Search NASA⌕ Search

SEARCH · Search NASA

Results for “POLISHING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

Investigation of rotor blade roughness effects on turbine performance

The cold air test program was completed on the SSME (Space Shuttle Main Engine) HPFTP (High Pressure Fuel Turbopump) turbine with production nozzle vane rings and polished coated rotor blades with a smooth surface finish of 30 microinch (0.76 micrometer) RMS (Root Mean Square). The smooth blades were polished by an abrasive flow machining process. The test results were compared with the air test results from production rough coated rotor blades with a surface finish of up to 400 microinch (10.16 micrometer) RMS. Turbine efficiency was higher for the smooth blades over the entire range tested. Efficiency increased 2.1 percentage points at the SSME 104 percent RPL (Rated Power Level) condition. This efficiency improvement could reduce the SSME HPFTP turbine inlet temperature by 57 degrees Rankine (32 degrees Kelvin) increasing turbine durability. The turbine flow parameter increased and the mid-span outlet swirl angle became more axial with the smooth rotor blades.

Boynton, J. L.↗

Effect of the Surface Condition of a Wing on the Aerodynamic Characteristics of an Airplane

In order to determine the effect of the surface conditions of a wing on the aerodynamic characteristics of an airplane, tests were conducted in the N.A.C.A. full-scale wind tunnel on the Fairchild F-22 airplane first with normal commercial finish of wing surface and later with the same wing polished. Comparison of the characteristics of the airplane with the two surface conditions shows that the polish caused a negligible change in the lift curve, but reduced the minimum drag coefficient by 0.001. This reduction in drag if applied to an airplane with a given speed of 200 miles per hour and a minimum drag coefficient of 0.025 would increase the speed only 2.9 miles per hour, but if the speed remained the same, the power would be reduced 4 percent.

AIRPLANES - FAIRCHILD 22 (Amer ) WIND TUNNEL TEST↗

Effects of Range of Stress and of Special Notches on Fatigue Properties of Aluminum Alloys Suitable for Airplane Propellers

Laboratory tests were made to obtain information on the load-resisting properties of X76S-T aluminum alloy when subjected to static, impact, and repeated loads. Results are presented from static-load test of unnotched specimens in tension and in torsion and of notched specimens in tension. Charpy impact values obtained from bend tests on notched specimens and tension impact values for both notched and unnotched specimens tested at several different temperatures are included. The endurance limits obtained from repeated bending fatigue tests made on three different types of testing machine are given for unnotched polished specimens, and the endurance limits of notched specimens subjected to six different ranges of bending stress are also reported. The results indicated that: (a) polished rectangular specimens had an endurance limit about 30 percent less than that obtained for round specimens; (b) a comparison of endurance limits obtained from tests on three different types of machine indicated that there was no apparent effect of speed of testing on the endurance limit for the range of speeds used (1,750 to 13,000 rpm). (c) the fatigue strength (endurance limit) of the X76S-T alloy was greatly decreased by the presence of a notch in the specimens; (d) no complete fractures of the entire specimens occurred in notched fatigue specimens when subjected to stress cycles for which the mean stress at the notch during the cycle was a compressive stress; for this test condition a microscopic cracking occurred near the root of the notch and was used as a criterion of failure of the specimen. (e) as the mean stress at the notch was decreased from a tensile (+) stress to a compressive (-) stress, it was found that the alternating stress that could be superimposed on the mean stress in the cycle without causing failure of the specimens was increased.

ALUMINUM ALLOYS-ALCOA X76ST-FATIGUE↗

The Efficiency of Small Bearings in Instruments of the Type Used in Aircraft

This report deals with the construction and properties of bearings and pivots for use in instruments. The static and running friction for both thrust and radial loads was determined for a number of conical pivots and cylindrical and ball bearings. The static rocking friction was also measured for several conical and ball bearings under a heavy load, especially to determine their suitability for use in N. P. L. (National Physical Laboratory) type wind tunnel balance. In constructing conical pivots and sockets it was found that the pivots should be hardened and highly polished, preferably with a revolving lap, and that the sockets should be made by punching with a hardened and polished punch. It was found that for a light load the conical pivots give less friction than any other type, and their wearing qualities when hardened are excellent. Very small ball bearings are unsatisfactory because the proportional accuracy of the balls and races is not high enough to insure smooth running. For rocking pivots under heavy loads it was found that a ball-and-socket bearing, consisting of a hemispherical socket and a sphere of smaller diameter concentric with it, with a row of small balls resting between the two, was superior to a pivot resting in a socket. It was found that vibration such as occurs in an airplane will greatly reduce the static friction of a pivot or bearing, in some cases to as little as one-twentieth of its static value.

Norton, F H↗

Liquid metal drop ejection

The aim of this project was to demonstrate the possibility of ejecting liquid metals using drop on demand printing technology. The plan was to make transducers for operation in the 100 MHz frequency range and to use these transducers to demonstrate the ability to eject drops of liquid metals such as gallium. Two transducers were made by indium bonding piezoelectric lithium niobate to quartz buffer rods. The lithium niobate plates were thinned by mechanical polishing to a thickness of 37 microns for operation at 100 MHz. Hemispherical lenses were polished in the opposite ends of the buffer rods. The lenses, which focus the sound waves in the liquid metal, had an F-number equals 1. A mechanical housing was made to hold the transducers and to allow precise control over the liquid level above the lens. We started by demonstrating the ability to eject drops of water on demand. The drops of water had a diameter of 15 microns which corresponds to the wavelength of the sound wave in the water. A videotape of this ejection was made. We then used a mixture of Gallium and Indium (used to lower the melting temperature of the Gallium) to demonstrate the ejection of liquid metal drops. This proved to be difficult because of the oxide skin which forms on the surface of the liquid. In some instances, we were able to eject metal drops, however, this was not consistent and reproducible. An experiment was set up at NASA-Lewis to stabilize the process of drop on demand liquid metal ejection. The object was to place the transducer and liquid metal in a vacuum station so that no oxide would form on the surface. We were successful in demonstrating that liquid metals could be ejected on demand and that this technology could be used for making sheet metal in space.

Khuri-Yakub, B. T.↗

Investigations into mirror fabrication metrology analysis

This final report describes the work performed under this delivery order from June 1993 through August 1994. The scope of work included three distinct tasks in support of the AXAF-I program. The objective of the first task was to perform investigations of the grinding and polishing characteristics of the zerodur material by fabricating several samples. The second task was to continue the development of the integrated optical performance modeling software for AXAF-I. The purpose of third and final task was to develop and update the database of AXAF technical documents for an easy and rapid access. The MSFC optical and metrology shops were relocated from the B-wing of Building 4487 to Room BC 144 of Building 4466 in the beginning of this contract. This included dismantling, packing, and moving the equipment from its old location, and then reassembling it at the new location. A total of 65 zerodur samples, measuring 1 inch x 2 inches x 6 inches were ground and polished to a surface figure of lambda/10 p-v, and a surface finish of 5A rms were fabricated for coating tests. A number of special purpose tools and metal mirrors were also fabricated to support various AXAF-I development activities. In the metrology area, the ZYGO Mark 4 interferometer was relocated and also upgraded with a faster and more powerful processor. Surface metrology work was also performed on the coating samples and other optics using ZYGO interferometer and WYKO profilometer. A number of new features have been added to the GRAZTRACE program to enhance its analysis and modeling capabilities. A number of new commands have been added to the command mode GRAZTRACE program to provide a better control to the user on the program execution and data manipulation. Some commands and parameter entries have been reorganized for a uniform format. The command mode version of the convolution program CONVOLVE has been developed. An on-line help system and a user's manual have also been developed for the benefit of the users. The database of AXAF technical documents continues to progress. The titles, company name, date, and location of over 390 documents have been entered in this database. This database provides both a data search and retrieval function, and a data adding function. These functions allow a user to quickly search the data files for documents or add new information. A detailed user's guide has also been prepared. This user guide includes a document classification guide, a list of abbreviations, and a list of acronyms, which have been used in compiling this database of AXAF-I technical documents.

Dimmock, John O.↗

The realuminizing of the 7-meter-diameter solar simulator collimating mirror

This paper describes the modification of a three-electron-beam (EB) gun system for vacuum depositing a highly reflective aluminum coating on a 7.01-m (23-ft) -diam nickel-plated aluminum collimating mirror. The mirror is part of the JPL 7.62-m space simulator that was recently modernized with a new high vacuum pumping system, solar lamp power supplies, solar optic lens system, and refurbished collimating mirror. The 7.01-m 12,700-kg (14-ton) spherical collimating mirror was removed from this facility for replating with 381 micron (0.015 in.) of electroless nickel and polished to a specular finish for realuminizing. The space chamber served as the vacuum coating vessel for the realuminizing coating process. The mirror is the primary reflector for the solar simulation system and the aluminized reflective surface is its most critical performance element. The uniformity of thickness and high reflectivity of the coating in visible and near-ultraviolet (UV) light governs the accuracy of the beam for solar testing. The uniformity of the thin-film thickness also controls the durability of the mirror over time. The mirror was polished to a 64-percent reflectivity with a uniformity of 1.5 percent. The performance goal for the aluminizing was 89 percent with +/- 0.5-percent variation over the mirror.

Noller, E. W.↗

Wear-Resistant, Self-Lubricating Surfaces of Diamond Coatings

In humid air and dry nitrogen, as-deposited, fine-grain diamond films and polished, coarse-grain diamond films have low steady-state coefficients of friction (less than 0.1) and low wear rates (less than or equal to 10(exp -6) mm(exp 3)/N-m). In an ultrahigh vacuum (10(exp -7) Pa), however, they have high steady-state coefficients of friction (greater than 0.6) and high wear rates (greater than or equal to 10(exp -4) mm(exp 3)/N-m). Therefore, the use of as-deposited, fine-grain and polished, coarse-grain diamond films as wear-resistant, self-lubricating coatings must be limited to normal air or gaseous environments such as dry nitrogen. On the other hand, carbon-ion-implanted, fine-grain diamond films and nitrogen-ion-implanted, coarse-grain diamond films have low steady-state coefficients of friction (less than 0.1) and low wear rates (less than or equal to 10(exp -6) mm(exp 3)/N-m) in all three environments. These films can be effectively used as wear-resistant, self-lubricating coatings in an ultrahigh vacuum as well as in normal air and dry nitrogen.

Miyoshi, Kazuhisa↗

Effects of the LDEF orbital environment on the reflectance of optical mirror materials

Specimens of eight different optical mirror materials were flown in low earth orbit as part of the Long Duration Exposure Facility (LDEF) manifest to determine their ability to withstand exposure to the residual atomic oxygen and other environmental effects at those altitudes. Optical thin films of aluminum, gold, iridium, osmium, platinum, magnesium fluoride-overcoated aluminum and reactively deposited, silicon monoxide-protected aluminum, all of which were vacuum deposited on polished fused silica substrates, were included as part of Experiment S0010, Exposure of Spacecraft Coatings. Two specimens of polished, chemical vapor deposited (CVD) silicon carbide were installed in sites available in Experiment A0114, Interaction of Atomic Oxygen with Solid Surfaces at Orbital Altitudes, which included trays in two of the spacecraft bays, one on the leading edge and the other on the trailing edge. One of the silicon carbide samples was located in each of these trays. This paper will compare specular reflectance data from the preflight and postflight measurements made on each of these samples and attempt to explain the changes in light of the specific environments to which the experiments were exposed.

Herzig, Howard↗

Aubrite basalt vitrophyres: High sulfur silicate melts and a snapshot of aubrite formation

Two aubrite basalt vitrophyre clasts have been found within AMNH thin sections from the Parsa EH3 chondrite and the Khor Temiki aubrite. Polished sections of the Parsa Aubrite Inclusion (PAI) and the Khor Temiki Inclusion (KTI) were studied by optical, electron probe microanalysis (EPMA), and scanning electron microscopy (SEM) techniques with broad-beam and low absorbed EPMA currents used to minimize glass volatile loss. Some data have previously been reported for PAI and KTI may possibly correlate to a previously reported inclusion in Khor Tiimiki. In polished sections, PAI and KTI are approximately equal 4 mm in diameter and contain a large volume of glass. The clasts have similar textural characteristics and are akin to lunar vitrophyre textures. The glasses have high alkali rhyodacitic compositions Al-though PAI is peraluminous, KTI is significantly peralkaline. Additionally, the glasses have elevated sulfur concentrations that are extremely high by geochemical standards. SEM examination for beam overlap of microscopic CaS, FeS, and (Mg, Mn, Fe) S inclusions showed no such contamination. Furthermore, homogeneity of glass S content and low FeO contents help rule out contamination. Materials research data show that under reducing conditions alumino-silicate melts can dissolve up to several weight percent sulfur in the absence of Fe. The high S and alkali contents, the lack of associated high shock features, and the rationalized phase equilibria suggest that PAI and KTI are igneous melting products of an E-chondrite-like source material. Although large-scale impact melting cannot totally be ruled out, the above observations eliminate the possibility of in-situ shock melting.

Fogel, R. A.↗

NDE of PWA 1480 single crystal turbine blade material

Cantilever bending fatigue specimens were examined by fluorescent liquid penetrant and radioactive gas penetrant (Krypton) Nondestructive Evaluation (NDE) methods and tested. Specimens with cast, ground, or polished surfaces were evaluated to study the effect of surface condition on NDE and fatigue crack initiation. Fractographic and metallurgical analyses were performed to determine the nature of crack precursors. Preliminary results show that fatigue strength was lower for specimens with cast surfaces than for specimens with machined surfaces. The liquid penetrant and gas penetrant techniques both provided indications of a large population of defects on the cast surfaces. On ground or polished specimen surfaces, the gas penetrant appeared to estimate the actual number of voids more accurately than the liquid penetrant.

Klima, Stanley J.↗

Emittance characterization of thermal control paints, coatings and surfaces using a calorimetric technique

Thermal control surfaces are used in every spacecraft thermal management system to dissipate heat through radiant heat transfer. This paper describes the thermal performance of several thermal control paints, coatings, and surfaces, as characterized by a calorimetric vacuum emissometer. The emissometer is designed to measure the functional emittance of a surface based on heat transfer from an underlying substrate to the surface and from the surface or near surface to a surrounding cold wall. Emittance measurements were made between 200 and 350 K. Polished aluminum, used here as a standard, was found to have a total hemispherical emittance of 0.06, as expected. A velvet black paint, also used here as a standard, was found to have an emittance of 0.94 at room temperature. Other surfaces of interest included a polyurethane-based black paint designated Z-306, a highly polished 316L stainless steel, and an atomic oxygen beam-textured carbon-carbon composite.

Jaworske, Donald A.↗

Measuring Thicknesses With In Situ Ultrasonic Transducers

Several pulsed ultrasonic transducers attached to workpiece for measurement of changes in thicknesses of workpiece at transducer locations during grinding and polishing, according to proposal. Once attached, each transducer remains attached at original position until all grinding and polishing operations complete. In typical application, workpiece glass or ceramic blank destined to become component of optical system.

Dunn, Daniel E.↗

Measurements of Total Hemispherical Emissivity of Several Stably Oxidized Nickel-Titanium Carbide Cemented Hard Metals from 600 F to 1,600 F

The total hemispherical emissivity of several nickel-titanium carbide cemented hard metals have been measured over a temperature range from 600 F to l,600 F. A variety of cemented hard metals were obtained from the Kennametal Corporation. A brief discussion of the apparatus employed and the procedures used for this investigation is included. The results of the tests of specimens in the as-received and polished states indicate a nearly constant emissivity for each material tested over the temperature range considered and only slight differences in emissivity values for the different materials. Values obtained on the stably oxidized specimens range from 0.90 to 0.94 at 6000 F and o.88 to 0.92 at 1,600 F for the as-received specimens and from 0.82 to 0.89 at 600 F and 0.85 to 0.87 at 1,600 F for the polished specimens. The surface analysis of the oxidized materials as obtained by X-ray diffraction methods and metallographic techniques are presented as an aid to reproducing the surface on which these measurements were made.

Wade, William R.↗

Experimental Investigation of the Heat-Transfer Rate to a Series of 20 deg Cones of Various Surface Finishes at a Mach Number of 4.95

The heat-transfer rates were measured on a series of cones of various surface finishes at a Mach number of 4.95 and Reynolds numbers per foot varying from 20 x 10(exp 6) to 100 x 10(exp 6). The range of surface finish was from a very smooth polish to smooth machining with no polish (65 micro inches rms). Some laminar boundary-layer data were obtained, since transition was not artificially tripped. Emphasis, however, is centered on the turbulent boundary layer. The results indicated that the turbulent heat-transfer rate for the highest roughness tested was only slightly greater than that for the smoothest surface. The laminar-sublayer thickness was calculated to be about half the roughness height for the roughest model at the highest value of unit Reynolds number tested.

Jones, Jim J.↗

Preston Probe Calibrations at High Reynolds Number

The overall goal of the research effort is to study the performance of two Preston probes designed by NASA Langley Research Center across an unprecedented range of Reynolds number (based on friction velocity and probe diameter), and perform an accurate calibration over the same Reynolds number range. Using the Superpipe facility in Princeton, two rounds of experiments were performed. In each round of experiments for each Reynolds number, the pressure gradient, static pressure from the Preston probes and the total pressure from the Preston probes were measured. In the first round, 3 Preston probes having outer diameters of 0.058 inches, 0.083 inches and 0.203 inches were tested over a large range of pipe Reynolds numbers. Two data reduction methods were employed: first, the static pressure measured on the Preston probe was used to calculate P (modified Preston probe configuration), and secondly, the static pressure measured at the reference pressure tap was used to calculate P (un-modified Preston probe configuration). For both methods, the static pressure was adjusted to correspond with the static pressure at the Preston probe tip using the pressure gradient. The measurements for Preston probes with diameters of 0.058 inches, and 0.083 inches respectively were performed in the test pipe before it was polished a second time. Therefore, the measurements at high pipe Reynolds numbers may have been affected by roughness. In the second round of experiments the 0.058 inches and 0.083 inches diameter, un-modified probes were tested after the pipe was polished and prepared to ensure that the surface was smooth. The average velocity was estimated by assuming that the connection between the centerline velocity and the average velocity was known, and by using a Pitot tube to measure the centerline velocity. A preliminary error estimate suggests that it is possible to introduce a 1% to 2% error in estimating the average velocity using this approach. The evidence on the errors attending the second data set is somewhat circumstantial, and the measurements have not been repeated using a better approach, it seems probable that the correlation given applies to un-modified Preston probes over the range 6.4 less than x* less than 11.3.

Smits, Alexander J.↗

Characterization of ZnSe Single Crystals Grown by Physical Vapor Transport

ZnSe bulk crystals were grown by self-seeded physical vapor transport technique in horizontal and vertical configurations. The impurities and defects in the grown crystals were studied by glow discharge mass spectroscopy (GDMS) and low temperature photoluminescence (PL) measurements. The PL results on the starting material and the grown crystals are consistent with the low impurity levels measured by GDMS. The crystalline quality of the grown crystals were examined by synchrotron white beam X-ray topography (SWBXT) and high resolution triple X-ray diffraction (HRTXD). The SWBXT shows that, aside from twins, the overall crystalline quality of the vapor grown ZnSe crystals, especially in the contactless grown region, was quite high. The HRTXD results are in line with the SWBXT findings. The comparison between the HRTXD on a chemical-mechanically polished and a cleaved surface seems to indicate that polishing damage can obscure the true microstructure in the as-grown ZnSe crystals.

Su, Ching-Hua↗

The Mars Environmental Compatibility Assessment MECA Abrasion Tool

The Mars Environmental Compatibility Assessment (MECA) experiment, an instrument suite to be flown on Mars Surveyor 2001, will include a tool for doing simple mineralogical scratch and streak tests on particles from the Martian regolith. The Abrasion Tool will be applied to particles that adhere to highly polished substrates of various hardnesses. Granular soil components will be subjected to a compressive force of about 3 N using a leaf spring. The spring will be applied with a paraffin actuator capable of a 0.76 mm throw to achieve a maximum displacement of about 7.5 mm at the tip of the tool. The pressure per grain will be dependent on the grain size, the number of grains that adhere to the substrate and the number of grains in compression. The pressure per particle is expected to be on the order of 100 MPa - 1 GPa. The MECA sample wheel containing the substrates will be rotated after the particles are placed in compression to produce scratches or pits. A primary goal of the Abrasion Tool is to identify quartz (Mohs' hardness = 7) using substrates of varying hardnesses. Quartz is considered hazardous to future human explorers of Mars because it can cause silicosis of the lungs if it is of respirable size. It is also hazardous to machinery, structures, and space suits because of its ability to abrade and scratch surfaces. Since large quantities of minerals harder than quartz are not expected, any scratches produced on polished quartz substrates might be reasonably attributed to quartz particles, although there may be minerals such as impact metamorphic diamond in the soils. Careful calibration of the tool will be necessary to ensure that grains are not overloaded; for example, a steel ball pressed into glass will produce a Hertzian fracture, even though it is softer than glass. Other minerals, such as magnetite (Mohs'hardness = 6.5) have been shown to scratch glass ceramics such as Zerodur (Mohs' hardness = 6.5). Thus, minerals can be differentiated: note that regardless of the mineral species, if any particle is harder than 6.5 it will certainly be an interesting discovery for both planetary geology and human exploration concerns. The scratches will be identified using the 6X optical microscope and profiled with the atomic force microscope included in the MECA instrument suite. Analysis of the scratch morphology will yield evidence concerning the shape of the particle responsible for producing each scratch. For example, angular grains should leave vertical cracks with microconchoidal lateral chipping, while rounded grains might leave chattermarks, or nested partial Hertzian cracks. Particle shape can thus be inferred from these indentation modes, as well as material hardness. In addition, particle size information may also be available if pits caused by rolling particles can be identified. Converse to scratching, the minerals may be crushed at their contact points, and be smeared onto the target substrates to leave what geologists refer to as "streaks". These are coldwelded trails of mineral material that have structure and color indicative of mineral composition. The AFM will determine the morphology of these streaks, while the microscope will ascertain the color. On the harder substrates, we might expect streaking to dominate; on the softer substrates, scratching may dominate. Progressions of material interactions across the substrate selection will be a valuable source of data for mineral discrimination. It should also be noted that many minerals have coatings (such as iron oxides), and these will have to be differentiated from the host mineral grains; laboratory tests will establish the effects of such coatings on the scratch results. Finally, we note that the microscope will provide corroborative data regarding likely mineral species by grain shapes, fracture patterns, surface textures, colr, and UV fluorescence reactions.

Kuhlman, K. R.↗