Oxygen migration in TiO{sub 2}-based higher-k gate stacks
We report on the stability of high-permittivity (high-k) TiO{sub 2} films incorporated in metal-oxide-silicon capacitor structures with a TiN metal gate electrode, focusing on oxygen migration. Titanium oxide films are deposited by either Ti sputtering [physical vapor deposition (PVD)] followed by radical shower oxidation or by plasma-enhanced atomic layer deposition (PEALD) from titanium isopropoxide (Ti{l_brace}OCH(CH{sub 3}){sub 2{r_brace}4}) and O{sub 2} plasma. Both PVD and PEALD films result in near-stoichiometric TiO{sub 2} prior to high-temperature annealing. We find that dopant activation anneals of TiO{sub 2}-containing gate stacks at 1000 deg. C cause 5 A or more of additional SiO{sub 2} to be formed at the gate-dielectric/Si-channel interface. Furthermore, we demonstrate for the first time that oxygen released from TiO{sub 2} diffuses through the TiN gate electrode and oxidizes the poly-Si contact. The thickness of this upper SiO{sub 2} layer continues to increase with increasing TiO{sub 2} thickness, while the thickness of the regrown SiO{sub 2} at the gate-dielectric/Si interface saturates. The upper SiO{sub 2} layer degrades gate stack capacitance, and simultaneously the oxygen-deficient TiO{sub x} becomes a poor insulator. In an attempt to mitigate O loss from the TiO{sub 2}, top and bottom Al{sub 2}O{sub 3} layers are added to the TiO{sub 2} gate dielectric as oxygen barriers. However, they are found to be ineffective, due to Al{sub 2}O{sub 3}-TiO{sub 2} interdiffusion during activation annealing. Bottom HfO{sub 2}/Si{sub 3}N{sub 4} interlayers are found to serve as more effective oxygen barriers, reducing, though not preventing, oxygen downdiffusion.