Optimization of Hydride Rim Formation in Unirradiated Zr-4 Cladding

The purpose of this work is to build on the results reported in the M2 milestone M2FT 13PN0805051, document number FCRD-USED-2013-000151 (Hanson, 2013). In that work, it was demonstrated that unirradiated samples of zircaloy-4 cladding could be pre-hydrided at temperatures below 400°C in pure hydrogen gas and that the growth of hydrides on the surface could be controlled by changing the surface condition of the samples and form a desired hydride rim on the outside diameter of the cladding. The work performed at Pacific Northwest National Laboratory since the issuing of the M2 milestone has focused its efforts to optimize the formation of a hydride rim on available zircaloy-4 cladding samples by controlling temperature variation and gas flow control during pre-hydriding treatments. Surface conditioning of the outside surface was also examined as a variable. The results of test indicate that much of the variability in the hydride thickness is due to temperature variation occurring in the furnaces as well as how hydrogen gas flows across the sample surface. Efforts to examine other alloys, gas concentrations, and different surface conditioning plan to be pursed in the next FY as more cladding samples become available.

Cladding↗

The Development of Expansion Plug Wedge Test for Clad Tubing Structure Mechanical Property Evaluation

To determine the tensile properties of irradiated fuel cladding in a hot cell, a simple test was developed at the Oak Ridge National Laboratory (ORNL) and is described fully in US Patent Application 20060070455, “Expanded plug method for developing circumferential mechanical properties of tubular materials.” This method is designed for testing fuel rod cladding ductility in a hot cell using an expandable plug to stretch a small ring of irradiated cladding material. The specimen strain is determined using the measured diametrical expansion of the ring. This method removes many complexities associated with specimen preparation and testing. The advantages are the simplicity of measuring the test component assembly in the hot cell and the direct measurement of the specimen’s strain. It was also found that cladding strength could be determined from the test results.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Industry Application Emergency Core Cooling System Cladding Acceptance Criteria Early Demonstration

The U. S. NRC is currently proposing rulemaking designated as “10 CFR 50.46c” to revise the loss-of-coolant-accident (LOCA)/emergency core cooling system (ECCS) acceptance criteria to include the effects of higher burnup on cladding performance as well as to address other technical issues. The NRC is also currently resolving the public comments with the final rule expected to be issued in April 2016. The impact of the final 50.46c rule on the industry may involve updating of fuel vendor LOCA evaluation models, NRC review and approval, and licensee submittal of new LOCA evaluations or re-analyses and associated technical specification revisions for NRC review and approval. The rule implementation process, both industry and NRC activities, is expected to take 4-6 years following the rule effective date. As motivated by the new rule, the need to use advanced cladding designs may be a result. A loss of operational margin may result due to the more restrictive cladding embrittlement criteria. Initial and future compliance with the rule may significantly increase vendor workload and licensee cost as a spectrum of fuel rod initial burnup states may need to be analyzed to demonstrate compliance. Consequently, there will be an increased focus on licensee decision making related to LOCA analysis to minimize cost and impact, and to manage margin. The proposed rule would apply to a light water reactor and to all cladding types.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Implementing Fuel Cladding Bonding and Assessing its Impact on Axial Gas Communication

Fuel rods irradiated in light-water reactors to burnup values above 45 MWd/kgU are subject to the formation of a chemical and mechanical bond between the fuel and cladding upon gap closure. The formation of the bond subsequently inhibits the ability of fission gases released from the fuel to flow freely to the plenum of the rod. The flowing of gases within fuel rods is referred to as axial gas communication. During transients, such as loss of coolant accidents, the bond may influence cladding deformation prior to breaking. Upon bond breakage, gases are able to more freely communicate to the lower pressure regions of the rod. The impact of bonding on gas communication and the ballooning behavior of the cladding during a loss of coolant accident is of interest to the nuclear industry in support of burnup extension for the existing light-water reactor fleet. In this report, a model to capture the effects of fuel cladding bonding in the BISON fuel performance code is presented. The theory of the model along with implementation testing is provided. A summary of a previously developed axial gas communication is given to set the stage for how the two models may be coupled together. A full-length pressurized-water reactor fuel rod demonstration is highlighted to evaluate the impact of including bonding on axial gas communication calculations using a preliminary coupling methodology. An overview of the next steps regarding the modeling of bonding, axial gas communication, and a more tightly coupled framework is also provided.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Unraveling the Mechanics: Computational Modeling of Residual Stresses in U10Mo Fuel with Aluminum Cladding

LEU (Low Enriched Uranium) plate-type fuel elements consist of a high-density, low-enrichment U–Mo alloy-based fuel foil encapsulated in an aluminum cladding and is fabricated through the Hot Isostatic Pressing (HIP) technique. Understanding the mechanism of possible failure modes of nuclear fuel is critical to mitigate potential consequences. One of the major contributing factors in various failure modes is stress and it greatly affects the integrity under temperature, pressure, and irradiation. These stresses could originate from various sources, including manufacturing, and operation, and can lead to deformation, cracking, or even complete failure of fuel elements. This study focuses on the development of a computational model that accurately predicts the residual stresses generated in the U10Mo fuel during fabrication. It has been observed that cladding creep has a substantial impact on the residual stresses in the U10Mo fuel post the HIP fabrication process. Furthermore, during the HIP bonding process the fuel plate system is heated to a temperature of 560 oC and as a result, the aluminum cladding transitions from (Al 6061-T6 to -O). This presents a challenge in capturing the change in material properties accurately. Therefore, a temperature dependent creep model such as hyperbolic sine creep model is considered to estimate the creep properties of the Aluminum cladding. The proposed calibrated creep model accurately predicts the residual stresses in the U10Mo fuel foil and agrees well with the experiments.

42 ENGINEERING↗

Thermal creep model for CWSR zircaloy-4 cladding taking into account the annealing of the irradiation hardening

After irradiation and cooling in a pool, spent nuclear fuel assemblies are either transported for wet storage to a devoted site or loaded in casks for dry storage. During dry transportation or at the beginning of dry storage, the cladding is expected to be submitted to creep deformation under the hoop stress induced by the internal pressure of the fuel rod. The thermal creep is a potential mechanism that might lead to cladding failure. A new creep model was developed, based on a database of creep tests on as-received and irradiated cold-worked stress-relieved Zircaloy-4 cladding in a wide range of temperatures (310 degrees C to 470 degrees C) and hoop stress (80 to 260 MPa). Based on three laws-a flow law, a strain-hardening recovery law, and an annealing of irradiation hardening law this model allows the simulation of not only the transient creep and the steady-state creep, but also the early creep acceleration observed on irradiated samples tested in severe conditions, which was not taken into account in the previous models. The extrapolation of the creep model in the conditions of very long-term creep tests is reassuring, proving the robustness of the chosen formalism. The creep model has been assessed in progressively decreasing stress conditions, more representative of a transport. Set up to predict the cladding creep behavior under variable temperature and stress conditions, this model can easily be implemented into codes in order to simulate the thermomechanical behavior of spent fuel rods in various scenarios of postirradiation phases. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Fabrication of FeCrAl cladding for accident tolerant fuel

General Electric (GE) is working with the US Department of Energy (DOE) to develop a high performance nuclear fuel that will have enhanced tolerance to failure under severe accident conditions. The leading FeCrAl alloy candidate for the cladding is APMT, a powder metallurgy alloy developed by Kanthal/Sandvik for high temperature applications. Zirconium alloys have been used for cladding the fuel for over six decades. That is, zirconium alloys can be fabricated as several meters long tubes with an outside diameter of about 10 mm and a wall thickness in the order of 1 mm or less. The GE team is working to demonstrate that APMT can be fabricated as long thin walled tubes for the cladding application. A first production route for 10 x 0.5 mm APMT tubes was established showing that pilgering and drawing are viable processes to fabricate the APMT cladding. The mechanical properties of APMT were evaluated before and after the cold forming. Yield strength, tensile strength and hardness increased and elongation decreased due to cold forming, which was expected. No abnormality has been noted in the microstructures. The 3D image visualization of TIG welded APMT rodlet and the images of welding areas taken at different locations show no welding defects such as distortion, porosity or lack of penetration along/adjacent to the welded areas, confirming overall good welds and no opening or defects across the entire width of the tube thickness. Tests have shown no effect of welding on the hardness or mechanical strength in the area nearing the weld.

36 MATERIALS SCIENCE↗

Alloying effect of Nb and Sn on the Zirconium alloy fuel claddings behavior at high temperature oxidation in steam - 6.1 STP-2016-0072

As the material of fuel claddings for water cooled reactors most commonly used binary and multicomponent zirconium alloys Zr-Nb (E110,M5), Zr-Sn-Fe (Zircaloy-2,-4) and Zr-Nb-Sn-Fe (E635, Zirlo) are used, which improvement extends, in particular, by varying their composition by Nb, Sn and Fe. At the same time, the importance is given to ensuring the safe operation of the fuel rods not only in normal conditions but also in emergency situations such as LOCA. In this paper the researches results of the studies of influence of alloying elements Nb, Sn (and Fe) on corrosion resistance and embrittlement at high temperature steam oxidation of fuel claddings based on alloys types Zr-xNb (x=1.0/2.5) and Zr-xNb-ySn-zFe (x=0.6/2.4; y=0.24/1.1; z=0.18/0.34) made with using zirconium sponge are presented. High temperature steam oxidation tests were carried out at temperatures of 1000, 1100 and 1200 deg. C with continuous measurement of the weight gain during the experiment and subsequent cooling in steam with rate ∼ 20 deg. C/s. The studies of kinetics of high-temperature oxidation in steam, structural-phase state changes, alloying elements distribution, absorbed hydrogen content and residual ductility after rapid cooling of the oxidized specimens were made. The difference in the oxidation kinetics of the materials studied was revealed, it decreases with the oxidation temperature increase. At the same time, an increase of the Sn content in the alloy influences on specimens 'breakaway' oxidation intensification at 1000 deg. C. It is shown that the mechanical properties of fuel claddings oxidized under the same conditions depend on their alloying composition, the hydrogen fraction absorbed by the specimen and formed by the oxidation ZrO2, a-Zr(O) and 'ex-β' layers structure, which in turn varies depending on the alloy composition. The increase of Nb, Sn and Fe content in the zirconium alloy leads to decrease in residual ductility of fuel claddings after high temperature steam oxidation. According to obtained results the most resistant to high-temperature steam oxidation and embrittlement at temperatures of 1000-1200 deg. C among the materials studied is Zr-1Nb alloy. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

In-Pile testing of CrN, TiAIN, and AlCrN coatings on Zircaloy cladding in the Halden reactor - 2016-0011

CrN coating came out as superior and remained completely intact after the irradiation, as evidenced by SEM analysis. Based on these promising results, an in-pile experiment with coated Zircaloy claddings (containing fuel) was performed in the Halden reactor in PWR conditions in 2014. The experimental rig contained four Zircaloy-4-clad fuel rods-three coated (CrN, TiAlN, and AlCrN) and one uncoated. Due to a mechanical deformation of tubes for cooling water within the rig, the fuel rods were insufficiently cooled, resulting in a higher-than-normal cladding temperature. Nevertheless, an SEM examination showed that the CrN coating largely remained intact apart from several local spots where the coating had cracked or disappeared. Underneath the cracked coating, oxide formation was observed in the Zircaloy-4 cladding. The TiAlN and AlCrN coatings both disappeared after the irradiation. (authors)

36 MATERIALS SCIENCE↗

Chromium-Based Mitigation Coatings on SiC Materials for Fuel Cladding

SiC composites are undergoing assessment under the Advanced Fuels Campaign for Light Water Reactors (LWR) as an Accident Tolerant Fuel (ATF) cladding. As noted, the main concern has been the hydrothermal corrosion of SiC under all LWR chemistries, resulting in cladding oxidation and recession unacceptable for the duration of burn-up. Improvements in future fuel burn-up further increase recession mitigation requirements. Hermeticity of ceramic cladding may also be a concern in terms of quality control. Coatings are being investigated as a practical solution to address concerns regarding SiC cladding for both accident conditions and normal operations. SiC materials were coated by various technologies to produce Cr-based mitigation coatings as a corrosion barrier in LWR water chemistry. In all cases, deposition of Cr compounds requires that SiC behave as a cathode during processing, which requires surface electrical conductivity. Morphology and phase analysis of the coatings are still undergoing investigation, mainly for predicting differential swelling, thermal expansion and microcracking. Autoclave corrosion and in-pile irradiation in a PWR water loop will follow in mid-2016. (authors)

36 MATERIALS SCIENCE↗

Thermal Dehydration of Aluminum (Oxy)hydroxides on Fuel Cladding Material - 20200

The aluminum cladding of research-reactor fuel undergoes general corrosion with resulting formation of adherent aluminum (oxy)hydroxide films during in-reactor and post-discharge exposure to water under various conditions and temperatures. These (oxy)hydroxides contain chemically-bound water that poses challenges for extended dry storage due to the risk of thermal or radiolytic decomposition releasing free water and/or hydrogen and oxygen gases. This study comprised laboratory experiments of thermal drying behavior of aluminum (oxy)hydroxides to identify approaches for reducing bound water on fuel cladding prior to sealed dry storage. Effective drying strategies for adherent (oxy)hydroxides on fuel cladding will improve the safety of dry storage by mitigating potential avenues for additional corrosion and/or generation of flammable gases inside the storage canister. This work is part of a broader investigation to address knowledge gaps and technical data needs for dry storage of aluminum-clad spent nuclear fuel (ASNF), which included investigation of (oxy)hydroxide formation on aluminum alloy substrates immersed in water, characterization of service-grown films from ASNF, and radiolytic yield of hydrogen from (oxy)hydroxide powders and films. The current work comprises experimental thermal dehydration of aluminum trihydroxides (bayerite and gibbsite) characteristic of low-temperature (<80 deg. C) corrosion in water and aluminum oxyhydroxide (boehmite) characteristic of high temperature (>80 deg. C) corrosion in water. First, commercially produced (oxy)hydroxide powders (boehmite and gibbsite) were tested via thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC). The effort aimed to identify or confirm key temperature ranges/thresholds for the thermal decomposition reactions, as well as impacts of ramp rate and hold times, for drying of isolated, high-surface-area (oxy)hydroxides. The information gleaned from powder tests was used to guide subsequent drying tests on adherent (oxy)hydroxide films grown on aluminum alloy substrates. TGA was used to analyze small samples of the aluminum coupons with adherent (oxy)hydroxide films. Specimens were characterized both pre- and post-drying using X-ray diffraction (XRD) to determine the film composition and scanning electron microscopy (SEM) to determine its morphology. Drying of adherent (oxy)hydroxide films was anticipated to pose additional complications relative to drying of (oxy)hydroxide powders. Anticipated challenges include achieving sufficient drying of the (oxy)hydroxide at low-enough temperature to avoid melting or other undesirable phase changes in the aluminum substrate and overcoming transport limitations of water through the thickness of a dense film or through a tortuous pore structure to reach the outer surface of the film. Inn addition, dehydration of (oxy)hydroxides significantly changes the film density, which may lead to substantial alterations in the morphology, including potential cracking and spalling of the film. TGA/DSC tests of gibbsite powders resulted in successful conversion to boehmite or alumina, depending on the maximum temperature reached. At low ramp rates (≤5 deg. C/min), the conversion to boehmite occurred around 300 deg. C (210-340 deg. C). XRD confirmed that boehmite was the only phase detected after tests reaching 450 deg. C. The transition to alumina occurred around 510 deg. C (470-550 deg. C), with XRD detecting only alumina after tests reaching at least 600 deg. C. Boehmite powders dehydrated to alumina at about 400 deg. C (330-460 deg. C) for coarse (77-μm particle diameter) powder and about 490 deg. C (420-520 deg. C) for fine (0.7-μm particle diameter) powder. For all powders tested, the maximum percent mass loss after drying to high temperature slightly exceeded the theoretical mass loss for complete dehydration of the stoichiometric (oxy)hydroxide to alumina, which is likely attributable to physisorbed water in the powder. Drying of a thick (∼8.6 μm), predominantly bayerite adherent film displayed a dramatic change in film morphology, with the initially continuous trihydroxide film cracking into sections on the order of 50 μm square and partially delaminating. The outermost layer of the film completely faked of in some regions. The layer exposed under the spalled oxide also displayed prominent cracking, with spacing on the order of 10 μm, but this surface layer appeared to remain completely adhered to the aluminum substrate. TGA showed mass losses per unit surface area up to ∼1.0 mg/cm{sup 2}. XRD characterization of the remaining oxide was inconclusive, with no crystalline phases detected. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Technology Development for Dry Storage of Aluminum-Clad Spent Nuclear Fuel - 20490

A candidate disposition pathway for the > 13 MTHM of aluminum-clad spent nuclear fuel (ASNF), owned and managed by the U.S. Department of Energy, is the drying and placement of the SNF into sealed-canister dry storage, with the ASNF-in- canisters 'road-ready' for transportation to and final direct disposal in a repository waste package. Technical information gaps in fuel drying, and fuel dry storage behavior, have previously challenged the declaration of technology readiness for drying and placement of this fuel into the DOE Standard Canister design for > 50 years of safe dry storage. The principal technical information gaps included: i) characterization and thermal dehydration behavior of aluminum (oxy)hydroxide films attendant on the cladding due to film formation during reactor operation and during post-discharge up to long-term wet storage histories; and ii) G-value data to enable estimation of the radiolytic gas generation from the cladding with its (oxy)hydroxide films. Thus, the oxide films on the ASNF challenged the safety of a sealed storage canister with thermal and radiolytic decomposition of the waters on the films that can lead to corrosion, pressurization, and flammability issues. These gaps in the technical information base have largely been closed. This paper discusses the investigations at the Idaho National Laboratory (INL) and the Savannah River National laboratory (SRNL), and outlines the pending technology development work for input to an engineering design to enable a road-ready dry storage system for ASNF. The ASNF inventory considered for road-ready dry storage is stored at the Savannah River Site (SRS) and at the Idaho Nuclear Technology and Engineering Center (INTEC) at the INL. The ASNF inventory in the SRS L Basin is from foreign and domestic research reactors (FRR and DRR), and is diverse in terms of design, irradiation, and post-reactor-discharge storage conditions; these factors yield a range of characteristics of cladding oxide films on ASNF. Mixed aluminum (oxy)hydroxide (boehmite and bayerite/gibbsite) films, non-uniform in thicknesses up to a maximum local thickness bounded by 25 μm, were observed on ASNF materials removed from wet storage in the L Basin and in non-sealed dry storage at the SRS following reactor service and a long-term (up to 40+ years) interim storage history. The ASNF inventory at INTEC, in both wet and vented dry storage, is predominantly from the Advanced Test Reactor (ATR), but it also includes DRR and FRR fuel. To address a profound behavior of these films, radiolysis testing of aluminum specimens with mixed type boehmite/bayerite oxide films was performed to develop basic data on G-values for production of radiolytic hydrogen under dry storage conditions with nominal relative humidity, temperature, and cover gas. Modeling and simulation of canister internal environments with postulated inventories of oxide films provides estimation of the evolution of the conditions of the canister loaded with ASNF. Simultaneous Thermal Analysis (TGA/DSC) of hydrated oxide powders, and laboratory-scale aluminum specimens with a bayerite film (∼10 μm) using TGA methods, inform drying time/temperature conditions to be used for the ASNF. A demonstration project is recommended for Verification and Validation of the drying and storage of the ASNF. Remaining major tasks leading up to the hot demonstration include scale-up radiolysis testing and scale-up drying testing. Engineering design with the information from the technology program will establish the safety basis and enable long-term (> 50 years) dry storage compatibility with ASNF in the DOE Standard Canister pending its transportation to and disposal in a repository. This full capability would show the ASNF-in-canister storage system to be road-ready. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Development of Zirconium-Silicide Coatings for Improved Performance Zirconium-Alloy Fuel Cladding

There is considerable interest in the development of coatings for zirconium-alloy fuel cladding used in light water reactors (LWR) to improve their oxidation resistance during high temperature accident conditions and to enhance performance under normal operating conditions. These coatings should also enhance the heat transfer characteristics of the cladding surface so that heat from the fuel rod is efficiently transferred into the water coolant. One potential candidate coating material is zirconium-silicide. Transition metal silicides have been generally shown to have outstanding oxidation resistance. Zirconium-silicide is particularly attractive because Zr is strongly oxophilic, so that the Zr-silicide layer is expected to bond more strongly to the inner, native ZrO{sub 2} layer. The relative proximity of the free energy of formation of oxides of Zr and Si can lead to alternating multilayered oxide structures with radiation damage resistance. Additionally, oxidation of zirconium silicide can produce excellent corrosion resistant glassy zircon (ZrSiO{sub 4}) and silica (SiO{sub 2}), possessing self-healing qualities. This paper reports results of our results of high temperature oxidation tests of bulk zirconium-silicide and coatings of zirconium-silicide deposited on zirconium-alloy test flats and cladding tube configurations using plasma vapor deposition (PVD) process. We also report our initial results on the experimental facility for studying boiling characteristics of coated cladding tubes in prototypic pressurized water conditions. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enrichment Penalty for Molybdenum Cladded Accident Tolerant Fuel

A tri-layered fuel cladding has been proposed as an enhanced accident tolerant fuel (EATF) design. The EATF cladding has an inner layer of zirconium alloy, a layer of molybdenum, and an outer layer of zirconium alloy. Due to its high melting point, high temperature creep resistance, and improved resistance to steam corrosion, the molybdenum layer will better tolerate a loss of active coolant accident than the standard single layer zircaloy cladding currently in use. The addition of the molybdenum layer to the cladding, however, has a deleterious effect on the fuel management due to the high thermal neutron capture cross section of Mo{sup 95}. This negative reactivity effect must be counterpoised by increasing the fuel enrichment in order to maintain a constant cycle length. This work presents a prima facie quantification of the enrichment increase required to maintain cycle length for a standard PWR 3 x 18 month cycle. The quantification of the required enrichment increase is necessary in order for a more thorough financial analysis to be performed for the prospective new fuel design. (author)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Anisotropic Effects of Loading on Zircaloy Cladding Performance

This presentation provides recent results related to the mechanical behavior of Zircaloy cladding for the Light Water Reactor Fuels Workshop/CRAFT Initiative Update presented by the Advanced Fuels Campaign. This presentation focuses on Zircaloy cladding response to pellet-cladding interactions and how mechanical anisotropy makes the cladding sensitive to the testing mode. Results are compared to existing material models used by BISON, and implications for reactor performance are briefly discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enhanced Stress Relaxation Behavior via Basal ⟨a⟩ Dislocation Activity in Zircaloy-4 Cladding

Herein this work evaluates the stress relaxation behavior of textured Zircaloy-4 cladding to understand how mechanical anisotropy influences pellet-cladding interactions. Uniaxial and biaxial stress relaxation tests are performed using full-tube axial tension and internal pressurization, respectively, aiming to achieve 0.25%, 1%, and 2% equivalent strains in the cladding samples at a temperature of 300°C. Internal pressure relaxation test results display enhanced stress relaxation compared to axial testing results, particularly for samples loaded beyond yield. Results of electron backscatter diffraction indicate increased deformation microstructure during loading and increased strain homogenization and recovery during relaxation for samples loaded via internal pressurization. Analysis indicates that the increased production and activity of basal ⟨a⟩ dislocations play a significant role in the enhanced relaxation measured in samples subjected to internal pressurization.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High Temperature Steam Corrosion of Cladding for Nuclear Applications: Experimental

Stability of cladding materials under off-normal conditions is an important issue for the safe operation of light water nuclear reactors. Metals, ceramics, and metal/ceramic composites are being investigated as substitutes for traditional zirconium-based cladding. To support down-selection of these advanced materials and designs, a test apparatus was constructed to study the onset and evolution of cladding oxidation, and deformation behavior of cladding materials, under loss-of-coolant accident scenarios. Preliminary oxidation tests were conducted in dry oxygen and in saturated steam/air environments at 1000OC. Tube samples of Zr-702, Zr-702 reinforced with 1 ply of a ß-SiC CMC overbraid, and sintered a-SiC were tested. Samples were induction heated by coupling to a molybdenum susceptor inside the tubes. The deformation behavior of He-pressurized tubes of Zr-702 and SiC CMC-reinforced Zr-702, heated to rupture, was also examined.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Cladding burst behavior of Fe-based alloys under LOCA

Burst behavior of austenitic and ferritic Fe-based alloy tubes has been examined under a simulated large break loss of coolant accident. Specifically, type 304 stainless steel (304SS) and oxidation resistant FeCrAl tubes were studied alongside Zircaloy-2 and Zircaloy-4 that are considered reference fuel cladding materials. Following the burst test, characterization of the cladding materials was carried out to gain insights regarding the integral burst behavior. Given the widespread availability of a comprehensive set of thermo-mechanical data at elevated temperatures for 304SS, a modeling framework was implemented to simulate the various processes that affect burst behavior in this Fe-based alloy. The most important conclusion is that cladding ballooning due to creep is negligible for Fe-based alloys. Thus, unlike Zr-based alloys, cladding cross-sectional area remains largely unchanged up to the point of burst. Furthermore, for a given rod internal pressure, the temperature onset of burst in Fe-based alloys appears to be simply a function of the alloy's ultimate tensile strength, particularly at high rod internal pressures.

42 ENGINEERING↗