Vapor-phase synthesis of a solid precursor for {alpha}-alumina through a catalytic decomposition of aluminum triisopropoxide
Highlights: Black-Right-Pointing-Pointer A new solid precursor for {alpha}-alumina was prepared at about 200 Degree-Sign C from aluminum tri-isopropoxide vapor. Black-Right-Pointing-Pointer The obtained precursor was calcined at 1200 Degree-Sign C to form {alpha}-alumina particles, 75 nm in surface area equivalent diameter. Black-Right-Pointing-Pointer The weight loss of the precursor upon calcination was 24%, lower than that of Al(OH){sub 3}, a conventional alumina precursor. -- Abstract: A new solid precursor, hydrous aluminum oxide, for {alpha}-alumina nanoparticles was prepared by thermal decomposition of aluminum triisopropoxide (ATI) vapor in a 500 mL batch reactor at 170-250 Degree-Sign C with HCl as catalyst. The conversion of ATI increased with increasing temperature and catalyst content; it was nearly complete at 250 Degree-Sign C with the catalyst at 10 mol% of the ATI. The obtained precursor particles were amorphous, spherical and loosely agglomerated. The primary particle size is in the range 50-150 nm. The ignition loss of the precursor was 24%, considerably lower than 35% of Al(OH){sub 3}, the popular precursor for alumina particles. Upon calcination of the precursor at 1200 Degree-Sign C in the air with a heating rate of 10 Degree-Sign C/min and a holding time of 2 h, the phase was completely transformed into {alpha}. The spherical particles composing the precursor turned worm-like by the calcination probably due to sintering between neighboring particles. The surface area equivalent diameter of the resulting {alpha}-alumina was 75 nm.