Computed Tomography 3-D Imaging of the Metal Deformation Flow Path in Friction Stir Welding

In friction stir welding (FSW), a rotating threaded pin tool is inserted into a weld seam and literally stirs the edges of the seam together. To determine optimal processing parameters for producing a defect free weld, a better understanding of the resulting metal deformation flow path is required. Marker studies are the principal method of studying the metal deformation flow path around the FSW pin tool. In our study, we have used computed tomography (CT) scans to reveal the flow pattern of a lead wire embedded in a FSW weld seam. At the welding temperature of aluminum, the lead becomes molten and is carried with the macro-flow of the weld metal. By using CT images, a 3-dimensional (3D) image of the lead flow pattern can be reconstructed. CT imaging was found to be a convenient and comprehensive way of collecting and displaying tracer data. It marks an advance over previous more tedious and ambiguous radiographic/metallographic data collection methods.

Schneider, Judy↗

Study of Radiographic Linear Indications and Subsequent Microstructural Features in Gas Tungsten Arc Welds of Inconel 718

This study presents examples and considerations for differentiating linear radiographic indications produced by gas tungsten arc welds in a 0.05-in-thick sheet of Inconel 718. A series of welds with different structural features, including the enigma indications and other defect indications such as lack of fusion and penetration, were produced, radiographed, and examined metallographically. The enigma indications were produced by a large columnar grain running along the center of the weld nugget occurring when the weld speed was reduced sufficiently below nominal. Examples of respective indications, including the effect of changing the x-ray source location, are presented as an aid to differentiation. Enigma, nominal, and hot-weld specimens were tensile tested to demonstrate the harmlessness of the enigma indication. Statistical analysis showed that there is no difference between the strengths of these three weld conditions.

Walley, J. L.↗

Friction stir welding process to repair voids in aluminum alloys

The present invention provides an in-process method to repair voids in an aluminum alloy, particularly a friction stir weld in an aluminum alloy. For repairing a circular void or an in-process exit hole in a weld, the method includes the steps of fabricating filler material of the same composition or compatible with the parent material into a plug form to be fitted into the void, positioning the plug in the void, and friction stir welding over and through the plug. For repairing a longitudinal void (30), the method includes machining the void area to provide a trough (34) that subsumes the void, fabricating filler metal into a strip form (36) to be fitted into the trough, positioning the strip in the trough, and rewelding the void area by traversing a friction stir welding tool longitudinally through the strip. The method is also applicable for repairing welds made by a fusing welding process or voids in aluminum alloy workpieces themselves.

Rosen, Charles D.↗

Control of Structure in Conventional Friction Stir Welds through a Kinematic Theory of Metal Flow

In friction stir welding (FSW), a rotating pin is translated along a weld seam so as to stir the sides of the seam together. Metal is prevented from flowing up the pin, which would result in plowing/cutting instead of welding, by a shoulder on the pin. In conventional FSW, the weld metal rests on an "anvil", which supports the heavy "plunge" load on the tool. In this study, both embedded tungsten wires along and copper plating on the faying surfaces were used to trace the flow of AA2219 weld metal around the C-FSW tool. The effect of tool rotational speed, travel speed, plunge load, and pin thread pitch on the resulting weld metal flow was evaluated. Plan, longitudinal, and transverse section x-ray radiographs were examined to trace the metal flow paths. The results are interpreted in terms of a kinematic theory of metal flow in FSW.

Rubisoff, H.A.↗

Probabilistic Estimation of Critical Flaw Sizes in the Primary Structure Welds of the Ares I-X Launch Vehicle

The primary structure of the Ares I-X Upper Stage Simulator (USS) launch vehicle is constructed of welded mild steel plates. There is some concern over the possibility of structural failure due to welding flaws. It was considered critical to quantify the impact of uncertainties in residual stress, material porosity, applied loads, and material and crack growth properties on the reliability of the welds during its pre-flight and flight. A criterion--an existing maximum size crack at the weld toe must be smaller than the maximum allowable flaw size--was established to estimate the reliability of the welds. A spectrum of maximum allowable flaw sizes was developed for different possible combinations of all of the above listed variables by performing probabilistic crack growth analyses using the ANSYS finite element analysis code in conjunction with the NASGRO crack growth code. Two alternative methods were used to account for residual stresses: (1) The mean residual stress was assumed to be 41 ksi and a limit was set on the net section flow stress during crack propagation. The critical flaw size was determined by parametrically increasing the initial flaw size and detecting if this limit was exceeded during four complete flight cycles, and (2) The mean residual stress was assumed to be 49.6 ksi (the parent material s yield strength) and the net section flow stress limit was ignored. The critical flaw size was determined by parametrically increasing the initial flaw size and detecting if catastrophic crack growth occurred during four complete flight cycles. Both surface-crack models and through-crack models were utilized to characterize cracks in the weld toe.

Pai, Shantaram S.↗

Advanced Welding Concepts

Four advanced welding techniques and their use in NASA are briefly reviewed in this poster presentation. The welding techniques reviewed are: Solid State Welding, Friction Stir Welding (FSW), Thermal Stir Welding (TSW) and Ultrasonic Stir Welding.

Ding, Robert J.↗

Laser Peening Effects on Friction Stir Welding

Friction Stir Welding (FSW) is a welding technique that uses frictional heating combined with forging pressure to produce high strength bonds. It is attractive for aerospace applications. Although residual stresses in FSW are generally lower when compared to conventional fusion welds, recent work has shown that significant tensile residual stresses can be present in the weld after fabrication. Therefore, laser shock peening was investigated as a means of moderating the tensile residual stresses produced during welding. This slide presentation reviews the effect of Laser Peening on the weld, in tensile strength, strain, surface roughness, microhardness, surface wear/friction, and fatigue crack growth rates. The study concluded that the laser peening process can result in considerable improvement to crack initiaion, propagation and mechanical properties in FSW.

Hatamleh, Omar↗

Microhardness and Strain Field Characterization of Self-Reacting Friction Stir and Plug Welds of Dissimilar Aluminum Alloys

Friction stir welding (FSW) is a solid state welding process with potential advantages for aerospace and automotive industries dealing with light alloys. Self-reacting friction stir welding (SR-FSW) is one variation of the FSW process being developed at the National Aeronautics and Space Administration (NASA) for use in the fabrication of propellant tanks. Friction plug welding is used to seal the exit hole that remains in a circumferential SR-FSW. This work reports on material properties and strain patterns developed in a SR-FSW with a friction plug weld. Specifically, this study examines the behavior of a SR-FSW formed between an AA 2014-T6 plate on the advancing side and an AA 2219-T87 plate on the retreating side and a SR-FSW (AA 2014-T6 to AA 2219-T87) with a 2219-T87 plug weld. This study presents the results of a characterization of the micro-hardness, joint strength, and strain field characterization of SR-FSW and FPW joints tested at room temperature and cryogenic temperatures.

Horton, Karla Renee↗

Controlling Force and Depth in Friction Stir Welding

Feedback control of the penetration force applied to a pin tool in friction stir welding has been found to be a robust and reliable means for controlling the depth of penetration of the tool. This discovery has made it possible to simplify depth control and to weld with greater repeatability, even on workpieces with long weld joints. Prior to this discovery, depths of penetration in friction stir welding were controlled by hard-tooled roller assemblies or by depth actuators controlled by feedback from such external sensors as linear variable-differential transformers or laser-based devices. These means of control are limited: A hard-tooled roller assembly confines a pin tool to a preset depth that cannot be changed easily during the welding process. A measurement by an external sensor is only an indirect indicative of the depth of penetration, and computations to correlate such a measurement with a depth of penetration are vulnerable to error. The present force-feedback approach exploits the proportionality between the depth and the force of penetration Unlike a depth measurement taken by an external sensor, a force measurement can be direct because it can be taken by a sensor coupled directly to the pin tool. The reading can be processed through a modern electronic servo control system to control an actuator to keep the applied penetration force at the desired level. In comparison with the older depth-control methods described above, this method offers greater sensitivity to plasticizing of the workpiece metal and is less sensitive to process noise, resulting in a more consistent process. In an experiment, a tapered panel was friction stir welded while controlling the force of penetration according to this method. The figure is a plot of measurements taken during the experiment, showing that force was controlled with a variation of 200 lb (890 N), resulting in control of the depth of penetration with a variation of 0.004 in. (0.1 mm).

Adams, Glynn↗

Ultrasonic Stir Welding

NASA Marshall Space Flight Center (MSFC) developed Ultrasonic Stir Welding (USW) to join large pieces of very high-strength metals such as titanium and Inconel. USW, a solid-state weld process, improves current thermal stir welding processes by adding high-power ultrasonic (HPU) energy at 20 kHz frequency. The addition of ultrasonic energy significantly reduces axial, frictional, and shear forces; increases travel rates; and reduces wear on the stir rod, which results in extended stir rod life. The USW process decouples the heating, stirring, and forging elements found in the friction stir welding process allowing for independent control of each process element and, ultimately, greater process control and repeatability. Because of the independent control of USW process elements, closed-loop temperature control can be integrated into the system so that a constant weld nugget temperature can be maintained during welding.

Nabors, Sammy↗

Finite Element Thermal Model for Ultrasonic Welding of Thermoplastic Composites

Ultrasonic welding, UW, is a fast and energy-efficient technique for joining thermoplastic composites. It involves the use of high-frequency mechanical vibrations and a static welding force to melt and join adherends. Ultrasonic welding is an enabling technology to reduce the cost and complexity of in-space construction because lightweight thermoplastic composite components can be packaged compactly for launch and then efficiently assembled using supervised autonomous robotic technologies on site. However, the temperatures in space present challenges to UW, and it is critical that the efficacy of process parameters selected for manufacturing in space is understood prior to launch. To this end, a three-dimensional finite element model is presented in this technical presentation. The model incorporates equations for effects of viscoelastic heating and heat transfer on the welding process. The proposed model is applied to predict the temperature distribution in single lap shear, SLS, samples composed of AS4/PEEK (TC1200) composite that were welded using a terrestrial machine as part of a comprehensive weldability study. Thermocouple and infrared spot sensor data from the SLS samples provide empirical temperature measurements for calibration and validation of the UW thermal model. Calibration and validation of the model is an important step given the significant uncertainties in material properties such as the loss modulus and necessary assumptions in the physics implementations which allow the model to converge in an acceptable amount of time. The validated thermal model can be used to simulate the process for the space environment. Future validation sample testing is planned in a vacuum chamber. The result will be a model capable of guiding process parameter selection to ensure acceptable weld bonds when manufacturing in space.

Josh Fody↗

Modeling Study of Hatch Spacing’s Effect on Grain Morphology in Repairing Damaged Metal Parts with Welding and Hatch Spacing’s Potential Use in Lunar Exploration

The welding process is a potential way of repairing a damaged metal component, especially cavity damage caused by a harsh environment like the lunar environment, which is characterized by large temperature differences and reduced gravity. The adjustment of welding parameter (e.g., hatch spacing) can improve production efficiency in the repair process. Seen from the microstructural level, hatch spacing sensitivity affects the metallic grain evolution and morphology in the welding process, which can further influence a repaired part’s mechanical properties; however, the study of hatch spacing’s effect on microstructure is challenging. Traditional experimental procedures are costly and time-consuming, and any change in hatch spacing value needs roll-back of experimental procedure. A modeling study can address the above challenges in experimental observation. In this research, a modeling approach based on the Kinetic Monte Carlo (KMC) Potts theory was used to simulate grain evolution and morphology with three hatch spacings. Through quantifying and analyzing the predicted grain morphologies, the effect of hatch spacing on microstructure in a welding-fabricated part was investigated. The predicted grain morphologies were validated with an EBSD image of welding microstructure, which has been published before. The primary grain morphologies were columnar grains with a small amount of fine equiaxed grains formed in the scanning path centerline. When increasing the hatch spacing, the columnar grains become larger and more lengthy, while the effect of hatch spacing on the equiaxed grains is not obvious.

Welding for repairing↗

Welding of high chromium steels

A brief description is given of different groups of high chromium steels (rustless iron and stainless steels) according to their composition and more generally accepted names. The welding procedure for a given group will be much the same regardless of the slight variations in chemical composition which may exist within a certain group. Information is given for the tensile properties (yield point and ultimate strength) of metal sheets and welds before and after annealing on coupons one and one-half inches wide. Since welds in rustless iron containing 16 to 18 percent chromium and 7 to 12 percent nickel show the best combination of strength and ductility in the 'as welded' or annealed condition, it is considered the best alloy to use for welded construction.

IRON - STAINLESS↗

Electron Beam Welding of Additively Manufactured Niobium Alloy Heat Pipes

Additively manufactured refractory alloy-liquid metal heat pipes are being developed and tested for thermal management systems within nuclear propulsion and power applications. This study investigated electron beam (EB) welded joints on a laser powder bed fusion printed niobium alloy (C-103) and the impact of multiple joined heat pipe sections on working fluid flow and container leak-tightness. Results showed that EB welded joints connecting multiple heat pipe sections do not impact working fluid wicking behavior and the printed C-103 material and the EB welds joining the tubular sections created a leak-tight container. Interestingly, CT data showed an order of magnitude greater number and volume of porosity indications in the ground mating surface weld compared to the as-printed mating surface weld. The work concluded that AM is a viable manufacturing process for niobium alloy heat pipes and provided valuable insights for future AM heat pipe research and development.

Electron beam welding↗

Portable machine welding head automatically controls arc

Portable weld tool makes weld repairs out-of-station and on the side opposite the original weld. It provides full automatic control of the arc voltage, current, wire feed, and electrode travel speed in all welding attitudes. The device is readily adaptable to commercially available straight polarity dc weld packs.

Oleksiak, C. E.↗

Study made to establish parameters and limitations of explosive welding

It is theorized that metal jetting must be present for welding to occur, therefore an explosive weld interface may indicate the relation between the metal jet velocity and shock wave velocity in welding. Parameters for effecting explosive welding in patches of 3 or 4 inches in diameter were established, and found applicable to explosive welding of patches of various sizes.

Polhemus, F. C.↗

Dual wire weld feed proportioner

Dual feed mechanism enables proportioning of two different weld feed wires during automated TIG welding to produce a weld alloy deposit of the desired composition. The wires are fed into the weld simultaneously. The relative feed rates of the wires and the wire diameters determine the weld deposit composition.

Nugent, R. E.↗

Automatic, nondestructive test monitors in-process weld quality

Instrument automatically and nondestructively monitors the quality of welds produced in microresistance welding. It measures the infrared energy generated in the weld as the weld is made and compares this energy with maximum and minimum limits of infrared energy values previously correlated with acceptable weld-strength tolerances.

Deal, F. C.↗