Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructural Refinement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Control of Carbide Precipitation During Electroslag Remelting-Continuous Rapid Solidification of GCr15 Steel

The effect of the electroslag remelting-continuous rapid solidification (ESR-CRS) process on element segregation and carbide precipitation in GCr15 bearing steel was investigated. The results showed that a microstructure with fewer primary carbides and less segregation can be achieved via the ESR-CRS process. In the specimen subjected to ESR, the morphology of primary carbide changed from angular to lumplike. After the ESR-CRS process, the dimension of primary carbide and the mass fraction of Cr in primary carbide decreased. With the increase of cooling intensity during the ESR-CRS process, the microstructure of ESR ingot became more refined and uniform and the size of large primary carbides in ESR ingot gradually decreased. Suppressing the formation of grain boundary cementite and primary carbide during ESR of GCr15 steel is beneficial to inhibiting the presence of large secondary carbide formation after annealing. With the increase of cooling intensity, the mass fraction of carbides in ESR ingot decreased and the mass fraction of Cr in carbides increased, whereas the types of carbides did not change; all the M{sub 3}C, M{sub 3}C{sub 2}, and M{sub 7}C{sub 3} exist before and after ESR-CRS. Al{sub 2}O{sub 3} inclusions promoted the formation of Ti(N,C) by serving as preferred heterogeneous nucleation sites, whereas the formation of Ti(N,C) was suppressed through the refinement of Al{sub 2}O{sub 3} inclusions by increasing the cooling intensity.

36 MATERIALS SCIENCE↗

Robustness of magnetocrystalline anisotropy and coercivity in Fe–Co–B

As a potential candidate for critical chemical element free permanent magnet, (Fe 0.7 Co 0.3 ) 2 B, shows promising intrinsic magnetic properties, including large magnetization, high Curie temperature and moderate magnetocrystalline anisotropy (MCA). Still, the coercivity that has been achieved is relatively low. To understand and improve coercivity, here we study the robustness of MCA related to the fluctuation of chemical composition and the structural distortion and its effect on coercivity in (Fe 0.7 Co 0.3 ) 2 B from first principles DFT (density functional theory) calculation and micromagnetic simulation. A fluctuation of cobalt content of 10%, or 1% isotropic lattice strain, or 2% tetragonal distortion reduces MCA energy up to 30%. By considering randomly distributed local MCA energy reduction up to 30%, the calculated coercivity of anisotropic bulk magnets reduced from 3.6 kOe to 2.2 kOe. Rational microstructure design, such as grain size refinement and development of strong crystal texture of MCA easy-axis (i.e., degree of alignment for (Fe 0.7 Co 0.3 ) 2 B grains), can enhance coercivity and mitigate the effect of local MCA reduction. In addition to acceptable intrinsic magnetic properties, the promising hard magnetic phase needs good MCA robustness to facilitate the development of practical magnets.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Cyclic deformation and lattice strain distribution of high Nb containing TiAl alloy

Low cycle fatigue of lamellar TiAl with 8.5 at.-%Nb was studied with a total strain amplitude of 0.28% at three temperatures: room temperature, 750°C and 900°C. At room temperature, the material exhibited cyclic hardening and the fracture mode was mainly interlamellar. At 750°C and 900°C, the material showed cyclic softening and the fracture mode was translamellar. The lattice strain in γ phase was almost tensile and larger tensile lattice strain in γ phase seems detrimental. Besides, the opposite direction of {201} γ and {100} α2 lead to crack propagation along α 2 /γ interfaces. B2/β o phase always suffered compressive lattice strain in the tests. Finally, the destruction of lamellar microstructure was the reason for colony refinement at 750°C and 900°C.

phase transformation↗

Advanced Synthesis of Na 4 Si 24

The recently discovered orthorhombic allotrope of silicon, Si 24 , is an exciting prospective material for the future of solar energy due to a quasi-direct bandgap near 1.3 eV, coupled with the abundance and environmental stability of silicon. Synthesized via precursor Na 4 Si 24 at high temperature and pressure (~850 °C, 9 GPa), typical synthesis results have yielded polycrystalline samples with crystallites on the order of 20 μm. Several approaches to increase the crystal size have yielded success, including in-situ thermal spikes and refined selection of the starting materials. Microstructural analysis suggests that coherency exists between diamond silicon (d-Si) and Na 4 Si 24 . This hypothesis has led to the successful attempts at single crystal synthesis by selecting large crystals of d-Si along with metallic Na as the precursors rather than powdered and mixed precursor material. The new synthesis approach has yielded single crystals of Na 4 Si 24 greater than 100 μm. These results represent a breakthrough in synthesis that enables further characterization and utility. The promise of Si 24 for the future of solar energy generation and efficient electronics is strengthened through these advances in synthesis.

catalysis (heterogeneous)↗

Residual Stress Distribution and Microstructure of a Multiple Laser-Peened Near-Alpha Titanium Alloy

Laser peening without coating (LPwC) was performed on a Ti-2.5 Cu alloy with multiple passes (1, 3 and 5), using a Nd:YAG laser (1064 nm) at a constant overlap rate of 70% and power density of 6.7 GW cm{sup −2}. Hardness and residual stress profiles indicated thermal softening near the surface (< 100 μm) and bulk softening due to adiabatic heating. Maximum hardness (235 HV at 500 μm) and maximum residual stress (− 890 MPa at 100 μm) were observed for LPwC with 1 pass. Surface roughness and surface 3-D topography imaging showed that the surface roughness increased with the increase in the number of passes. XRD results indicated no significant β phases. However, peak shifts, broadening and asymmetry were observed and interpreted based on dislocation activity. Microstructures indicated no melting or resolidification or refinement of grains at the surface. Twin density was found to increase with the increase in the number of passes.

36 MATERIALS SCIENCE↗

Effect of Accumulative Roll Bonding on Plastic Flow Properties of Commercially Pure Zirconium

Accumulative roll bonding (ARB) has been considered as one of the promising techniques for fabrication of ultra-fine grained (UFG) metallic materials. The ARB process consists of several cycles of cutting, stacking, and rolling of metal sheets, so very high strains can be induced in the material resulting in significant grain refinement and in the formation of UFG microstructures. The ARB technique has been applied to a wide range of metallic materials such as Al and Al alloys, Mg, Fe and steels, Zr, Cu, as well as composite materials. UFG metallic materials processed via ARB show increased strength. Despite a significant body of experimental research into the deformation behaviour of the ARB-processed materials, the fundamentals of their plastic deformation are not fully understood yet. This work focuses on the effect of grain refinement via ARB-processing on the mechanical behavior and on the strain-rate sensitivity of commercially pure Zr (99.8% purity). The mechanical properties of the as-received coarse-grained (CG) and UFG (as-ARB processed) samples were studied at room temperature at two different strain rates. Mechanical strain rate jump tests were performed during tensile deformation to estimate the instantaneous strain-rate sensitivity. The evolution of surface relief during plastic deformation of pure Zr in both CG and UFG conditions was studied. The features of plastic deformation of pure Zr in both CG and UFG conditions are discussed.

36 MATERIALS SCIENCE↗

Microstructural Analysis of Severe Plastic Deformed Twin Roll Cast AZ31 for the Optimization of Superplastic Properties

In recent years magnesium alloys have attracted significant attention as potential candidates to replace many of the heavier metals used in some automotive applications. However, the limited formability of magnesium and its alloys at room temperature has driven interest in the superplastic forming magnesium as an alternative shaping method. Severe plastic deformation techniques have become a well studied method of refining the grain size and modifying the microstructural characteristics of many magnesium alloys to achieve greater superplastic properties. In this study twin roll cast (TRC) AZ31 magnesium alloy was subjected to equal channel angular pressing (ECAP) and friction stir welding (FSW). The influence of these severe plastic deformation processes on the grain size, texture and grain boundary character distribution was investigated to identify the optimum severe plastic deformation process for the superplastic forming of AZ31.

Young, John P.↗

Direct numerical simulation of mechanical response in synthetic additively manufactured microstructures

Additive manufacturing (AM) processes for metals can yield as-built microstructures that vary significantly from their cast or wrought counterparts. These microstructural variations can in turn, have profound effects on the properties of a component. Here, a modeling methodology is presented to investigate microstructurally-influenced mechanical response in additively manufactured structures via direct numeral simulation. Three-dimensional, synthetic voxelized microstructures are generated by kinetic Monte Carlo (kMC) additive manufacturing process simulations performed at four scan speeds to create a thin-wall cylindrical geometry notionally constructed using a concentric-pathed directed energy deposition AM process. The kMC simulations utilize a steady-state molten pool geometry that is held constant throughout the study. Resultant microstructures are mapped onto a highly-refined conformal finite-element mesh of a part geometry. A grain-scale anisotropic crystal elasticity model is then used to represent the constitutive response of each grain. Here, the response of the structure subjected to relatively simple load conditions is studied in order to provide understanding of both the influence of AM processing on microstructure as well as the microstructure's influence on the macroscale mechanical response.

42 ENGINEERING↗

Facile synthesis of B-type carbonated nanoapatite with tailored microstructure

Nanolime and a phosphate-based chelating agent were used to synthesize B-type carbonated apatite. Developed Rietveld refinement strategies allowed one to determine process yield, product crystallinity as well as structural (unit cell) and microstructural (size, strain) parameters. The effect of synthesis temperature (20–60 °C) as well as Ca/P ratio (1.5–2.5) and solid content (10–30 wt%) of the starting batch on these properties were investigated. FTIR, TEM and gas adsorption data provided supporting evidence. The process yield was 42–60 wt% and found to be governed by the Ca/P ratio. The purified products had high specific surface area (107–186 m{sup 2}/g) and crystallinity (76–97%). The unit cell parameters, correlated to the degree of structural carbonate, were sensitive to the Ca/P ratio. Instead, temperature governed the microstructural parameters. Less strained and larger crystals were obtained at higher temperatures. Long-term aging up to 6 months at 20 °C compensated for higher crystal growth kinetics at higher temperature. - Graphical abstract: Controlled synthesis of carbonated apatite at moderate temperatures using nanolime and sodiumhexametaphosphate as starting reagent. - Highlights: • Chemical synthesis of nano-sized apatite with tailored microstructure was performed. • Colloidal Ca(OH){sub 2} and a phosphorus-based chelating agents were used as reagents. • The method is simple and reproducible which facilitate industrial process scale-up. • Rietveld refinement strategies for product characterization were developed. • Rietveld analyses provided yield, microstructural and structure information.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Refinement performance and mechanism of an Al-50Si alloy

The microstructure and melt structure of primary silicon particles in an Al-50%Si (wt.%) alloy have been investigated by optical microscopy, scanning electron microscopy, electron probe micro-analysis and a high temperature X-ray diffractometer. The results show that the Al-50Si alloy can be effectively refined by a newly developed Si-20P master alloy, and the melting temperature is crucial to the refinement process. The minimal overheating degree {delta}T{sub min} ({delta}T{sub min} is the difference between the minimal overheating temperature T{sub min} and the liquidus temperature T{sub L}) for good refinement is about 260 deg. C. Primary silicon particles can be refined after adding 0.2 wt.% phosphorus amount at sufficient temperature, and their average size transforms from 2-4 mm to about 30 {mu}m. The X-ray diffraction data of the Al-50Si melt demonstrate that structural change occurs when the melting temperature varies from 1100 deg. C to 1300 deg. C. Additionally, the relationship between the refinement mechanism and the melt structure is discussed.

36 MATERIALS SCIENCE↗

Effect of Deformation Parameters on Microstructure and Properties During DIFT of X70HD Pipeline Steel

Grain refinement is a critical approach to improve the strength of materials without damaging the toughness. The grains of deformation-induced ferrite are considerably smaller than those of proeutectoid ferrite. Grain refinement is crucial to the application of deformation-induced ferrite. The composition of ferrite and bainite or martensite is important in controlling the performance of X70HD pipeline steel, and cooling significantly influences the control of their ratio and grain size. By analyzing the static and dynamic phase-transition points using Gleeble-3800 thermal simulator, thermal simulations were performed through two-stage deformations in the austenite zone. Ferrite transformation rules were studied with thermal simulation tests under different deformation and cooling parameters based on the actual production of cumulative deformation. The influence of deformation parameters on the microstructure transformation was analyzed. Numerous fine-grain deformation-induced ferrites were obtained by regulating various parameters, including deformation temperature, strain rate, cooling rate, final cooling temperature and other parameters. Results of metallographic observation and microtensile testing revealed that the selection of appropriate parameters can refine the grains and improve the performance of the X70HD pipeline steel.

36 MATERIALS SCIENCE↗

Enhanced strength and toughness in ultra-fine grained 99.9% copper obtained by cryo-hydrostatic extrusion

Highlights: • Cryo-HE can increase the yield strength of Cu by more than threefold. • In cryo-HE of Cu, the grain refinement is stronger by 30% than in room-HE. • Cryo-HE with post-annealing effectively creates a bimodal microstructure in Cu. • Short-term post-annealing applied to cryo-HE-treated Cu can double its ductility. • Grain refinement with recrystallization results in a slight increase of Cu toughness. - Abstract: Ultrafine grained 99.9% Cu with enhanced strength and toughness was produced by hydrostatic extrusion conducted at the temperature of liquid nitrogen. The cryo-extruded Cu has a tensile yield strength of 490 MPa, hardness of 145 HV0.2, and tensile fracture toughness of 39.5 MPa m{sup 1/2}, which means that their values increased by 380%, 185% and ~10%, respectively, compared to those of the starting material. The significant strengthening is due to the strong grain refinement to 320 nm and the high energy of defects stored during the processing at liquid nitrogen temperature. The short term post deformation annealing doubles the ductility of material even by above 10% of the elongation to fracture at a slight expense of the yield strength (485 MPa). The observed behavior of Cu can be explained in terms of its low stacking fault energy, the susceptibility to dynamic recrystallization within the working zone of the extrusion die, and the triaxial strain components with the very large strain gradients, combined with the significant adiabatic heating effect active during the hydrostatic extrusion. The better homogeneity of the grain refinement and the higher efficiency of the distribution of defects and of the energy storage accompanied by the decreased dislocation mobility during the cryo hydrostatic extrusion contributed to the higher strength.

36 MATERIALS SCIENCE↗

Mesh Computing Remote Automatic Workflow

The software suite uses a microservice architecture using Docker and `docker-compose`. The microservices are as follows: 1. User interface. This interface is written in JavaScript using the Svelte framework. It exposes form elements and a 3D visualizer to prompt the user through the definition of microstructure parameters, and setting parameters for mesh generation and refinement. 2. Mesh generator. This is a container running the Python package for DREAM3D to generate a voxelized mesh that represents a microstructure defined by the user in the interface. 3. Cubit runner. This is a secure shell protocol tool that makes the submitting the DREAM mesh to an HPC instance and starts to run Cubit shell commands to smooth the grain boundaries with its `sculpt` library, applies user-defined boundary node sets, and bundles and returns the simulation-ready meshes and input files as a zipped directory.

Harris, BrennanKay↗

Enhancement in hard magnetic properties of (Nd, Pr)–Fe–B melt-spun ribbons

The coercivity of RE 2 Fe 14 B-type permanent magnets is strongly influenced by the microstructural features such as grain boundary (GB) phases as well as grain sizes. Here, we have combined micromagnetic simulations and experiments to elucidate the role of excess RE (Nd/Pr) in determining the resulting hard magnetic properties of Nd–Pr–Fe–B melt-spun ribbons. The intrinsic coercivity (H c ) at room temperature significantly enhanced from 9.7 kOe to 15.3 kOe with the increase in the Nd/Pr content. Furthermore, the effect of non-magnetic grain refining refractory carbide (TiC) on both the microstructure and magnetic hardening was studied. The addition of TiC showed a very high coercivity H c of up to 19.0 kOe at room temperature. Micromagnetic simulation indicates that the coercivity enhancement is mainly due to the reduction of inter-grain magnetic interaction, which is due to the RE-rich nonmagnetic grain boundary (GB) phase and/or TiC distributed at the GB. This work provides useful information on the roles of non-magnetic grain boundary phases for improving the coercivity of Nd–Pr–Fe–B magnets. Combined with experimental and modeling results, we have discussed the mechanism responsible for the enhancements in coercivity and the suitability of the alloys for high-performance permanent magnet development.

36 MATERIALS SCIENCE↗

Effect of Friction Stir Processing on Microstructure and Tensile Properties of an Investment Cast Al-7Si-0.6Mg Alloy

Friction stir processing (FSP) is emerging as a promising tool for microstructural modification. The present study assesses the effects of FSP on the microstructure and mechanical properties of an investment cast Al-7Si-Mg alloy. FSP eliminates porosity and significantly refines eutectic Si particles. The extent of particle refinement varied with changes in processing conditions. High tool rotation rate and low to intermediate tool traverse speed generated a higher volume fraction of finer particles. Tensile ductility changed significantly as a result of FSP, whereas UTS improved only marginally. Yield strength was similar in both cast and FSPed samples under various heat treated conditions, with the highest value obtained after a T6 heat treatment. Further, FSP caused significant grain refinement in the stir zone, subsequently transforming into very coarse grains as abnormal grain growth (AGG) occurred during solution treatment at high temperature.

36 MATERIALS SCIENCE↗

The Effect of Rolling As-Cast and Homogenized U-10Mo Samples on the Microstructure Development and Recovery Curves

Over the past several years Pacific Northwest National Laboratory (PNNL) has been actively involved in supporting the U.S. Department of Energy National Nuclear Security Administration Office of Material Management and Minimization (formerly Global Threat Reduction Initiative). The U.S. High- Power Research Reactor (USHPRR) project is developing alternatives to existing highly enriched uranium alloy fuel to reduce the proliferation threat. One option for a high-density metal fuel is uranium alloyed with 10 wt% molybdenum (U-10Mo). Forming the U-10Mo fuel plates/foils via rolling is an effective technique and is actively being pursued as part of the baseline manufacturing process. The processing of these fuel plates requires systematic investigation/understanding of the pre- and post-rolling microstructure, end-state mechanical properties, residual stresses, and defects, their effect on the mill during processing, and eventually, their in-reactor performance. In the work documented herein, studies were conducted to determine the effect of cold and hot rolling the as-cast and homogenized U-10Mo on its microstructure and hardness. The samples were homogenized at 900°C for 48 h, then later annealed for several durations and temperatures to investigate the effect on the material’s microstructure and hardness. The rolling of the as-cast plate, both hot and cold, was observed to form a molybdenum-rich and -lean banded structure. The cold rolling was ineffective, and in some cases exacerbated the as-cast defects. The grains elongated along the rolling direction and formed a pancake shape, while the carbides fractured perpendicularly to the rolling direction and left porosity between fractured particles of UC. The subsequent annealing of these samples at sub-eutectoid temperatures led to rapid precipitation of the ' lamellar phase, mainly in the molybdenum-lean regions. Annealing the samples above the eutectoid temperature did not refine the grain size or the banded microstructure. However, annealing the samples led to quick recovery in hardness as evidenced by a drop in Vickers hardness of 20%. Hot rolling was performed at 650 and 800°C. The hot-rolling mill loads (load separation force) were approximately 40 to 50% less than the cold-rolling for the same reduction and thickness. It was observed that hot rolling the samples with 50% or more reduction in thickness were responsible for dynamic recrystallization in the hot-rolled samples and led to grain refinement. Unlike the cold-rolled samples, the hot-rolled samples did not fracture the carbides and appeared to heal the casting defects. The recovery phenomenon was similar to the cold-rolled samples above the eutectoid temperatures, but owing to the refined grain size, the precipitation of the lamellar phase was far more rapid in these samples and the hardness increased more rapidly than in the cold rolled sample when heated below the eutectoid temperature. The data generated from these rolling efforts has been used to make the process modeling efforts more robust and applicable to all USHPRR partner rolling mills. The flow stress for cold rolling the samples was determined to be between 170-190 ksi, with frictional forces between 0.2 and 0.4 for the PNNL mill. The measured roll separation forces and those simulated using finite element methods for hot and cold rolling for the PNNL rolling mill were in good agreement.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The Effect of Rolling As-Cast and Homogenized U-10Mo Samples on the Microstructure Development and Recovery Curves

Over the past several years Pacific Northwest National Laboratory (PNNL) has been actively involved in supporting the U.S. Department of Energy National Nuclear Security Administration Office of Material Management and Minimization (formerly Global Threat Reduction Initiative). The U.S. High-Power Research Reactor (USHPRR) project is developing alternatives to existing highly enriched uranium alloy fuel to reduce the proliferation threat. One option for a high-density metal fuel is uranium alloyed with 10 wt% molybdenum (U-10Mo). Forming the U-10Mo fuel plates/foils via rolling is an effective technique and is actively being pursued as part of the baseline manufacturing process. The processing of these fuel plates requires systematic investigation/understanding of the pre- and post-rolling microstructure, end-state mechanical properties, residual stresses, and defects, their effect on the mill during processing, and eventually, their in-reactor performance. In the work documented herein, studies were conducted to determine the effect of cold and hot rolling the as-cast and homogenized U-10Mo on its microstructure and hardness. The samples were homogenized at 900°C for 48 h, then later annealed for several durations and temperatures to investigate the effect on the material’s microstructure and hardness. The rolling of the as-cast plate, both hot and cold, was observed to form a molybdenum-rich and -lean banded structure. The cold rolling was ineffective, and in some cases exacerbated the as-cast defects. The grains elongated along the rolling direction and formed a pancake shape, while the carbides fractured perpendicularly to the rolling direction and left porosity between fractured particles of UC. The subsequent annealing of these samples at sub-eutectoid temperatures led to rapid precipitation of the α + γ ' lamellar phase, mainly in the molybdenum-lean regions. Annealing the samples above the eutectoid temperature did not refine the grain size or the banded microstructure. However, annealing the samples led to quick recovery in hardness as evidenced by a drop in Vickers hardness of 20%. Hot rolling was performed at 650 and 800°C. The hot-rolling mill loads (load separation force) were approximately 40 to 50% less than the cold-rolling for the same reduction and thickness. It was observed that hot rolling the samples with 50% or more reduction in thickness were responsible for dynamic recrystallization in the hot-rolled samples and led to grain refinement. Unlike the cold-rolled samples, the hot-rolled samples did not fracture the carbides and appeared to heal the casting defects. The recovery phenomenon was similar to the cold-rolled samples above the eutectoid temperatures, but owing to the refined grain size, the precipitation of the lamellar phase was far more rapid in these samples and the hardness increased more rapidly than in the cold rolled sample when heated below the eutectoid temperature. The data generated from these rolling efforts has been used to make the process modeling efforts more robust and applicable to all USHPRR partner rolling mills. The flow stress for cold rolling the samples was determined to be between 170-190 ksi, with frictional forces between 0.2 and 0.4 for the PNNL mill. The measured roll separation forces and those simulated using finite element methods for hot and cold rolling for the PNNL rolling mill were in good agreement.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Containerless drop tube solidification and grain refinement of NiAl3

The possibility of undercooling Ni-Al alloys below the liquidus in order to produce a single phase peritectic structure by containerless drop tube solidification was studied. Containerless process is a technique for both high purity contamination free studies as well as for investigating the undercooling and rapid solidification of alloys by suppression of heterogeneous nucleation on container walls. In order to achieve large undercoolings one must avoid heterogeneous nucleation of crystallization. It was shown that the Marshall Space Flight Center drop tubes ae unique facilities for containerless solidification experiments and large undercoolings are possible with some alloys. The original goal of undercooling the liquid metal well below the liquidus to the peritectic temperature during containerless free to form primarily NiAl3 was achieved. The microstructures were interesting from another point of view. The microstructure from small diameter samples is greatly refined. Small dendrite arm spacings such as these could greatly facilitate the annealing and solid state transformation of the alloy to nearly 10% NiAl3 by reducing the distance over which diffusion needs to occur. This could minimize annealing time and might make it economically feasible to produce NiAl3 alloy.

Ethridge, E. C.↗