Interface-correlated bonding properties for a roll-bonded Ti/Al 2-ply sheet
Highlights: • The feasible post roll-bonding annealing condition of Ti/Al clad was deduced. • The optimum thickness of the TiAl{sub 3} IMC diffusive layer is about 200 nm. • A ‘zipper-like’ failure mode at the interface yields the maximum bonding strength. - Abstract: We investigated the influence of annealing conditions on the interface-correlated microstructural evolution and subsequent bonding properties of a warm roll-bonded Ti/Al clad sheet. A TiAl{sub 3} intermetallic compound layer with a thickness of 160 nm was initially generated at the joint interface between the Ti and Al alloys by warm rolling. When the annealing time and temperature were increased to a maximum of 6 h and 650 °C, respectively, the thickness of the TiAl{sub 3} layer increased to 320 nm. The feasible annealing conditions for the optimum bonding strength were within 550 °C-6 h and 600 °C-3 h. An improvement in the bonding strength between Ti and Al is strongly correlated with the generation of considerable metallurgical bonding. This is manifested in the zipper-like failure mode that occurs at the TiAl{sub 3} joint interface for a layer thickness of less than 300 nm.