Search NASA⌕ Search

SEARCH · Search NASA

Results for “Ultimate tensile strength”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Impact Resistance of Uncoated SiC/SiC Composites

Two-dimensional woven SiC/SiC composites fabricated by melt infiltration method were impact tested at room temperature and at 1316 C in air using 1.59-mm diameter steel-ball projectiles at velocities ranging from 115 to 400 m/s. The extent of substrate damage with increasing projectile velocity was imaged and analyzed using optical and scanning electron microscopy, and non-destructive evaluation (NDE) methods such as pulsed thermography, and computed tomography. The impacted specimens were tensile tested at room temperature to determine their residual mechanical properties. Results indicate that at 115 m/s projectile velocity, the composite showed no noticeable surface or internal damage and retained its as-fabricated mechanical properties. As the projectile velocity increased above this value, the internal damage increased and mechanical properties degraded: At velocities >300 m/s, the projectile penetrated through the composite, but the composite retained approx.50% of the ultimate tensile strength of the as-fabricated composite and exhibited non-brittle failure. Predominant internal damages are delamination of fiber plies, fiber fracture and matrix shearing.

Bhatt, Ramakrishna T.↗

Application of an Elongated Kelvin Model to Space Shuttle Foams

The space shuttle foams are rigid closed-cell polyurethane foams. The two foams used most-extensively oil space shuttle external tank are BX-265 and NCFL4-124. Because of the foaming and rising process, the foam microstructures are elongated in the rise direction. As a result, these two foams exhibit a nonisotropic mechanical behavior. A detailed microstructural characterization of the two foams is presented. Key features of the foam cells are described and the average cell dimensions in the two foams are summarized. Experimental studies are also conducted to measure the room temperature mechanical response of the two foams in the two principal material directions (parallel to the rise and perpendicular to the rise). The measured elastic modulus, proportional limit stress, ultimate tensile strength, and Poisson's ratios are reported. The generalized elongated Kelvin foam model previously developed by the authors is reviewed and the equations which result from this model are summarized. Using the measured microstructural dimensions and the measured stiffness ratio, the foam tensile strength ratio and Poisson's ratios are predicted for both foams and are compared with the experimental data. The predicted tensile strength ratio is in close agreement with the measured strength ratio for both BX-265 and NCFI24-124. The comparison between the predicted Poisson's ratios and the measured values is not as favorable.

Sullivan, Roy M.↗

Modeling Creep Effects in Advanced SiC/SiC Composites

Because advanced SiC/SiC composites are projected to be used for aerospace components with large thermal gradients at high temperatures, efforts are on-going at NASA Glenn to develop approaches for modeling the anticipated creep behavior of these materials and its subsequent effects on such key composite properties as internal residual stress, proportional limit stress, ultimate tensile strength, and rupture life. Based primarily on in-plane creep data for 2D panels, this presentation describes initial modeling progress at applied composite stresses below matrix cracking for some high performance SiC/SiC composite systems recently developed at NASA. Studies are described to develop creep and rupture models using empirical, mechanical analog, and mechanistic approaches, and to implement them into finite element codes for improved component design and life modeling

Lang, Jerry↗

Failure Analysis of T-38 Aircraft Burst Hydraulic Aileron Return Line

During maintenance troubleshooting for fluctuating hydraulic pressures, a technician found that a right hand aileron return line, on the flight hydraulic side, was ruptured (Fig. 1, 2). This tubing is part of the Hydraulic Flight Control Aileron Return Reducer to Aileron Manifold and is suspected to be original to the T-38 Talon trainer aircraft. Ailerons are small hinged sections on the outboard portion of a wing used to generate rolling motion thereby banking the aircraft. The ailerons work by changing the effective shape of the airfoil of the outer portion of the wing [1]. The drawing, Northrop P/N 3-43033-55 (6/1960), specifies that the line is made from 0.375 inch OD, aluminum 5052-0 tubing with a 0.049 inch wall thickness. WW-T-787 requires the tube shall be seamless and uniform in quality and temper [2]. The test pressure for this line is 3000 psi, and the operational pressure for this line is estimated to be between 45 psi and 1500 psi based on dynamic loading during flight. Examination of the fracture surface found evidence of arrest bands originating on the inner diameter (Fig 3). Ductile dimples are observed on the tube fractures (Fig. 4). The etched cross-section revealed thinning and work-hardening in the burst region (Fig. 5). The wall thickness just outside the work-hardened fracture region measured 0.035". Barlow's Formula: P = 2St/D, where P is burst pressure, S is allowable stress, t is wall thickness and D is the outer diameter of tube. Using the ultimate tensile strength of 28 ksi and a measured wall thickness of 0.035 inches at burst, P = 5.2 ksi (burst pressure). Using the yield of 13 ksi (YS) for aluminum 5052-0, plastic deformation will happen at P = 2.4 ksi suggesting plastic deformation occurred at a proof pressure of 3.0 ksi. Conclusion: The burst resulted from high stress, low-cycle fatigue. Evidence of arrest bands originating on the inner diameter. Fracture is predominately shear dimples, characteristic of high load ductile fractures (Fig 6). Section wall reduction in the burst region. Plastic deformation and thinning of the out-of-specification tube wall likely happened during the initial proof testing years ago. Metallography of tubing away from rupture site confirmed tubing was seamless. Based on the tube microstructure, it is likely that the initial wall thickness was about 30 % thinner than the requirement of 0.049 inches. Fracture initiated on the ID and progressed to the OD (shear lip). The tube is made of the correct material of 5052-0 aluminum as verified using Optical Emission Spectroscopy (Table 2). The tubing hardness tested 77 HV100 (77 HRE). This hardness is slightly above the requirement for 70 HRE maximum for aluminum 5052-0 in AMS 2658C [3].

Martinez, J. E.↗

Post-Flight Characterization of Samples for the MISSE-7 Spacesuit Fabric Exposure Experiment

Six samples of pristine and dust-abraded outer layer spacesuit fabrics were included in the Materials International Space Station Experiment-7, in which they were exposed to the wake side low Earth orbit environment (LEO) on the International Space Station (ISS) for 18 months in order to determine whether abrasion by lunar dust increases radiation degradation. The fabric samples were characterized using optical microscopy, field emission scanning electron microscopy, and tensile testing before and after exposure on the ISS. Comparison of pre- and post-flight characterizations showed that wake side LEO environment darkened and reddened all six fabrics, increasing their integrated solar absorptance by 7 to 38 percent. There was a decrease in the ultimate tensile strength and elongation to failure of lunar dust abraded Apollo spacesuit fibers by a factor of four and increased the elastic modulus by a factor of two. The severity of the degradation of the fabric samples over this short exposure time demonstrates the necessity to find ways to prevent or mitigate radiation damage to spacesuits when planning extended missions to the Moon.

Gaier, James R.↗

Degradation of Spacesuit Fabrics in Low Earth Orbit

Six samples of pristine and dust-abraded outer layer spacesuit fabrics were included in the Materials International Space Station Experiment-7, in which they were exposed to the wake-side low Earth orbit environment on the International Space Station (ISS) for 18 months in order to determine whether abrasion by lunar dust increases radiation degradation. The fabric samples were characterized using optical microscopy, optical spectroscopy, field emission scanning electron microscopy, atomic force microscopy, and tensile testing before and after exposure on the ISS. Comparison of pre- and post-flight characterizations showed that the environment darkened and reddened all six fabrics, increasing their integrated solar absorptance by 7 to 38 percent. There was a decrease in the ultimate tensile strength and elongation to failure of lunar dust abraded Apollo spacesuit fibers by a factor of four and an increase in the elastic modulus by a factor of two.

Gaier, James R.↗

Stochastic Nonlinear Response of Woven CMCs

It is well known that failure of a material is a locally driven event. In the case of ceramic matrix composites (CMCs), significant variations in the microstructure of the composite exist and their significance on both deformation and life response need to be assessed. Examples of these variations include changes in the fiber tow shape, tow shifting/nesting and voids within and between tows. In the present work, the influence of scale specific architectural features of woven ceramic composite are examined stochastically at both the macroscale (woven repeating unit cell (RUC)) and structural scale (idealized using multiple RUCs). The recently developed MultiScale Generalized Method of Cells methodology is used to determine the overall deformation response, proportional elastic limit (first matrix cracking), and failure under tensile loading conditions and associated probability distribution functions. Prior results showed that the most critical architectural parameter to account for is weave void shape and content with other parameters being less in severity. Current results show that statistically only the post-elastic limit region (secondary hardening modulus and ultimate tensile strength) is impacted by local uncertainties both at the macro and structural level.

Kuang, C. Liu↗

Development of Aluminum-Lithium 2195 Gores by the Stretch Forming Process

Aluminum-Lithium alloy 2195 exhibits higher mechanical properties and lower density than aluminum alloy 2219, which is the current baseline material for Space Launch System (SLS) cryogenic tank components. Replacement of Al 2219 with Al-Li 2195 would result in substantial weight savings, as was the case when this replacement was made on the shuttle external tank. A key component of cryogenic tanks are the gores, which are welded together to make the rounded ends of the tanks. The required thicknesses of these gores depend on the specific SLS configuration and may exceed the current experience base in the manufacture of such gores by the stretch forming process. Here we describe the steps taken to enhance the formability of Al-Li 2195 by optimizing the heat treatment and stretch forming processes for gore thicknesses up to 0.75", which envelopes the maximum expected gore thicknesses for SLS tanks. An annealing treatment, developed at Marshall Space Flight Center, increased the forming range and strain hardening exponent of Al-Li 2195 plates. Using this annealing treatment, one 0.525" thick and two 0.75" thick gores were manufactured by the stretch forming process. The annealing treatment enabled the stretch forming of the largest ever cross sectional area (thickness x width) of an Al-Li 2195 plate achieved by the manufacturer. Mechanical testing of the gores showed greater than expected ultimate tensile strength, yield strength, modulus, and elongation values. The gores also exhibited acceptable fracture toughness at room and LN2 temperatures. All of the measured data indicate that the stretch formed gores have sufficient material properties to be used in flight domes.

Volz, M. P.↗

Development of Aluminum-Lithium 2195 Gores by the Stretch Forming Process

Aluminum-Lithium alloy 2195 exhibits higher mechanical properties and lower density than aluminum alloy 2219, which is the current baseline material for Space Launch System (SLS) cryogenic tank components. Replacement of Al 2219 with Al-Li 2195 would result in substantial weight savings, as was the case when this replacement was made on the shuttle external tank. A key component of cryogenic tanks are the gores, which are welded together to make the rounded ends of the tanks. The required thicknesses of these gores depend on the specific SLS configuration and may exceed the current experience base in the manufacture of such gores by the stretch forming process. Here we describe the steps taken to enhance the formability of Al-Li 2195 by optimizing the heat treatment and stretch forming processes for gore thicknesses up to 0.75", which envelopes the maximum expected gore thicknesses for SLS tanks. An annealing treatment, developed at Marshall Space Flight Center, increased the forming range and strain hardening exponent of Al-Li 2195 plates. Using this annealing treatment, one 0.525" thick and two 0.75" thick gores were manufactured by the stretch forming process. The annealing treatment enabled the stretch forming of the largest ever cross sectional area (thickness x width) of an Al-Li 2195 plate achieved by the manufacturer. Mechanical testing of the gores showed greater than expected ultimate tensile strength, yield strength, modulus, and elongation values. The gores also exhibited acceptable fracture toughness at room and LN2 temperatures. All of the measured data indicate that the stretch formed gores have sufficient material properties to be used in flight domes.

Volz, M. P.↗

The Effects of Fiber Orientation and Adhesives on Tensile Properties of Carbon Fiber Reinforced Polymer Matrix Composite with Embedded Nickel-Titanium Shape Memory Alloys

Nickel-titanium (NiTi) shape memory alloy (SMA) sections were embedded within carbon fiber reinforced polymer matrix composite (CFRPPMC) laminates and their tensile properties were evaluated with simultaneous monitoring of modal acoustic emissions. The test specimens were fabricated in three different layup configurations and two different thin film adhesives were applied to bond the SMA with the PMC. A trio of acoustic sensors were attached to the specimens during tensile testing to monitor the modal acoustic emission (AE) as the materials experienced mechanical failure. The values of ultimate tensile strengths, strains, and moduli were obtained. Cumulative AE energy of events and specimen failure location were determined. In conjunction, optical and scanning electron microscopy techniques were used to examine the break areas of the specimens. The analysis of AE data revealed failure locations within the specimens which were validated from the microscopic images. The placement of 90 deg plies in the outer ply gave the strongest acoustic signals during break as well as the cleanest break of the samples tested. Overlapping 0 deg ply layers surrounding the SMA was found to be the best scenario to prevent failure of the specimen itself.

shape memory alloy↗

Mechanical Tensile Testing of Titanium 15-3-3-3 and Kevlar 49 at Cryogenic Temperatures

Titanium 15-3-3-3 and Kevlar 49 are highly desired materials for structural components in cryogenic applications due to their low thennal conductivity at low temperatures. Previous tests have indicated that titanium 15-3-3-3 becomes increasingly brittle as the temperature decreases. Furthermore, little is known regarding the mechanical properties of Kevlar 49 at low temperatures, most specifically its Young's modulus. This testing investigates the mechanical properties of both materials at cryogenic temperatures through cryogenic mechanical tensile testing to failure. The elongation, ultimate tensile strength, yield strength, and break strength of both materials are provided and analyzed here.

James, Bryan L.↗

Recombinant Spidroins Fully Replicate Primary Mechanical Properties of Natural Spider Silk

Dragline spider silk is among the strongest and toughest bio-based materials, capable of outperforming most synthetic polymers and even some metal alloys.1,2,3,4 These properties have gained spider silk a growing list of potential applications that, coupled with the impracticalities of spider farming, have driven a decades-long effort to produce recombinant spider silk proteins (spidroins) in engineered heterologous hosts.2 However, these efforts have so far been unable to yield synthetic silk fibers with mechanical properties equivalent to natural spider silk, largely due to an inability to stably produce highly repetitive, high molecular weight (MW) spidroins in heterologous hosts.1,5 Here we address these issues by combining synthetic biology techniques with split intein (SI)- mediated ligation for the bioproduction of spidroins with unprecedented MW (556 kDa), containing 192 repeat motifs of the Nephila clavipes MaSp1 dragline spidroin. Fibers spun from these synthetic spidroins display ultimate tensile strength (σ), modulus (E), extensibility (ε), and toughness (UT) of 1.03 +/- 0.11 GPa, 13.7 +/- 3.0 GPa, 18 +/- 6%, and 114 +/- 51 MJ/m3, respectively-equivalent to the performance of natural N. clavipes dragline silk.6 This work demonstrates for the first time that microbially produced synthetic silk fibers can match the performance of natural silk fibers by all common metrics (σ, E, ε, UT), providing a more dependable source of high-strength fibers to replace natural spider silks for mechanically demanding applications. Furthermore, our biosynthetic platform can be potentially expanded for the assembly and production of other protein-based materials with high MW and repetitive sequences that have so far been impossible to synthesize by genetic means alone.

spider silk↗

The Effects of Fiber Orientation and Adhesives on Tensile Properties of Carbon Fiber Reinforced Polymer Matrix Composite with Embedded Nickel-Titanium Shape Memory Alloys

Tensile tests of Nickel-titanium (NiTi) shape memory alloys (SMA) embedded within carbon fiber reinforced polymer matrix composite (CFRP/PMC) laminates were evaluated with simultaneous monitoring of modal acoustic emissions (MAE). Three different layup configurations utilizing two different thin film adhesives were applied to bond the materials. Ultimate tensile strengths, strains, and moduli were obtained along with cumulative AE energy of events and specimen failure location. Scanning electron microscopy was used to examine the break areas of the specimens post-test. Microscopy was used to validate failure locations revealed from MAE analysis. A unique finding within this research showed that 90° plies in the outer ply gave the strongest acoustic signals as well as the cleanest fracture of the specimens tested. Overlapping 0° ply layers surrounding the SMA was found to be the best scenario to prevent failure of the specimen itself.

Derek Quade↗

Exploration of Failure and Potential Damage Markers in Ti-6Al-4V

To improve prognostics for predicting component life, coupon tests were conducted on Ti-6Al-4V to investigate the development of damage. Various test types were employed (tension, creep, stress relaxation, and fatigue) under a wide range of temperatures and loading rates to engage various amounts of time-dependent and damage behavior. Both stiffness degradation and Poisson’s ratio were monitored to see if they were useful in indicating the initiation and accumulation of damage and subsequently the onset of failure. Stiffness exhibited large decreases with increasing strain when calculated using engineering stress and strain. However, minimal stiffness change was observed when using the true-stress and true- strain values. Detailed microscopy and image analysis were performed to document the actual physical damage that occurred within the various specimens. Two types of damage were observed: shallow surface cracks and internal pores. The severity of damage was greater in the region of localized necking and diminished further away from the neck. The area fraction of pores was higher in the necked region, yet even there it did not exceed more than a few percent and, in most cases, was significantly lower. It was observed that conditions that induced more time-dependent deformation (e.g., slower strain rate testing) resulted in a larger number of pores and larger pore sizes. The pores were always found to occur in the softer β-phase. The severity of observed damage was inconsistent with the large drop in engineering stiffness, but was more aligned with stiffness changes from the true-stress and -strain values. Poisson’s ratio was monitored on every test and showed promise as a damage indicator. It was found to be more sensitive than either the ultimate tensile strength or the inception of tertiary creep. However, calculation of Poisson’s ratio was found to be more involved than expected because of anisotropy and the presence of strain gradients along the specimen at large applied strains. First, the material had a moderate texture and resulted in anisotropy of the strains. Second, the evolution of Poisson’s ratio as a function of axial strain showed strange and unexpected behaviors, which necessitated more extensive analyses of its development. This led to an investigation on the use of small versus large strain approaches and the importance of making consistent measurements; that is, axial and transverse strain measurements over the same volume of material. Additionally, finite element analysis of a tensile sample indicated that non- uniform strain occurred in the sample prior to attaining the maximum strength. This, along with the location at which transverse strain was measured, had a significant influence on the resulting values of Poisson’s ratio. Based on this, lessons learned are offered for future testing.

Ti-6Al-4V↗

Space Environmental Effects on Additively Manufactured (AM) Parts on MISSE-9/10

The Materials on International Space Station Experiment (MISSE) experiments have made a continuous presence on the ISS and allowed for testing of performance and durability of materials exposed to the Low Earth Orbit (LEO) space environment. Additive Manufacturing (AM) has been included on several MISSE flights, and many companies (Made in Space and Stratasys) and NASA centers wanted to test various AM material samples. The goal of studying Space Environmental Effects on AM Parts with MISSE 9/10 was to fly promising metal and polymer AM material samples (dogbones) that could have future manufacturing capabilities in space and conduct post-flight analysis of these materials via mechanical and optical properties. On these flights, MISSE-9 contained three Inconel and 12 polymer samples and MISSE-10 included three Inconel and 16 polymer samples. Before flying to the ISS, all the samples underwent thermal vacuum bakeout (at 60°C for 24 hours and 10-6 torr). After bakeout, control and flight experiments were weighed, and optical properties were taken. Optical properties such as solar absorptance and infrared emittance were taken on the control samples and the flight samples (preflight and postflight). To understand more about the mechanical properties of the AM samples, tensile testing was conducted on the samples to determine the yield and ultimate tensile strength of the dogbone samples against the control. Lastly, the torque on the fasteners securing the dogbone samples were loosened and measured using a torque wrench, and they were compared to their preflight torque specification required. Optical properties and masses were recorded before flight, and the postflight results were recorded and collected in June 2022 to study the effects. With the postflight analysis, NASA engineers can now better characterize how UV radiation and thermal cycling affect the material properties.

Materials on International Space Station Experimen↗

Stress Corrosion Evaluation of NiTiHf Alloy for the International Space Station Environmental Control and Life Support System

A stress corrosion evaluation was performed on NiTiHf alloy because this material is considered a bearing material candidate for the Environmental Control and Life Support System. Stressed round tensile specimens survived exposures to alternate pretreat, alternate brine, baseline pretreat, baseline brine, and 3.5% NaCl alternate immersion. Metallographic evaluations did not detect stress corrosion on exposed samples. The ultimate tensile strength values varied significantly for this material, which is common for bearing materials. This variation was observed on both, exposed and nonexposed specimens. The results of this work indicate that this material has potential applications as a bearing material.

International Space Station (ISS)↗

Microstructural Evolution and Mechanical Properties of LP-DED NASA HR-1 – A Hydrogen Resistant AM Superalloy for Space Propulsion Applications

The National Aeronautics and Space Administration (NASA) has actively pursued metal additive manufacturing (AM) technologies for spaceflight applications since the late 2000s. AM offers transformative advantages in cost, schedule, part consolidation, and design flexibility. Among the various AM techniques, laser powder directed energy deposition (LP-DED) is particularly well suited for fabricating complex geometries with fine feature resolution. In propulsion systems that utilize high-pressure gaseous hydrogen—such as liquid hydrogen rocket engines—hydrogen environment embrittlement (HEE) presents a serious threat to material performance 1,2 . Mechanical property degradation under these conditions can compromise component reliability, especially under cyclic loading. To address this challenge, NASA developed NASA HR-1 (Hydrogen Resistant-1) as a solution for liquid rocket engine components operating in hydrogen-rich environments, using the LP-DED technique 3-9 . A key component in a liquid rocket engine is the exhaust nozzle, which is typically regeneratively cooled (regen) due to the high heat flux. NASA HR-1 was specifically developed for regen nozzle applications using hydrogen as a propellant, providing resistance to HEE, a critical issue for many materials. The AM version of NASA HR-1 was also formulated to achieve high ultimate tensile strength, along with high yield strength and ductility in this environment 5,6 . Low-cycle fatigue (LCF) is another important consideration in nozzle design, as components are expected to endure multiple starts and missions. Additionally, the LP-DED version of the alloy exhibits improved thermal conductivity compared to its wrought counterpart, which benefits nozzle cooling. Overall, NASA HR-1 offers an excellent balance of high strength, HEE resistance, LCF performance, thermal conductivity, and ductility to meet the demanding requirements of channel-cooled nozzles and other components used with hydrogen and other propellants. The LP-DED–processed NASA HR-1 requires several post-processing heat treatment steps to achieve the material properties desirable for its intended application 6 . These steps include stress relief, homogenization, solution annealing, and aging for precipitation hardening. The stress relief treatment mitigates residual stresses accumulated during the LP-DED process and minimizes the potential for distortion. Homogenization, a common step for AM materials, reduces elemental segregation and promotes recrystallization to develop a more equiaxed grain structure. The subsequent solution annealing treatment heats the part to a solid solution temperature to dissolve the undesirable η-phase that forms during cooling from homogenization, followed by rapid cooling to retain an η-phase–free microstructure. Finally, aging promotes precipitation of the strengthening γ′ phase in the alloy. The integration of compositional design and optimized thermal processing enables high-quality LP-DED NASA HR-1 components with excellent microstructural and mechanical stability. Improved chemical and microstructure homogeneity enhances ductility and fatigue resistance—both critical for safe and reliable operation in high-pressure hydrogen environments. NASA has successfully fabricated and hot-fire tested multiple subscale and full-scale channel wall nozzles using LP-DED NASA HR-1 5,6, 9-14 . These efforts included process refinements to support thin-wall construction and various channel geometries. Throughout development, several key observations emerged. After homogenization, the as-built columnar grain structure transforms into a fully equiaxed microstructure. However, subsequent treatments—such as solution annealing and aging—result in changes that are more difficult to track. The grain structure remains largely unchanged, and the γ′ precipitates, typically 5–10 nm in diameter, are beyond the resolution of scanning electron microscopy (SEM). While transmission electron microscopy (TEM) can resolve these fine precipitates, TEM sample preparation is time-consuming and difficult for LP-DED material. As an alternative, differential scanning calorimetry (DSC) offers a useful, qualitative approach to monitor precipitate evolution throughout different stages of heat treatment. The overall goal is to improve the understanding of how heat treatment affects the microstructure and mechanical performance of LP-DED NASA HR-1. This paper presents heat treatment design considerations, microstructural characterization, mechanical testing – including tensile and LCF testing in both air and hydrogen environments.

Superalloy↗

Shear Assisted Processing and Extrusion of Aluminum Alloy 7075 Tubing at High Speed

Conventional extrusion of aluminum alloy 7075 is limited to 1-2 meters per minute in order to avoid surface tearing and cracking. An emerging technique called Shear Assisted Processing and Extrusion (ShAPE) was used to extrude aluminum alloy 7075 tubing at a speed of 7.4 meters per minute without inducing surface defects. The faster extrusion speed is attributed to the unique flow characteristics inherent to the ShAPE process compared to conventional extrusion. Tubes with an inner diameter of 10 mm, outer diameter of 12 mm, and length of 2 meters were extruded at temperatures ranging from 340°C to 466°C. Tensile testing was performed per ASTM B557-15 with strain measured using digital image correlation. An ultimate tensile strength of 565 ± 4.6 MPa, yield strength of 496 ± 8.7 MPa, and elongation of 16.4 ± 1.0 % were measured for extrusion made at 362°C and heat treated to the T6 condition.

Shear Assisted Processing and Extrusion, Friction ↗