Search NASA⌕ Search

SEARCH · Search NASA

Results for “Tensile Testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Instrumented impact and residual tensile strength testing of eight-ply carbon eopoxy specimens

Instrumented drop weight impact testing was utilized to examine a puncture-type impact on thin carbon-epoxy coupons. Four different material systems with various eight-ply lay-up configurations were tested. Specimens were placed over a 10.3-mm diameter hole and impacted with a smaller tup (4.2-mm diameter) than those used in previous studies. Force-time plots as well as data on absorbed energy and residual tensile strength were gathered and examined. It was found that a critical impact energy level existed for each material tested, at which point tensile strength began to rapidly decrease with increasing impact energy.

Nettles, A. T.↗

An Assessment of Variability in the Average Tensile Properties of a Melt-Infiltrated SiC/SiC Composite

Woven SiC/SiC Ceramic Matrix Composites (CMCs), manufactured by the slurry-cast, melt-infiltration process are under consideration as combustor liner materials in aircraft gas turbine engines. Tensile properties (elastic modulus, proportional limit strength, in-plane tensile strength and strain to failure) of the CMC, manufactured during two separate time periods (9/99 and 1/01) were determined at 816 and 1024 C by conducting tensile tests on specimens machined from the CMC plates. A total of 24 tensile tests were conducted for each temperature and CMC variant combination. In this study average tensile properties of the two cMC variants were statistically compared to evaluate significant differences, if any, within the CMC's properties.

Kalluri, Sreeramesh↗

Crystal plasticity modeling and analysis for the transition from intergranular to transgranular failure in nickel-based alloy Inconel 740H at elevated temperature

The precipitation-strengthened Nickel alloy Inconel® 740H® (IN740H) exhibits increased ductility at higher applied strain rates during quasi-static tensile tests at an elevated temperature of 760°C. The examination of fracture surfaces in this context reveals a noteworthy transition of underlying fracture mechanisms from transgranular to intergranular fracture as the applied strain rate decreases from 1×10 -3 / s to 0.83×10 -4 / s . To thoroughly understand the mechanical response of IN740H under these conditions, this study develops a crystal plasticity finite element (CPFE) model. Further, this model incorporates various deformation mechanisms including dislocation slips, climb, and grain boundary sliding, which are relevant to the test conditions. The model is calibrated using data from both tensile tests at different strain rates and creep tests across a broad stress range at 760°C, enabling the accurate determination of model parameters for each mechanism. Simulation results well captured the experimental observations of different failure modes. At higher strain rates, the model shows a dominance of dislocation slip leading to heterogeneous plastic deformation and formation of transgranular shear bands causing the failure, while at lower strain rates, an increased activity of grain boundary sliding causes grain boundaries crack leading to intergranular failure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Cu/Nb nano-composite wires processed by severe plastic deformation for applications in high pulsed magnets: effects of the multi-scale microstructure on the mechanical properties

Copper-based high strength and high electrical conductivity nano-composite wires reinforced by Nb nano-tubes are prepared by severe plastic deformation, applied with an Accumulative Drawing and Bundling process (ADB), for the windings of high pulsed magnets. The ADB process leads to a multi-scale Cu matrix containing up to N = 85{sub 4} (52.2.10{sup 6}) continuous parallel Nb tubes with diameter down to few tens nano-meters. After heavy strain, the Nb nano-tubes exhibit a homogeneous microstructure with grain size below 100 nm. The Cu matrix presents a multi-scale microstructure with multi-modal grain size distribution from the micrometer to the nano-meter range. The use of complementary characterization techniques at the microscopic and macroscopic level (in-situ tensile tests in the TEM, nano-indentation, in-situ tensile tests under high energy synchrotron beam) shed light on the interest of the multi-scale nature of the microstructure to achieve extreme mechanical properties, therefore allowing for design guidelines to further improve these properties. (authors)

36 MATERIALS SCIENCE↗

Effects of sigma-phase formation on some mechanical properties of a wrought nickel-base superalloy (IN-100)

The effect of sigma phase formation on an extruded and forged nickel base superalloy with the composition of the casting alloy IN-100 was studied. By adding only aluminum and titanium to remelt stock, three compositions were produced which had varying propensities for sigma formation. These compositions were given a four step heat treatment and were stress-ruptured or tensile tested. The very sigma prone composition had a shorter rupture life than the sigma-free or moderately sigma prone compositions when tested at 843 and 885 C. Elongation in room temperature tensile tests was considerably lower for the very sigma prone composition than for the other two wrought compositions after prolonged exposure at 732 or 843 C.

Dreshfield, R. L.↗

Fundamental Study of Micro-Defects in Electropolished EB-Welded and Hydroformed SRF Accelerating Structures

In the area of niobium elecropolishing fundamentals, we focused on understanding the influence of the surface topology, and geometry (with effects from gravity included. The formation of a viscous film is essential for the electropolishing process to take place. The exact nature and composition of the film formed on niobium is still unknown because of its solubility in the electrolyte. Extensive pitting may take place at surface where a stable film cannot form. This has to be taken into consideration while determining the speed with which the SRF cavities are rotated while EP. Hydrodynamic aspects must be taken into consideration while optimizing the polishing parameters. There is improvement in surface finish with polishing time. There is a huge change in surface quality when the EP time is increased from 2 hours to 4 hours but not much change takes place when the time is further increased to 6 hours. So keeping the economic points in view, about 100 um defect layer removal may be sufficient to get the desired performance. In the area of Electropolishing of untreated and treated niobium with Weld Joints we studied untreated and treated Nb, especially for the heat affected areas next to welded bumps, electropolished for different durations. The electropolishing of the untreated Nb caused the formation of pits on the surface at about 15 min but they disappeared when the electropolishing duration was more than 15 min. Electropolishing for 120 min smoothened the surface of untreated Nb by levelling the surface, but the severe formation of pits on the whole surface was found after 240 min. The treatment of Nb significantly changed the Nb surface morphology which was covered by grains of different size that looked light or dark in the optical microscope. The treated Nb was susceptible to pitting during the entire electropolishing starting from 15 min and the dark grains had more susceptibility to pitting than the light grains. In addition, electropolishing for 240 min again resulted in severe pit formation. In the area of Bulge test and microstructure studies, we worked to create a useful constitutive relationship for the complex stress state that accompanies SRF cavity formation. To do so, bulge tests were performed on Cu and Nb tube samples that exhibited the greatest degrees of uniaxial elongation after HT. The data from the bulge tests and an accompanying set of tensile tests provided input to a finite-element model that recreated the bulge tests numerically. As expected the model based on the bulge test results fit the experimental data well at least at low stress levels safely below the bursting pressure. Not so for that based on the tensile results. The results of the study emphasize the importance of for bulge testing rather than tensile testing when deriving the constitutional relationships eventually needed for modelling the hydroforming of Nb SRF cavities.

43 PARTICLE ACCELERATORS↗

Correlation of Microstructure and Mechanical Properties of Metal Big Area Additive Manufacturing

Metal Big Area Additive Manufacturing (MBAAM) is a novel wire-arc additive manufacturing method that uses a correction-based approach developed at the Oak Ridge National Laboratory (ORNL). This approach is an integrated software method that minimizes the dynamic nature of welding and compensates for build height. The MBAAM process is used to fabricate simple geometry thin walled specimens, using a C-Mn steel weld wire, to investigate the scatter in mechanical properties and correlate them to the underlying microstructure. The uni-axial tensile tests show isotropic tensile and yield properties with respect to building directions, although some scatter in elongation is observed. Large scatter is observed in the Charpy Impact tests. The microstructure characterization reveals mostly homogenous ferrite grains with some pearlite, except for some changes in morphology and grain size at the interface between the build and the base plate. The measured properties and microstructure are compared with the toughness and strength values reported in the literature, and a hypothesis is developed to rationalize the differences. Overall, the MBAAM process creates stable, isotropic, and weld-like mechanical properties in the deposit, while achieving a precise geometry obtained through a real-time feedback sensing, closed loop control system.

36 MATERIALS SCIENCE↗

Notch effects on room temperature tensile and bend properties of Ni3Al and Ni3Al+B

The notched mechanical properties of Ni3Al and Ni3Al+B prepared by powder metallurgy techniques have been determined in both tension and bending at room temperature. Tensile tests performed using double-notched specimens containing relatively blunt notches produced intergranular fracture in both Ni3Al and Ni3Al+B, with evidence of fracture initiating in an intergranular manner ahead of the blunt notch in both cases. Estimates of notched fracture toughness from bend tests and of local grain boundary fracture stress from the notched tensile tests suggest an increase in these values with boron addition.

Khadkikar, P. S.↗

Composition-dependence of 316 austenitic stainless steel deformation and aging properties for high-temperature applications - 18696

The present article is part of a broader effort aimed at assessing the possibility of tailoring the plasticity of austenitic stainless steels for structural applications in nuclear reactors. Three annealed heats of 316 stainless steel with large differences in stacking fault energy, carbon content, and ferrite content were used to study deformation and aging behaviors. Deformation of samples was investigated at room temperature by conventional tensile testing and at 350 deg. C by in situ neutron diffraction tensile testing. Aging was studied after 15 h at 750 deg. C through X ray diffraction and nano-indentation. (authors)

36 MATERIALS SCIENCE↗

Water-assisted mechanical testing of polymeric thin-films

Thin films with a nanometer-scale thickness are of great interest to both scientific and industrial communities due to their numerous applications and unique behaviors different from the bulk. However, the understanding of thin-film mechanics is still greatly hampered due to their intrinsic fragility and the lack of commercially available experimental instruments. In this review, we first discuss the progression of thin-film mechanical testing methods based on the supporting substrate: film-on-solid substrate method, film-on-water tensile tests, and water-assisted free-standing tensile tests. By comparing past studies on a model polymer, polystyrene, the effect of different substrates and confinement effect on the thin-film mechanics is evaluated. These techniques have generated fruitful scientific knowledge in the field of organic semiconductors for the understanding of structure–mechanical property relationships. Here, we end this review by providing our perspective for their bright prospects in much broader applications and materials of interest.

42 ENGINEERING↗

Stiffness reductions during tensile fatigue testing of graphite/epoxy angle-ply laminates

The monitoring of modulus decay during fatigue testing as an indicator of damage accumulation and incipient failure has frequently been postulated. The present study was designed to generate tensile fatigue data under carefully controlled test conditions. A computerized data acquisition system was used to permit the measurement of dynamic modulus without interrupting the fatigue cycling. Two different 8-ply laminate configurations, viz, (+ or - 45)2s and (+ or - 67.5)2s, of a T300/5208 graphite/epoxy composite were tested. The (+ or 45)2s laminate did exhibit some modulus decay, although there was no well-defined correlation with applied stress level or number of cycles. The (+ or - 67.5)2s laminate did not exhibit any measurable modulus decay. Secondary effects observed included a slight recovery of the modulus decay after a test interruption, and a significant viscoelastic (creep) response of the (+ or - 45)2s laminate during fatigue testing.

Odom, E. M.↗

Mechanisms of Oxide Formation in the Self-Reacting Friction Stir Weld Process

The initial objective of this study was to evaluate the effect of an extended delay time between preweld cleaning and the completion of a self-reacting friction stir welding (SRFSW) process on the resulting quality of various thickness panels of AA2219-T87. The current NASA standard specifies no more than a 48 hour delay between preweld cleaning and actual welding. The concern is whether increasing the cleaning delay time results in development of the residual oxide defect (ROD) in SRFSW. This concern emanates from the possibility of increased time correlating with increased oxide layer thickness on the faying surfaces. Oxide content on the faying surfaces has been reported to correlate with the occurrence of the ROD which reduces mechanical properties. When the SRFSW process was first adopted by the NASA Marshall Space Flight Center (MSFC), unexpected low tensile values that resulted were attributed to oxides within the weld that appeared to follow the former faying surface contours. Mitigation of the ROD was achieved through a combination of modifications to the processing parameters, tool designs, and incorporation of a weld seam offset. Two operations are involved in preweld cleaning: the first is removal of oil and grease, and the second is removal of surface oxides. In arc welding, improper cleaning of the faying surfaces of aluminum welded joints can increase the sensitivity toward development of defects. As the aluminum is locally melted, these contaminants contribute toward the development of porosity, inclusions, entrapped oxides, and other discontinuities which can degrade the strength of the weld joint. For weldment of large structures, the weld joint is typically cleaned, fit-up, and tack welded prior to the final full penetration welding pass. Because of the stringent joint fit-up requirements for mismatch and peaking for launch vehicle structures, the joint fit-up can sometimes contribute to lengthy delays between cleaning and tack welding, especially for circumferential weld joints on large diameter components. When the conventional friction stir welding (CFSW) process was introduced at the NASA MSFC, there was no procedure for cleaning prior to the solid-state joining process. As the process expanded to include SRFSW, preparation of the faying, crown, and root surfaces were implemented to overcome the ROD. Although the solid-state process is not expected to reach temperatures high enough for dissociation of the native oxide layer, concern remained regarding the redeposition of the native oxide layer within the stir zone. NASA has previously established the allowable time at 48 hours between preweld cleaning and a SRFSW process. The effect of potential 2 contamination resulting from an extended delay to 188 hours was subsequently evaluated for SRFSWs using tensile testing and metallographic imaging. Tensile specimens were tested at room temperature (RT), and at cryogenic conditions of liquid nitrogen (LN2) and liquid hydrogen. No detrimental effect on weld quality, as determined by weld strength, was reported for cleaning delays of 48, 120, 168, 240 or 288 hours. While no trends were established in this study, which extended the delay from 48 to 188 hours, there were a few outliers in terms of ultimate tensile strength (UTS). According to M. Fisher's 2014 Boeing Company Memo no. EYBF-MAF-14-029, all outliers were above the minimum acceptance criteria, but out of family with respect to the average values. As the robustness and reliability of any process ultimately depends on the average values as well as the outliers, an understanding of the cause of these outliers will ultimately improve the process. This report examines those outliers and their possible causes.

Schneider, J. A.↗

Characteristics of laser welded wrought Mg-Al-Mn alloy

Magnesium alloys have gained increased attention in recent years as a structural metal because of their property merits, which necessitates the development of welding techniques qualified for applications in the aeronautic and automotive industries. Laser welding is known to be an excellent method for joining metals. In this paper, a 3 kW CO{sub 2} laser beam was used to weld the wrought Mg-Al-Mn alloy. The characteristics of the microstructure and the mechanical properties of the joints were analyzed by optical microscopy (OM), energy dispersive spectrometry (EDS), scanning electron microscopy (SEM), tensile testing and hardness testing. The experimental results show that the wrought Mg-Al-Mn alloy can be joined successfully using optimized welding conditions. The results of tensile testing show that the highest ultimate tensile strength (UTS) of the joints is up to 94% of that of the base metal. The base metal consists of a typical rolled structure, the narrow heat affected zone (HAZ) has no obvious grain coarsening, and the fusion zone consists of fine grains with a high density of {gamma}-Mg{sub 17}Al{sub 12} precipitates. The hardness test results indicate that the microhardness in the fusion zone is higher than that of the base metal. The elemental analysis reveals that the Mg content in the weld is lower than that of the base metal, but the Al content is slightly higher.

36 MATERIALS SCIENCE↗

Effect of Grain Boundary and Crystallographic Orientation on the Stress Corrosion Behavior of an Al-Zn-Mg Alloy

The effect of grain boundary and crystallographic orientation on the stress corrosion behavior of an Al-4.5Zn-1.4Mg alloy was investigated by comparing the performance of constant load stress corrosion test (CLSCT) and tensile test of specimens parallel to the longitudinal and transverse directions of the extruded plate. The results revealed that the strength of the longitudinal and transverse specimens decreased by 9.68 and 18.13%, respectively, after 10-day CLSCT. The transverse specimens show poor resistance to stress corrosion cracking (SCC). The grain boundaries (GB) of the longitudinal section are less dense, and more of them are distributed along the extrusion direction compared with the cross section with selected areas of the same size. The SCC of all specimens starts from the side faces of the specimen, and it is dominated by intergranular cracking. But the corrosion of the transverse specimens was more serious. The cracks of all specimens tend to propagate along the GBs with misorientation of about 50°-60°, and the difference of Schmidt factor (SF) values of grains on both sides of the crack is significantly large. The crack of longitudinal specimens propagates relatively parallel to the tensile direction, while propagation of the crack in transverse specimens is more zigzag.

36 MATERIALS SCIENCE↗

Effect of Microstructure Refinement on Hardness Homogeneity of Aluminum Alloy 1100 Processed by Accumulative Roll Bonding

This work examines the effect of grain refinement via accumulative roll bonding (ARB) on the homogeneity of microstructure and hardness through the thickness of commercially pure aluminum AA1100 sheets. The use of 7 cycles of ARB was shown to produce homogeneous ultrafine-grained microstructure, reducing the grain size to 0.46 and 1.03 µm in normal direction and rolling direction, respectively. Examination by electron backscattered diffraction indicates that continuous dynamic recrystallization was the main mechanism for the formation of submicron equiaxed grains bounded with high-angle grain boundaries (HAGBs). The fraction of HAGBs increased gradually reaching a maximum of 71.6% after 7 cycles. Through-thickness hardness measurements using Vickers and nanoindentation tests show an increase from 43.5 Hv (0.85 GPa) for as-received sample to 63 Hv (1.1 GPa) after 7 cycles. The heterogeneity in hardness through the thickness of the as-received material was shown to restrain the evolution of uniform hardness across the sheet thickness with increasing ARB cycles. Tensile tests showed that the tensile strength is increased to 250 MPa, which is about 2 times its initial value. Owing to the high stacking fault energy of AA1100, strong dynamic recovery occurred with increasing ARB strain which was balanced with the strain hardening property of the material. This resulted in plastic instability at small strains and thus early necking during the tensile test.

36 MATERIALS SCIENCE↗

Enhanced Strength of 304 SS-Ti6Al4V Laser-Welded Joints Containing Composite Interlayers

This paper investigates the microstructural characterization of the fracture propagation edge during laser beam welding of Ti6Al4V and 304 stainless steel using Cu, V, and Ni interlayers as a single Cu interlayer and composite interlayer structures with different Cu interlayer thicknesses. This study attempts to increase the Ti-SS joint strength through the use of the composite interlayers. X-ray diffraction characterization based on a 0.5-mm-thick Cu interlayer showed that the SS/Cu/Ti joint contained considerable brittle IMCs; however, the fracture surface of the SS/Cu-V/Ti composite interlayer sample did not contain any Fe-Ti IMCs or Cr{sub 2}Ti. EBSD observation indicated that the crack propagated transgranularly from solidified CuTi in the interdendritic regions of the FeTi compounds in the composite interlayer sample; however, the crack propagated intergranularly along Fe{sub 2}Ti grain boundaries in the single interlayer sample. The investigation based on a 1-mm-thick Cu interlayer showed that the SS/Ni-Cu1/Ti sample was stronger than the SS/Cu1/Ti sample due to a lack of CuTi at 3.5 kW. The tensile strength of the SS/Cu1-V/Ti joint was greater than that of the SS/Ni-Cu1/Ti joint due to the formation of ductile NiTi instead of brittle NiTi{sub 2}. The microstructures of the fracture edges after tensile testing illustrated that the eutectic CuTi + CuTi{sub 2} fractured at the SS/Cu1/Ti joint after tensile testing, while CuTi{sub 2} and eutectoid αTi + CuTi{sub 2} compounds fractured during the tensile experiment at the SS/Ni-Cu1/Ti and SS/Cu1-V/Ti joints, respectively. Investigations based on both the 0.5- and 1-mm-thick Cu interlayers showed that the tensile strength and elongation of the composite interlayer joints at a laser power of 3.5 kW were greater than those of the single interlayer joints.

36 MATERIALS SCIENCE↗

High-temperature secondary hydriding experiments with E110 and E110G claddings - 2016-0031

Secondary hydriding can take place during a loss-of-coolant accident event after the ballooning and burst of the zirconium alloy cladding. The oxidation and hydrogen uptake in the ballooned section can produce the weakest segment of the rod. This phenomenon was investigated in the past mainly for Zircaloy-4 cladding. We investigated the effect of secondary hydriding in VVER reactors with E110 and E110G alloys. A high-temperature facility was built to carry out high-temperature treatment of fuel cladding samples. The burst of tubes was reached with inner pressurization at 750 and 800 C. After burst the samples were oxidized in the same furnace for different periods and at different temperatures. The oxidized samples were tested in a tensile test machine with four-point bending tests. The microstructure of the samples was analyzed by optical and scanning electron microscopy. The hydrogen content of the cladding was measured by heat extraction, prompt gamma activation analyses, and neutron radiography methods. The experiments indicated that the ballooned section after oxidation became the weakest segment of the VVER fuel. According to the mechanical testing, the cladding samples were brittle even after a short oxidation time (200 s at 1,000 C) without any sign of ductile behavior. The comparison of E110 and E110G samples showed that the E110 tubes lost their load-bearing capability or even integrity much earlier than the E110G samples treated under similar conditions. (authors)

36 MATERIALS SCIENCE↗

Weldability of high-toughness iron - 12 percent-nickel alloys with reactive metal additions of titanium, aluminum, or niobium

Three exceptionally high toughness Fe-12Ni alloys designed for cryogenic service were welded by using the gas tungsten arc welding process. Evaluation of their weldability included equivalent energy fracture toughness tests, transverse weld tensile tests at -196 and 25 C, and weld crack sensitivity tests. The Fe-12Ni-0.25Ti alloy proved extremely weldable for cryogenic applications, having weld and heat affected zone properties comparable to those of the wrought base alloy. The Fe-12Ni-0.5Al alloy had good weld properties only after the weld joint was heat treated. The Fe-12Ni-0.25Nb alloy was not considered weldable for cryogenic use because of its poor weld joint properties at -196 C and its susceptibility to hot cracking.

Delvetian, J. H.↗