Search NASA⌕ Search

SEARCH · Search NASA

Results for “Wire”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 307 records · Page 17

High-speed imaging of transition from fluid breakup to phase explosion in electric explosion of tungsten wires in air

High-speed visible imaging of sub-microsecond electric explosion of wires at the low specific energy deposition threshold reveals three distinct modes of wire failure as capacitor charge voltage and energy deposition are increased. For 100 micron diameter gold-plated tungsten wires of 2 cm length, deposited energies of 1.9 eV/atom produces a liquid column that undergoes hydrodynamic breakup into droplets with radii of order of wire diameter on timescales of 200 μs. Instability growth, column breakup, and droplet coalescence follow classic Rayleigh-Plateau predictions for instability of viscous fluid column. Above 3.2 eV/atom of deposited energy, wires are seen to abruptly transition to an expanding mixture of micron scale liquid-droplets and vapor within one frame (less than 3.33 μs), which has been termed ‘phase explosion’ in literature. Between these two limits, at 2.5 eV/atom of deposited energy, wire radius is unchanged for the first 10 μs before the onset of a rapid expansion and disintegration that resembles homogenous nucleation of mechanically unstable bubbles. Here, thermodynamic calculations are presented that separate cases by temperature obtained during heating: below boiling point, near boiling point, and exceeding boiling point.

42 ENGINEERING↗

Influence of Ti and Ta doping on the irreversible strain limit of ternary Nb3Sn superconducting wires made by the restacked-rod process

Nb{sub 3}Sn superconducting wires made by the restacked-rod process (RRP{reg_sign}) were found to have a dramatically improved resilience to axial tensile strain when alloyed with Ti as compared to Ta. Whereas Ta-alloyed Nb{sub 3}Sn in RRP wires showed permanent damage to its current-carrying capacity (I{sub c}) when tensioned beyond an intrinsic strain as small as 0.04%, Ti-doped Nb{sub 3}Sn in RRP strands exhibits a remarkable reversibility up to a tensile strain of about 0.25%, conceivably making Ti-doped RRP wires more suitable for the high field magnets used in particle accelerators and nuclear magnetic resonance applications where mechanical forces are intense. A strain cycling experiment at room temperature caused a significant drop of I{sub c} in Ta-alloyed wires, but induced an increase of I{sub c} in the case of Ti-doped strands. Whereas either Ti or Ta doping yield a similar enhancement of the upper critical field of Nb{sub 3}Sn, the much improved mechanical behavior of Ti-alloyed wires possibly makes Ti a better choice over Ta, at least for the RRP wire processing technique.

43 PARTICLE ACCELERATORS↗

Morphological evolution of InAs/InP quantum wires through aberration-corrected scanning transmission electron microscopy

Evolution of the size, shape and composition of self-assembled InAs/InP quantum wires through the Stranski Krastanov transition has been determined by aberration-corrected Z -contrast imaging. High resolution compositional maps of the wires in the initial, intermediate and final formation stages are presented. (001) is the main facet at their very initial stage of formation, which is gradually reduced in favour of {114} or {118}, ending with the formation of mature quantum wires with {114} facets. Significant changes in wire dimensions are measured when varying slightly the amount of InAs deposited. These results are used as input parameters to build three-dimensional models that allow calculation of the strain energy during the quantum wire formation process. The observed morphological evolution is explained in terms of the calculated elastic energy changes at the growth front. Regions of the wetting layer close to the nanostructure perimeters have higher strain energy, causing migration of As atoms towards the quantum wire terraces, where the structure is partially relaxed; the thickness of the wetting layer is reduced in these zones and the island height increases until the (001) facet is removed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study of the implosion characteristics of quasi-spherical wire arrays on the Angara-5-1 facility at currents of up to 4 MA

Results are presented from experimental studies of the spatial distribution of the density of matter in the central part of the discharge gap and the formation of the temporal profile of the X-ray power in the course of implosion of quasi-spherical wire arrays at discharge currents of up to 4 MA. The spatial distribution of the X-ray intensity in the central part of the discharge gap and the temporal profile of the X-ray power are used as implosion characteristics of quasi-spherical wire arrays. The quasi-spherical arrays were formed by the radial stretching of unstrained wires of initially cylindrical and conical wire arrays under the action of the electrostatic field. The temporal profile of the output X-ray pulse in the photon energy range of 0.1-1 keV is shown to depend on both the geometrical parameters of the quasi-spherical array and the longitudinal distribution of its mass. It is found that a 40% increase in the wire mass due to deposition of an additional mass in the equatorial region of a quasi-spherical array leads to a 15% increase in the average current radius of the pinch and a 30% decrease in the X-ray yield. Experiments with quasi-spherical arrays made of kapron fibers with deposited Al and Bi conducting layers were also carried out. It is demonstrated that application of such arrays makes it possible to control the profile and duration of the generated X-ray pulse by varying the mass, material, and location of the deposited layer. It is found that deposition of an additional mass in the form of a thin Bi stripe on tungsten wires near the cathode end of the array allows one to mitigate the influence of the cathode zipper effect on the pinch compression and formation of the X-ray pulse in tungsten arrays.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Initial Temperature Testing of Advanced Manufactured Melt Wire Package

As a part of the In-Pile Instrumentation Program, The Idaho National Laboratory (INL) has recently established in-house capabilities to fabricate and test new advanced manufactured sensors for measuring the peak irradiation temperature inside a nuclear test reactor. Although nuclear test reactors can use standard methods of real-time temperature monitoring, such as thermocouples, the complexity of feedthroughs and attachment complications to collect real-time measurements greatly increases the cost of the experiment. Passive monitoring techniques may be utilized that exploit the melting point of well characterized material (standard melt wires), however, the limited space available for instrumentation during experiments is also a challenge. To accommodate the challenge, INL has expanded its temperature detection instrumentation capabilities paired with the advancement of in-house advanced manufacturing options to include printed melt wires for peak irradiation temperature measurement. The advanced manufactured melt wire package can determine peak temperatures in experiments that can fit the challenging space available during irradiation. Recent results and knowledge from this ongoing work have made it possible to develop unique temperature sensors that can accomplish user specific temperature ranges inside the harsh environments experienced during radiation testing. This report summarizes the initial temperature testing using fabricated melt wires with two different melting temperatures, silver (melting temperature of ~960 °C) and solder (melting temperature of ~160 °C), that were initially tested for their relative melting points using non-standard method of furnace and hot plate testing under normal air conditions. Future work will include more controlled way of testing printed melt wires under inert gas with multiple temperature measurements followed by comparison of standard melt wire package performance for baseline characterization.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Additive manufacturing enabled hot-wire apparatus with suppressed edge effect error

This invention describes a method of structuring a metal or metal coated wire in a manner such that it provides enhanced accuracy when used in a hot-wire apparatus for transient thermal conductivity measurements for low-density materials. This is accomplished by using a diameter varying structure with two ends of the wire of sufficiently small diameter that the edge-effect induced error can be reduced by generating a more uniform temperature profile along the wire, whereas in conventional apparatus the temperatures always drop at the ends of a finite wire due to its ends that are being cooled by the wire-supports.

36 MATERIALS SCIENCE↗

Commissioning a Vibrating Wire System for Quadrupole Fiducialization

Quadrupoles will be placed between the undulator segments in LCLS to keep the electron beam focused as it passes through. The quadrupoles will be assembled with their respective undulator segments prior to being placed into the tunnel. Beam alignment will be used to center the quadrupoles, along with the corresponding undulators, on the beam. If there is any displacement between the undulator and the quadrupole axes in the assemblies, the beam will deviate from the undulator axis. If it deviates by more than 80{micro}m in vertical or 140{micro}m in horizontal directions, the undulator will not perform as required by LCLS. This error is divided between three sources: undulator axis fiducialization, quadrupole magnetic axis fiducialization, and assembly of the two parts. In particular, it was calculated that the quadrupole needs to be fiducialized to within 25{micro}m in both vertical and horizontal directions. A previous study suggested using a vibrating wire system for finding the magnetic axis of the quadrupoles. The study showed that the method has high sensitivity (up to 1{micro}m) and laid out guidelines for constructing such a system. There are 3 steps in fiducializing the quadrupole with the vibrating wire system. They are positioning the wire at the magnet center (step 1), finding the wire with position detectors (step 2), and finding the quadrupole tooling ball positions relative to the position detector tooling balls (step 3). A previous study investigated the error associated with each step by using a permanent quadrupole magnet on an optical mover system. The study reported an error of 11{micro}m for step 1 and a repeatability of 4{micro}m for step 2. However, the set up used a FARO arm to measure tooling balls and didn't allow to accurately check step 2 for errors; an uncertainty of 100{micro}m was reported. Therefore, even though the repeatability was good, there was no way to check that the error in step 2 was small. Following the recommendations of that study, we used a CMM (Coordinate Measuring Machine) instead of the FARO arm for measuring the tooling balls. In addition, a roller cam positioner system replaced the optical movers for moving the quadrupole. With the exception of the quadrupole itself, the system was identical to what will be used in fiducializing the undulator quadrupoles. In this study, we investigate the new vibrating wire set up, including the error associated with each step of fiducialization. A vibrating wire system was constructed to fiducialize the quadrupoles between undulator segments in the LCLS. This note is a continuation of previous work to study the ability of the system to fulfill the fiducialization requirements.

43 PARTICLE ACCELERATORS↗

Surface characteristics and damage distributions of diamond wire sawn wafers for silicon solar cells

This paper describes surface characteristics, in terms of its morphology, roughness and near-surface damage of Si wafers cut by diamond wire sawing (DWS) of Si ingots under different cutting conditions. Diamond wire sawn Si wafers exhibit nearly-periodic surface features of different spatial wavelengths, which correspond to kinematics of various movements during wafering, such as ingot feed, wire reciprocation, and wire snap. The surface damage occurs in the form of frozen-in dislocations, phase changes, and microcracks. The in-depth damage was determined by conventional methods such as TEM, SEM and angle-polishing/defect-etching. However, because these methods only provide local information, we have also applied a new technique that determines average damage depth over a large area. This technique uses sequential measurement of the minority carrier lifetime after etching thin layers from the surfaces. The lateral spatial damage variations, which seem to be mainly related to wire reciprocation process, were observed by photoluminescence and minority carrier lifetime mapping. Our results show a strong correlation of damage depth on the diamond grit size and wire usage.

14 SOLAR ENERGY↗

Staphylococcus-Infected Tunneled Dialysis Catheters: Is Over-the-Wire Exchange an Appropriate Management Option?

Purpose: Over-the-wire exchange of tunneled dialysis catheters is the standard of care per K/DOQI guidelines for treating catheter-related bacteremia. However, Gram-positive bacteremia, specifically with staphylococcus species, may compromise over-the-wire exchange due to certain biological properties. This study addressed the effectiveness of over-the-wire exchange of staphylococcus-infected tunneled dialysis catheters compared with non-staphylococcus-infected tunneled dialysis catheters. Methods: Patients who received over-the-wire exchange of their tunneled dialysis catheter due to documented or suspected bacteremia were identified from a QA database. Study patients (n = 61) had positive cultures for Staphylococcus aureus, Staphylococcus epidermidis, or coagulase-negative staphylococcus not otherwise specified. Control patients (n = 35) received over-the-wire exchange of their tunneled dialysis catheter due to infection with any organism besides staphylococcus. Overall catheter survival and catheter survival among staphylococcal species were assessed. Results: There was no difference in tunneled dialysis catheter survival between study and control groups (P = 0.46). Median survival time was 96 days for study catheters and 51 days for controls; survival curves were closely superimposed. There also was no difference among the three staphylococcal groups in terms of catheter survival (P = 0.31). The median time until catheter removal was 143 days for SE, 67 days for CNS, and 88 days for SA-infected catheters. Conclusions: There is no significant difference in tunneled dialysis catheter survival between over-the-wire exchange of staphylococcus-infected tunneled dialysis catheters and those infected with other organisms.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

Transfissural Route Used for Preoperative Localization of Small Pulmonary Lesions with a Short Hook Wire and Suture System

PurposeWe retrospectively evaluated the results of the transfissural route for preoperative localization with a short hook wire and suture system for video-assisted thoracoscopic surgery (VATS).MethodsEleven patients with 11 tumors underwent CT-guided transfissural placement of a hook wire before VATS. This route was selected for all patients, because the distance between the tumor and interlobar fissure was much shorter than the required distance traversed using the conventional approach. Complications were evaluated using the National Cancer Institute Common Terminology Criteria for Adverse Events Version 4.0.ResultsThe hook wire was successfully placed using the transfissural route in all but one case. Of these ten successful placements, two tumors needed a second puncture for optimal placement, because the CT scan showed that the first hook wire was not properly placed in the lung. In one patient, we did not attempt replacement after the first placement was incorrect. In ten successful procedures, the mean distance traversed in the parenchyma of the unaffected lung lobe was 27.9 mm. The distance between the pleura and placed hook wire was significantly shorter than the estimated distance between the pleura and hook wire using the conventional route (mean 16.3 vs. 40.9 mm; P = 0.0002). Grade 1 adverse events occurred (11 pneumothoraxes and 4 pulmonary hemorrhages). No grade 2 or higher adverse event was observed.ConclusionsThe transfissural route used for preoperative localization before VATS is useful for selected patients because this route may allow for more limited lung parenchyma resection.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

Charge Transport through Organic Molecular Wires Embedded in Ultrathin Insulating Inorganic Layer

Dense phase silica layers with thickness of a few nanometers featuring embedded organic molecular wires of type p-oligo(phenylenevinylene) are shown by visible light sensitized electrochemical measurements to transport charges across the insulating membrane. Here, we find that such hybrid materials combination allows electronic charge transport only through the wires, while blocking molecular transport. Embodiment of the wire molecules in the silica was accomplished by atomic layer deposition under mild temperature conditions. Grown on Co oxide films for water oxidation, with the wire molecules covalently anchored on the oxide surface, the layer functions as a proton conducting separation membrane. Characterization by XPS, FT-IR and STEM/EDX confirms the integrity of the silica-encapsulated organic wires. Cyclic voltammetry with redox couple of selected potential relative to the energy levels of the wire molecules shows that the membrane is free of pinholes. The new type of membrane allows separation of incompatible redox reaction environments on the length scale of nanometers while enabling controlled electron transport between them. Finally, this opens up the coupling of carbon dioxide reduction with water oxidation, the essential reactions of artificial photosynthesis, in an integrated nanoscale photosystem.

36 MATERIALS SCIENCE↗

Magnetic control over the fundamental structure of atomic wires

When reducing the size of materials towards the nanoscale, magnetic properties can emerge due to structural variations. Here, we show the reverse effect, where the structure of nanomaterials is controlled by magnetic manipulations. Using the break-junction technique, we find that the interatomic distance in platinum atomic wires is shorter or longer by up to ~20%, when a magnetic field is applied parallel or perpendicular to the wires during their formation, respectively. The magnetic field direction also affects the wire length, where longer (shorter) wires are formed under a parallel (perpendicular) field. Our experimental analysis, supported by calculations, indicates that the direction of the applied magnetic field promotes the formation of suspended atomic wires with a specific magnetization orientation associated with typical orbital characteristics, interatomic distance, and stability. A similar effect is found for various metal and metal-oxide atomic wires, demonstrating that magnetic fields can control the atomistic structure of different nanomaterials when applied during their formation stage.

36 MATERIALS SCIENCE↗

Addressing the efficiency of the energy transfer to the water flow by underwater electrical wire explosion

Experimental and hydrodynamic simulation results of submicrosecond time scale underwater electrical explosions of planar Cu and Al wire arrays are presented. A pulsed low-inductance generator having a current amplitude of up to 380 kA was used. The maximum current rise rate and maximum power achieved during wire array explosions were dI/dt<=830 A/ns and approx10 GW, respectively. Interaction of the water flow generated during wire array explosion with the target was used to estimate the efficiency of the transfer of the energy initially stored in the generator energy to the water flow. It was shown that efficiency is in the range of 18%-24%. In addition, it was revealed that electrical explosion of the Al wire array allows almost double the energy to be transferred to the water flow due to efficient combustion of the Al wires. The latter allows one to expect a significant increase in the pressure at the front of converging strong shock waves in the case of cylindrical Al wire array underwater explosion.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Self-assembly of tin wires via phase transformation of heteroepitaxial germanium-tin on germanium substrate

This work demonstrates and describes for the first time an unusual strain-relaxation mechanism by the formation and self-assembly of well-ordered tin wires during the thermal annealing of epitaxial Ge{sub 0.83}Sn{sub 0.17}-on-Ge(001) substrate. Fully strained germanium-tin alloys (Ge{sub 0.83}Sn{sub 0.17}) were epitaxially grown on Ge(001) substrate by molecular beam epitaxy. The morphological and compositional evolution of Ge{sub 0.83}Sn{sub 0.17} during thermal annealing is studied by atomic force microscopy, X-ray diffraction, transmission electron microscopy. Under certain annealing conditions, the Ge{sub 0.83}Sn{sub 0.17} layer decomposes into two stable phases, and well-defined Sn wires that are preferentially oriented along two orthogonal 〈100〉 azimuths are formed. The formation of the Sn wires is related to the annealing temperature and the Ge{sub 0.83}Sn{sub 0.17} thickness, and can be explained by the nucleation of a grain with Sn islands on the outer front, followed by grain boundary migration. The Sn wire formation process is found to be thermally activated, and an activation enthalpy (E{sub c}) of 0.41 eV is extracted. This thermally activated phase transformation, i.e., 2D epitaxial layer to 3D wires, occurs via a mechanism akin to “cellular precipitation.” This synthesis route of Sn wires opens new possibilities for creation of nanoscale patterns at high-throughput without the need for lithography.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Variation of effective filament diameter, irreversibility field, anisotropy, and pinning efficiency in Bi-2212 round wires

Abstract In recent years Bi 2 Sr 2 CaCu 2 O x (Bi-2212) received increasing attention due to its round wire multifilamentary architecture, a unique feature in high- T c superconductor. In fact, round wires are preferable for magnet designs, including solenoids for nuclear magnetic resonance (NMR) or research purpose and accelerator magnets. However, due to the narrow over-pressure heat treatment conditions necessary to obtain high J c and to the peculiar microstructure of Bi-2212 wires, a full understanding of the correlations between the different properties has not yet been developed. In this paper we investigate the effect of a vital part of Bi-2212 optimization, the maximum heat-treatment temperature T max in the range of 885 °C–896 °C, on the variations of J c , effective filament diameter d eff , anisotropy γ , INTER- and intra-grain irreversibility fields and pinning energies U 0 , all critical parameters in unravelling the complex mix of vortex pinning and connectivity that ultimately determines the critical current density. We found that d eff of the higher J c wires heat-treated at lower temperature is much smaller than for the lower J c wires. Moreover, a systematic increase of the irreversibility field and a decrease of the intrinsic Bi-2212 anisotropy underpins the higher J c . The analysis of the pinning energies reveals that there is little sample-to-sample variation in the INTER-grain pinning, whereas in all samples the intra-grain pinning has an enhancement below ∼40–45 K becoming more and more evident with increasing J c . These results suggest that the overall J c performance are not only related to the wire microstructure and connectivity, which obviously affect the INTER-grain properties, but they are also intimately related to the intrinsic and intra-grain properties such as γ and U 0 .

Physics↗

Optical Absorption Spectroscopy Probes Water Wire and Its Ordering in a Hydrogen-Bond Network

Water wires, quasi-one-dimensional chains composed of hydrogen-bonded (H-bonded) water molecules, play a fundamental role in numerous chemical, physical, and physiological processes. Yet direct experimental detection of water wires has been elusive so far. Based on advanced many-body theory that includes electron-hole interactions, we report that optical absorption spectroscopy can serve as a sensitive probe of water wires and their ordering. In both liquid and solid water, the main peak of the spectrum is discovered to be a charge-transfer exciton. In water, the charge-transfer exciton is strongly coupled to the H-bonding environment where the exciton is excited between H-bonded water molecules with a large spectral intensity. In regular ice, the spectral weight of the charge-transfer exciton is enhanced by a collective excitation occurring on proton-ordered water wires, whose spectral intensity scales with the ordering length of water wire. The spectral intensity and excitonic interaction strength reaches its maximum in ice XI, where the long-range ordering length yields the most pronounced spectral signal. Our findings suggest that water wires, which widely exist in important physiological and biological systems and other phases of ice, can be directly probed by this approach. Published by the American Physical Society 2025

Tang, Fujie (ORCID:0000000197615359)↗

Critical Current Distributions of Recent Bi-2212 Round Wires

Bi 2 Sr 2 CaCu 2 O 8+x (Bi-2212) is the only high-field, high-temperature superconductor (HTS) capable of reaching a critical current density J c (16 T, 4.2 K) of 6500 A·mm –2 in the highly desirable round wire (RW) form. However, state-of-the-art Bi-2212 conductors still have a critical current density (J c ) to depairing current density (J d ) ratio around 20 to 30 times lower than that of state-of-the-art Nb–Ti or REBCO. Previously, we have shown that recent improvements in Bi-2212 RW J c are due to improved connectivity associated with optimization of the heat treatment process, and most recently due to a transition to a finer and more uniform powder manufactured by Engi-Mat. One quantitative measure of connectivity may be the critical current (I c ) distribution, since the local I c in a wire can vary along the length due to variable vortex-microstructure interactions and to factors such as filament shape variations, grain-to-grain connectivity variations and blocking secondary phase distributions. Modeling the experimental V-I transition measured on a low resistance shunt as a complex sum of voltage contributions of individual filament and wire sub-sections allows a numerical extraction of the I c distribution from the d 2 V/dI 2 treatment of the V-I curves. Here we compare ~0.1 m length I c distributions of Bi-2212 RWs with recent state-of-the-art very high-J c Engi-Mat powder and lower J c and older Nexans granulate powder. We do find that the I c spread for Bi-2212 wires is about twice the relative standard of high-J c Nb–Ti well below H irr . We do not yet see any obvious contribution of the Bi-2212 anisotropy to the I c distribution and are rather encouraged that these Bi-2212 round wires show relative I c distributions not too far from high-J c Nb–Ti wires.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Increase in the energy density of the pinch plasma in 3D implosion of quasi-spherical wire arrays

Results are presented from experimental studies of the characteristics of the soft X-ray (SXR) source formed in the implosion of quasi-spherical arrays made of tungsten wires and metalized kapron fibers. The experiments were carried out at the Angara-5-1 facility at currents of up to 3 MA. Analysis of the spatial distribution of hard X-ray emission with photon energies above 20 keV in the pinch images taken during the implosion of quasi-spherical tungsten wire arrays (QTWAs) showed that a compact quasi-spherical plasma object symmetric with respect to the array axis formed in the central region of the array. Using a diffraction grazing incidence spectrograph, spectra of SXR emission with wavelengths of 20–400 Å from the central, axial, and peripheral regions of the emission source were measured with spatial resolutions along the array radius and height in the implosion of QTWAs. It is shown that the emission spectra of the SXR sources formed under the implosion of quasi-spherical and cylindrical tungsten wire arrays at currents of up to 3 MA have a maximum in the wavelength range of 50–150 Å. It is found that, during the implosion of a QTWA with a profiled linear mass, a redistribution of energy in the emission spectrum takes place, which indicates that, during 3D implosion, the energy of longitudinal motion of the array material additionally contributes to the radiation energy. It is also found that, at close masses of the arrays and close values of the current in the range of 2.4{sup −3} MA, the average energy density in the emission source formed during the implosion of a quasi-spherical wire array is larger by a factor of 7 than in the source formed during the implosion of a cylindrical wire array. The experimental data were compared with results of 3D simulations of plasma dynamics and radiation generation during the implosion of quasi-spherical wire arrays with a profiled mass by using the MARPLE-3D radiative magnetohydrodynamic code, developed at the Keldysh Institute of Applied Mathematics, Russian Academy of Sciences.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗