability for multi-ion spectra differentiation as standard image recognition algorithms can lead to a misinterpretation of data, there is no unique relation between track diameter and particle energy, and there are overlapping pit diameter relationships for multiple particle species. In this report, we address these issues by first developing an algorithm to overcome user bias during image processing. Second, we use calibration of the detector response for protons, carbon and helium ions (alpha particles) from 0.1 to above 10 MeV and measurements of statistical energy loss fluctuations in a forward-fitting procedure utilizing multiple, differently filtered CR-39, altogether enabling high-sensitivity, multi-species particle spectroscopy. To validate this capability, we show that inferred CR-39 spectra match Thomson parabola ion spectrometer data from the same experiment. Filtered CR-39 spectrometers were used to detect, within a background of ~ 2 × 10 11 sr -1 J -1 protons and carbons, (1.3 ± 0.7) × 10 8 sr -1 J -1 alpha particles from laser-driven proton-boron fusion reactions.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Failure modes of protection layers produced by atomic layer deposition of amorphous TiO 2 on GaAs anodes

Amorphous titanium dioxide (a-TiO 2 ) films formed by atomic layer deposition can serve as protective coatings for semiconducting photoanodes in water-splitting cells using strongly alkaline aqueous electrolytes. Herein, we experimentally examine the mechanisms of failure for p + -GaAs anodes coated with a-TiO 2 films (GaAs/a-TiO 2 ). Galvanic displacement of exposed GaAs by Au allowed imaging of pinholes in the a-TiO 2 coatings, and enabled collection of quantitative and statistical data associated with pinhole defects. A combination of imaging, electrochemical measurements, and quantitative analyses of corrosion products indicated that extrinsic pinholes were present in the a-TiO 2 films before electrochemical operation. During electrochemical operation these pinholes led to pitting corrosion of the underlying GaAs substrate. The dominant source of pinholes was the presence of atmospheric particulate matter on the GaAs surface during deposition of the a-TiO 2 layer. The pinhole density decreased substantially when the thickness of the a-TiO 2 coating increased beyond 45 nm, and approached zero when the thickness of the film exceeded 112 nm. The density of pinholes in films thinner than 45 nm decreased when the a-TiO 2 coating was deposited in an environmentally controlled cleanroom. Pinhole-free GaAs/a-TiO 2 devices were also tested via chronoamperometry to quantify the rate of pinhole formation during electrochemistry. The time-to-failure increased with thickness, suggesting that the failure mechanism may involve diffusion or migration through the film. However, other mechanisms may also contribute to the degradation of thicker films (>112 nm). Nevertheless, as previously hypothesized, extrinsic pinhole defects formed during deposition and testing control the short-term protective performance of the a-TiO 2 film for GaAs anodes evolving O 2 from water.

25 ENERGY STORAGE↗

Catalytic open-circuit passivation by thin metal oxide films of p-Si anodes in aqueous alkaline electrolytes

Ni and NiO x -based protective thin films are shown to catalyze the oxidation of Si in the presence of O 2 in strongly alkaline KOH(aq) even in the absence of illumination. The O 2 in solution drove the open-circuit potential of the electrode to >0.4 V, which is positive of the Si passivation potential. The elevated electrochemical potential of the surface promoted formation of passive oxides on exposed Si regions of Si/Ni electrodes. Catalytic passivation of Si extended the durability of an np + -Si(100)/NiO x photoanode to >400 h while operating under simulated day/night cycles. In contrast, electrodes without a Ni(O x ) layer and/or without O 2 in solution displayed direct etching of the Si and corrosion pitting during non-illuminated, simulated nighttime episodes of day/night cycling. The O 2 -derived catalyzed passivation of Si using thin films can be generalized to multiple phases of NiO x as well as to materials other than Ni. Finally, relative to operation in aqueous alkaline conditions, decreasing the pH of the electrolyte decreased the dissolution rate of the protective oxide layer formed by the catalyzed passivation process, and consequently increased the durability of the photoanode, but yielded lower photoelectrode fill factors for water oxidation due to the relatively large kinetic overpotentials for the electrocatalyzed oxygen-evolution reaction at near-neutral pH.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The corrosion behavior of borosilicate glass in the presence of cementitious waste forms

Borosilicate glasses are widely used for radioactive waste disposal due to their ability to incorporate a variety of contaminants and radionuclides while exhibiting high durability in various disposal scenarios. This research evaluated the dissolution of borosilicate glass using both single-pass-flow-through (ASTM C1662-18) and product consistency test (ASTM C1285-21) methods with different solutions, including a cementitious-contacted water (called grout-contacted, GC, from this point) and solutions with varying levels of dissolved cementitious species such as Si, Ca, Al. Here, the results indicated that the presence of Ca plays a crucial role in suppressing glass corrosion, as evidenced by the slower normalized dissolution rates, which were one order of magnitude lower for boron and two orders of magnitude lower for rhenium, observed in both Ca-amended and GC solutions compared to the pH 12 buffer solution. This effect is attributed to the formation of a dense, low-porosity, and strongly bonded calcium silicate hydrate (CSH) layer on the glass surface, which implies that a glass corrosion process is influenced by ion exchange involving alkali ions Na + , K + , Ca 2+ , and hydrogen-containing species. A small number of glass particles treated in the GC solution showed minor corrosion pits in the form of shallow craters with an average diameter of approximately 500 μm. This observation is correlated with a significant reduction, 2000 to 3000 times lower, in the cumulative volume of glass pores, indicating that smaller pore voids were “sealed” in the presence of Ca 2+ ions, likely attributed to the formation of CSH precipitation or other corrosion products such as calcium carbonate saturated from the grout solution. These findings suggest that the presence of dissolved Ca in the GC solution can slow down the dissolution of borosilicate glass, contrary to the expected trend of higher dissolution rates resulting from exposure to high alkaline and thus higher pH solutions.

36 MATERIALS SCIENCE↗

Defect-Limited Carrier Lifetime in Epitaxially Strained Germanium-On-Silicon Heterostructures

Epitaxially strained germanium-on-silicon (Ge-on-Si) heterostructures are central to next-generation photonic and electronic devices, yet their performance remains strongly constrained by defect-limited carrier lifetimes. In this work, we investigate the impact of defects on the carrier lifetime in relaxed Ge-on-Si and strained Ge-on-Si heterostructures. High-resolution X-ray diffraction quantifies the strain-state in Ge and reveals signatures of strain relaxation due to lattice mismatch. Cross-sectional and plan-view transmission electron microscopy analyses enable direct visualization of interfacial defects and quantification of threading dislocation densities (TDDs) within the Ge layer. However, the presence of a dense misfit dislocation network obscures the threading dislocation signatures, preventing reliable TDD determination by plan-view transmission electron microscopy in strained-Ge (..epsilon..-Ge). To assess the defect density in this case, etch-pit density measurements were performed, providing an alternative means of quantifying the TDDs in the ..epsilon..-Ge layer. Carrier lifetime measurements by microwave-reflection photoconductive decay reveal a clear relationship with TDDs ranging from 5 x 103 cm-2 to 2 x 1010 cm-2, confirming Shockley-Read-Hall recombination as the limiting mechanism at lower defect densities, with TDD-dominated recombination at higher defect densities. The Ge-on-Si relaxed heterostructure exhibited lifetimes much lower (~12 ns) than the lattice-matched Ge on gallium arsenide (GaAs) (~158 ns) heterostructure. Introducing controlled tensile strain reduces defect formation, suppresses strain-relaxation pathways, and leads to measurable improvements in minority carrier lifetime from 12 ns to 171 ns. These results establish a direct relation between defect suppression and carrier recombination dynamics in both relaxed Ge-on-Si grown directly on Si and strained Ge-on-Si heterostructures incorporating compound-semiconductor buffer layers, offering a materials-driven pathway for engineering Ge with improved carrier lifetime for photonic applications.

36 MATERIALS SCIENCE↗

A first-principles study of hydrogen surface coverage on δ-Pu (100), (111), and (110) surfaces

Hydriding corrosion of plutonium leads to surface cracking, pitting, and ultimately structural failure. Laboratory experiments demonstrate that hydriding begins on the surface or near the subsurface of plutonium. However, there has not yet been a systematic evaluation of hydrogen surface coverage on plutonium. In this work, we compute the surface energies of the low facet surfaces of face-centered cubic δ-Pu. The adsorption free energies of expected hydrogen structures at low and high coverage are presented along with the likely progression for filling sites as the H 2 partial pressure increases. Implications for near-equilibrium pressure hydride nucleation and non-equilibrium millibar pressure hydriding are discussed.

36 MATERIALS SCIENCE↗

Modeling ablator defects as a source of mix in high-performance implosions at the National Ignition Facility

Recent indirect drive inertial confinement fusion implosions on the National Ignition Facility (NIF) [Spaeth et al., Fusion Sci. Technol. 69, 25 (2016)] have crossed the threshold of ignition. However, performance has been variable due to several factors. One of the leading sources of variability is the quality of the high-density carbon (HDC) shells used as ablators in these experiments. In particular, these shells can have a number of defects that have been found to correlate with the appearance of ablator mix into the hot spot and a degradation in nuclear yield. These defects include pits on the ablator surface, voids in the ablator bulk, high-Z debris from the Hohlraum wall that adheres to the capsule surface, and finally the inherent granular micro-structure of the crystalline HDC itself. This paper summarizes high-resolution modeling of each of these mix sources in two recent high-performance NIF implosion experiments. The simulated impact from a range of individual capsule defects is found to be broadly consistent with the trends seen in experiment, lending credence to the modeling results and the details of the mixing process that they reveal. Interestingly, modeling of the micro-structure inherent to HDC shows that this perturbation source results in considerable mixing of the deuterium–tritium fuel with ablator material during the implosion. The reduction in fuel compression from this mix results in an approximately factor of two reduction in neutron yield in current implosions and emphasizes the importance of mitigating this significant performance degradation.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Seismic refraction tracks porosity generation and possible CO 2 production at depth under a headwater catchment

Significance To understand groundwater in weathered bedrock aquifers, we explore (bio)geochemical reactions using geophysical measurements. The result leads to a conceptual model for the three-dimensional distribution of geochemical alteration in the subsurface—well beyond the typical approach of inferring (bio)geochemical reactions in the subsurface from pits, boreholes, and outcrops. With this geophysical technique we discovered the prevalence of gas beneath the water table at this site. This geophysical viewing of the subsurface highlights patterns of water movement, reactions of clays, and microbial and abiotic gas-producing reactions recorded in the subsurface and thus illuminates storage, flow, and reactions of groundwater in bedrock systems. Protecting the groundwater resource beneath our feet will rely on such enhanced capacities to see into the subsurface.

58 GEOSCIENCES↗

Dose reconstruction for plutonium-239 intakes at the Rocky Flats Plant

Purpose: The Rocky Flats (RF) Plant was a weapons manufacturing facility that operated from the early 1950s to 1989. Its primary missions were the production of plutonium (Pu) pits for thermonuclear weapons and the processing of retired weapons for Pu recovery. The purpose of this study was to estimate radiation doses to a cohort of 4499 RF workers from an intake of 239 Pu, the primary plutonium isotope handled at the site. Materials and methods: The latest biokinetic models of the International Commission on Radiological Protection, or site-specific variations of those models, were used to estimate 239 Pu intakes for each worker based on model fits to bioassay data often coupled with lung measurements. Results: Urinary excretion and lung retention data for most 239 Pu intakes could be fit reasonably well by a mixture of Pu dioxide and moderately soluble material. For some workers, better fits were obtained by application of other absorption types including Type S, 239 Pu nitrate, or pure 239 Pu dioxide, or by assuming intake via a wound. The lungs typically received the highest tissue doses, with fifty-year committed equivalent doses in the range of 0.5–1 Sv for 275 workers, 1–5 Sv for 115 workers, and greater than 5 Sv for 12 workers. Conclusions: RF was a unique site regarding a large number of lung measurements available for determining the appropriate absorption types for inhaled material. Further, this provided higher confidence in reconstructed 239 Pu doses than is generally gained from urinary data alone.

61 RADIATION PROTECTION AND DOSIMETRY↗

Room temperature corrosion behaviour of plastically deformed AISI 304 stainless steel by friction stir welding in neutral and acidified chloride solutions

Severe plastic deformation of 304L stainless steel plate was carried out by friction stirring under an isothermal tool temperature at 825°C. The friction stirred zone showed extensive grain refinement, high fraction of low angle grain boundaries due to dislocation rearrangement, Σ3 and Σ9 special grain boundaries and discrete Fe–Cr–Mn-rich particles. Electrochemical polarisation measurements were done on the base metal (BM) and friction stir welded (FSW) specimens in the neutral and acidified 3.5% NaCl solutions. The BM showed marginally better pitting resistance in the neutral chloride solution than the FSW because of a larger fraction of special grain boundaries, and larger grain size. Whereas in acidified 3.5% NaCl solution, the FSW showed better corrosion resistance than the BM. Furthermore, the surface film of the FSW had a lower impedance and a lower defect concentration than the BM indicating higher diffusivity of point defects in the FSW.

36 MATERIALS SCIENCE↗

Precision Polishing of Ablator Capsules via in situ Process Monitoring and Machine Learning–Based Optimization

In inertial confinement fusion (ICF) experiments seeking output gains of unity and beyond, the quality of the ablator capsule is paramount for minimizing the hydrodynamic mix that quenches the central hot spot. Defects in the form of foreign particles or missing mass on the surface and within the wall of the capsule are primary offenders. High-density carbon capsules made for ICF experiments at the National Ignition Facility are precision polished to achieve surface smoothness on the order of a few nanometers as well as to minimize isolated defects in the form of pits. Given the critical role of this process, we are developing smart manufacturing techniques with the goal of elevating the efficiency of this process. Our approach is to use MEMS (micro-electromechanical systems)–based sensors to capture the fine vibration signals generated during the polishing process and combine them with synchronized visual feedback as needed. Beyond using these sensors for process monitoring, we use specific deep learning methods to analyze the data and extract correlations with both the process parameters and the final performance of the polishing run. Here, in this work, we describe the multiple fronts we have explored in this regard and the results we have gotten so far. This approach promises to have the potential to ultimately provide real-time feedback that can be used to ensure the progress of the run as well as a means for faster optimization.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Development of a high current density, high temperature superconducting cable for pulsed magnets

Abstract A low AC loss Rare Earth Barium Copper Oxide (REBCO) cable, based on the VIPER cable technology has been developed by Commonwealth Fusion Systems for use in high field, REBCO based tokamaks. The new cable is composed of partitioned and transposed copper ‘petals’ shaped to fit together in a circular pattern with each petal containing a REBCO tape stack and insulated from each other to reduce AC losses. A stainless steel jacket adds mechanical robustness—also serving as a vessel for solder impregnation—while a tube runs through the middle for cooling purposes. Additionally, fiber optic sensors are placed under the tape stacks for quench detection. To qualify this design, a series of experiments were conducted as part of the SPARC tokamak Central Solenoid Model Coil program—to retire the risks associated with full scale, fast ramping, high flux HTS Central Solenoid (CS) and Poloidal Field (PF) coils for tokamak fusion power plants and net energy demonstrators. These risk study and risk reduction experiments include (1) AC loss measurement and model validation in the range of ~5 T/s, (2) an IxB electromagnetic loading of over 850 kN/m at the cable level and up to 300 kN/m at the stack level, (3) a transverse compression resilience of over 350 MPa, (4) manufacturability at tokamak relevant speeds and scales, (5) cable to cable joint performance, (6) fiber optic based quench detection speed, accuracy, and feasibility, and (7) overall winding pack integration and magnet assembly. The result is a cable technology, now referred to as PIT VIPER, with AC losses that measure fifteen times lower (at ~5 T/s) than its predecessor technology; a 2% or lower degradation of critical current (Ic) at high IxB electromagnetic loads; no detectable Ic degradation up to 570 MPa of transverse compression on the cable unit cell; end to end magnet manufacturing, consistently producing Ic values within 7% of the model prediction; cable to cable joint resistances at 20 K on the order of ~15 nΩ; and fast, functional quench detection capabilities that do not involve voltage taps. This cable technology will be tested comprehensively in a Central Solenoid Model Coil to prove its readiness for compact, high field tokamak operation.

Sanabria, Charlie (ORCID:0000000150175309)↗

Evidence of Kramer extrapolation inaccuracy for predicting high field Nb 3 Sn properties

Future applications requiring high magnetic fields, such as the proposed Future Circular Collider, demand a substantially higher critical current density, J c , at fields ≥16 T than is presently available in any commercial strand, so there is a strong effort to develop new routes to higher J c Nb 3 Sn. As a consequence, evaluating the irreversibility field (H irr ) of any new conductor to ensure reliable performance at these higher magnetic fields becomes essential. To predict the irreversibility field for Nb 3 Sn wires, critical current measurements, I c , are commonly performed in the 12-15 T range and the Kramer extrapolation is used to predict higher field properties. Here, the Kramer extrapolation typically models the contribution only for sparse grain boundary pinning, yet Nb 3 Sn wires rely on a high density of grain boundaries to provide the flux pinning that enables their high critical current density. However, whole-field range VSM measurements up to 30 T recently showed for Nb 3 Sn RRP® wires that the field dependence of the pinning force curve significantly deviates from the typical grain boundary shape, leading to a 1-2 T overestimation of Hirr when extrapolated from the typical mid-field data taken only up to about 15 T. In this work we characterized a variety of both RRP® and PIT Nb 3 Sn wires by transport measurements up to 29 T at the Laboratoire National des Champs Magnétiques Intenses (LNCMI), part of the European Magnetic Field Laboratory in Grenoble, to verify whether or not such overestimation is related to the measurement technique and whether or not it is a common feature across different designs. Indeed we also found that when measured in transport the 12-15 T Kramer extrapolation overestimates the actual H irr in both types of conductor with an inaccuracy of up to 1.6 T, confirming that high field characterization is a necessary tool to evaluate the actual high field performance of each Nb 3 Sn wire.

36 MATERIALS SCIENCE↗

Calibration of the 2-Phase Bubble Tracking Model for Liquid Mercury Target Simulation with Machine Learning Surrogate Models

The Spallation Neutron Source (SNS) at Oak Ridge National Laboratory is one of the most powerful accelerator-driven neutron sources in the world. The intense protons strike on SNS's mercury target to provide bright neutron beams, which also leads to severe fluid-structure interactions inside the target. Prediction of resultant loading on the target is difficult particularly when helium gas is injected into mercury to reduce the loading and mitigate the pitting damage on vessel walls. A 2-phase material model that incorporates the Rayleigh-Plesset (R-P) model is expected to address this multi-physics problem. However, several uncertain parameters in the R-P model require intensive simulations to determine their optimal values. With the help of machine learning and the measured target strain, we have studied the major uncertain parameters in this R-P model and developed a framework to identify optimal parameters that significantly reduce the discrepancy between simulations and experimental strains. The preliminary results show the possibility of using this mercury/helium mixture and surrogate models to predict a better match of target strain response when the helium gas is injected.

Lin, Lianshan↗

Measurement of Ehrlich-Schwoebel barrier contribution to the self-organized formation of ordered surface patterns on Ge(001)

Normal-incidence 1-keV Ar + ion bombardment leads to amorphization and ultrasmoothing of Ge at room temperature, but at elevated temperatures the Ge surface remains crystalline and is unstable to the formation of self-organized nanoscale patterns of ordered pyramid-shaped pits. The physical phenomenon distinguishing the high-temperature patterning from room-temperature ultrasmoothing is believed to be a surface instability due to the Ehrlich-Schwoebel barrier for diffusing vacancies and adatoms, which is not present on the amorphous material. This real-time grazing-incidence small-angle x-ray scattering study compares smoothing of a prepatterned Ge sample at room temperature with patterning of an initially flat Ge sample at an elevated temperature. In both experiments, when the nanoscale structures are relatively small in height, the average kinetics can be explained by a linear theory. Furthermore, the linear theory coefficients, indicating surface stability or instability, were extracted for both experiments. A comparison between the two measurements allows estimation of the contribution of the Ehrlich-Schwoebel barrier to the self-organized formation of ordered nanoscale patterns on crystalline Ge surfaces.

36 MATERIALS SCIENCE↗