Search NASA⌕ Search

SEARCH · Search NASA

Results for “polymer degradation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 289 records · Page 16

Hydration of a Side-Chain-Free n-Type Semiconducting Ladder Polymer Driven by Electrochemical Doping

Here, we study the organic electrochemical transistors (OECTs) performance of the ladder polymer, poly(benzimidazobenzophenanthroline) (BBL) in an attempt to better understand how an apparently hydrophobic side-chain-free polymer is able to operate as an OECT with favorable redox kinetics in an aqueous environment. We examine two BBLs of different molecular masses from different sources. Both BBLs show significant film swelling during the initial reduction step. By combining electrochemical quartz crystal microbalance (eQCM) gravimetry, in-operando atomic force microscopy (AFM), and both ex-situ and in-operando grazing incidence wide-angle x-ray scattering (GIWAXS), we provide a detailed structural picture of the electrochemical charge injection process in BBL in the absence of any hydrophilic side-chains. Compared with ex-situ measurements, inoperando GIWAXS shows both more swelling upon electrochemical doping than has previously been recognized, and less contraction upon dedoping. The data show that BBL films undergo an irreversible hydration driven by the initial electrochemical doping cycle with significant water retention and lamellar expansion that persists across subsequent oxidation/reduction cycles. This swelling creates a hydrophilic environment that facilitates the subsequent fast hydrated ion transport in the absence of the hydrophilic side-chains used in many other polymer systems. Due to its rigid ladder backbone and absence of hydrophilic side-chains, the primary BBL water uptake does not significantly degrade the crystalline order, and the original dehydrated, unswelled state can be recovered after drying. The combination of doping induced hydrophilicity and robust crystalline order leads to efficient ionic transport and good stability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tuning Film Stresses for Open-Air Processing of Stable Metal Halide Perovskites

Challenges to upscaling metal halide perovskites (MHPs) include mechanical film stresses that accelerate degradation, dominate at the module scale, and can lead to delamination or fracture. In this work, we demonstrate open-air blade coating of single-step coated perovskite as a scalable method to control residual film stress after processing and introduce beneficial compression in the thin film with the use of polymer additives such as gellan gum and corn starch. The optoelectronic properties of MHP films with compression are improved with higher photoluminescence yields. MHP film stability is significantly improved under compression, under humidity, heat, and thermal cycling. By measuring the evolution of film stresses, we demonstrate for the first time that stress relaxation occurs in MHP films with tensile stress that correlates with film degradation. Finally, this discovery of a new mechanism underpinning MHP degradation shows that film stress can be used as a parameter to screen MHP devices and modules for quality control before deployment as a design for reliability criterion.

14 SOLAR ENERGY↗

Carbon Fiber Reinforced Epoxy Vitrimer: Robust Mechanical Performance and Facile Hydrothermal Decomposition in Pure Water

Conventional carbon fiber reinforced thermosetting polymers (CFRPs) are neither recyclable nor repairable due to their crosslinked network. The rapid growing CFRP market raises a serious concern of the waste management. In this work, a viable method to develop a readily recyclable CFRP based on epoxy vitrimer is introduced. First, a self-catalytic epoxy prepolymer with built-in hydroxy and tertiary amine groups is designed, which upon reaction with an anhydride formed a catalyst-free epoxy vitrimer. The epoxy prepolymer is synthesized from a diamine and an excess of bisphenol A epoxy resin. The hydroxyls and tertiary amines of the epoxy prepolymer efficiently catalyze both curing and the dynamic transesterification of the crosslinked polymer without the need of a catalyst. Then, the epoxy vitrimer is used as the matrix resin to prepare CFRP. The resulting CFRP exhibited a tensile strength as high as 356 MPa. More interestingly, the matrix of the CFRP is efficiently degraded in pure water at above 160 °C. This is because the built-in tertiary amines catalyze the hydrolysis of the ester bonds of the crosslinked network. The simple method developed in this work provides a framework for the development of recyclable CFRP.

Liu, Tuan↗

LiNi0.8Mn0.1Co0.1O2 Thin Films Prepared by Polymer-Assisted Deposition for the Study of Cathode-Electrolyte Interphases in Lithium-Ion Batteries

High-nickel layered oxide cathodes such as LiNi0.8Mn0.1Co0.1O2 (NMC811) are critical for next-generation lithium-ion batteries (LIBs) due to their superior energy density and reduced reliance on cobalt. However, many Ni-rich cathodes suffer from rapid capacity fade and structural instability originating from complex interfacial reactions at the cathode-electrolyte interface. Traditional composite electrodes exhibit degradation mechanisms that are challenging to quantitatively understand due to additives, including binders and carbon black. In this study, we demonstrate a new synthesis approach for binder- and additive-free NMC811 thin films using polymer-assisted deposition (PAD). PAD-NMC811 are model thin-film cathodes for investigating interfacial phenomena that can be obscured in composite cathodes. Structural and chemical characterization by X-ray diffraction, soft X-ray absorption spectroscopy, and atomic force microscopy show that PAD-NMC811 films possess high phase purity, crystallinity, chemical homogeneity, and morphological uniformity. Electrochemical analyses using cyclic voltammetry and galvanostatic cycling revealed electrochemical behavior consistent with that of composite electrodes, along with a moderate capacity fade indicative of cathode-electrolyte interphase (CEI) formation. Our findings illustrate the effectiveness of PAD synthesis of thin films tailored for detailed mechanistic studies, which offer critical insights into CEI evolution and cathode degradation pathways.

25 ENERGY STORAGE↗

La- and Mn-doped cobalt spinel oxygen evolution catalyst for proton exchange membrane electrolysis

Discovery of earth-abundant electrocatalysts to replace iridium for the oxygen evolution reaction (OER) in a proton exchange membrane water electrolyzer (PEMWE) represents a critical step in reducing the cost for green hydrogen production. Here we report a nanofibrous cobalt spinel catalyst codoped with lanthanum (La) and manganese (Mn) prepared from a zeolitic imidazolate framework embedded in electrospun polymer fiber. The catalyst demonstrated a low overpotential of 353 millivolts at 10 milliamperes per square centimeter and a low degradation for OER over 360 hours in acidic electrolyte. A PEMWE containing this catalyst at the anode demonstrated a current density of 2000 milliamperes per square centimeter at 2.47 volts (Nafion 115 membrane) or 4000 milliamperes per square centimeter at 3.00 volts (Nafion 212 membrane) and low degradation in an accelerated stress test.

36 MATERIALS SCIENCE↗

Metal-olsalazine coordination polymers for medical applications

Olsalazine (H 4 olz), a prodrug of the anti-inflammatory 5-aminosalicylic acid, is used as a ligand to synthesize a suite of M(H 2 olz) and M 2 (olz) materials, where M is a dication (e.g. Mg, Ca, Sr, Fe, Co, Ni, Cu, Zn). A family of metal olsalazine coordination polymers, coordination solids, and metal organic frameworks are described, which include 1-, 2-, and 3-dimensional structures. The materials resist degradation at acidic pH and release olsalazine preferentially at neutral pH. The mesoporous M 2 (olz) frameworks exhibit high surface areas with hexagonal pore apertures that are approximately 27 Å in diameter and contain coordinatively unsaturated metal sites. Biologically active molecules containing a Lewis-basic functional group can be grafted directly to the open metal sites of the frameworks. Dissolution of the frameworks under physiological conditions releases olsalazine (H 4 olz) and the grafted molecules so that multiple therapeutic components can be delivered together at different rates.

Levine, Dana A.↗

Conservation of model degraded pine wood with selected organosilicons studied by XFM and nanoindentation

Previous research found that some organosilicon treatments proved effective in stabilizing waterlogged wood dimensions during drying. The present research aimed to determine the mechanism of wood stabilization by these chemicals to understand their mode of action. Here, the study used chemically (ChP) and biologically degraded (BP) model Scots pine wood treated with Methyltrimethoxysilane (MTMS), (3-Mercaptopropyl) trimethoxysilane (MPTMS), or 1,3-Bis(diethylamino)-3-propoxypropanol)-1,1,3,3-tetramethyldisiloxane (DEAPTMDS). Synchrotron-based X-ray fluorescence microscopy (XFM) was used to investigate the penetration of organosilicons into the wood cellular structure and cell walls, and nanoindentation was used to study the mechanical properties of the treated wood cell walls. All treatments resulted in high volumetric anti-shrink efficiency (ASE V ) values of 74-82%, except for MTMS-treated ChP with an ASE V of 52%. The multiscale XFM results revealed that all applied organosilicons penetrated throughout the whole wooden blocks and deposited in both cell lumina and cell walls. The retention of all applied organosilicons was highest in BP wood, and so was the dimensional stabilization effect. MTMS-treated ChP had the lowest measured cell wall infiltration, which likely contributed to its lower ASE v . DEAPTMDS treatments plasticized the cell walls and resulted in lowered nanoindentation elastic modulus (E s NI ) and hardness (H) for all types of wood. MTMS and MPTMS had modest effects on cell wall mechanical properties, and the effect depended on the type of wood. The final effect of organosilicon treatment on the dimensional wood stabilization and mechanical properties of wood cell walls depended not only on the type of the applied organosilicon but also the type of wood degradation. This means that the treatment cannot be considered universal, and specific approaches are needed for the conservation of individual wooden objects. Although some mechanisms are now better understood, such as the need for organosilicons to infiltrate the cell walls and the plasticizing effect of DEAPTMDS, other aspects will benefit from a more detailed analysis of the molecular interactions between organosilicons and wood polymers.

59 BASIC BIOLOGICAL SCIENCES↗

Foundry-compatible high-resolution patterning of vertically phase-separated semiconducting films for ultraflexible organic electronics

Solution processability of polymer semiconductors becomes an unfavorable factor during the fabrication of pixelated films since the underlying layer is vulnerable to subsequent solvent exposure. A foundry-compatible patterning process must meet requirements including high-throughput and high-resolution patternability, broad generality, ambient processability, environmentally benign solvents, and, minimal device performance degradation. However, known methodologies can only meet very few of these requirements. Here, a facile photolithographic approach is demonstrated for foundry-compatible high-resolution patterning of known p- and n-type semiconducting polymers. This process involves crosslinking a vertically phase-separated blend of the semiconducting polymer and a UV photocurable additive, and enables ambient processable photopatterning at resolutions as high as 0.5 μm in only three steps with environmentally benign solvents. The patterned semiconducting films can be integrated into thin-film transistors having excellent transport characteristics, low off-currents, and high thermal (up to 175 °C) and chemical (24 h immersion in chloroform) stability. Moreover, these patterned organic structures can also be integrated on 1.5 μm-thick parylene substrates to yield highly flexible (1 mm radius) and mechanically robust (5,000 bending cycles) thin-film transistors.

36 MATERIALS SCIENCE↗

Effect of Remnant Carbon and Etching of Particles on Pyrolysis Bonded Silicon Carbide (PBSC)

Silicon carbide (SiC) formed through pyrolysis of preceramic polymers loaded with SiC particles has gained significant attention for applications such as coatings, composite matrix modifications, and most importantly additive manufacturing. This work presents combined synchrotron XRD, Raman spectroscopy, scanning electron microscopy, nano-indentation, and Vickers indentation of pyrolysis bonded SiC to shed light on the changes of composition and mechanical properties of these materials. Characterization was performed on samples that were heat treated ranging from the synthesis 850 °C up to 1500 °C. Pre-treatments of the powders prior to pellet synthesis, such as heat treatment and etching using a hydrofluoric acid (HF), were investigated. It is shown that the degradation of mechanical properties when exposed to higher temperatures is due to the burnout of amorphous carbon clusters remnant of the pyrolysis process of the preceramic polymer. Furthermore, prior HF etching and removal of the native oxide layer of the powders showed improved density and hardness values in the final pellets. The average Vickers hardness of the control samples were 4.59 GPa and later 3.74 GPa when exposed to 1500 °C, while the samples synthesized using powders that were etched with HF had an average hardness value of 9.37 GPa and later 6.86 GPa when exposed to 1500 °C.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Characterization of the degradation of gamma-irradiated elastomers using Raman spectroscopy

This report presents key findings from Raman spectroscopic analysis of gamma-irradiated rubber samples extracted from a laminated lead-damped rubber (LDR) seismic isolation device. The samples were exposed to gamma radiation from a 60Co source in a Foss Therapy Services gamma irradiator, reaching absorbed doses up to 1600 kGy. A distinct threshold near 400 kGy was identified, beyond which significant spectral changes were observed. Two Raman peaks - at approximately 425 cm-1 and 2440 cm-1 - were tracked as a function of dose using Gaussian fitting. The 425 cm-1 peak, attributed to sulfur–sulfur (S–S) bond stretching (resulting from vulcanization of the rubber), exhibited a dose-dependent upshift, indicating radiation-induced crosslinking within the sulfur-based polymer network. Conversely, the 2440 cm-1 peak, likely associated with vibrational modes of additives or impurities, showed a downward shift with increasing dose, suggesting chain scission and degradation of non-rubber constituents. These results provide first-of-a-kind insights into the microstructural evolution of elastomers under high-dose gamma irradiation and establish a preliminary dose threshold for significant degradation. Future work will incorporate multi-modal characterization—including Fourier Transform Infrared (FTIR) spectroscopy, scanning electrom microscopy (SEM) of the rubber surface morphology, thermogravimetric analysis (TGA) to determine changes in thermal stability, and mechanical testing—to correlate molecular-level changes with macroscopic performance of these elastomers as damping media in seismic isolation devices. These findings are expected to provide regulatory guidance and design criteria for qualifying low-damping rubber seismic isolators in advanced nuclear reactor applications.

36 - MATERIALS SCIENCE↗

Revealing in-plane movement of platinum in polymer electrolyte fuel cells after heavy-duty vehicle lifetime

Fuel cell heavy-duty vehicles (HDVs) require increased durability of oxygen-reduction-reaction electrocatalysts, making knowledge of realistic degradation mechanisms critical. Here identical-location micro-X-ray fluorescence spectroscopy was performed on membrane electrode assemblies. The results exposed heavy in-plane movement of electrocatalyst after HDV lifetime, suggesting that electrochemical Ostwald ripening may not be a local effect. Development of local loading hotspots and preferential movement of electrocatalyst away from cathode catalyst layer cracks was observed. The heterogeneous degradation exhibited by a modified cathode gas diffusion layer membrane electrode assembly after HDV lifetime was successfully quantified by the identical-location approach. Further synchrotron micro-X-ray diffraction and micro-X-ray fluorescence experiments were performed to obtain the currently unknown correlation between electrocatalyst nanoparticle size increase and loading change. A direct correlation was discovered which developed only after HDV lifetime. Finally, the work provides a route to engineer immediate system-level mitigation strategies and to develop structured cathode catalyst layers with durable electrocatalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Hierarchically Templated Synthesis of 3D‐Printed Crosslinked Cyclodextrins for Lycopene Harvesting

Abstract Plants produce a wide range of bioactive phytochemicals, such as antioxidants and vitamins, which play crucial roles in aging prevention, inflammation reduction, and reducing the risk of cancer. Selectively harvesting these phytochemicals, such as lycopene, from tomatoes through the adsorption method is cost‐effective and energy efficient. In this work, a templated synthesis of 3D‐printed crosslinked cyclodextrin polymers featuring nanotubular structures for highly selective lycopene harvesting is reported. Polypseudorotaxanes formed by triethoxysilane‐based telechelic polyethylene glycols and α‐cyclodextrins (α‐CDs) are designed as the template to (1) synthetically access urethane‐based nanotubular structures at the molecular level, and (2) construct 3D‐printed architectures with designed macroscale voids. The polypseudorotaxane hydrogels showed good rheological properties for direct ink writing, and the 3D‐printed hydrogels were converted to the desired α‐CD polymer network through a three‐step postprinting transformation. The obtained urethane‐crosslinked α‐CD monoliths possess nanotubular structures and 3D‐printed voids. They selectively adsorb lycopene from raw tomato juice, protecting lycopene from photo‐ or thermo‐degradations. This work highlights the hierarchically templated synthesis approach in developing functional 3D‐printing materials by connecting the bottom‐up molecular assembly and synthesis with the top‐down 3D architecture control and fabrication.

Chemistry↗

Manganese‐Based Spinel Cathodes: A Promising Frontier for Solid‐State Lithium‐Ion Batteries

Recently, all-solid-state lithium-ion batteries (ASSLIBs), which exhibit improved safety and enhanced energy density compared to conventional commercialized lithium-ion batteries (LIBs), thereby have garnered extensive research interest. Among the promising cathode candidates, Mn-based spinel cathodes LiMn 2 O 4 (LMO) and LiNi 0.5 Mn 1.5 O 4 (LNMO), with the unique characteristics of low cost, structural stability, and 3D Li-ion diffusion channels, have demonstrated excellent performance in LIBs and presented great potential in ASSLIBs applications. However, several challenges, including structural degradations, poor interfacial contact, large interfacial resistance, and Mn-dissolution/diffusion during the electrochemical cycling, hinder their practical applications and commercialization in the ASSLIBs. Particularly, the high-voltage LNMO cathodes suffer from the challenge of electrochemical incompatibility with most of the solid-state electrolytes (SSEs). Herein, the spinel structure, the electrochemical behavior, and the structural degradation of the LMO/LNMO are explored. The characteristics and recent progress of the mitigating strategies to the challenges of various SSEs, including polymer-, oxide-, composite-, sulfide-, halide-, and LiPON-based SSEs, are introduced when paired with LMO/LNMO. Finally, the directions for future research to advance Mn-based spinel cathodes and fulfill the requirements of the next-generation ASSLIBs are also discussed.

Dou, Yu [Concordia University, Montreal, QC (Canad↗

Elucidation of odd-chain dicarboxylate metabolism in Acinetobacter baylyi and application to polyethylene upcycling

Polyethylene (PE) is a versatile polymer, but its end-of-life management is challenging due to its recalcitrant structure. We present a promising approach combining chemical degradation and bio-upcycling to convert postconsumer PE waste into a value-added bioproduct. Specifically, PE was degraded into acetic acid and C 4 –C 7 dicarboxylic acids by nitric acid. We then elucidated the catabolic pathways for glutarate (C 5 ) and pimelate (C 7 ) in the nonmodel bacterium Acinetobacter baylyi ADP1 through RNA sequencing, phenotyping, and enzymatic assays. Whole-genome sequencing of evolved isolates also identified a crucial IclR family transcriptional regulator, DcaS, which acts as a repressor of dicarboxylate metabolism. The reverse-engineered strain exhibited enhanced substrate utilization compared to the wild-type strain. Using rational metabolic engineering, the PE deconstruction products were bioconverted into the valuable chemical lycopene, highlighting the potential of this microbial chassis to produce value-added bioproducts from postconsumer PE waste, thus promoting a circular economy for plastics.

metabolic engineering↗

Role of Amorphous Chains in Nanoplastic Formation from Semicrystalline Polymers

Semicrystalline polymers, e.g., polyethylene terephthalate (PET), release micro- (100 nm to 1 mm) and nanoplastics (up to 100 nm) [MNPL] when they are degraded under quiescent conditions. However, the exact molecular mechanisms leading to material fragmentation into MNPL are unknown. Here, we monitor the evolution of chain molecular weight and the MNPL production kinetics during hydrolysis of PET pellets. We find that only ~0.6% of the amorphous phase ester bonds are hydrolyzed at the onset of MNPL release. Then, by combining a random scission model with measured amorphous spacings, we estimate that only ~15% of the stress transmitters in the amorphous phase, namely, bridges and entangled loops, have failed by this point. Thus, spontaneous fragmentation of the semicrystalline nanostructure occurs despite significant intercrystalline connectivity. We resolve this apparent contradiction by proposing that fragmentation can only occur when progressive tie-chain scission causes the material to undergo the ductile/brittle transition. Mechanistically, we speculate that the internal stresses responsible for material fragmentation are caused by processing (i.e., residual stresses) and/or sample densification induced by chemi-crystallization. We discuss additional factors that may affect our analysis and thus require further investigation, such as skin-core effects, preferential degradation of stress transmitters and/or recrystallization processes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Complementary roles for mechanical and solvent-based recycling in low-carbon, circular polypropylene

Plastic recycling presents a vexing challenge. Mechanical recycling offers substantial greenhouse gas emissions savings relative to virgin plastic production but suffers from degraded aesthetic and mechanical properties. Polypropylene, one of the most widely used and lowest-cost plastics, features methyl pendants along the polymer backbone, rendering it particularly susceptible to declining properties, performance, and aesthetics across a succession of mechanical recycles. Advanced processes, such as solvent-assisted recycling, promise near-virgin quality outputs at a greater energy and emissions footprint. Mechanical and advanced recycling are often presented as competing options, but real-world plastic waste streams are likely to require preprocessing regardless of whether they are routed to an advanced process. This study quantifies the life-cycle greenhouse gas implications of multiple recycling strategies and proposes a system in which mechanical and solvent-assisted recycling can be leveraged together to boost recycling rates and satisfy demand for a wider range of product applications. Polypropylene can be recovered from mixed-plastic bales produced at material recovery facilities and processed through mechanical recycling, with a varying fraction sent for further upgrading via solvent-assisted recycling to produce material approved for food packaging and other higher-quality applications. The resulting mechanically recycled rigid polypropylene reduces life-cycle greenhouse gas emissions by 80% relative to the same quantity of virgin material, while the upgraded higher-quality material achieves GHG savings of 30%.

36 MATERIALS SCIENCE↗

Electrochemical mechanisms of leakage‐current in photovoltaic modules

Abstract This paper analyzes the mechanisms and pathways for leakage current flow observed in Si photovoltaic modules subjected to high temperature and humidity and a large voltage bias with respect to ground. The current inside of the frame is in the form of electron motion, but in the glass and polymer, it is in at least a large part attributable to the movement of ions. When the mode of current flow changes from electronic to ionic conduction, electrochemical reactions will take place at the interface. This can include reactions that produce volatile chemical species like H 2 , CO x , and O 2 , along with ionic species such as OH − and H 3 O + . Here, we see evidence of the importance of different charge carriers with different diffusion rates and the influence of electrochemical processes involved. The application of negative voltage to the cell circuit affects the resistivity of glass producing surfaces with poor conductivity but with some increases in the electrochemical potential producing complicated interactions that are important when the voltage is changed. In the polymer, there is the development of a space charge region and a chemical gradient providing two oppositional forces to current flow, which when released create a complicated discharge process. Here, we give a basic understanding of the charge/discharge of PV cells highlighting how the specific mechanisms are important in understanding some of the degradation processes in PV modules. We find that there is evidence of multiple significant charge carrier species with different diffusion time scales. The glass/polymer interface forms a depleted region of higher resistance after prolonged exposure to current. Charge also builds up at the polymer to cell antireflective coating interface and mostly flows to the gridlines to experience electrochemical reactions. These complexities result in non‐linear behavior where the apparent resistivities of the different layers change during charge/discharging processes, making the modeling of the current flow extremely difficult.

14 SOLAR ENERGY↗